Braskem Lhb118 21af Blown Film Extrusion Linear Low Density Polyethylene

Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 309458
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 2.1 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction 0.15

    As an accredited Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: Braskem LHB118/21AF LLDPE in 25 kg moisture-resistant bags, 55 bags per pallet, shrink-wrapped for secure handling and storage.
    Container Loading (20′ FCL) 20′ FCL container loading of Braskem LHB118/21AF LLDPE blown film resin, typically palletized 25 kg bags, stowed for export transport.
    Shipping Braskem LHB118/21AF LLDPE resin ships as non-hazardous, free-flowing pellets in 25 kg moisture-barrier bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Store dry, cool, away from direct sunlight and heat. Handle with standard industrial practices; protect from moisture, contamination, and punctures. No special DOT/IMDG/IATA hazard classification required.
    Storage Store Braskem LHB118/21AF LLDPE resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers closed to prevent moisture and contamination. Avoid strong oxidizers. Use proper grounding to control static. Maintain clean, palletized stacks; rotate stock. Follow local regulations and SDS recommendations.
    Shelf Life Braskem LHB118/21AF: store sealed in original packaging, cool, dry, away from sunlight; shelf life 24 months under recommended conditions.
    Application of Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene

    Extrusion Melt Fracture Thresholds in Heavy-Duty Sack Liner Production

    Blown film extrusion of Braskem LHB118/21AF immediately encounters the melt fracture boundary inherent to butene-copolymer linear low density polyethylene. The narrow molecular weight distribution characteristic of this resin class concentrates shear stress at the die lip during high-output extrusion, producing sharkskin surface defects when wall shear stresses exceed a critical threshold of approximately 0.14 MPa at the die land. The AF suffix in the grade designation corresponds to a fluoropolymer-based processing aid package that migrates to the die lip surface during the first 15-30 minutes of extrusion, coating the metal surface with a slip layer that delays gross melt fracture onset. Die gap selection for this grade requires apertures of 2.0-2.5 mm, rather than the 0.5-1.0 mm routinely specified for tubular LDPE, to reduce shear rate at equivalent screw speeds. Grooved feed extruders with 30:1 length-to-diameter ratios dominate processing of this resin on production lines; 75 mm screw diameters paired with 300 mm annular dies deliver output rates of 220-300 kg/h at screw speeds of 80-110 rpm. Barrel temperature profiling typically follows a rising profile of 190 °C in the feed zone, 200 °C in the compression zone, 210 °C in the metering zone, and 220-230 °C at the adapter and die zones, stabilizing melt temperature at 215-225 °C. Operation above 240 °C accelerates antioxidant depletion and initiates gel formation in recycled trim re-feed streams, a failure mode observed on high-output lines where edge trim ratios exceed 15%. Bubble stability at blow-up ratios between 2.0:1 and 2.5:1 requires internal bubble cooling; high-stalk configurations with frost line heights of 4-6 die diameters improve dart impact retention at the expense of haze. Heavy-duty sack liners manufactured from this grade at 80-150 µm thickness serve packaging of mineral fillers, granular fertilizers, and polymer masterbatch compounds where filled sack weights exceed 25 kg. Mechanical qualification relies on ASTM D1709 Type A dart impact values of 85-110 g at 25 µm thickness and Elmendorf tear resistance measured per ASTM D1922, which typically falls within 150-200 g in the machine direction and 350-450 g in the cross direction for 0.918 g/cm³ butene LLDPE films. Seal integrity of heavy-duty sacks is validated through heat seal strength testing per ASTM F88, with jaw temperatures of 115-130 °C on continuous band sealers running at 12-20 m/min. Drop test performance for UN-certified dangerous goods packaging requires film thickness calculations that account for tear propagation energy absorption, a parameter that degrades when filler content in the polymer compound exceeds 3 wt% due to stress concentration at filler aggregates.

    Pallet unitization films manufactured from butene LLDPE of density 0.918 g/cm³ place simultaneous demands on elastic recovery, puncture resistance, and film-to-film slip in automated stretch hood equipment. The transverse orientation step inherent to stretch hood film production subjects the blown film web to elongation ratios of 1.5:1 to 2.0:1 at ambient temperature, requiring sufficient intrinsic tear resistance to survive orientation without micro-tear formation. LHB118/21AF processed through a three-layer coextrusion configuration with varying slip agent concentrations per layer produces films of 60-120 µm final thickness with differential coefficient of friction values on the inner and outer surfaces. The inner surface requires a coefficient of friction between 0.20 and 0.35 to permit slip during hood deployment, while the outer surface is formulated to 0.10-0.15 for pallet stacking with minimal abrasion. Antiblock additive particle size distribution in the 21AF package, typically synthetic amorphous silica with a median particle diameter of 2-4 µm, controls the optical and tribological balance. Puncture resistance measured per ASTM D5748 at 50 mm/min probe speed typically falls within 25-35 N for a 100 µm three-layer structure when the core layer contains at least 40% of the total film thickness. Elastic recovery after 100% elongation is measured per ISO 527-3, with butene-based LLDPE demonstrating permanent set values of 10-15%, a limitation versus metallocene-catalyzed grades that achieve 5-8% permanent set. This residual deformation manifests as hood loosening after prolonged warehouse storage, particularly in environments exceeding 35 °C where thermal relaxation accelerates. Processing on rotary arm stretch hood machines requires consistent film flatness, achieved through oscillating haul-off mechanisms calibrated to distribute gauge variation below ±5% across the web width. Published data for this specific grade in high-acceleration stretch hood applications at machine cycles exceeding 100 pallets per hour is limited; standard packaging machinery operating parameters are the only verifiable reference points.

    What Dart Impact Retention Is Observed in 25 µm Greenhouse Films After 18 Months of UV Exposure?

    Agricultural greenhouse and low-tunnel cladding represents a service environment where photodegradation kinetics, pesticide chemical attack, and thermal stress interact through mechanisms that cannot be simulated by single-factor accelerated aging. Unmodified LHB118/21AF blown film at 25 µm thickness retains less than 40% of its initial ASTM D1709 dart impact value after 12 months of continuous outdoor exposure in temperate latitudes, as carbonyl index measurements shift from initial values below 0.05 to values exceeding 0.3 absorbance units at 1715 cm⁻¹. This degradation pathway proceeds through Norrish Type I and Type II photochemical reactions initiated by UV-B radiation in the 290-320 nm wavelength band. HALS stabilization at addition levels of 0.30-0.50 wt% of a hindered amine light stabilizer such as bis(2,2,6,6-tetramethyl-4-piperidyl) sebacate extends useful service life to 24-36 months by radical scavenging mechanisms that retard polymer chain scission. Light transmission of greenhouse cladding films produced from this grade falls between 85% and 92% in the photosynthetically active radiation band of 400-700 nm when measured per ASTM D1003, a range that remains acceptable for most horticultural crops including Solanaceae and Cucurbitaceae. Haze values between 10% and 20% diffuse incident light, an advantage for greenhouse environments where direct radiation causes leaf scorch. Thermal retention performance depends on the 7-14 µm infrared transmission characteristic, which for LLDPE films is regulated by blending with mineral fillers such as calcined kaolin at 3-8 wt% to increase far-infrared opacity. Pesticide contact, particularly sulfur-based fungicides containing elemental sulfur, generates sulfuric acid species that catalyze hydrolysis of polymer chains and deactivate HALS stabilizers through acid-base neutralization. Coextruded structures employing an EVA outer layer over an LHB118/21AF core provide chemical resistance while preserving mechanical performance. Mulch film applications using 15-25 µm film thickness require carbon black loadings of 2-3 wt% for weed suppression, with the butene LLDPE matrix providing adequate puncture resistance for mechanical laying equipment operating at speeds up to 8 km/h.

    Blend Composition at 50 µm Film ThicknessMD Tensile at Break (MPa) per ASTM D882CD Elmendorf Tear (g) per ASTM D1922Dart Impact (g) per ASTM D1709 Type AHaze (%) per ASTM D1003
    100% LHB118/21AF35-42380-45090-1108-14
    70% LLDPE / 30% LDPE30-36300-38070-906-10
    50% LLDPE / 50% LDPE25-32220-30055-755-8
    30% LLDPE / 70% LDPE20-26150-22045-604-7
    100% Tubular LDPE (reference)16-2080-12035-504-6

    Compiled from multiple blown film grade technical datasheets for butene-copolymer LLDPE and tubular LDPE; published data for LHB118/21AF specifically across all blend ratios is limited.

    Food contact compliance for LHB118/21AF blown film applications falls within the regulatory positive lists for olefin polymers at densities from 0.85 to 1.00 g/cm³. FDA 21 CFR 177.1520(a)(3)(i) covers olefin polymers intended for food contact, with conditions of use determined by extraction testing under simulated solvents per 21 CFR 176.170 tables. The resin may be used for contact with aqueous, acidic, alcoholic, and fatty foods at temperatures up to 100 °C, subject to the limitations that the final film thickness does not exceed 0.13 mm for fatty food contact and that no hot-filled application exceeds 80 °C without withdrawal of specific migration data. Under EU Regulation (EU) No 10/2011 Annex I, the monomer 1-butene and polymer substrates derived exclusively from ethylene and butene are positively listed, with overall migration testing per EN 1186 yielding values below the 10 mg/dm² limit specified in Article 12. Specific migration testing for the antioxidant additives present in the 21AF package, typically tris(2,4-di-tert-butylphenyl) phosphite at 800-1500 ppm, is conducted per EN 13130 under food simulant A, B, and D2 conditions. Organoleptic inertness is validated through sensory panel testing per EN 1230 or equivalent national standards. The fluoropolymer processing aid added to suppress melt fracture is bound within the polymer matrix at typical use levels of 300-500 ppm and does not migrate at detectable limits. The slip agent erucamide, when present in formulations requiring reduced coefficient of friction, migrates to the film surface over 24-72 hours post-extrusion; its specific migration limit under EU 10/2011 is not formally listed, but compliance with the overall migration limit serves as the controlling regulatory boundary. Batch-to-batch traceability must comply with Commission Regulation (EC) No 2023/2006 on good manufacturing practice for food contact materials, including documented raw material lot linkage to finished film run codes. For microwave reheating contact, the film structure must not exceed 100 °C at the food interface and must not be exposed to microwave susceptor temperatures exceeding 160 °C.

    Regulation / StandardDesignation ReferenceCompliance RequirementBoundary Condition for LHB118/21AF
    FDA 21 CFR177.1520(a)(3)(i)Olefin polymer positive list for food contactDensity 0.918 g/cm³ within 0.85-1.00 g/cm³ range
    EU Regulation(EU) No 10/2011, Annex IAuthorized monomers incl. ethylene, 1-buteneOverall migration limit 10 mg/dm² per Article 12
    EU GMP(EC) No 2023/2006Quality assurance system, traceabilityRaw material lot to finished film run code linkage
    REACH(EC) No 1907/2006 Article 33SVHC communication dutyNo SVHC above 0.1 wt% declared in grade datasheet
    CONEG / TPCHModel Toxics in PackagingSum of Pb, Cd, Hg, Cr(VI) < 100 ppmPolymer matrix and additive system below threshold

    Collation Shrink Blends: The 70:30 LDPE Ceiling

    Collation shrink film for consumer multi-pack bottling applications blends LHB118/21AF with high-melt-strength tubular LDPE at a maximum 30 wt% LLDPE loading to preserve machine-direction shrink tension without weld seam failure. Published data for this specific configuration is limited; processor trials on twin-head blown film lines with 55 mm extruder diameters confirm orientation-induced shrinkage of 12-18% in the machine direction at a blow-up ratio of 2.2:1 and a melt temperature of 215 °C.

    Corona discharge surface activation of LHB118/21AF blown film achieves wetting tension values of 38-42 mN/m immediately post-treatment, sufficient for solventless polyurethane adhesive lamination to metallized PET and biaxially oriented polypropylene. Treatment decay proceeds logarithmically with time, requiring lamination within 72 hours of corona exposure under normal warehouse conditions of 23 °C and 50% relative humidity. Adhesive bond strength measured per ASTM F904 at 200 mm/min peel speed typically falls within 2.5-4.0 N/15 mm when lamination is executed within this window, but degrades below 1.5 N/15 mm when the dyne level falls below 36 mN/m. Ink adhesion on reverse-printed laminations requires a minimum surface energy of 40 mN/m for solvent-based flexographic printing with polyamide or nitrocellulose binder systems. For extrusion lamination with molten LDPE at 315-325 °C melt temperature, the LLDPE substrate must withstand thermal shrinkage below 1.5% in the machine direction when measured per ASTM D1204, otherwise tunnel defects form in the laminate structure. Gauge uniformity across the web, controlled to ±5%, governs bond consistency; gauge bands outside this tolerance create localized pressure variations in the lamination nip that result in optical defects detectable as haze streaks in metallized structures. The butene LLDPE substrate layer contributes stiffness and sealability to the final laminate, with seal initiation temperature measured per ASTM F88 at 105-110 °C and plateau seal strength of 8-12 N/15 mm at 115 °C jaw temperature. Substrate films of 30-40 µm nominal thickness are slit to width tolerances of ±0.5 mm; edge quality is assessed by physical inspection for stringing or tear initiation at the slit edge, defects that propagate during lamination unwind tension of 30-50 N per 100 cm web width.

    When Tie-Resin Compatibility Governs Delamination Resistance in Five-Layer Barrier Structures

    The five-layer coextrusion sequence PP//tie//EVOH//tie//LLDPE, or alternatively LLDPE//tie//PA//tie//LLDPE for puncture-critical applications, places specific demands on the LHB118/21AF layer that serves as both structural substrate and sealant layer. Interlayer adhesion measured per ASTM F904 requires bond strengths exceeding 3.0 N/15 mm between the tie resin and LLDPE layer; values below 2.0 N/15 mm in the sealant layer indicate incompatibility between the anhydride-modified tie resin and the processing aid carried by the LLDPE. The fluoropolymer processing aid present in LHB118/21AF can reduce surface energy at the coextrusion interface, potentially compromising interlayer adhesion if the tie resin is employed at insufficient thickness or if die residence time exceeds 90 seconds. Die zone temperature control within ±3 °C is essential for coextrusion because viscosity matching between the LLDPE melt at 220 °C and the EVOH or PA melt at 230-240 °C determines interfacial stability. Viscosity ratio at the interface must remain between 1:1 and 2:1; deviation beyond this range triggers interfacial instability that manifests as wavy delamination patterns in the finished film. For retort-adjacent applications where the LLDPE layer functions as the innermost sealant at thicknesses of 40-60 µm, the butene comonomer distribution governs seal integrity at temperatures up to 121 °C. Butene-based LLDPE sealant layers demonstrate seal strength retention of 85-90% after 30-minute exposure at 70 °C in steam, whereas octene-based LLDPE grades retain 95% or higher, a limitation that must be factored into specification decisions. Barrier film structures employing LHB118/21AF as the sealant layer are processed on 5-layer blown film lines with die diameters of 250-400 mm at output rates of 180-350 kg/h depending on layer ratio configuration. The seal initiation temperature of 105-110 °C measured per ASTM F88 permits high-speed form-fill-seal operation at 25-40 bags per minute without requiring excessive seal jaw dwell times. Delamination resistance under flex-crack testing, an established failure mode in distribution, is evaluated using Gelbo flex testing per ASTM F392, with acceptable performance defined as no visible delamination after 100 flex cycles at ambient temperature.

    Frozen-Food Packaging Film Tear Propagation at −25 °C

    Low-temperature impact toughness in frozen-food packaging manufactured from butene LLDPE blown film derives from the alpha-olefin short-chain branching distribution that reduces crystallinity and shifts the glass transition temperature to approximately −95 °C. Tear propagation resistance at −25 °C measured per ASTM D1922 decays 10-20% relative to ambient values, a reduction that remains acceptable for most frozen vegetable and prepared meal formats but requires structural reinforcement for sharp-edged product geometries such as frozen french fries or breaded cutlets. Films of 50-70 µm thickness processed from LHB118/21AF maintain sufficient cold-temperature dart impact per ASTM D1709 to pass distribution drop tests from 1.2 m height when the film temperature at impact does not fall below −30 °C. Below this threshold, brittle fracture occurs and published data for this specific grade in ultra-low-temperature storage applications below −40 °C is limited. Seal integrity of frozen-food pouches after thermal cycling between −25 °C and ambient temperature is evaluated through leak testing per ASTM F2096 with a pressure differential of 250 Pa; continuous seal runs achieved at 115-120 °C on horizontal form-fill-seal machines demonstrate no channel formation after ten freeze-thaw cycles. A critical operational boundary exists for packaging of frozen foods containing sharp crystalline ice structures: repeated impact during distribution at −40 °C reduces impact resistance by 30-40% relative to ambient values, requiring upthicknessing by 20-30% or migration to octene-based LLDPE grades with superior low-temperature performance. The addition of 10-15 wt% metallocene plastomer to the sealant layer formulation improves low-temperature seal reliability but modifies the coefficient of friction and increases blocking tendency, requiring compensatory increases in antiblock loading above 2,000 ppm synthetic silica.

    Free Quote

    Competitive Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene is a 1-butene-comonomer linear low density polyethylene grade formulated for tubular blown film processing. The grade designation carries three primary identifiers: the 118 field corresponds to a nominal density of 0.918 g/cm³ when measured according to ASTM D1505 or ISO 1183-1:2022, the 21 field corresponds to a nominal melt flow rate of 1.0 g/10 min at 190 °C and 2.16 kg load when measured according to ASTM D1238 or ISO 1133-1:2022, and the AF suffix denotes an anti-fog additive system according to producer nomenclature. The resin is supplied as pellets with a bulk density near 0.54–0.56 g/cm³ according to ISO 60. The intended blown film gauge range is 20–150 µm. Published producer literature lists agricultural films, greenhouse covers, industrial liners, carrier bags, and freezer films as application areas. The additive package contains processing stabilizers, slip agent, antiblock, and anti-fog; exact concentrations are proprietary and must be confirmed using lot-specific certificates of analysis. Film properties depend on downstream processing, gauge, blow-up ratio, and cooling rate; resin properties alone do not guarantee final film performance.

    How does melt temperature influence bubble stability and gel formation on single-screw blown film lines?

    In single-screw blown film processing with 24:1–30:1 L/D barrier screws and 150–250 mm dies, melt temperature affects die pressure, bubble stability, gel formation, and additive migration. The recommended melt temperature window is 180–240 °C, with feed 160–190 °C, compression 190–210 °C, metering 210–230 °C, and die 220–240 °C. Below 180 °C, the 1.0 g/10 min melt flow rate produces high viscosity; on a 60 mm grooved-feed extruder head pressure can exceed 350 bar. Above 240 °C, thermo-oxidative degradation consumes the stabilizer package and can create oxidized gels. Above 245 °C, anti-fog additive volatilization can deposit on the air ring and disrupt bubble stability. Frost line height should be held at 3–5 die diameters; for a 200 mm die at 2.5:1 blow-up ratio, 400–600 mm frost line height typically produces gauge variation below ±6%. Higher frost lines increase transverse-direction orientation; lower frost lines increase machine-direction orientation and can reduce dart impact.

    Moisture pickup during storage is rarely a processing problem at ambient humidity below 60% RH because polyolefins are hydrophobic. In subtropical or monsoon conditions above 60% RH, surface moisture can produce pinholes and bubble instability; pre-drying at 40–50 °C for 2–4 h in a desiccant hopper is then used. Predrying above 60 °C may cause pellet agglomeration and partial additive loss.

    On a 45 mm smooth-bore extruder with 24:1 L/D and a 150 mm die, typical output ranges from 35 to 55 kg/h depending on screw speed, back pressure, and die gap. The specific energy consumption is approximately 0.25–0.35 kWh/kg. At back pressures above 300 bar, shear heating raises melt temperature by 10–15 °C above die set point, which reduces viscosity and can destabilize the bubble. Automatic gauge control systems using segmented air rings respond best when the frost line height is stable. Frequent gauge variations above ±8% at 2.5:1 blow-up ratio indicate insufficient melt homogenization, worn screw elements, or poor die lip adjustment.

    Film mechanical properties and conversion performance at 50 µm thickness

    Published technical data for the 0.918 g/cm³ butene LLDPE blown film grade category contain the following representative values at 50 µm thickness. These values are typical, not lot-release specifications; lot-specific certificates of analysis must govern.

    Table 1: Representative physical and film properties for Braskem LHB118/21AF
    PropertyTest methodRepresentative value
    DensityASTM D1505 / ISO 1183-1:20220.918 g/cm³
    Melt flow rateASTM D1238 / ISO 1133-1:20221.0 g/10 min
    Melting peakASTM D3418122 °C
    Vicat softening temperatureASTM D1525 / ISO 306103 °C
    Dart impact F50ASTM D1709 method A90 g
    Elmendorf tear MDASTM D1922180 gf
    Elmendorf tear TDASTM D1922350 gf
    Secant modulus 1% MDASTM D882180 MPa
    Tensile strength at break MDASTM D88238 MPa
    Tensile strength at break TDASTM D88230 MPa
    Elongation at break MDASTM D882600%
    Elongation at break TDASTM D882750%
    HazeASTM D100313%
    Gloss 45°ASTM D245760 GU
    Dynamic coefficient of friction film-to-filmASTM D18940.20

    The mechanical data show asymmetric tear behavior. At 50 µm and 2.5:1 blow-up ratio, the Elmendorf tear ratio is approximately 1:1.9. Dart impact under ASTM D1709 method A is typically 90 g, which is higher than conventional LDPE at equivalent gauge. Puncture resistance measured under ASTM D5748 is commonly 50–65 N. Seal initiation temperature measured according to ASTM F88 on 25 mm strips with 0.5 s dwell and 0.275 MPa jaw pressure is typically 95–105 °C for a 3 N/25 mm minimum seal strength. Hot tack measured by ASTM F1921 at 110 °C typically exceeds 2.5 N/25 mm. Exact values are lot-dependent.

    After film conversion, additive migration is time and temperature dependent. Slip agents from the oleamide or erucamide class bloom to the surface and reduce film-to-film dynamic coefficient of friction below 0.30 after 24–48 h at 23 °C. At 5 °C, migration is slower and slip development may require 7 days. In freezer film, low-temperature blocking remains acceptable. The antiblock component is typically silica or talc; excessive loading can increase haze and reduce gloss. Anti-fog activity in agricultural film after 6–12 months of outdoor exposure may decline because the polar additive is washed away; replacement by spray-applied anti-fog is sometimes required. Blocking force measured according to ASTM D3354 on 50 µm film is typically below 1.5 N/cm² after 48 h at 50 °C.

    Compared with high-pressure tubular LDPE, LHB118/21AF possesses a strictly linear polyethylene backbone with short-chain branches from 1-butene. The absence of long-chain branching reduces extensional strain hardening; high-stalk stability is therefore lower unless internal bubble cooling is used. The tensile strength and dart impact allow downgauging in liners and heavy-duty shipping sacks by 10–20% relative to LDPE at equal load-bearing performance. Compared to metallocene octene LLDPE grades, the butene-based molecular structure generally yields lower dart impact and puncture resistance but also lower melt pressure and lower melt fracture sensitivity on conventional smooth-bore blown film lines. On a 60 mm grooved-feed extruder at 80 kg/h output, head pressure for this product class is typically 250–320 bar; a metallocene octene LLDPE of equivalent melt flow rate can exhibit 280–380 bar under the same conditions. The narrower comonomer distribution of metallocene grades produces higher gloss and lower haze; LHB118/21AF typically shows 12–15% haze at 50 µm. Blending with high-pressure LDPE at 10–20% can reduce haze and improve bubble stability but may sacrifice dart impact and increase seal initiation temperature.

    Table 2: Performance category comparison at 50 µm film thickness
    AttributeBraskem LHB118/21AF butene LLDPEConventional tubular LDPEMetallocene octene LLDPE
    Molecular architectureLinear, short-chain branching onlyLong-chain branchedLinear with narrow comonomer distribution
    Melt flow ratio I21.6/I2.1625–2945–7016–22
    Bubble stability in high-stalk geometryModerate; internal bubble cooling recommendedHighModerate to high
    Dart impact F5090 g60 g250 g
    Puncture resistance55 N35 N85 N
    Haze12–15%5–8%3–5%
    Seal initiation95–105 °C100–110 °C90–100 °C
    Melt pressure at equivalent outputLower than mLLDPELowerHigher due to narrow MWD

    When LHB118/21AF is coextruded with EVOH or polyamide barrier layers

    In multi-layer barrier structures, the grade is placed in sealant and core layers. Its 1.0 g/10 min melt flow rate provides sufficient coextrusion melt strength when combined with HDPE, PP, and maleic anhydride tie resins in blown film dies. Skin-layer melt temperature is set at 210–230 °C to avoid degradation of EVOH while maintaining interlayer adhesion. The AF suffix anti-fog additive can migrate to the inner surface in agricultural applications; migration accelerates at 30–40 °C and 80% RH. In multi-layer structures, the anti-fog additive can interact with polyamide scavengers and reduce seal strength if the inner layer is less than 15% of total thickness. Coextrusion die gaps are kept at 1.8–2.5 mm when EVOH is used to reduce interfacial flow instabilities. High shear rates at the die lip should be avoided; melt temperatures above 230 °C in the outer polyolefin layers may create orange peel surface defects on thick barrier film. Published data for this specific multi-layer configuration with LHB118/21AF is limited; pre-production trials are required.

    Food-contact status should be confirmed against the manufacturer’s Regulatory Data Sheet. The resin may comply with FDA 21 CFR 177.1520(c)3.1a for olefin polymers and EU Regulation 10/2011 when authorized additives are used; however, the anti-fog additive package requires a specific migration evaluation under EU 10/2011. Storage should be in a dry environment below 40 °C and away from direct sunlight to prevent additive loss and yellowing. Re-pelletized or heavily recycled fractions above 10–15% may reduce the anti-fog persistence and increase film haze. Processors should avoid blending with amine-based antifog concentrates unless the stabilizer interaction has been evaluated; published data for this additive combination is limited. The resin is not recommended for rotomolding, injection molding, or cast film processes because the formulation and melt flow rate are not optimized for those conversion methods.

    Top