| HS Code | 536492 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Index | 2.1 g/10 min (190°C/2.16 kg) |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Crystallization Temperature | 106 °C |
| Recommended Process | Blown film extrusion |
| Additive Package | Anti-fog |
| Form | Pellets |
| Color | Natural |
| Film Thickness | 38 µm |
| Tensile Strength At Break Md | 30 MPa |
| Tensile Strength At Break Td | 25 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Dart Impact | 120 g |
| Elmendorf Tear Md | 200 g |
| Elmendorf Tear Td | 300 g |
| Haze | 12% |
| Gloss 45 | 50 |
As an accredited Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene is packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Braskem LHB 118/21 AF LLDPE blown film extrusion polyethylene in 25-kg bags, palletized, shrink-wrapped, and secured. |
| Shipping | Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene is shipped as solid pellets in 25 kg moisture-barrier bags or bulk bags, palletized and shrink-wrapped. Store under cover in a well-ventilated area, cool and dry, away from ignition sources. Not regulated for transport; use standard forklift handling and avoid puncturing packaging. |
| Storage | Store Braskem LHB 118/21 AF LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed in original packaging. Protect from moisture, dust, and contamination. Separate from strong oxidizers. Avoid excessive stacking and static buildup. Follow the manufacturer’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Braskem LHB 118/21 AF LLDPE has a 12-month shelf life when stored unopened, cool, dry, and protected from direct sunlight. |
Agricultural bale-wrap conversion of Braskem LHB 118/21 AF is typically run on a three-layer blown film line with screw diameters of 65/80/65 mm and 30:1 L/D, a 350 mm die diameter, 1.8–2.2 mm die gap, blow-up ratio of 2.5:1–3.0:1, and frost line height 800–1200 mm above the die face. Melt temperature is held between 190°C and 210°C, and die zones are set with a flat profile to avoid transverse-direction thickness bands that amplify during bale wrapping. The resin has a nominal density of 0.918 g/cm³ per ASTM D1505 and a melt flow rate of 1.0 g/10 min per ASTM D1238 at 190°C/2.16 kg. The hopper formulation is 100 phr LHB 118/21 AF with 1.0–2.5 wt% HALS/UV masterbatch, 0.5–1.2 wt% white TiO₂ masterbatch, and up to 15 wt% same-line edge-trim recycle. Finish-product compliance follows EN 13206:2017 for thermoplastic bale-wrap films, with tensile properties per ISO 527-3, tear propagation per ASTM D1922, and dart impact per ASTM D1709 Method A. The production-scale failure mode recorded on wrapping machines is not tensile yield but low-temperature flexing at fold lines when film temperature drops below −10°C; under those conditions transverse-direction tear resistance becomes the limiting property, and converters typically increase HALS addition toward the upper 2.5 wt% limit and reduce recycle content below 10 wt% to preserve fold-line integrity. Converted articles from this segment include 25–30 µm round-bale silage wrap, clamp silage sheets, silage bags, and grain storage covers.
Blown film lines producing freezer-grade packaging from LHB 118/21 AF operate with 1.8 mm die gap, 2.2:1–2.8:1 blow-up ratio, 195–215°C melt temperature, and corona treatment to 38–40 dyn/cm surface energy after bubble collapse. The web is run at 40–70 µm thickness; the frost line is held at 5–7 die diameters to prevent blocking between film plies before winding. Formulation addition ratio is 100 phr LHB 118/21 AF with 1.0–2.0 wt% of an antiblock/slip masterbatch; if bubble stability is insufficient on a given line, 10–20 wt% LDPE with melt flow rate 0.25 g/10 min is added. For food-contact use, compliance is evaluated under 21 CFR §177.1520 and Regulation (EU) No 10/2011; overall migration is limited to 10 mg/dm² using EN 1186-1 total immersion testing. The compliance matrix for this segment is summarized below.
| Requirement scope | Standard designation | Test method | Limit |
|---|---|---|---|
| US FDA food contact | 21 CFR §177.1520 | Extraction per 21 CFR §176.170 | Olefin polymer compliance |
| EU overall migration | Regulation (EU) No 10/2011 | EN 1186-1 | 10 mg/dm² |
| EU good manufacturing practice | Regulation (EC) No 2023/2006 | Audit and documentation | Traceability |
Terminal finished product types include IQF vegetable pouches, frozen fruit bags, ice-glazed poultry packaging, and frozen dough liners. The primary sealing defect observed on vertical-form-fill-seal lines is channel leaker formation when sealant temperature falls below 105°C at 0.2–0.4 s dwell; converters therefore hold sealing jaw temperature between 110°C and 140°C. Cold-storage conditioning at −30°C for 24 h followed by drop testing is used to qualify bag toughness; published data for this specific LHB 118/21 AF configuration is limited, but the tests are specified in converter incoming inspections.
The sealant web in a barrier laminate is converted from LHB 118/21 AF on a blown film line with 1.5–2.0 mm die gap, 2.0:1–2.5:1 blow-up ratio, and 190–210°C melt temperature. When target sealant thickness falls from 20 µm to 12 µm, the processing conflict shifts to hot-tack window and gauge uniformity; sealing jaw temperatures must remain between 110°C and 140°C, dwell time is shortened to 0.3–0.5 s, and any thickness deviation greater than ±1.0 µm produces channel leakers at the seal fold. The sealant formulation is 80–100 wt% LHB 118/21 AF with 0–20 wt% LDPE; a fluoroelastomer processing aid is added at 0.03–0.08 wt% to suppress melt fracture. Slip additives are omitted or limited to 0.2 wt% because migratory erucamide reduces bond strength after solventless adhesive lamination at 1.5–2.5 g/m² coat weight and 5–7 days cure at 35°C. Compliance is under FDA 21 CFR §177.1520 and Regulation (EU) No 10/2011; laminate seal strength is verified per ASTM F88/F88M. Converted laminates emerging from this process include stand-up pouches, pillow bags for dry snacks, sachet films, and lidding membranes.
Industrial sacks produced from LHB 118/21 AF are blown as heavy-gauge tubular film at 80–200 µm thickness with 2.0–2.5 mm die gap, 1.8:1–2.2:1 blow-up ratio, and 200–220°C melt temperature. The lower blow-up ratio increases machine-direction stiffness and reduces transverse gauge variation before flexographic printing, gusseting, and bottom sealing. The blown film compound is 70–100 wt% LHB 118/21 AF with 0–30 wt% high-density polyethylene to raise secant modulus, plus 1–3 wt% white masterbatch for opacity. Where the converted sack functions as an inner liner for UN-certified FIBCs, the finished liner must pass stacking and drop tests referenced in ISO 21898:2004 and the applicable UN Recommendations on the Transport of Dangerous Goods Chapter 6.5; mechanical evaluation uses ISO 527-3, ASTM D1709, and ASTM D1922. The critical fill-spill test is conducted after conditioning at −20°C for 24 h; published data for this specific LHB 118/21 AF formulation is limited, but converter trials record failures at the gusset fold when dart impact value per ASTM D1709 Method A falls below the specification for the filled mass. Downstream sacks and liners produced in this segment include FIBC liners, chemical powder sacks, resin pellet bags, fertilizer sacks, and mineral aggregate bags.
On palletizing lines where a single tubular film is stretched over a load at pre-stretch ratios of 70–120%, LHB 118/21 AF is extruded on a three-layer blown film line with 2.2 mm die gap, 3.0:1–3.5:1 blow-up ratio, and 190–210°C melt temperature. The tube is collapsed, gusseted, slit, and wound on jumbo reels for conversion into stretch hoods. The compound formulation uses 100 phr LHB 118/21 AF with 1–3 wt% tackifier masterbatch and 0.5–1.5 wt% polyethylene wax processing aid; slip agents are omitted because slip reduces the cling force required for load stability. Compliance is verified through ISO 527-3 for tensile properties and ASTM D4649 for stretch film evaluation, with REACH registration applicable to the compound. At pre-stretch ratios above 150%, local thinning at corner creases initiates stress-whitening and tear propagation; process limits are set so that gauge retention at the gusset corner remains above 40 µm. Finished stretch hood articles include stretch hoods for palletized appliances, beverage bottles, insulation batts, and chemical drums.
Greenhouse cover film extrusion from LHB 118/21 AF is performed on three-layer blown film lines with 2.0–2.4 mm die gap, 2.5:1–3.0:1 blow-up ratio, and tower height 8–10 m; total film thickness is 150–200 µm. The formulation ratio is 100 phr LHB 118/21 AF with 0.6–1.5 wt% NOR-HALS masterbatch, 0.3–0.8 wt% UVA masterbatch, 0.5–1.2 wt% anti-drip masterbatch, and up to 15 wt% recycled LLDPE. Sulfur burner fumigation imposes an additive-selection boundary: repeated exposure to sulfur vapor above 1,500 ppm can deactivate tertiary HALS chemistries; NOR-HALS types are therefore specified after 3–5 fumigation cycles, based on stabilizer supplier technical bulletins. Compliance is assessed under EN 13206:2017 for agricultural films and REACH; thickness uniformity is checked per ISO 4593, and tensile properties per ISO 527-3. The final agricultural film articles are greenhouse covers, high-tunnel films, low-tunnel films, and shade-house cladding.
Concrete slab vapor retarder film from LHB 118/21 AF is extruded at 0.3–0.5 mm thickness with 2.0 mm die gap, 1.8:1–2.2:1 blow-up ratio, and 190–210°C melt temperature. Compounding for vapor retarder sheet uses 100 phr LHB 118/21 AF with 2–4 wt% carbon black masterbatch for UV stabilization, 0.5–1.0 wt% processing aid, and 10–20 wt% post-industrial regrind. Compliance follows ASTM E1745 for flexible water vapor retarders used beneath concrete slabs; Class A permeance is required at ≤0.1 perm as tested per ASTM E96 desiccant method. Finished product types include underslab vapor retarders, crawl-space liners, and temporary construction dust barriers.
Competitive Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem LHB 118/21 AF is a 1-butene-based linear low-density polyethylene formulated specifically for blown film extrusion. The commercial designation encodes the base resin architecture: the 118 field identifies a nominal density of 0.918 g/cm³ when determined under ISO 1183-1, and the 21 field corresponds to a nominal melt flow rate of 2.1 g/10 min at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. The AF suffix denotes a formulated anti-fog additive package intended for films exposed to condensation in low-temperature and high-moisture packaging environments. The grade is supplied as ready-to-extrude pellets, which reduces the need for converter-side addition of separate anti-fog masterbatch in monolayer applications. Because the resin is produced with a 1-butene comonomer, its solid-state and melt rheology differ from higher alpha-olefin copolymers, from high-pressure low-density polyethylene, and from metallocene-catalyzed LLDPE grades commonly used in similar film structures.
The primary intended use is blown film for chilled produce overwrap, cut-fruit packaging, refrigerated display bags, and agricultural tunnel covers where fog formation reduces visible light transmission or package appeal. Film thickness in such applications typically ranges from 15 µm to 80 µm, depending on downstream form-fill-seal equipment, required puncture resistance, and package weight. The anti-fog effect is not instantaneous after extrusion; it develops as the surface-active additive migrates through amorphous regions to the film surface. Migration is temperature-dependent, slower at 4 °C than at 23 °C, and should be accounted for in converter conditioning protocols. No single harmonized ISO or ASTM method governs all anti-fog evaluations; commercial assessments frequently rely on condensation chamber tests developed by packaging laboratories, which limits direct ranking transfer between production lines unless test geometry and thermal history are identical.
Short-chain branching in butene-based LLDPE produces a less developed tie-molecule population than hexene- or octene-based copolymers of equivalent density. The practical consequence is that LHB 118/21 AF generally exhibits lower dart impact strength, lower Elmendorf tear propagation resistance, and higher internal haze than metallocene or Ziegler-Natta hexene/octene grades at the same film gauge. This is a conversion trade-off rather than a defect. The butene backbone provides lower melt viscosity and more moderate shear thinning than many metallocene grades, permitting stable extrusion on lower-torque blown film lines. However, because the resin lacks long-chain branching, bubble stability at high blow-up ratios is more sensitive than that of tubular or autoclave LDPE. Operators must control neck height and cooling air more tightly than would be required for low-density polyethylene of similar melt index.
Compared with the unmodified LHB 118/21 base resin, the AF version is not expected to alter nominal density or melt flow rate beyond the additive contribution. The surface effects are more relevant: anti-fog additive exudation can increase surface friction and blocking tendency, particularly after corona treatment or prolonged roll storage. Compared with an autoclave LDPE of melt index near 2.0 g/10 min, LHB 118/21 AF offers higher dart impact at equivalent thickness but lower melt strength at die melt temperatures. LDPE remains the preferred material for certain high-stalk frozen food bags where low-temperature stiffness and optical clarity dominate. LHB 118/21 AF is selected where puncture resistance, tear resistance, and downgauging are more important than maximum bubble stability. Metallocene hexene or octene copolymers may provide better optical and mechanical balance, but they often require higher extrusion pressure and narrower die gaps; LHB 118/21 AF tolerates a wider processing window on standard single-screw lines.
On production-scale blown film equipment, LHB 118/21 AF is normally processed on single-screw extruders with 25:1 to 30:1 L/D ratios. Barrier screws with spiral or Maddock mixing sections are used to avoid unmelts and to disperse the anti-fog additive. Die gap should be held between 1.5 mm and 2.5 mm. Older narrow-gap LDPE dies often generate excessive shear stress at the die lip, producing sharkskin on thicker film from this grade. Melt temperature at the die head is typically maintained between 185 °C and 220 °C. Temperatures above 230 °C may accelerate depletion of stabilizers and degrade the anti-fog ester package. Temperatures below 175 °C may cause feed-zone pressure spikes and visible unmelts in the film. Barrel profiles are generally flat or slightly reverse; excessive front-zone temperature above 190 °C can improve surface finish but lowers melt strength and destabilizes the bubble neck.
Blow-up ratios from 2.0:1 to 3.5:1 are common. Frost line height between 6 and 10 die diameters is used to balance machine-direction and transverse-direction orientation. Higher frost lines generally increase machine-direction tensile strength but may reduce transverse-direction tear resistance and increase shrink. Excessive frost line distance causes bubble sag, gauge variation, and instability under fluctuating ambient air currents. Internal bubble cooling and high-capacity external cooling rings improve specific output per die circumference. On conventional air-cooled lines, specific output around 0.8 kg/h/cm to 1.2 kg/h/cm of die circumference is achievable, but published data for this exact grade under high-output internal bubble cooling conditions remains limited outside proprietary extrusion trials. Batch-to-batch melt flow rate variation within supplier tolerance can shift die pressure and neck height. On coextruded structures with polyamide or EVOH skins, viscosity mismatch should be corrected by die temperature adjustment or layer redistribution rather than by large screw-speed changes alone.
Anti-fog performance is a migration-controlled process rather than an equilibrium surface property. The additive package moves through amorphous regions to the film surface, lowers the contact angle of condensed water, and spreads droplets into a continuous transparent layer. At cold display temperatures between 1 °C and 8 °C, migration is slower than at ambient conditioning. Converter trials commonly condition film for 24 h to 72 h at 25 °C before evaluating anti-fog behavior. Under commercial cold-chain cycling, anti-fog action depends on cumulative condensation-drying cycles. The surface-active species is gradually removed by condensate drainage, and performance decays after repeated cycles. The additive does not eliminate the need for package ventilation or temperature control. In sealed packs containing high-respiring produce, internal humidity can approach saturation. The film must rapidly shed condensation; if the surface is corona-treated for printability or lamination, excessive surface oxidation can alter surface polarity and reduce initial anti-fog activity. Dyne levels above 40 mN/m are typical for adhesion, but overtreatment can hydrophilize the surface before the anti-fog additive blooms.
Blocking and printability are the most commonly reported converter-side limitations. If anti-fog additive bloom is excessive, the coefficient of friction increases and film may block on rolls after winding under high compression. Finished rolls should be stored below 30 °C for no more than 48 h before high-speed bag converting unless winder tension and compression are controlled. In coextruded structures, LHB 118/21 AF is often placed in the food-contact sealant layer because its density and melt index permit low-temperature heat sealing. Exact seal initiation temperature must be determined on the final sealing jaw configuration because pressure, dwell time, and film thickness shift the measured response. The grade does not adhere directly to polyamide or ethylene-vinyl alcohol copolymer; tie-layer resins are required in multilayer barrier films. The anti-fog additive in a sealant layer may migrate toward the outer surface or toward interfacial regions. Barrier layers can restrict additive transport, reducing surface concentration and anti-fog persistence unless the skin layer itself contains a portion of the additive or an additional masterbatch is used.
The following matrix identifies common quality-control and regulatory methods used for evaluating blown film from LHB 118/21 AF. It is not a certificate of analysis; actual batch values are supplied with the commercial documentation.
| Property or requirement | Standard or regulation | Typical condition or note |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg |
| Density | ISO 1183-1 | Compression-moulded specimen, 23 °C |
| Tensile properties of film | ASTM D882 | Crosshead speed 500 mm/min |
| Elmendorf tear | ASTM D1922 | Single-ply or multi-ply as specified by converter |
| Dart impact | ISO 7765-1 or ASTM D1709A | Dart head 38 mm |
| Haze | ASTM D1003 | Thickness-dependent; report specimen gauge |
| Gloss | ASTM D2457 | 60° geometry |
| Seal strength | ASTM F88/F88M | Jaw speed 200 mm/min |
| Olefin polymer food-contact status | 21 CFR 177.1520, (EU) No 10/2011 | Final film migration limits are converter responsibility |
For thickness-dependent mechanical and optical properties, specimens are typically conditioned at 23 °C and 50% RH for 40 h according to ASTM D618 or ISO 291. The reported values depend on film gauge, blow-up ratio, frost line height, and additive distribution; a value measured on 25 µm film cannot be linearly extrapolated to 70 µm film without re-testing.
Operational boundaries should be defined by the final packaging line. High-speed form-fill-seal equipment imposes simultaneous demands on seal initiation, hot tack, slip, and anti-fog surface bloom. If the film is stored under high humidity or wound at excessive tension, roll blocking can occur even when laboratory coefficient of friction values remain within specification. Corona treatment should be set to the minimum level required for downstream adhesion; excessive surface oxidation can delay anti-fog activity and increase odor transmission from the package. The grade should not be processed above 230 °C for extended residence times. Prolonged exposure at elevated temperature accelerates additive deterioration and can produce oxidized film edges. When regrind is incorporated, film properties change; excessive regrind levels in the presence of anti-fog additives can raise gel counts and reduce bubble stability. Published data for the exact regrind tolerance of LHB 118/21 AF in high-output multilayer structures is limited; converter trials are required to establish acceptable scrap ratios on a specific line.
In agricultural tunnel film, anti-fog behavior is paired with UV stabilizer masterbatches and is consumed gradually. The ester-based anti-fog agent migrates to the surface and is lost through condensate drainage. Ultraviolet exposure degrades the polyethylene surface and increases roughness; fine cracks typically appear first at fold lines and clamping points. Anti-fog persistence in such films depends on film slope angle, temperature gradient, and stabilizer package, not solely on the base resin additive content. For post-harvest produce packaging, the grade is used where condensation control and mechanical toughness must be maintained simultaneously under cold-chain distribution. The critical operational limit is the depletion of surface-active additive after repeated condensation cycles; once anti-fog activity fails, light transmission through the film drops and package visibility deteriorates before bulk mechanical properties are affected.