Braskem Lh537 Lldpe Cast Film Extrusion Polyethylene

Braskem LH537 LLDPE Cast Film Extrusion Polyethylene

    • Product Name: Braskem LH537 LLDPE Cast Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 606090
    Density 0.921 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 3.3 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600 %
    1 Secant Modulus 200 MPa
    Dart Impact 120 g
    Haze 3 %
    Gloss 45 80
    Coefficient Of Friction 0.20
    Seal Initiation Temperature 105 °C

    As an accredited Braskem LH537 LLDPE Cast Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH537 LLDPE Cast Film Extrusion Polyethylene is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Braskem LH537 LLDPE Cast Film Extrusion Polyethylene, palletized 25 kg bags, stretch-wrapped, securely loaded for ocean export.
    Shipping Braskem LH537 LLDPE Cast Film Extrusion Polyethylene ships as non-hazardous polyethylene resin pellets in 25 kg bags on pallets, stretch-wrapped for moisture protection. Transport in clean, dry containers or trucks. Store cool, dry, away from sunlight, heat, and contaminants. Standard freight; no special dangerous goods handling required.
    Storage Store at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed, palletized, and off the floor. Protect from moisture, dust, contamination, and physical damage. Avoid prolonged UV exposure, excessive stacking, and dust accumulation. Use good housekeeping and grounding to control static. Follow manufacturer’s SDS and local regulations.
    Shelf Life Braskem LH537 LLDPE typically has a 24-month shelf life from production when stored unopened, dry, cool, ventilated, and away from sunlight.
    Application of Braskem LH537 LLDPE Cast Film Extrusion Polyethylene

    Pre-stretch Film Behaviour on High-Speed Rotary Wrappers

    On high-speed rotary pallet wrappers equipped with powered pre-stretch heads operating at film feeds of 200–250 m/min, load-containment cast film derived from LH537 is typically extruded at 20–23 µm nominal gauge and slit to 500 mm machine rolls. The formulation places the base resin at 78–85 wt% of the blend, with a C6 or C8 linear low density polyethylene added at 10–15 wt% to raise dart impact and puncture resistance, and LDPE at 5–7 wt% to improve melt curtain stability and reduce neck-in across a 2 800 mm cast die. A polyisobutylene-based cling masterbatch is dosed at 1.2–1.8 wt% total compound, producing one-sided cling forces between 1.5 N and 3.5 N when tested according to ASTM D5458-16. Compliance for European machine-wrap rolls frequently references EN 14932:2018 for thermoplastic stretch films used in logistics and bale wrapping, while tensile properties are measured under ISO 527-3 at 500 mm/min and puncture resistance under ASTM D5748-18. The downstream production sequence on a cast film line uses a barrier screw at 30:1 L/D with a melt temperature of 240–260 °C, a die gap of 0.7–0.9 mm, an air gap of 120–160 mm, and a chill roll held at 18–22 °C to quench the web before downstream treatment. Slit rolls are loaded onto rotary wrappers where the film is pre-stretched at 200–250% before application; retained load after 24 h on a pallet at 23 °C must remain above 80% of initial tension in most distribution network specifications. Terminal products include 23 µm machine pallet wrap, 20 µm hand stretch wrap, and pre-stretched rolls for semi-automatic turntable wrappers; all configurations require edge trimming tolerance below ±0.5 mm to prevent slitter-induced nicks that propagate under high draw.

    Slitter operators observe that a chill roll temperature excursion above 25 °C increases cling-layer transfer to the roll face within 30 min, evidenced by web wrap-around on the stripper roll; a drop in line speed below 250 m/min then produces gauge bands at ±2.0 µm. Pre-stretch equipment fitted with load cells records a retained load loss of 10–15% after 72 h creep on a pallet when outer-layer cling force falls below 1.2 N under ASTM D5458-16; above 3.5 N, tail breakage during cut-and-transfer cycles becomes more frequent. These thresholds define the operating envelope for LH537-based formulations on high-speed rotary wrappers and are not transferable to blown-film stretch hood equipment.

    For fresh produce overwrap lines running at 60–120 packs/min, cast web at 12–25 µm is produced as a single-layer structure in which LH537 constitutes 92–100 wt% of the polymer phase; the balance is an antiblock masterbatch at 0.5–1.5 wt% and a slip additive at 300–800 ppm active erucamide. The relevant compliance framework for direct food contact in the United States is FDA 21 CFR 177.1520(c) for olefin polymers, with the finished film subject to the overall migration limits of EU 10/2011 when sold into European markets. Processing conditions on the cast line include a melt temperature of 225–245 °C, chill roll temperature of 14–18 °C, and air gap below 100 mm to maintain optical clarity measured at less than 5% haze under ISO 14782. The film is corona-treated online to 38–42 mN/m before slitting to width for use on horizontal form-fill-seal machines where fin-seal jaws operate at 105–125 °C and dwell times of 0.3–0.6 s. Terminal products include bakery tray overwrap, whole-produce flow packs for leafy greens requiring a respiration window in the film, and lightweight bundling films for retail food trays. The lower melt temperature compared with pallet stretch film reduces oxidative degradation in the sealant layer but narrows the die-lip shear window; line operators must maintain die pressure above 80 bar to prevent melt fracture, and with relative humidity above 60% corona-treated film should be converted within 72 h because surface energy decays below 36 mN/m on storage.

    What Governs Peel Adhesion in Temporary Surface Protection Films for Anodised Aluminium?

    The peel force required to remove a temporary cast protective film from an anodised aluminium profile is controlled by the viscoelastic behaviour of the coextruded skin layer rather than by the bulk density of the base resin. In this structure LH537 is used at 70–80 wt% of the total extrudate as the core layer for tensile strength and puncture resistance, while the skin layer contains a metallocene plastomer at 20–30 wt% of the skin formula to produce pressure-sensitive adhesion without a separate coating step. The downstream process is a three-layer cast coextrusion line with feedblock distribution and a die width of 2 200 mm; the chill roll is run at 25–35 °C with a matte finish to control unwinding and provide a 60–90% surface contact area. Industry compliance is anchored to ASTM D3330/D3330M-04 for 180° peel adhesion from stainless steel, ISO 2409:2013 for coating/substrate interface cleanliness after removal, and ASTM D882 for tensile elongation at break. Peel forces are normally maintained between 0.8 N/25 mm and 3.0 N/25 mm depending on the substrate surface energy; values below 0.5 N/25 mm produce edge-lift on outdoor profiles, while values above 4.0 N/25 mm cause deformation of thin masking sections during high-speed application. Terminal product configurations include 60–80 µm films for anodised aluminium profiles, 40–60 µm films for stainless steel panels, and 25–35 µm films for polycarbonate sheet; each is supplied in 1 000 mm machine rolls with an application temperature range of 10–35 °C. A known operational boundary is that LH537-based protective films should not be applied to freshly painted coil coatings unless the paint supplier confirms that the cling layer does not contain low-molecular-weight species that can migrate into the coating within 72 h.

    Agricultural Bale Wrap Silage Sealing and Fermentation Control

    Silage bale wrap extruded from LH537 is formulated at 85–92 wt% base resin, 5–10 wt% LDPE or C8 linear density modifier, 2–4 wt% carbon black masterbatch, and 0.3–0.6 wt% hindered amine light stabiliser/UV package. The carbon black loading is not cosmetic; it maintains film integrity under ultraviolet exposure by limiting accelerated oxidative chain scission during 12-month outdoor bale storage. The material is extruded at 25 µm nominal thickness on a cast film line with a die width of 2 400 mm, an air gap of 150–200 mm, and a chill roll at 30–40 °C to reduce blocking before slitting to 750 mm bale-wrap rolls. Compliance is tested under EN 14932:2018 for thermoplastic stretch films used in agricultural baling, with tensile stress at break measured under ISO 527-3 and UV exposure under ASTM G154 cycle 1 for 500 h. Downstream bale wrappers apply the film at 55–70% pre-stretch and 4–6 film layers per bale, producing an anaerobic silage environment that limits aerobic yeast and mould proliferation. Terminal products include round bale silage wrap, haylage wrap, and tube-wrap film for silage compaction. The main processing limitation is that carbon black masterbatch at the upper end of the stated range lowers melt drawing stability; line operators should reduce line speed by 10–15% when running at 3 wt% carbon black to avoid draw resonance.

    Because the cast web is intended as the heat-seal layer inside a three-component laminated pouch, seal initiation temperature and hot-tack strength are the controlling parameters for converter acceptance. LH537 is compounded at 65–80 wt% of the sealant film, with a metallocene polyethylene at 20–35 wt% to lower seal initiation to 95–105 °C and to extend hot-tack strength above 2 N/25 mm at 110 °C under ASTM F1921-24. The cast film is extruded at 20–30 µm, corona-treated to 42–46 mN/m, and adhesive-laminated to a reverse-printed polyester or metallised polyester outer web; the finished laminate must pass ASTM F88/F88M seal strength testing with values above 10 N/15 mm at 130 °C jaw temperature. Regulatory compliance for dry food pouches uses FDA 21 CFR 177.1520(c) and EU 10/2011 with fatty-food simulant D2 migration protocol where applicable, while packaging converters frequently add internal specification limits for residual solvents below 5 mg/m² under DIN 55664. Terminal product types include stand-up pouches for dry cereal, detergent refill pouches, and medical device overwrap where the sealant layer must not contaminate the sealed product. The critical processing limitation is that excessive corona dose above 50 mN/m can oxidise the surface and reduce interlayer adhesion against solvent-based adhesives by creating weak boundary layers.

    When Cast LLDPE Replaces Blown LDPE in Controlled-Environment Hygiene Films

    In controlled-environment hygiene film converting, cast extrusion from LH537 replaces blown LDPE when the downstream operation demands gauge uniformity below ±3% across a 1 800 mm web and a low-gloss matte surface for automated diaper line feeding. The cast film formulation contains 70–85 wt% LH537, 8–15 wt% titanium dioxide white masterbatch, 1–3 wt% slip/antiblock masterbatch, and 0.05–0.10 wt% fluoropolymer processing aid to suppress die-lip build-up. The production process runs through a cast die at a melt temperature of 235–255 °C and an embossed chill roll at 22–28 °C, followed by inline slitting to 10–20 µm film and adhesive lamination to a polypropylene spunbond nonwoven. Compliance for absorbent hygiene laminates supplied in the EU relies on REACH Annex XVII substance restrictions and component testing under ISO 13934-1:2013 for tensile strength and EDANA NWSP 110.4.R0 for thickness and basis weight, rather than food-contact standards. Terminal products include non-breathable backsheet films for adult incontinence products, feminine hygiene pads, and infant diaper outer layers; the LH537 cast film is not marketed as a breathable monolithic grade, so water vapour transmission rates remain below 15 g/m²·24 h under ISO 15106-3 unless the film is microperforated downstream. The relevant processing boundary is that at line speeds below 80 m/min, the low melt tension of LH537 can cause draw resonance on a polished chill roll; an embossed roll and an air gap below 120 mm mitigate this condition.

    Free Quote

    Competitive Braskem LH537 LLDPE Cast Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH537 is a butene-1 copolymer linear low density polyethylene pellet grade qualified for cast film extrusion. The melt flow rate is controlled to 2.0 g/10 min when measured under ASTM D1238-20 at 190 °C and 2.16 kg; density is controlled to 0.918 g/cm³ under ASTM D1505-18. The polymer architecture—a linear ethylene backbone with short-chain branching introduced by butene comonomer—places the material between conventional high-pressure low density polyethylene and metallocene-catalyzed LLDPE in melt elasticity, dart impact, and shear-thinning response. The grade is intended for monolayer and coextruded cast film structures including stretch wrap, industrial overwrap, and lamination film. The following sections define the specification envelope, processing boundaries, and comparative behavior against other polyethylene film resins.

    The values below are manufacturer-published typical ranges for the resin and for cast film converted at 25 µm thickness. They are not specification limits; individual certificates of analysis take precedence.

    Typical property envelope for Braskem LH537 resin and cast film
    Property Test method Typical range
    Melt flow rate ASTM D1238-20 1.8–2.2 g/10 min
    Density ASTM D1505-18 0.917–0.919 g/cm³
    Melting peak temperature ISO 11357-3:2018 118–124 °C
    Vicat softening temperature ASTM D1525-17e1 90–100 °C
    Tensile strength at break, machine direction ASTM D882-18 30–45 MPa
    Tensile strength at break, transverse direction ASTM D882-18 25–40 MPa
    Elongation at break, machine direction ASTM D882-18 500–750%
    Elongation at break, transverse direction ASTM D882-18 600–850%
    Dart impact, F50 ASTM D1709-16a 60–110 g
    Elmendorf tear, machine direction ASTM D1922-15 80–150 gf
    Elmendorf tear, transverse direction ASTM D1922-15 250–400 gf
    Haze ASTM D1003-13 1.5–4.0%
    Gloss at 60° ASTM D2457-13 60–80

    What distinguishes the butene comonomer distribution in cast film processing?

    Compared with high-pressure LDPE, the linear backbone of LH537 reduces long-chain branching density and therefore melt elasticity. This changes the relationship between extruder head pressure and output: at constant melt temperature and screw speed, a LLDPE with 2.0 g/10 min melt index generally exhibits higher shear viscosity at die-lip shear rates than an LDPE of equivalent melt index, so barrel pressure and heater load must be monitored. The short-chain linear architecture permits rapid crystallization and a relatively narrow melting range, allowing the web to be drawn at higher line speed before blocking occurs at the chill roll.

    Production-scale cast film lines for this grade typically employ single-screw extruders with L/D 30:1 or greater, screen packs of 40/60/80 mesh, die gaps of 0.5–0.8 mm, and chill roll temperatures of 15–30 °C. Air gap is normally held at 20–50 mm to limit neck-in while avoiding melt web instability. Melt temperatures between 240 °C and 280 °C are applied; excursions above 290 °C increase die lip deposit formation and produce optical haze drift. Below 230 °C, incomplete melting of high molecular weight fractions can create unmelted gels and surface defects.

    When LLDPE rheology forces a wider die gap than LDPE

    Because of the lower melt strength and higher shear viscosity of LLDPE, die gaps optimized for high-pressure LDPE cast film are not always transferable. A converter moving from a high-pressure LDPE to LH537 may need to open the die gap from 0.3 mm to 0.5–0.8 mm to reduce die-lip shear stress and delay shark skin at high output. If the die gap is not widened, melt fracture may appear at lower throughput than expected. Draw resonance in the air gap is controlled by reducing the air gap and increasing chill roll adhesion rather than by reducing line speed alone.

    In multilayer cast film, LH537 is used as a core or back layer. The core contributes to overall mechanical drawdown and dart impact measured under ASTM D1709-16a, while outer skins may be modified with high-clarity LDPE or metallocene-catalyzed LLDPE to adjust surface gloss and coefficient of friction. The coefficient of friction is separately controlled with slip additive and measured under ASTM D1894 on the finished film.

    Lot-to-lot comonomer distribution and Elmendorf tear response

    Ziegler-Natta-catalyzed butene LLDPE resins can exhibit lot-to-lot variation in short-chain branching distribution across molecular weight fractions. That variation affects tear and dart impact even when density and melt index remain within specification. For LH537, incoming resin should be monitored on the first cast film roll after grade change using ASTM D1922-15 Elmendorf tear and ASTM D1709-16a dart impact. A downward shift in machine-direction tear may indicate an increase in high molecular weight fraction or insufficient homogenization; documented batch-to-batch variance on some cast lines has required adjustment of chill roll temperature by 2–5 °C to recover acceptable transverse direction tear.

    Optical properties of cast LLDPE film are sensitive to gel defects and oxidative degradation. Haze is measured per ASTM D1003-13 and gloss at 60° per ASTM D2457-13. Gels in the melt can create optical defects; their formation is promoted by prolonged residence time above 280 °C or by inadequate purging after previous high-viscosity materials. The grade should be purged with a suitable LLDPE purge material before and after processing, especially on extruders where upstream resin contains high levels of processing aids.

    If downgauging below 15 µm requires melt temperature reduction

    When cast stretch film is downgauged from 25 µm to 12 µm, the specific output per unit width may remain high but the melt web becomes more sensitive to thermal degradation. Reducing melt temperature from 260 °C to 240 °C while maintaining die temperature uniformity can help retain melt strength and reduce gel formation. The draw ratio is then increased, which raises machine-direction orientation; tensile strength at break under ASTM D882-18 typically rises, while Elmendorf tear may fall. This trade-off must be evaluated against the application requirement for puncture resistance measured under ASTM D5748 or equivalent.

    LH537 is supplied in pellet form and may contain antioxidant and processing stabilizer packages. Slip and antiblock additives are frequently added by masterbatch or pre-compounded in the film-grade variant, depending on the end-use friction specification. For food-contact applications, the olefin polymer base may be cited under FDA 21 CFR 177.1520(c) and European Commission Regulation (EU) No 10/2011, provided the finished film meets migration limits for its intended food category. The converter must verify overall migration under EN 1186 or the applicable standard because pellet compliance does not automatically extend to a finished printed or laminated structure.

    The resin is not hygroscopic; predrying is not required when pellets are stored in dry ambient conditions. If pellets are exposed to condensation due to temperature cycling from cold storage to warm factory air, surface moisture can create melt voids and surface streaks; a dry-air purge at 60–70 °C for 2–4 h is recommended before extrusion. The grade is not inherently stabilized for long-term outdoor UV exposure; applications requiring extended weathering require carbon black or HALS stabilization. Avoid blending with excessive levels of pro-oxidant transition metal stearates or post-industrial scrap of unknown thermal history because these can accelerate chain scission and reduce film tear resistance.

    Short-chain branching density compared with mLLDPE and high-pressure LDPE

    In comparison with high-pressure LDPE, LH537 lacks the long-chain branching that contributes to melt tension and strain-hardening; the result is a different neck-in and draw resonance envelope. Against metallocene-catalyzed LLDPE, the Ziegler-Natta butene comonomer distribution of LH537 is broader and more heterogeneous; this reduces optical clarity slightly and lowers dart impact at equivalent density but may improve extrusion throughput stability and reduce melt pressure spikes on single-screw extruders. Against hexene-based LLDPE, the butene comonomer produces lower tear and toughness at the same density; therefore the grade is selected where cost and drawability dominate over extreme puncture and tear performance. These differences are routinely quantified by ASTM D882-18, ASTM D1709-16a, and ASTM D1922-15.

    A substitution trial from LDPE or mLLDPE should include a standard output sweep on the target cast line. The converter records extruder barrel temperatures, extruder head pressure, line speed, chill roll temperature, and film thickness. Samples are tested for tensile properties under ASTM D882-18, tear under ASTM D1922-15, dart impact under ASTM D1709-16a, haze under ASTM D1003-13, and gloss under ASTM D2457-13. Only after the resulting film property envelope matches the target application can the grade be released for continuous production.

    Top