Braskem Lh218 Linear Low Density Polyethylene

Braskem LH218 Linear Low Density Polyethylene

    • Product Name: Braskem LH218 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 336757
    Product Name Braskem LH218 Linear Low Density Polyethylene
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Temperature 96 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    1 Secant Modulus 240 MPa
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 45 60
    Coefficient Of Friction 0.2

    As an accredited Braskem LH218 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH218 Linear Low Density Polyethylene supplied in 25 kg polyethylene-lined bags, palletized, stretch-wrapped, and secured for bulk shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with Braskem LH218 Linear Low Density Polyethylene bags, palletized, dry, ambient, securely stowed, weight-compliant for export.
    Shipping Braskem LH218 Linear Low Density Polyethylene ships as non-hazardous resin pellets. Standard packaging: 25 kg polyethylene bags or octabins, palletized and shrink-wrapped. Transport in clean, dry, covered trucks or containers. Not regulated by DOT, IMDG, IATA, ADR/RID. Store away from moisture, direct sunlight, and excessive heat.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed, palletized, and protected from moisture, dust, and contamination. Avoid prolonged high temperatures to prevent degradation or blocking. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months when stored in original packaging in a dry, ventilated area, away from direct sunlight, below 50°C.
    Application of Braskem LH218 Linear Low Density Polyethylene

    Braskem LH218 is a butene-based linear low density polyethylene supplied as pellet with nominal density of 0.918 g/cm³ and nominal melt flow index of 2.0 g/10 min when measured under ISO 1133-1:2022 at 190°C/2.16 kg. In monolayer blown film extrusion for high-toughness industrial liners and garment bags, the grade is processed on grooved-feed or smooth-bore extruders with screw length-to-diameter ratios between 30:1 and 32:1, a barrier section, and a Maddock mixing element. Melt temperatures are maintained between 190°C and 210°C; sustained operation above 220°C reduces bubble stability, oxidizes the polymer melt, and increases gel speck formation. Die gap is set at 2.0 mm to 2.5 mm, blow-up ratio is held between 2.3:1 and 3.0:1, and frost line height is positioned 5 to 8 die diameters above the air ring. On a 75 mm single-screw blown film line with dual-lip air ring and internal bubble cooling, output commonly ranges from 120 kg/h to 180 kg/h at film thicknesses of 15 µm to 100 µm. Industrial liner acceptance criteria typically require tensile elongation at break of at least 500% in both machine and transverse directions per ISO 527-3:2018, and dart drop impact of not less than 80 g at 25 µm gauge per ASTM D1709 Method A. Film haze measured per ASTM D1003-21 is usually between 10% and 18% for a 25 µm film. The base olefin polymer falls within the scope of FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 for food-contact applications only when the finished film is tested for overall migration under EN 1186-1:2002; industrial non-food liners are specified against REACH Regulation (EC) No 1907/2006 and EU Directive 2011/65/EU. The main processing limitation is bubble instability when frost line height drops below 4 die diameters at high take-off speed, which creates transverse gauge bands and increases blocking tendency in collapsed film.

    What Limits Seal Strength in PE/PE Laminate Sealant Webs During Step-Down Gauge Transitions?

    In recyclable PE/PE flexible packaging, Braskem LH218 is used as the sealant web in gauges of 20 µm to 30 µm, laminated against a printed MDPE or HDPE outer web. The controlling variable is not ultimate heat seal force but the thickness tolerance of the sealant layer under transverse gauge transition. Seal initiation temperature for a butene LLDPE of 0.918 g/cm³ density typically sits between 95°C and 105°C, while the DSC peak melting point is near 122°C per ASTM D3418-21. A sealant formulation of 80 wt% LH218, 15 wt% LDPE with density 0.923 g/cm³, and 5 wt% anti-block masterbatch containing 5% synthetic silica reduces seal initiation temperature by 5°C to 8°C compared with neat LLDPE. The anti-block masterbatch is dosed to produce 2500 ppm silica in the final sealant layer. Hot-tack strength is measured per ASTM F1921 and seal strength per ASTM F88/F88M-21; typical seal strength for a 25 µm sealant web sealed at 130°C and 0.3 MPa for 0.5 s is expected to exceed 10 N/15 mm. Processing on a three-layer blown film line uses a die gap of 1.8 mm to 2.2 mm, blow-up ratio of 2.0:1 to 2.5:1, and melt temperature of 185°C to 205°C. The main limitation is that at 15 µm target gauge, a thickness variation of ±2 µm in the transverse direction can produce a 15% to 25% loss in hot-tack force due to reduced thermal mass under the seal bar. Recycled content in the sealant web should remain below 30 wt%; each 10 wt% addition of post-industrial LLDPE regrind tends to increase gel counts and reduce seal strength by 3% to 5%. Amine-based slip concentrates should be avoided in high-temperature lamination because their migration can produce seal contamination and variable coefficient of friction during pouch converting.

    Three-layer cast stretch film lines running at linear speeds of 400 m/min to 700 m/min require a core resin with controlled melt viscosity to prevent draw resonance and edge weave. LH218 is added into the core layer at 55 wt% to 70 wt% of total throughput, while the cling layer and release layer are formulated with metallocene polyethylene or polyisobutylene cling agents. Total film gauge is typically 12 µm to 23 µm, with cling layer thickness allocation of 8% to 12% of total gauge. Extruder barrel temperatures are set between 220°C and 260°C, the slot die gap is 0.5 mm to 0.8 mm, and the chill roll temperature is maintained at 15°C to 25°C. Corona treatment is applied at 1.0 kW/m² to 2.0 kW/m² to raise surface tension above 38 mN/m per ASTM D2578-23. Cling force measured by ASTM D5458 is usually controlled between 200 g and 450 g for a 20 µm film, and machine-direction elongation at break should exceed 400% per ASTM D882. The main failure mode on high-speed cast lines is melt resonance when the draw ratio exceeds 60:1 or when the melt temperature drops below 215°C, causing film thickness oscillation and inconsistent pre-stretch performance on pallet unitization equipment.

    Agricultural Silage Film: UV Stabilizer Loading and Film Ductility Retention

    Agricultural silage and bale-wrap films formulated with Braskem LH218 are produced in thicknesses from 150 µm to 200 µm, usually as three-layer blown films with white outer and black inner layers. The outer white layer receives 8 wt% to 12 wt% of a masterbatch containing 10% hindered amine light stabilizer and 5% UV absorber in a PE carrier, yielding a total HALS concentration of 0.4 wt% to 0.6 wt% and titanium dioxide concentration of 0.8 wt% to 1.2 wt%. The black inner layer is compounded with 3 wt% to 5 wt% of a 40% carbon black masterbatch. Processing on a three-layer blown film line with internal bubble cooling uses melt temperatures of 195°C to 215°C, blow-up ratio of 2.0:1 to 2.5:1, and frost line height of 7 to 10 die diameters. Weathering resistance is evaluated under ISO 4892-2:2013 or ASTM G154-23; films are typically required to retain at least 50% of initial tensile elongation after 2000 h of accelerated weathering. Terminal products include silage bales, agricultural stretch hoods, and greenhouse side curtains. Published data for this specific grade in long-term field exposure is limited; end users should validate UV stabilization in the target geography because additive depletion rates depend on thermal history, surface-to-volume ratio, and pesticide contact. The film should not be stored in contact with halogenated disinfectants or solvents because stress cracking can develop in stressed film folds under partial wetting.

    When FFS Lines Demand Bag Drop Impact Above 120 cm at −30°C

    On form-fill-seal lines for heavy-duty shipping sacks used in fertilizer, polymer pellet, and industrial chemical packaging, Braskem LH218 is employed as the impact-absorbing core layer in three-layer films with total thickness of 160 µm to 200 µm. The outer skin is an HDPE or MDPE layer at 15% to 20% of total gauge, the core is LH218 at 55% to 60% of total gauge, and the inner seal skin is an HDPE/MDPE layer at 20% to 25% of total gauge containing 2% to 3% slip and anti-block masterbatch. Extrusion is performed on a three-layer blown film line with a 200 mm to 300 mm die, internal bubble cooling, blow-up ratio of 2.0:1 to 2.5:1, and melt temperatures of 190°C to 210°C. Dart drop impact measured per ASTM D1709 Method B on a 180 µm film is commonly specified above 700 g, and tensile elongation at break should exceed 700% per ISO 527-3. Bag drop impact at −30°C is controlled by film ductility and seal geometry; side seal strength on FFS lines is measured after sealing at 150°C to 180°C using ASTM F88. The main bottleneck is that excessive melt temperature above 215°C reduces the molecular entanglement required for low-temperature impact retention, while too low a blow-up ratio below 1.8:1 increases machine-direction orientation and lowers transverse tear resistance. The table below gives a typical three-layer heavy-duty sack structure using LH218 as the core.

    LayerThickness allocationThickness at 180 µm totalResin/additiveFunction
    Outer skin15–20%27–36 µmHDPE or MDPE + 4–6% carbon black masterbatchAbuse resistance, printability
    Core55–60%99–108 µmBraskem LH218Impact and tear toughness
    Inner seal skin20–25%36–45 µmHDPE/MDPE + 2–3% slip/antiblockSealability, slip

    Frozen food packaging lines that run at −25°C storage and −40°C blast freezing require films with low-temperature seal integrity and resistance to stress cracking at fold lines. LH218 is converted into monolayer or three-layer frozen food pouches with total gauge from 40 µm to 80 µm. The seal layer should not be down-gauged below 20 µm, because below this thickness the failure mode shifts from peel to delamination under frozen compression loads. Seal strength is measured after conditioning at −20°C per ASTM F88; a 50 µm film sealed at 140°C and 0.35 MPa for 0.5 s typically retains at least 8 N/15 mm. Blown film processing uses a blow-up ratio of 2.2:1 to 2.8:1, melt temperature of 190°C to 205°C, and die gap of 1.8 mm to 2.2 mm. For direct food contact, the finished pouch must comply with FDA 21 CFR 177.1520 or Regulation (EU) No 10/2011, and extractives testing should be carried out under the intended frozen and reheating conditions because additive migration is temperature-dependent.

    On three-layer cast film lines producing liquid pouch films and overwrap, edge trim and roll start-up scrap containing Braskem LH218 are re-introduced in the core layer at 10 wt% to 20 wt% of total throughput. A continuous melt filter with 100 µm or 125 µm screens is installed upstream of the feedblock to limit gel seeds. Regrind addition above 30 wt% tends to raise visible gel counts above 5 defects per m² in thin-gauge film and reduces clarity. Extruder temperature profiles are kept between 220°C and 250°C, and the cast roll temperature is maintained at 18°C to 25°C. The main operational constraint is that inconsistent regrind particle size below 2 mm can create feeding surging and output variation of ±3% on a 300 kg/h cast line, which is visible as transverse gauge bands after stretching. The compliance matrix below summarizes regulatory anchors for typical downstream packaging applications.

    Target applicationRegulation or standardTest methodAcceptance limit
    Food-contact sealant webRegulation (EU) No 10/2011EN 1186-1:2002Overall migration 10 mg/dm²
    Food-contact film in USAFDA 21 CFR 177.1520Extractives per 21 CFROlefin polymer compliance
    Packaging waste heavy metalsDirective 94/62/ECDigestion and ICP-OESSum Pb, Cd, Hg, Cr(VI) 100 mg/kg
    RoHS restricted substancesDirective 2011/65/EUIEC 62321Pb 1000 mg/kg, Cd 100 mg/kg
    Free Quote

    Competitive Braskem LH218 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH218 Linear Low Density Polyethylene is a pelletized injection-moulding grade classified as a butene-comonomer linear-low-density polyethylene. The grade is specified in Braskem product literature with a nominal density of 0.918 g/cm³ when tested under ASTM D1505 and a nominal melt flow rate of 2.2 g/10 min at 190 °C and 2.16 kg load under ASTM D1238. These two values position LH218 in the moderate-flow, low-density segment of the Braskem polyethylene range; the combined property set supports injection moulding of caps, closures, thin-wall containers, housewares, toys, and general-purpose consumer goods. The linear backbone provides higher tensile and puncture resistance than branched low-density polyethylene at comparable wall thickness, while the density remains low enough to preserve impact toughness and flexibility. Braskem publishes typical values rather than formal specification limits for most mechanical properties; full molecular weight distribution, comonomer content, and batch-specific additive concentrations are not routinely disclosed in standard product literature.

    Because the resin is polymerized with a linear backbone and short-chain branches from butene, the melt rheology differs from both high-pressure LDPE and Ziegler-Natta or metallocene ethylene-hexene/octene copolymers. In injection moulding, the practical consequence is that flow length is governed primarily by molecular weight, melt temperature, and shear rate rather than by long-chain branching. LH218 does not exhibit the pronounced strain hardening that characterizes branched LDPE; this reduces bubble stability in blown-film operations and reduces melt tension, but it can improve dimensional repeatability in closed-mould filling.

    What Molecular Features Separate LH218 from High-Pressure LDPE?

    Long-chain branching in high-pressure LDPE creates a highly shear-thinning melt with elevated elasticity. LH218, by contrast, has a predominantly linear backbone; the short-chain branches supplied by butene disrupt lamellar crystallization without forming the long-chain branch network characteristic of autoclave or tubular LDPE. Capillary rheometry of comparable linear-low-density grades typically shows higher low-shear viscosity and lower extrudate swell than LDPE of the same ASTM D1238 melt flow rate. The lower extrudate swell reduces die-lip memory and can improve dimensional stability in injection moulded parts, but it also reduces melt elasticity and can increase sensitivity to gate blush if injection velocity is set excessively high. The density of 0.918 g/cm³ corresponds to unfilled polyethylene crystallinity in the 45–50% range, which is lower than injection-grade HDPE and contributes to lower flexural modulus but higher elongation at break.

    Under ASTM D638, the tensile yield strength of LH218 is typically reported near 10 MPa, whereas branched LDPE of similar melt flow rate may yield in the 8–9 MPa range depending on density and molecular architecture. The difference is attributable to the higher tie-molecule concentration accessible in linear polyethylene; tie chains connect adjacent crystalline lamellae and transfer load across amorphous regions. In product terms, a cap or container made from LH218 can often be designed with a thinner nominal wall than an LDPE equivalent when the failure mode is tensile, puncture, or repeated hinge flexing, provided rigidity does not control the application.

    Nominal Property Values and Corresponding Test Methods

    PropertyTest MethodTypical Value
    DensityASTM D15050.918 g/cm³
    Melt flow rate, 190 °C/2.16 kgASTM D12382.2 g/10 min
    Tensile yield strengthASTM D63810 MPa
    Tensile elongation at breakASTM D638>800%
    Flexural modulus, 1% secantASTM D790280 MPa
    Vicat softening temperature, 10 NASTM D152596 °C
    Hardness, Shore DASTM D224054
    Melting temperatureASTM D3418122 °C

    The values in the table are typical data drawn from public Braskem technical literature and are not to be interpreted as specification limits. Mechanical properties are determined on compression-moulded specimens; injection moulded parts may differ because of flow-induced orientation, cooling rate, and post-moulding crystallinity. If stiffness is the dominant design parameter, the 280 MPa flexural modulus is lower than injection-grade HDPE and must be compensated by ribbing or wall-section selection. The high elongation at break above 800% is characteristic of low-density linear polyethylene with butene short-chain branching and supports applications requiring ductility rather than rigidity.

    On production-scale injection moulding equipment, LH218 is typically processed with a general-purpose polyolefin screw having an L/D ratio between 20:1 and 22:1 and a compression ratio of 2.5:1 to 3:1. Barrel profiles are usually flat to slightly reverse from 180 °C in the rear zone to 210–230 °C at the nozzle; actual settings are adjusted to avoid excessive shear heating and to keep melt temperature within the recommended window. Melt temperatures above 230 °C are rarely necessary for thin-wall filling and may accelerate oxidative degradation if residence time is prolonged. Injection velocity should be established by short-shot analysis on the target tool. For thin-wall closures with nominal wall thickness from 0.8 mm to 1.5 mm, fill speeds producing hydraulic injection pressures in the 70–100 MPa range are generally suitable, but hot-runner systems with restricted gate diameters below 0.8 mm can require higher pressures. Hold-pressure time must extend beyond gate freeze; premature hold release in LLDPE can produce sink marks because the solidifying layer is less stiff than in filled or high-density grades.

    Mould temperature control in the 20–40 °C range is standard for unfilled LLDPE. Nonuniform cavity cooling creates differential shrinkage and warpage in flat closures and container bases. LLDPE of 0.918 g/cm³ density typically displays mould shrinkage in the 1.5–2.0% range, but thin-wall parts may shrink less because of orientation and rapid cooling. Drying is not mandatory for virgin material stored at ambient relative humidity below 60%. If sacks are opened in high-humidity environments, surface moisture may produce splay; a dehumidified-air hopper dryer at 60–70 °C for 2 h is generally sufficient. Purging between resins with different density or melt index should follow the machine manufacturer’s procedure; a low-MFR polyethylene or commercial purging compound is used to reduce contamination in hot-runner drops.

    When Downgauging from LDPE to LH218 is Considered for Thin-Wall Packaging

    Substitution of branched LDPE by LH218 is technically justified when the part is ductility-limited rather than stiffness-limited. For a closure or cap that must resist cracking at the hinge or thread root, the linear backbone and higher elongation at break under ASTM D638 provide an advantage at equivalent wall thickness. In container bodies where sidewall deflection under top load is the failure mode, the lower flexural modulus relative to HDPE becomes the controlling variable; wall thickness reduction without adding ribs may produce unacceptable deformation even though tensile yield strength is adequate. The melt flow rate of 2.2 g/10 min is sufficient for many multi-cavity tools, but shear-rate-dependent viscosity data should be obtained when runner lengths exceed 200 mm or when hot-runner manifold balance is critical. Because LH218 exhibits less shear thinning than LDPE, flow length is less sensitive to injection velocity, and gate blush often becomes the upper boundary for fill speed.

    Relative to octene-LLDPE grades, LH218 has a shorter comonomer branch length. Butene short-chain branching is less efficient at tying adjacent crystalline lamellae; at equivalent density and MFR, octene-LLDPE typically yields higher dart impact and environmental stress crack resistance. The trade-off is often processability and cost. LH218’s 2.2 g/10 min MFR positions it for injection moulding, whereas many octene grades with comparable mechanical performance have lower MFR and require higher injection pressures. For applications where environmental stress crack resistance in aggressive surfactant-containing products is critical, a hexene or octene grade may be preferred even if it forces a higher melt temperature.

    Published quantitative ESCR data for LH218 under ASTM D1693 are limited; designers should request testing for aggressive detergent-alcohol environments. For food-contact applications, Braskem technical literature should be consulted for the current regulatory statement. Olefin polymer grades of this type are commonly evaluated against FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, but specific conditions of use, overall migration limits, and organoleptic requirements depend on the packaged formulation and service temperature.

    Short-term tensile tests alone do not capture long-term failure in snap-fit assemblies. For a snap-fit cap, the strain at the snap-fit undercut should be compared with the material’s yield strain; LH218’s yield stress of 10 MPa and low flexural modulus imply that snap-fit retention is governed by geometry rather than material stiffness. Fatigue life under repeated hinge flexing is generally superior to brittle HDPE alternatives, but published flexural fatigue data for LH218 are limited; component-level testing is recommended. Creep at ambient temperature is higher than HDPE because of lower crystallinity; designers should not rely on sustained torque retention in high-temperature closures without accelerated creep testing.

    Typical injection moulding defects observed with this MFR/density combination include gate blush, splay from damp pellets, and warp from unbalanced cooling. Gate blush tends to appear when injection velocity is increased to solve a short shot; reducing injection acceleration or enlarging the gate often resolves the defect without raising melt temperature. Splay is frequently traced to surface moisture rather than degradation; if drying does not eliminate splay, the next variable to examine is nozzle drool or hot-runner contamination. Warp in flat lids often results from asymmetrical cooling; differential mould temperature can be adjusted before changing material fill rate.

    Operational boundaries include a recommended upper melt temperature near 260 °C; prolonged residence above this threshold can initiate oxidative chain scission or crosslinking even with the incorporated stabilizer package. The additive package is not intended to provide long-term weathering. Outdoor exposure of unpigmented LH218 can lead to UV embrittlement unless a carbon-black masterbatch or HALS/UV-stabilizer system is incorporated. Mixing with halogenated polymers such as PVC or with acetal resins in the same machine is to be avoided because their decomposition products can corrode tooling and degrade the polyethylene at processing temperature. For applications requiring higher stiffness, HDPE injection grades with density above 0.952 g/cm³ offer a more direct performance upgrade than LH218; conversely, HDPE’s lower elongation and higher flexural modulus can be disadvantageous in closures requiring repeated hinge flexing. The selection between LH218 and higher-density resins is therefore governed by the ratio of flexural modulus demand to impact or elongation demand, not by melt flow rate alone.