Braskem Lh218 Cast Film Extrusion Linear Low Density Polyethylene

Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 549422
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 2.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Haze 3%
    Gloss 45 85
    Coefficient Of Friction 0.20
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g

    As an accredited Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH218 is typically supplied in 25 kg polyethylene-lined bags on pallets, with 1,000 kg bulk bags available.
    Container Loading (20′ FCL) 20′ FCL: Braskem LH218 Cast Film Extrusion LLDPE resin, palletized 25 kg bags, moisture-protected, evenly distributed, securely braced for ocean shipment.
    Shipping Braskem LH218 LLDPE ships as non-hazardous resin pellets, typically in 25 kg bags, bulk bags, boxes, or railcars. It is not regulated for transport per applicable regulations. Keep containers sealed, dry, clean, and away from heat, sunlight, moisture, and oxidizing agents. Handle with normal industrial hygiene.
    Storage Store Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing agents. Keep containers or bags closed to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and static buildup. Stack pallets securely and follow local regulations and supplier recommendations. Protect from UV radiation. Use appropriate grounding.
    Shelf Life Braskem LH218 Cast Film Extrusion LLDPE: 24-month typical shelf life stored cool, dry, away from direct sunlight in unopened packaging.
    Application of Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene

    On pallet-wrapping lines running at 45–60 wraps/min, machine stretch film based on Braskem LH218 is extruded at 10–23 µm gauge and supplied in 400–500 mm wide rolls for hand and machine application. LH218 enters at nominal density 0.918 g/cm³ according to ASTM D792 and nominal melt mass-flow rate 2.0 g/10 min according to ASTM D1238 at 190°C/2.16 kg. The cast line is typically a 2,000–3,500 mm external-deckle die equipped with a 100/150/100 mesh screen pack and a barrier single screw with 30:1 L/D. Melt temperature at the feedblock is held at 235–260°C, die gap is set to 0.8–1.3 mm, and primary chill roll temperature is 20–28°C with a 6–10°C secondary roll differential to control web flatness and blocking tendency.

    Formulation for machine stretch webs uses 80–90 wt% LH218, 5–10 wt% metallocene plastomer, 2–5 wt% polyisobutylene tackifier, 500–1,200 ppm erucamide slip, and 0.5–1.5 wt% synthetic silica antiblock. The tackifier is concentrated in the outer layer of a three-layer coextrusion, leaving the core layer tougher and the inner surface smoother for consistent roll release. Cling force is measured by ASTM D5458, and tensile elongation at break is measured by ASTM D882. In machine-applied pallet wrap, a minimum elongation at break of 300% in both machine and transverse directions is commonly specified. The processing conflict is that excess tackifier above 5 wt% raises outer-roll blocking force, and film telescoping occurs at the winder when cling force exceeds unwind tension during acceleration. Coefficient of friction is monitored by ASTM D1894 to maintain controlled unwind without shedding layers in transit.

    Edge trim regrind is returned at 10–20 wt%. Above 20 wt% regrind, gel defects become visible in 10 µm film as unoriented inclusions, and draw resonance appears as periodic gauge bands if haul-off speed exceeds 400 m/min while melt strength is low. Pre-drying is not required, but standing wet resin exposed to relative humidity above 60% should be avoided because surface water on pellets creates voids that weaken thin-gauge webs. Industrial pallet wrap is not food-contact; EU shipments require REACH SVHC documentation under Article 33 when the final article contains candidate-listed additives. Terminal products include hand rolls, machine rolls, and perforated pallet wrap for automated depalletizing lines.

    What Limits Calcium Carbonate Loading in Cast Extrusion of Breathable Hygiene Backsheets?

    Breathable cast precursor films for diaper backsheets are compounded from LH218 and calcium carbonate masterbatch at loadings of 45–60 wt% CaCO3. The calcium carbonate is 1.0–2.0 µm median particle size with stearic acid surface coating to reduce agglomeration. The precursor is produced as a cast web at 20–35 µm, then uniaxially oriented on a machine-direction orientation unit with draw ratios of 2.5:1–3.5:1 at preheat roll temperatures of 55–80°C and annealing roll temperatures 80–100°C. The drawing step creates microvoids around the mineral particles; water vapour transmission rate is measured by ASTM E96/E96M at 38°C and 90% RH. Typical hygiene backsheet specifications fall between 1,500 g/m²/day and 5,000 g/m²/day, depending on CaCO3 loading and final oriented gauge.

    The limiting loading of CaCO3 is not extruder torque alone but orientation stability after the MDO unit. At 60 wt% CaCO3, the web becomes sensitive to pinhole formation and edge fibrillation when the draw ratio exceeds 3.0:1. Below 45 wt% CaCO3, void formation is insufficient for typical MVTR requirements above 1,500 g/m²/day. The cast film die gap is widened to 1.5–2.0 mm because the mineral-filled melt has lower melt strength and higher die swell. Screw speed is lowered 10–20% relative to unfilled cast film, and melt temperature is limited to 210–240°C to reduce degradation of the surface treatment on the mineral. Processors monitor die pressure and screen-pack pressure drop because published data for this specific configuration is limited. Skin-contact hygiene materials are assessed under ISO 10993-5 and ISO 10993-10; the final backsheet must be non-cytotoxic and non-irritating. Terminal products include diaper backsheet, adult incontinence waistbands, and feminine hygiene outer covers.

    For fresh-cut produce and tray-sealed modified-atmosphere packs, a 25 µm cast lidding web is coextruded with LH218 as the sealant skin over a PP or PET rigid tray. The formulation for the sealant skin contains 85–95 wt% LH218, 5–15 wt% LDPE or metallocene plastomer, 0.3–1.0 wt% food-grade anti-fog agent, and 500–1,000 ppm slip. The anti-fog reduces condensed droplets under 4°C refrigerated display; light transmission and haze are measured by ASTM D1003, while seal strength is measured by ASTM F88/F88M after 0.4–0.6 s dwell at 1.8–2.2 bar. The cast line uses a 1,500–2,000 mm die, 0.7–1.1 mm die gap, melt temperature 230–255°C, and primary chill roll 18–25°C.

    The most critical non-conformance is migration of erucamide slip to the seal interface. At slip levels above 1,000 ppm or after 14 days of ambient ageing, heat seal strength measured by ASTM F88/F88M can fall below the packaging line’s minimum acceptable burst value. On high-speed tray lines running 60–80 packs/min, seal initiation must remain below 110°C; excessive slip or heat history shifts seal initiation upward. The anti-fog additive must be listed in EU Regulation 10/2011 Annex I for EU sales. US food-contact status is covered under FDA 21 CFR 177.1520, with use conditions in 21 CFR 176.170(c) for aqueous, acidic and low-alcohol foods up to the specified temperature-time profile. Oxygen transmission rate is crop-specific and is measured on the finished lidding web by ASTM D3985 at 23°C and 0% RH. Gauge variation above ±5% across the web creates uneven sealing and tray leakers at the corners. Terminal products include lidding film for mushroom trays, fresh-cut salad packs, and berry punnets.

    Regulatory and test matrix for LH218 cast film application segments
    Application segmentStandard/RegulationTest method / clauseTypical control boundary
    Machine stretch filmREACH Article 33SVHC documentationNo food-contact; candidate-list check
    Hygiene backsheetISO 10993-5 / ISO 10993-10Cytotoxicity / skin irritationNon-cytotoxic, non-irritating
    Food lidding webFDA 21 CFR 177.152021 CFR 176.170(c)Conditions of use for aqueous, acidic, low-alcohol foods
    Surface protection filmRoHS Directive 2011/65/EUASTM D3330/D3330MPeel adhesion 0.05–1.5 N/cm
    HFFS sealant webEU Regulation 10/2011EN 1186 / ASTM F88/F88MOverall migration ≤ 10 mg/dm²; seal strength set by line
    Agricultural silage wrapASTM D4329 / ISO 4892-2Accelerated weatheringUV retention for 12–18 months outdoor field service
    Frozen food webFDA 21 CFR 177.1520ASTM D1709 Method ADart impact at -40°C conditioning prior to test

    When LH218 is Extruded Below 15 µm as a Masking Web for Polished Metals and Glass

    Surface protection webs below 15 µm are run under low-shear screw configurations and low backpressure because shear heating narrows the processing window. Melt temperature is held at 210–240°C, die gap at 0.4–0.8 mm, and primary chill roll at 15–22°C with a polished or matte finish. The film is corona-treated in line to 40–42 mN/m wetting tension measured by ASTM D2578, then coated with a pressure-sensitive adhesive or coextruded with an acid-modified polyolefin skin. Low-tack protective articles are specified by peel adhesion measured on stainless steel by ASTM D3330/D3330M, with production ranges from 0.05 N/cm for high-gloss PMMA to 1.5 N/cm for textured aluminum.

    Neck-in and edge bead are the dominant process failures below 10 µm. The extrudate is pinned at the die edges with electrostatic edge pinning, and the draw ratio is set to 10:1–25:1 from die gap to final film gauge. Below 8 µm, draw resonance produces transverse thickness bands that interfere with uniform peel force. Gauge variability is measured by a non-contacting capacitance gauge and controlled to ±5% of nominal. Reclaimed edge trim is blended at 5–15 wt%; higher levels introduce gel and optical defects that become visible on polished substrates. Electronics protection articles require RoHS Directive 2011/65/EU compliance and customer-specific halide-free specifications. Terminal products include protection films for stainless steel appliances, glass sheets, polycarbonate panels, and coated metals during laser cutting or UV printing.

    High-Speed HFFS Sealant Thermodynamics in LH218-Based Cast Webs

    When LH218 is employed as the sealant skin in a three-layer cast film for horizontal form-fill-seal lines running 80–120 packs/min, the processing focus shifts from optical haze to seal initiation and hot tack under short dwell. The sealant skin is blended with 10–30 wt% metallocene plastomer with density 0.902–0.910 g/cm³ to lower seal initiation below 110°C. The core layer uses 0–20 wt% reclaimed edge trim and may include HDPE for stiffness if gauge exceeds 45 µm. The cast line uses an internal deckle die of 1,200–2,000 mm, 0.7–1.2 mm die gap, melt temperature 230–255°C, and a chill roll with matte texture to prevent air entrapment.

    Hot tack is measured by ASTM F1921 at 0.3 s dwell and 0.5–2.0 bar seal pressure, while final seal strength is measured by ASTM F88/F88M. The technical boundary is additive migration: erucamide slip loads above 1,000 ppm and long roll ageing can reduce seal strength at dwell times below 0.3 s because bloom transfers to the sealing interface. Processors therefore split the slip additive, placing 200–600 ppm in the sealant skin and the balance in the outer layer. Coefficient of friction is measured by ASTM D1894 and maintained at 0.20–0.40 kinetic, while haze is measured by ASTM D1003 and kept below 8% for clear overwrap. Oxygen barrier is provided by lamination to PET, BOPP, or aluminum foil; the cast sealant web is not the barrier layer.

    Food-contact grades for HFFS structures require FDA 21 CFR 177.1520 and EU Regulation 10/2011 compliance with overall migration tested by EN 1186 at the intended processing and shelf conditions. Terminal products include snack-bar flow packs, confectionery cold-seal overwrap, frozen seafood pouches, and zipper bags, where the sealant must be compatible with resealable zipper profiles without loss of seal force at the zipper interface.

    Agricultural silage wraps produced from LH218 are extruded at 25–35 µm gauge and 500–750 mm width for round and square bale wrapping machines. The formulation includes 1–4 wt% polyisobutylene tackifier, 0.05–0.20 wt% hindered amine light stabilizer package, and 0.3–1.0 wt% UV absorber. Since the film is stretched on the baling machine at 55–70% pre-stretch, tensile behaviour under high-speed stretch is the first release criterion. Elongation at break measured by ASTM D882 commonly exceeds 400% in the machine direction, but the application force at 50% pre-stretch is also recorded with a bale-wrapper load cell to ensure compatibility with the machine.

    The primary field failure is loss of cling due to dust accumulation and UV embrittlement at the film edges after 12–18 months. Accelerated weathering by ASTM D4329 or ISO 4892-2 is used to verify ultraviolet resistance, but published data for LH218-specific UV formulations is limited. Pre-drying is not required, though wet pellets from outdoor silos can introduce voids. The cast film conditions are similar to stretch film: melt temperature 240–270°C, die gap 0.8–1.2 mm, primary chill roll 20–25°C, and edge trim return at 10–20 wt%. Terminal products include round bale silage wraps, haylage films, and maize silage bale covers.

    A 70 µm Cast Web for Frozen Food Withstands Dart Impact at −40°C

    Vertical form-fill-seal lines for frozen vegetables and seafood demand cast webs with low-temperature ductility down to -40°C. The structure uses 80–90 wt% LH218 with 10–20 wt% ethylene-vinyl acetate or ULDPE to reduce brittle failure and improve dart impact. The final film thickness is 40–80 µm to resist ice-crystal puncture and seal-bar pressure. Dart impact is measured by ASTM D1709 Method A after conditioning at -40°C; tear resistance is measured by ASTM D1922 and tensile elongation by ASTM D882. The cast line runs a 1,500–2,500 mm die, 0.8–1.5 mm die gap, melt temperature 235–260°C, and primary chill roll 18–25°C.

    The operational boundary is regrind return. Frozen food web is often coloured white or printed, so gels and charred trim from regrind above 20 wt% become visible and reduce seal integrity. Extruder screens of 80/120/120/80 mesh and a gear pump are recommended to stabilize output and reduce melt-temperature variation to ±3°C. Food-contact status is covered under FDA 21 CFR 177.1520 and EU Regulation 10/2011; cold-temperature performance is not a regulatory requirement but is set by distribution risk assessment. Terminal products include frozen vegetable pillow packs, seafood pouches, and ice cream overwrap.

    Free Quote

    Competitive Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH218 cast film extrusion linear low density polyethylene is a butene-comonomer LLDPE supplied as natural pellets. The grade is controlled to a nominal density of 0.918 g/cm³ per ASTM D1505 and a melt mass-flow rate of 2.0 g/10 min per ASTM D1238 at 190 °C with a 2.16 kg load. Because the resin is specified for chill-roll cast film, it is used in monolayer and coextruded structures where rapid quench from the melt produces low haze and a smooth surface. The product’s butene short-chain branch structure provides a balance of puncture resistance, tear resistance, and seal performance distinct from LDPE or high-alpha-olefin metallocene LLDPE. On a typical cast-film extrusion line, LH218 is processed through a coathanger die onto a polished chill roll; the quench rate, air gap, and roll finish materially affect film crystallinity and optics. The absence of long-chain branching reduces melt elasticity relative to LDPE, so edge pinning and air-knife settings must be adjusted to maintain a stable melt curtain.

    How does butene short-chain branching influence shear viscosity and melt-curtain stability?

    The short-chain branches in LH218 are primarily ethyl branches derived from butene comonomer. These branches disrupt polyethylene crystallite formation, lower the melting point, and reduce the driving force for secondary crystallization. In capillary rheometry according to ISO 1133-1:2022 or ASTM D1238, the melt flow rate is a single-point viscosity-related measurement; it does not capture the shear-thinning response. Production-scale cast-film experience indicates that a butene LLDPE with a 2.0 g/10 min melt index displays less extensional strain hardening than an autoclave LDPE at equivalent melt temperature. This behavior reduces die swell but also requires a narrower air gap and more aggressive edge pinning when the melt curtain is drawn to thin gauge. The onset of draw resonance is typically reached at lower draw ratios for LLDPE than for LDPE, so maximum line speed on a given cast-film line is generally lower unless the die lip and air knife are configured for linear resin. These effects are monitored on line by measuring neck-in, edge bead thickness, and melt curtain position. Operators record fluctuations in die pressure and chill-roll amperage as indirect indicators of melt homogeneity. For LH218, die pressure on a 75 mm extruder with a 30:1 L/D screw is typically lower than for LDPE because of the shear-viscosity curve; however, specific pressure values must be established for each screw design, die width, and throughput.

    On a 75 mm single-screw extruder with a 30:1 L/D barrier screw and a 1200 mm coathanger die, starting conditions for LH218 can be set with feed zone at 180–200 °C, compression zones increasing to 230–240 °C, adapter at 240–250 °C, and die at 245–260 °C. The chill roll is typically maintained at 15–30 °C with a closed-loop water temperature controller. Die gap is set between 0.5 mm and 0.8 mm, and the air gap between die exit and chill roll is held at 15–25 mm. These settings are starting points and must be adjusted for gauge, line speed, and coextrusion structure. In field operation, instability at the die lip often appears as edge weave or curtain sag when the air gap exceeds 30 mm, while chill-roll sticking is more common when the roll temperature falls below 10 °C or when the film contains no antiblock. Melt curtain rupture at the edges is observed when die-lip temperature is below 220 °C or when the die gap is too narrow for the target throughput. Accumulation of low-molecular-weight material on the die lip is controlled by purging with a higher-viscosity polyolefin or by maintaining a stable die-temperature profile. The extruder screw speed is adjusted to maintain a constant die pressure and melt temperature; an overheated melt can produce gel specks in the film that are quantified by ASTM D3351.

    Optical and sealing property matrix in chill-roll film converting.

    For cast-film polyethylenes, optical properties are evaluated by ASTM D1003 for haze and ASTM D2457 for 45° gloss. In the cast-film process, quenching on a polished chill roll suppresses spherulite growth and surface roughness, so a 25 µm LLDPE film of density 0.918 g/cm³ commonly yields haze below 5% and 45° gloss above 70; grade-specific values for LH218 must be measured on the target line because cooling configuration and chill-roll finish dominate optics. Heat-seal performance is assessed by ASTM F88 for seal strength and ASTM F2029 for seal initiation temperature. Butene LLDPE at this density typically exhibits seal initiation in the range of 100–110 °C, which is higher than a metallocene hexene or octene LLDPE of equivalent density and melt index. This difference arises from the heterogeneous distribution of short-chain branches in Ziegler-Natta butene resins, which leaves some polymer chains with very low branch content and therefore higher melting domains. The sealing window is therefore narrower than a homogeneous metallocene LLDPE, and hot-tack performance may be lower. In practice, LH218 is combined with a lower-melting skin layer in coextruded structures when seal initiation below 100 °C is required. Puncture resistance and tear resistance of cast-film samples are evaluated by ASTM D1709 and ASTM D1922; those values depend strongly on film thickness, chill-roll temperature, and orientation balance. Published data for LH218-specific cast film at all thicknesses is limited, so converter trials are required for specification and capability studies.

    When a C₆ or C₈ metallocene LLDPE replacement is under evaluation for downgauging.

    Replacement of LH218 with a hexene- or octene-based metallocene LLDPE at equal density and melt index is not a drop-in change. Metallocene catalysts distribute comonomer more uniformly across the molecular weight distribution, yielding lower seal initiation temperature, higher dart impact, and higher Elmendorf tear per unit thickness than a conventional butene Ziegler-Natta LLDPE. The metallocene resin also has a more linear chain architecture and typically a narrower molecular weight distribution, which lowers melt strength and increases draw resonance sensitivity on cast-film lines. LH218 may tolerate higher melt temperatures without shear-induced gel formation because of its broader molecular weight distribution and stabilizer package; however, the exact boundary must be confirmed by gel counting per ASTM D3351 and by monitoring die-lip deposits. When a converter evaluates downgauging, the target film property is usually dart impact by ASTM D1709 or puncture resistance by ASTM D5748, both of which are lower for a butene LLDPE than for an octene metallocene at equal gauge. This does not make LH218 unsuitable; it means the film structure must be adjusted with a coextruded high-toughness skin or a higher gauge to meet the same distribution and end-use performance. Published comparative data for LH218 against specific metallocene grades may be limited because film properties are strongly affected by die gap, air gap, chill-roll finish, and orientation. Comparative trials on the intended cast-film line with identical die and roll settings are therefore necessary before selecting a substitute.

    Because LH218 is a linear low density polyethylene without long-chain branching, the melt has a lower elastic memory than LDPE and exits the die with reduced die swell. This helps maintain tight thickness uniformity across the web but increases the sensitivity of the melt curtain to air currents and slight die misalignment. In coextruded cast-film structures, LH218 is used in skin or core layers depending on the required sealing and toughness balance. When used as a core layer, the resin provides stiffness and abuse resistance while the skin layers may be a metallocene LLDPE for low seal initiation or an EVA copolymer for hot tack. When used as a skin layer, the chilled surface produces a smooth and clear outer layer but may require an antiblock masterbatch to prevent roll blocking during slitting. Antiblock addition levels for cast LLDPE typically range from 1000 ppm to 5000 ppm of synthetic silica, depending on film gauge and storage conditions. Slip additives such as erucamide or oleamide are used at 0.05–0.15 wt% to reduce coefficient of friction, measured by ISO 8295 or ASTM D1894. These additives migrate to the film surface over time; inline coefficient-of-friction values are therefore not stable until migration is complete, which can require 24–72 h at ambient conditions. The use of an antiblock or slip masterbatch changes die-lip deposit behaviour and can shorten the interval between die-face cleanings on high-output lines.

    Regulatory compliance and food-contact substance status under EU and US frameworks.

    The resin is an olefin polymer intended for food-contact applications when the finished film complies with the applicable national and regional requirements. The table below lists typical conformity positions for a polyethylene cast-film grade of this type; the current Braskem regulatory data sheet should be consulted for the specific product lot and application.

    FrameworkStandard or clauseTypical LH218 position
    Melt flow rateASTM D1238 / ISO 1133-1:20222.0 g/10 min at 190 °C, 2.16 kg
    DensityASTM D15050.918 g/cm³
    US food contact21 CFR 177.1520(c) 3.1a and 3.2aOlefin polymer; conditions of use to be determined by the finished article and food type
    EU food contactRegulation (EU) 10/2011 as amendedCompliance is assessed through overall migration limit of 10 mg/dm² for the final film and specific migration limits for additives
    REACH SVHCRegulation (EC) 1907/2006No candidate-list SVHC above 0.1% w/w in the substance as supplied
    Packaging heavy metalsDirective 94/62/EC and CONEG model legislationSum of lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg in packaging material

    This matrix is a general compliance checklist; the end-use film may also require compliance with specific clauses such as 21 CFR 177.1520(c) 3.1a for food types above 120 °C or Regulation (EU) 10/2011 Annex I migration testing with food simulants. Those requirements depend on the film structure, additives, and conversion conditions, not solely on LH218.

    Routinely, LH218 is blended with up to 20 wt% LDPE to increase melt curtain stability and to widen the processing window on older cast-film lines that lack an air knife or automated edge pinning. The addition of LDPE introduces long-chain branching and reduces draw resonance, but it also raises haze and may reduce dart impact if the LDPE fraction exceeds 20 wt%. Blending is performed either by dry blending pellets at the hopper or by using a preblended pellet. A dry blend can separate during conveying over long distances, producing gauge bands and variable melt pressure. The use of a gravimetric blender with mass-flow calibration is recommended to maintain blend ratio within ±0.5 wt%. On high-speed cast-film lines above 200 m/min, the blend ratio is often reduced because the high draw tends to orient the film and the increased melt strength of LDPE is less necessary. For antimicrobial or colour masterbatches, the carrier resin should be selected from a polyolefin compatible with LLDPE to prevent die-lip deposit and film defects. The addition rate for colour concentrates is typically 2–4 wt%, but the exact value depends on pigment loading and required opacity.

    What are the documented operational boundaries for melt temperature, die-lip deposit, and gel specks?

    Melt temperature is the primary control for gel formation and film quality. At die-exit melt temperature below 215 °C, a 2.0 g/10 min butene LLDPE may show incomplete melting or pressure fluctuations unless screw speed is reduced; at melt temperature above 285 °C, oxidative degradation promotes the formation of gel particles and can increase odour and colour. The gel particles are measured by ASTM D3351 and are reported as size and number per area. Die-lip deposit formation is accelerated when slip additives are present at the higher end of the dose range and when the die lip is operated above 270 °C. On a 1200 mm cast-film die, continuous production with a 0.1 wt% erucamide masterbatch may require die-lip cleaning every 8–12 h; the cleaning interval is shorter if the die-lip profile is nonuniform. Chill-roll fouling is another operational boundary. Low-molecular-weight additive bloom can transfer to the chill roll and cause optical defects in the web. The roll is cleaned with solvent or alkaline detergents, but the cleaning method must be compatible with the roll surface finish. A closed-loop chill-roll temperature control within ±1 °C is critical because higher temperature variation produces visible transverse bands of haze and gloss.

    For coextruded cast film structures in which LH218 is used as a core layer between metallocene LLDPE skins, the layer ratio is commonly 10–20% skin and 60–80% core, with tie layers used only when polar barrier polymers are present. This construction places the higher-toughness or lower-sealing resin at the surface where the seal bar contacts the film, while the LH218 core contributes body and stiffness. The die and feedblock temperatures must be balanced because the metallocene skin has a different shear-viscosity curve than LH218; a melt-temperature difference greater than 10–15 °C between layers can produce interfacial flow instabilities that appear as wavy film edges and inconsistent seal strength. In cast-film coextrusion, individual layer melt streams are joined in the feedblock before the die, so viscosity matching is more important than in blown-film coextrusion. If the skin-layer resin has a much lower viscosity than the LH218 core, it may encapsulate the core and create die-lip deposits; if the skin is more viscous, the core may migrate to the film surface. These defects are detected by cross-sectional microscopy or by differential scanning calorimetry of separated layers. Standard practice is to select skin resins with melt flow rates within ±1.0 g/10 min of the LH218 core or to adjust melt temperatures to bring apparent viscosities closer. The line speed, chill-roll temperature, and air gap are then adjusted to maintain gauge uniformity. This coextruded configuration is used for packaging films where low seal initiation and high puncture resistance are simultaneously required.

    Top