Braskem Lh118 Linear Low Density Polyethylene

Braskem LH118 Linear Low Density Polyethylene

    • Product Name: Braskem LH118 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 934257
    Product Name Braskem LH118 Linear Low Density Polyethylene
    Manufacturer Braskem
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm3
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 24 MPa
    Elongation At Break 800 %
    Flexural Modulus 240 MPa
    Haze 12 %
    Gloss 45 60
    Dart Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Coefficient Of Friction 0.20
    Antioxidant Yes
    Slip No
    Antiblock No

    As an accredited Braskem LH118 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH118 Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL: Braskem LH118 Linear Low Density Polyethylene, 25 kg bags, palletized, securely loaded, approx. 18–20 MT net.
    Shipping Braskem LH118 Linear Low Density Polyethylene is typically shipped as nonhazardous resin pellets in 25 kg moisture-resistant bags or bulk containers, palletized and stretch-wrapped. Transport in clean, dry trucks, railcars, or containers. Store under cover, away from sunlight, heat, moisture, and contamination. Do not puncture bags.
    Storage Store Braskem LH118 Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers or bags closed, off the floor on pallets, and protected from moisture, oils, and contaminants. Avoid excessive stacking and prolonged UV exposure. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life: 24 months from production when stored in original, unopened packaging, dry, away from direct sunlight, heat and contamination.
    Application of Braskem LH118 Linear Low Density Polyethylene
    During five-layer cast stretch film extrusion on a 75 mm barrier screw with 30:1 L/D ratio, Braskem LH118 is introduced into the middle layer at 15–25 wt% of total film weight. The grade is specified with nominal melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 and density of 0.918 g/cm³ per ASTM D1505-18. In this position, LH118 provides higher melt strength than a 2.0 g/10 min metallocene LLDPE and contributes to control of neck-in when the melt curtain exits a 0.6–0.8 mm die gap. Extruder barrel setpoints from feed throat to melt adapter are commonly held at 180 °C, 210 °C, 230 °C, and 245 °C; the chill roll temperature is fixed between 18 °C and 24 °C to reduce blocking while retaining cling transfer.A common formulation for a 23 µm machine film is 60 wt% metallocene LLDPE at 0.918 g/cm³ and 2.0 g/10 min, 25 wt% LH118, 10 wt% high-pressure LDPE at 0.923 g/cm³ and 0.8 g/10 min, and 5 wt% polyisobutene tackifier masterbatch. Cling is measured as peel force after 24 h conditioning at 23 °C under 50% relative humidity using ASTM D5458-12; films stored below 5 °C commonly exhibit cling force reduction greater than 25% because polyisobutene migration to the surface is retarded at lower temperature. Edge trim from this structure can be reintroduced at up to 15 wt% in the core layer, though trim derived from high-butene LLDPE structures may raise haze above 3.5% measured by ASTM D1003-13.Line speed is the principal processing conflict for cast film using LH118 in the core. At speeds above 600 m/min, transverse-direction thickness variation increases unless edge pinning and vacuum box settings are adjusted. Published data for LH118 at speeds above 800 m/min in this exact five-layer configuration is limited. On lines equipped with 700–1000 mm diameter chill rolls, winder tension is normally set to 12–17 N/m of web width to prevent telescoping and hard roll edges. End products include pre-stretched hand wrap, turntable wrap, and machine film; puncture resistance tested by ASTM D5748-19 and load retention by ASTM D5459-12 should be verified on the finished roll rather than predicted from dart impact data alone.

    What Limits LH118 Loadings in Three-Layer Frozen-Food Blown Film?

    Three-layer frozen-food lines running sealant skins of Braskem LH118 on a 250 mm die typically set die gap between 1.6 mm and 2.2 mm, blow-up ratio from 2.2 to 2.8, and frost line height of 500–750 mm above the die exit. The sealant layer usually represents 25–35 wt% of total film thickness, with the core and outer skin containing metallocene LLDPE or EVA for low-temperature impact resistance. Melt temperature at the adapter is maintained at 190–215 °C; operation above 230 °C leads to visible gel formation in the sealant layer after 4–6 h of continuous running on production-scale lines.Seal performance is evaluated on vertical form-fill-seal machines with dwell times between 0.2 s and 0.4 s. Heat seal initiation for a 70 µm film containing 30 wt% LH118 in the sealant layer is typically observed between 105 °C and 120 °C; below 105 °C, the failure mode shifts from cohesive peel to interfacial peel, which is unacceptable for frozen-food pouches handled at −25 °C. Hot tack force measured under ASTM F1921-12 at 0.2 s dwell is generally lower than a metallocene LLDPE reference; therefore LH118 is used as a sealant modifier rather than a direct replacement when package fill weights exceed 1 kg.Direct food contact compliance for the finished film must satisfy 21 CFR 177.1520(c)3.1 for olefin polymers. The applicable extractive limits depend on food type and use condition; frozen foods generally fall under use condition E or F. For export to EU markets, the film must also meet the overall migration limit of 10 mg/dm² under EU Regulation 10/2011, with fatty food simulant D2 at 20 °C for 10 days or equivalent test conditions. End products include printed pillow pouches for IQF seafood, vegetables, and marinated meat portions.Rotating wrapper arms on silage bale applicators expose LH118-based films to pre-stretch tensions above 70% elongation, which creates a specific set of retained mechanical requirements not captured by standard cast-film cling tests. A typical three-layer formulation for a 25 µm high-tension wrap uses 65 wt% Braskem LH118, 20 wt% high-pressure LDPE, 10 wt% metallocene LLDPE, and 5 wt% UV/colour masterbatch. The blown film line is run with a 2.5 m die circumference, melt temperature between 190 °C and 215 °C, and blow-up ratio of 2.0–2.4 to balance tear propagation in machine and transverse directions.EN 13206:2017 is the reference specification for bale wrap films in the EU; it sets requirements for retained elongation at break, puncture resistance, and cling after UV exposure. The weathering stabiliser package typically contains hindered amine light stabiliser at 0.15–0.25 wt% active. In production, insufficient HALS concentration is detected by carbonyl index increase at 1715 cm⁻¹ in FTIR after QUV-A weathering according to ISO 4892-3:2016. Films that develop a significant carbonyl index increase after 2000 h exposure tend to develop longitudinal splits on wrapper arms during high pre-stretch application; retained dart impact per ASTM D1709-15a and tear propagation per ASTM D1922-15 should be measured after UV ageing, not only on unexposed film.

    Melt Curtain Neck-In and Die Lip Oxidation on Woven PP Lamination Lines

    Braskem LH118 is melt-laminated onto woven polypropylene at blend fractions of 20–40 wt% with high-pressure LDPE. Below 20 wt% LH118, the coated PP fabric may show inadequate low-temperature flex resistance, while above 40 wt% the melt curtain becomes difficult to control at coating weights below 18 g/m². Processing is performed on a 90 mm single-screw extruder with compression ratio of 2.5:1, barrel temperatures from 180 °C to 260 °C, and die temperatures between 280 °C and 310 °C. These high die temperatures open the PP fabric surface for mechanical interlocking, but they also accelerate LLDPE degradation during residence times above 3 min; screw cooling is applied to keep the feed zone temperature below 65 °C.Adhesion is assessed by peel testing according to ASTM F88/F88M-15 after lamination. Without tie resin, peel force at the PP-coating interface is frequently below 5 N/15 mm, and failure is interfacial. Maleic anhydride grafted LLDPE at 3–5 wt% raises peel force through covalent bonding to the woven PP. Amine-functional silane coupling agents are avoided in this structure because primary amine residues at die temperatures above 280 °C can promote catalytic degradation and die lip build-up. End products include FIBC inner liners and flat-bottom valve sacks; the FIBC structure is validated under ISO 21898:2004 for safe working load classification.
    ApplicationReferenceMeasured propertyOperational limitation
    Cast stretch filmASTM D5458-12Cling force after 24 h at 23 °CBelow 5 °C storage reduces cling force by more than 25%
    Frozen-food sealant filmASTM F1921-12Hot tack at 0.2 s dwellLower than metallocene LLDPE reference
    Silage bale wrapISO 4892-3:2016Carbonyl index at 1715 cm⁻¹Significant increase after 2000 h indicates embrittlement risk
    Woven PP laminationASTM F88/F88M-15Peel force at PP interfaceBelow 5 N/15 mm without tie resin
    For heavy-duty shipping sack film on a bottom-seal conversion line, LH118 is used at 25 wt% with 70 wt% blown-film-grade LLDPE and 5 wt% white masterbatch; the film is extruded at 190–210 °C melt temperature and tested for dart impact per ASTM D1709-15a and Elmendorf tear per ASTM D1922-15 before conversion into 40–50 kg sack dimensions.
    Free Quote

    Competitive Braskem LH118 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH118 Linear Low Density Polyethylene is a pelletized film extrusion resin in the 0.918 g/cm³ density class. The nominal melt index, determined under ASTM D1238 at 190 °C with a 2.16 kg applied load, is 1.0 g/10 min; the corresponding density is measured according to ASTM D1505 or ISO 1183-1. Commercial documentation positions the grade for blown-film applications in technical packaging, agricultural film, liners, and general-purpose converter film. The exact additive formulation and film property data depend on the converter’s die configuration, screw geometry, and film gauge; grade suffixes may indicate the presence of antiblock or processing aid packages, and the certificate of analysis should be consulted before line qualification.

    Because the density falls below 0.920 g/cm³, the crystalline fraction is suppressed relative to medium-density and high-density polyethylene. This reduces the crystalline melting endotherm and widens the practical heat-seal window. The short-chain branching architecture characteristic of linear low-density polyethylene increases interlamellar tie-chain concentration compared with high-pressure low-density polyethylene at equivalent density. That molecular difference generally translates into higher tensile elongation, Elmendorf tear, and dart impact at a given film gauge. The precise comonomer type and branch distribution for LH118 are not always disclosed in commercial datasheets; for this class of resin, a butene-based Ziegler-Natta product is a common reference point, but octene-based or metallocene architectures must not be assumed without supplier confirmation.

    How does LH118 behave in blown-film extrusion compared with high-pressure LDPE?

    In blown-film extrusion, high-pressure low-density polyethylene exhibits pronounced shear thinning and high extensional melt strength, permitting stable bubble operation at low melt temperatures and blow-up ratios up to 3.5:1. A 1.0 melt-index linear low-density polyethylene such as LH118 has a flatter shear-viscosity curve and lower extensional melt strength. The bubble is therefore more sensitive to frost-line height, die lip gauge variation, and ambient air turbulence. To maintain bubble stability, converters commonly operate with a die gap of 1.5 mm to 2.5 mm, a blow-up ratio of 2.0:1 to 2.8:1, and a frost-line height between 3 and 7 die diameters. Melt temperatures are typically held in the 190 °C to 230 °C range. Sustained operation above 240 °C increases the rate of oxidative degradation and can produce gel-like defects in thin film. The lower melt strength of LH118 relative to high-pressure LDPE is not a processing defect; it enables film downgauging while retaining impact resistance, but it requires more precise bubble control on unvented monolayer lines.

    Compared with high-pressure LDPE, the linear structure reduces the amount of long-chain branching and therefore reduces melt elasticity. This alters die swell and film thickness orientation. After leaving the die, the melt exhibits less shear-thinning memory, which can increase the tendency for draw resonance under high haul-off speeds. Bubble cooling air ring settings should be adjusted with a lower initial velocity and a more gradual frost-line transition than would be applied to LDPE of the same melt index. Turbidity and gloss are also influenced by surface roughness from the die lip; the additive package in LH118 may include migratory slip or antiblock species that reduce coefficient of friction but can contribute to die lip plate-out over extended campaigns.

    Melt-pressure and solids accumulation in continuous conversion of LH118

    On single-screw extruders with 24:1 to 30:1 L/D ratios, the shear-thinning behavior of linear low-density polyethylene raises melt pressure more rapidly with increasing screw speed than would be observed with a branched high-pressure LDPE of the same melt index. The pressure coefficient is line-specific and cannot be transferred between machines without correcting for die diameter, flow channel geometry, screen pack restriction, and melt temperature. In continuous blown-film campaigns, die-lip oxidation solids are a primary cause of cosmetic defects after 24 h to 48 h of uninterrupted output. Oxidized low-molecular-weight species collect at the die lip and periodically transfer to the bubble as specks, gels, or surface roughness. The use of a barrier screw with a Maddock mixing element and a 40/80/40 mesh screen pack reduces unmelted resin and lowers the deposition rate, but it does not eliminate the need for periodic purging with a high-density polyethylene or a commercial purging compound.

    Formulation interactions are not neutral. Antiblock concentrates based on silica or calcium carbonate can accelerate metal wear in narrow die gaps and increase melt pressure when used above the supplier’s recommended loading. Processing aid packages based on fluoropolymer or silicone may be required to reduce die lip build-up and postpone melt fracture when running high-output, narrow-gap monolayer structures. If the converter observes sharkskin or melt fracture at low screw speeds, the standard corrective sequence is to increase the die gap, raise the die temperature, or add a polymer processing aid; increasing the melt temperature alone may increase degradation products and polymer gel formation.

    On a 45 mm single-screw extruder, the barrel profile typically moves from a feed-zone temperature of 170 °C to 190 °C, through a compression zone of 190 °C to 210 °C, and into a metering zone at 210 °C to 230 °C. The screw should not be operated above the torque limit specified for the gearbox if the downstream die is narrow. High melt temperature and long residence time jointly accelerate antioxidant consumption. The residence-time distribution across the screw becomes critical at low screw speeds and high barrel temperatures because stagnant melt near the feed-compression boundary can generate crosslinked particles that appear as optical defects in thin film at gauges below 40 µm.

    Specification parameterPublished or class-typical valueReference method
    Density0.918 g/cm³ nominalASTM D1505 / ISO 1183-1
    Melt index1.0 g/10 min at 190 °C/2.16 kgASTM D1238 / ISO 1133-1
    Melting endotherm121 °C to 124 °C class-typical for this density rangeISO 11357-3
    Vicat softening point95 °C to 100 °C class-typicalASTM D1525 / ISO 306
    Film dart impact at 25 µmGauge-dependent; supplier data requiredASTM D1709

    In coextruded barrier structures, LH118 may be used as a sealant skin because its lower density and melting point permit seal initiation at lower temperatures than medium-density grades. The seal window must be established by ASTM F88 seal-strength measurements over the intended dwell time and temperature. Seal initiation below 110 °C is commonly reported for 0.918 g/cm³ LLDPE, but the specific surface treatment, slip, and antiblock content of LH118 shift the curve. In blends with high-pressure LDPE, the seal strength increases at elevated temperature while remaining lower than that of low-density metallocene grades at equivalent density. Hot-tack performance measured by ASTM F1921 should be validated on vertical form-fill-seal lines before downgauging, because hot-tack failure produces leaker defects that are not predicted by ambient-temperature seal-strength testing alone.

    Why is butene-LLDPE not selected when high Elmendorf tear and puncture are decisive?

    When high Elmendorf tear, puncture energy, and slow crack resistance are the governing specifications, converters often select an octene- or metallocene-catalyzed LLDPE rather than a butene-based Ziegler-Natta film resin. The difference arises from short-chain branching length and distribution. Butene comonomer introduces two-carbon-side short branches, whereas octene introduces six-carbon-side short branches; the longer branches are more effective at bridging adjacent lamellae through tie chains. This changes tear propagation: a resin with higher tie-chain concentration absorbs more energy before yielding under ASTM D1922 tear and ASTM D1709 dart impact. Braskem LH118 remains suitable for cost-driven film constructions where gauge, dart penetration, and sealability are balanced; however, it does not match the extreme toughness of high-alpha-olefin metallocene LLDPE in freezer film or heavy sacks. If a converter replaces a high-pressure LDPE with LH118, tear and impact values at equal gauge typically improve. If the replacement target is an octene-based metallocene LLDPE, tear and impact are often lower, and a full film-property trial is required before specification approval.

    In extrusion lamination and cast-film operations, the lower melt strength of LH118 may require adjustments to air-knife position, chill-roll temperature, and draw ratio. Streak defects and edge weave are more likely at low thickness when draw resonance is induced by high draw ratios above 20:1. Published data for this specific configuration is limited; converters should not extrapolate blown-film data to cast-film productivity without pilot-line verification. The melt viscosity curve under ISO 11443 capillary rheometry should be measured over shear rates from 100 s⁻¹ to 1000 s⁻¹ to establish the shear-rate dependency for a given die geometry.

    Material handling and storage for LH118 follow standard polyolefin practice. Because the pellet surface is hydrophobic, absorbed moisture is not a primary concern; pre-drying is generally not required before blown-film extrusion. However, when pellets are moved from cold storage to a warm, humid production area, surface condensation can occur and may cause feeding irregularities in gravimetric hoppers. Residence time should follow the manufacturer’s lot documentation. Extended storage above 40 °C can accelerate antioxidant depletion and shift the melt index. The material should not be exposed to direct sunlight for prolonged periods, and it should be kept away from sources of copper or cobalt salts that destabilize polyolefins. Incompatible processing combinations include direct blending with high levels of certain amine-containing additives, which may interact with the catalyst residues or additive package and create discoloration under extended high-temperature processing.

    Jurisdiction or schemeTypical assessment basisVerification requirement
    US food contactFDA 21 CFR 177.1520Fabricated article testing required if food contact is intended
    EU food contactEU Regulation 10/2011 and amendmentsMigration testing of the final article required
    REACHRegulation (EC) No 1907/2006Substance registration and SVHC confirmation required
    RoHSDirective 2011/65/EUNot applicable to the polymer matrix; verify additive package