Braskem Lh0820 30af Blown Film Extrusion Linear Low Density Polyethylene

Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 168022
    Polymer Type Linear Low Density Polyethylene
    Comonomer Hexene-1
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.80 g/10 min
    Melt Flow Ratio I21 I2 30
    Melting Temperature 120 °C
    Vicat Softening Temperature 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break Md 25 MPa
    Tensile Strength At Break Td 20 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Impact Strength 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 45 60%
    Coefficient Of Friction 0.20
    Blocking 50 g
    Heat Seal Initiation Temperature 110 °C
    Anti Fog Yes

    As an accredited Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH0820/30AF LLDPE for blown film is packaged in 25 kg polyethylene-lined paper bags, 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags of Braskem LH0820/30AF LLDPE blown film extrusion resin, approximately 24.75 metric tons per container.
    Shipping Shipping description: Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene, solid polymer pellets, non-hazardous, not classified as dangerous goods for DOT/IMDG/IATA. Typically shipped in 25 kg bags, octabins, or bulk trucks/railcars. Keep dry, away from excessive heat; no placards required. Ensure packaging intact and labeled.
    Storage Store Braskem LH0820/30AF Blown Film Extrusion LLDPE resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed and palletized off the floor. Prevent moisture, dust, and contamination. Avoid prolonged UV exposure and static buildup. Store separately from incompatible materials and use first-in, first-out rotation. Follow manufacturer/SDS recommendations for safe handling.
    Shelf Life Shelf life is 24 months from production when stored in original, unopened packaging, dry, away from direct sunlight and heat.
    Application of Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene

    In heavy-duty industrial sack converting, the film web is produced from LH0820/30AF as the load-bearing layer where the nominal melt flow rate of 0.30 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg, together with the nominal density of 0.918 g/cm³ under ISO 1183-1:2019, supports the dart impact and tear resistance required for sack performance under UN Model Regulations Chapter 6.1 when the finished sack is certified for dangerous goods transport. Compliance in the EU industrial packaging segment is additionally governed by Directive 94/62/EC Article 11, with the sum of lead, cadmium, mercury, and hexavalent chromium limited to 100 mg/kg, and by REACH Annex XVII restrictions on restricted phthalates and polycyclic aromatic hydrocarbons in plastic materials. On a production scale, the formulation is typically run at 100 wt% LH0820/30AF for maximum puncture resistance, or in a two-layer structure with the core layer containing 10–30 wt% post-industrial recyclate and the outer sealing layer retained at 100 wt% virgin LH0820/30AF; published formulation data for dangerous-goods sack structures is limited outside converter-specific qualification documents. The extrusion process uses an 80 mm grooved-feed single-screw extruder with an L/D ratio of 30:1 and a barrier mixing section, coupled to a 400 mm spiral mandrel die with a die gap of 1.8–2.4 mm. A blow-up ratio of 2.0:1 to 3.0:1 is maintained, with melt temperature of 200–230 °C and frost line height adjusted to 2–4 die diameters for balanced MD/TD tear resistance. Terminal finished products include fertiliser sacks, petrochemical resin bags, mineral powder sacks, and construction adhesive bags.

    What Limits Thin-Gauge Bubble Stability in Agricultural Silage Bale Wrap Production?

    At 25–40 µm gauge on 70 mm 28:1 L/D grooved-feed blown-film units, monolayer silage wrap made from LH0820/30AF shows gauge variation below ±5% only when the die gap is held at 1.8–2.2 mm and the melt pressure at the adapter remains below 420 bar; higher pressures on 1.2 mm die gaps produce bubble chatter and reduce Elmendorf tear measured under ASTM D1922. The compliance benchmark for bale wrap is EN 14932:2006, Plastics – Thermoplastic stretch films for wrapping silage bales – Requirements and test methods, which sets dimensional, tensile, and cling performance requirements; the film is further characterised by ISO 527-3 tensile measurements and ISO 4892-2 accelerated weathering when a multi-season silage clamp exposure is specified. In formulation, LH0820/30AF is used at 98.5–99.2 wt% with 0.8–1.5 wt% HALS-based UV stabiliser masterbatch, while slip and antiblock masterbatch is adjusted to 0.2–0.5 wt% to control blocking on the rewound roll without reducing cling below the EN 14932 adhesion threshold. Processing requires a blow-up ratio of 2.0:1 to 2.5:1, a melt temperature of 195–225 °C, and internal bubble cooling sufficient to maintain frost line height at 1.5–2.5 die diameters; the absence of internal bubble cooling on older mono lines is a known cause of edge wrinkle and thickness non-uniformity at 25 µm. Terminal finished products include round bale wrap, clamp silage film, and silage pit sidewall liners.

    Where frozen vegetable and seafood converters require cold-temperature seal integrity, the sealant layer in three-layer coextruded blown film is specified with LH0820/30AF because its low melt flow rate contributes to puncture resistance at -25 °C while maintaining a seal initiation temperature compatible with high-speed vertical form-fill-seal machines. Food-contact compliance is established under Regulation (EU) No 1935/2004, Regulation (EU) No 10/2011 as amended, and FDA 21 CFR 177.1520 for olefin polymers, with overall migration limited to 10 mg/dm² under EU 10/2011 Annex III and specific migration limits for any added substance controlled under Annex I. The sealant layer is typically formulated at 70–85 wt% LH0820/30AF with 15–30 wt% low-density polyethylene to modify hot-tack, while the core and outer layers carry 0–20 wt% white masterbatch for opacity in frozen vegetable bags; the total structure is commonly 40–70 µm. Production uses a 3-layer coextrusion blown film line with die gap of 1.6–2.2 mm, blow-up ratio of 2.0:1 to 2.8:1, and melt temperature of 180–220 °C, with offline corona treatment applied to the outer layer only where print adhesion exceeds 38 dyn/cm under DIN ISO 8296. Terminal finished products include individually quick-frozen vegetable bags, frozen seafood pouches, ice cream pouches, and frozen meat interleaver film.

    InstrumentClause / test methodControl limit
    Regulation (EU) No 10/2011Annex III10 mg/dm² overall migration
    FDA 21 CFR 177.1520177.1520(b)Olefin polymer specification for food-contact layers
    Regulation (EC) No 1935/2004Article 3Manufacturing under good manufacturing practice
    Directive 94/62/ECArticle 11Sum of Pb, Cd, Hg, Cr(VI) ≤100 mg/kg

    Liquid Bag-in-Box Inner Liners and Oxygen Transmission Substitution Limits

    The sealant web in 5-layer liquid bag-in-box film is formulated around LH0820/30AF because the resin’s narrow molecular weight distribution allows stable coextrusion with EVOH barrier layers at a total structure thickness of 60–90 µm without inducing interfacial flow instability. The relevant food-contact framework is Regulation (EU) No 10/2011 with migration testing under EN 1186 and overall migration not exceeding 10 mg/dm², supplemented by FDA 21 CFR 177.1520 and, for wine and dairy applications, the sensory neutrality requirements of EN 1230-1. The oxygen transmission rate of the finished structure is verified under ASTM D3985 and is controlled by the EVOH layer, not the LLDPE skins; the LLDPE sealant layer alone contributes no measurable barrier below 1000 cm³/(m²·day·bar). Formulation allocation depends on layer position: the food-contact sealant layer is run at 100 wt% LH0820/30AF or a 90–100 wt% blend with LLDPE of higher melt flow rate, while tie layers are formulated with maleic anhydride grafted polyolefins at 5–10 wt%; the EVOH barrier layer is commonly 5–8 wt% of the total coextruded structure. The downstream process is 5-layer blown film coextrusion with a die gap of 1.8–2.4 mm, a blow-up ratio of 2.0:1 to 3.0:1, and melt temperature of 200–230 °C; a critical operational boundary is that EVOH and LH0820/30AF layers must be processed within a ±5 °C interlayer melt temperature window to prevent gel formation in the barrier layer and inconsistent adhesion at the tie interfaces. Terminal finished products include bag-in-box liners for wine, edible oil, liquid dairy concentrates, and water-based industrial liquids.

    Directly below the sealing jaw on a 45 µm poly-mailer converting line, the LLDPE web is subjected to dwell times below 0.5 s and sealing pressures above 3.0 bar, conditions that require LH0820/30AF to maintain seal integrity without film shrinkage when the jaw opens. Compliance for e-commerce mailer film is based on Directive 94/62/EC Article 11, which restricts the sum of lead, cadmium, mercury, and hexavalent chromium to 100 mg/kg, and on Regulation (EC) No 1907/2006 REACH Article 33 for SVHC communication in imported films; mechanical acceptance uses ASTM D1709 Method A dart drop and ASTM D1922 Elmendorf tear. The formulation is typically 100 wt% LH0820/30AF for the outer and sealing skins of a 3-layer mailer, with up to 30 wt% post-industrial recycled LLDPE in the core layer; black or grey opacity masterbatch is added at 2–4 wt%, and the overall recycled content is limited by the converter’s puncture resistance specification under ASTM D5748. Production runs on 3-layer coextrusion blown film lines with die gap 1.8–2.4 mm, blow-up ratio 2.5:1 to 3.0:1, and melt temperature 195–225 °C; the higher BUR improves MD tear balance but reduces line speed when gauge drops below 40 µm. Terminal finished products include opaque poly mailers, courier envelopes, garment return bags, and document sleeves.

    When Pallet Stretch Hood Film Is Downgauged Below 50 µm Without Increasing Blow-Up Ratio

    Downgauging pallet stretch hood film from 65 µm to 45 µm without shifting blow-up ratio from 2.0:1 to 2.8:1 produces a measurable loss in transverse tensile yield under ISO 527-3 and increases puncture propagation under ASTM D5748; converters compensate by specifying LH0820/30AF at 100 wt% in the load-bearing core layer and reducing the outer slip masterbatch to 0.1–0.3 wt% so that cling under ASTM D5458 does not mask the loss of MD tear resistance. No single EU harmonised compliance standard governs industrial stretch hood film; performance is specified through ASTM D5458-22 cling, ASTM D5748-19 puncture resistance, and ISO 527-3 tensile properties, while the packaging waste framework remains Directive 94/62/EC Article 11 with the 100 mg/kg heavy metal ceiling. The formulation can include 10–20 wt% LLDPE of 0.5–1.0 g/10 min melt flow rate in the outer skins to control bubble stability during high-speed winder transfer, but the core layer remains 100 wt% LH0820/30AF. Production uses a 3-layer blown film line with die gap 1.6–2.2 mm, blow-up ratio 2.5:1 to 3.0:1, melt temperature 200–230 °C, and internal bubble cooling; an operational boundary is that ambient warehouse temperature below 12 °C during film storage increases unwinding force and can cause machine-direction elongation to drop below the purchaser’s minimum. Terminal finished products include pallet stretch hoods for beverage multipacks, hygienic tissue transport units, and white goods protective overwrap.

    Free Quote

    Competitive Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH0820/30AF is a butene-based linear low-density polyethylene supplied for blown film extrusion. The manufacturer’s published nominal density is 0.920 g/cm³ when determined by ASTM D792 or ISO 1183-1:2019, and the melt flow rate is 0.8 g/10 min when measured at 190 °C under 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022. The suffix 30AF identifies a formulated additive package rather than a comonomer type; the product is intended to reduce blocking and modify film-to-film slip after migration of the incorporated surface additive system. The base resin is used in general-purpose blown film structures, including industrial liners, carrier films, pallet overwrap, agricultural covers, and lamination films where film structures specify LLDPE density between 0.918 g/cm³ and 0.922 g/cm³. Published mechanical data for 50 µm film are lot- and line-dependent and should be taken from the supplier certificate of analysis rather than treated as fixed nominal values.

    On a 90 mm single-screw blown film line with a 30:1 L/D barrier screw and a 200 mm low-pressure spiral mandrel die, LH0820/30AF is typically processed with barrel set points increasing from 175 °C to 215 °C, die temperatures near 210 °C, and melt temperatures between 195 °C and 220 °C. A die gap of 1.5–2.5 mm and a blow-up ratio of 2.0:1–3.0:1 are common starting points; at these settings, bubble stability is influenced by frost-line height and air-ring volumetric flow. If the frost line is held below 4 die diameters, film tensile orientation increases in the machine direction and transverse tear resistance may fall when measured under ASTM D1922. If the frost line is allowed to rise beyond 7 die diameters, the bubble can oscillate, producing gauge bands and reducing gauge uniformity below the typical ±5% capability of a well-adjusted line. Screen-pack differential pressure should be monitored; a sustained increase above 30–40 bar across a 20/40/60/80 mesh pack commonly indicates additive agglomeration or contamination requiring pack change.

    How Does the 30AF Additive Package Influence Blocking Force and Film-to-Film Slip?

    Because the additive package in the 30AF designation is formulated for film surface performance, the main functional effects are measured with ASTM D1894 for coefficient of friction and ASTM D3354 for blocking force. After film is wound, the slip component migrates to the surface over a maturation period that commonly ranges from 24 h to 72 h depending on film thickness, winding tension, and storage temperature. Film stored at 20–25 °C and tested before complete migration may show static coefficient of friction above 0.5, while matured film may stabilize in the 0.2–0.4 range; the exact value is lot-specific and is not guaranteed by nominal density or melt flow rate. Corona treatment on a blown film line with a 2.0–3.0 kW treater at 15–30 m/min line speed raises surface energy to levels suitable for lamination, but oxidation can temporarily reduce slip and increase blocking; inline testing under ASTM D618-conditioned film is therefore required to establish the minimum maturation window. The antiblock component introduces surface micro-roughness that lowers film-to-film contact area; this can increase haze from a possible 7–10% for the unmodified film to higher values depending on particle loading, measured under ASTM D1003. Published data for this specific configuration is limited, and converters should verify additive migration kinetics on their own winding and roll-storage conditions.

    Incoming resin lots are normally checked for density and melt flow rate before line start-up. A lot with density outside 0.918–0.922 g/cm³ or MFR outside 0.7–0.9 g/10 min can alter bubble geometry, seal strength, and extrusion pressure; calibrations under ISO 1183-1:2019 and ISO 1133-1:2022 are therefore required for meaningful lot-to-lot comparison. Pellet bulk density and flowability affect hopper feed, but these are not part of the standard certificate. Storage at ≤35 °C in dry, UV-shielded conditions is typical; outdoor storage, especially in high-UV regions, can degrade the pellet surface and increase yellowness index under ASTM E313.

    Comparative Position Against High-α-Olefin LLDPE and Long-Chain Branched LDPE

    In general-purpose film applications, the principal differentiation is comonomer architecture. Butene-based grades such as LH0820/30AF are positioned below hexene- and octene-based LLDPE in dart impact and tear resistance at comparable density and melt index, as measured by ASTM D1709 and ASTM D1922. The density of 0.920 g/cm³ and melt flow rate of 0.8 g/10 min place the grade in the standard film extrusion envelope; however, high-α-olefin grades with density 0.918–0.922 g/cm³ may show higher puncture toughness and lower seal initiation temperature under ASTM F88 or ASTM D5748. Published comparative data for this specific formulation is limited; application-specific measurements on converter lines with 40 µm or 50 µm films should replace generic ranking tables. In blends with long-chain branched LDPE at 10–20 wt%, the LDPE fraction raises melt strength, widens the bubble stability window, and permits smaller die gaps; the tradeoff includes reduced clarity and reduced tensile strength relative to the neat LLDPE film when measured under ASTM D882.

    Standard test matrix used for evaluating LH0820/30AF film and lot acceptance.
    PropertyTest methodConditionReporting basis
    DensityASTM D792 / ISO 1183-123 °C0.920 g/cm³
    Melt flow rateASTM D1238 / ISO 1133-1190 °C, 2.16 kg0.8 g/10 min
    Film tensile propertiesASTM D882 / ISO 527-3500 mm/minLot-specific MD/TD
    Elmendorf tearASTM D1922Standard methodLot-specific
    Dart drop impactASTM D1709Method A/BLot-specific
    Coefficient of frictionASTM D1894Film-to-filmLot-specific

    When Down-Gauging to Film Thicknesses Below 25 µm Requires Output Retention

    Down-gauging from 50 µm to 20–25 µm shifts the limiting property from tensile yield to dart impact and tear propagation. On a 250 mm die with internal bubble cooling, output is often governed by cooling capacity rather than extruder torque; specific output values of 0.8–1.2 kg/h/mm die circumference can be reached only when the frost line is reset for the thinner gauge and the blow-up ratio is maintained within 2.5:1–3.0:1. If the film fails a customer dart impact limit below the required value under ASTM D1709, the conventional corrective actions are to increase the film gauge by 5–10%, blend in 10–20% high-α-olefin LLDPE, or reduce stalk cooling to lower bubble-quench rates. Published data for this specific configuration is limited; the product should not be down-gauged without first establishing a converter-level film property window using the specific die type and air-ring package.

    For food-contact films, the base polyethylene is generally evaluated under FDA 21 CFR 177.1520(c) as an olefin polymer intended for use with food types and conditions of use appropriate to the film. The presence of the slip and antiblock additive package requires separate confirmation that all additives meet the applicable status in 21 CFR 178 sections or other national positive lists; product stewardship documentation should be obtained from Braskem before commercial use. Under European Union requirements, the resin may be assessed under Regulation (EC) No 1907/2006 (REACH) and Directive 2011/65/EU (RoHS) for heavy-metal restrictions; no intentional addition of cadmium, lead, mercury, or hexavalent chromium is implied by the standard polyolefin manufacturing route, but the converter must retain supplier declarations. The grade is not designed for medical-device or pharmaceutical primary packaging unless validated under ISO 10993 by the finished-device manufacturer. Pre-drying is generally unnecessary; if condensation has formed during cold storage, a gentle drying step below 70 °C can be used, but higher temperatures may accelerate additive migration and should be avoided.

    Melt Temperature and Extrusion Pressure Boundaries in Barrier-Screw Operations

    Extruder barrel set points are normally profiled from 170 °C at the feed throat to 210 °C at the metering section. The melt temperature should remain below 220 °C for this density class; sustained operation above that threshold can increase oxidation risk, as measured by a reduction in oxidative induction time under ISO 11357-6 or ASTM D3895. High melt pressure before the screen pack may be caused by low die gap or by increasing additive filtration. For a 90 mm barrier screw at 80–110 RPM, melt pressure at the breaker plate is often in the 200–350 bar range, but actual values are machine-specific. If the die pressure is above 400 bar, the recommended response is to increase die gap or melt temperature, or to blend up to 10–20% LDPE to reduce viscosity and increase shear thinning. At the die lip, melt fracture can appear when shear stress exceeds the critical level for the resin; the condition is frequently corrected by widening the die gap from 1.5 mm to 2.5 mm or by raising die temperature to 215–220 °C.

    Top