Braskem Lh 218 Lldpe Cast Film Extrusion Polyethylene

Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene

    • Product Name: Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 125110
    Product Name Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
    Grade LH 218
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Application Cast Film Extrusion
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 2.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 180 g
    Elmendorf Tear Strength Td 400 g
    Haze 5%
    Gloss 45 80%
    Coefficient Of Friction 0.2

    As an accredited Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene supplied in 25 kg polyethylene bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading for Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene: palletized 25 kg bags, shrink-wrapped, secured for export.
    Shipping Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene is shipped as non-hazardous solid resin pellets in moisture-barrier bags, octabins, or bulk containers. Standard dry van, railcar, or truck transport is used. Keep dry, away from heat and contamination. No special dangerous goods handling required. Store in original packaging until use.
    Storage Store Braskem LH 218 LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original packaging sealed and pallets on a clean, dry surface. Avoid prolonged moisture exposure and excessive stacking. Maintain good housekeeping to prevent dust and static buildup. Follow manufacturer SDS, local regulations, and first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 24 months from production when stored unopened, dry, below 50°C, and away from direct sunlight.
    Application of Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene

    Pallet-unitization stretch film demands cling additive migration control on high-speed rotary wrappers

    On high-speed rotary wrappers operating at pre-stretch ratios of 150% to 300%, cast LLDPE webs in the 12–25 µm gauge band are converted into pallet loads. The film exits a flat die with a die gap between 0.55 mm and 0.90 mm and is pinned to a polished chill roll maintained at 18–35 °C. On a 90 mm single-screw extruder with a 30:1 L/D barrier screw, barrel temperatures from 180 °C in the feed zone to 250 °C at the adapter are typical. Melt temperature at the die lip is held below 280 °C to limit oxidative gel formation. Chill roll temperature, air-knife velocity, and electrostatic edge pinning determine melt curtain stability. Neck-in of 20–45 mm per side at 400 m/min line speed requires an over-width die deckle. Cling is generated by polyisobutylene or PIB masterbatch at 0.5–3.0 wt%. PIB migration to the film surface proceeds over 24–72 h; immediate on-roll cling is lower than final values. Excessive PIB loading above 3.0 wt% increases unwind blocking and transfer to corrugated board. Insufficient loading below 0.5 wt% produces tail failures during wrapping. Transverse gauge uniformity is controlled by automatic die bolts and beta-gauge feedback; a deviation above ±3.0% at 23 µm causes camber and stretch inconsistency. Mechanical properties are verified by puncture resistance per ASTM D5748-21, tensile elongation at break per ASTM D882, and tear resistance per ISO 6383-2:2004. Melt flow rate should be confirmed per ISO 1133-1:2022 before setting extruder barrel temperatures. Published data for Braskem LH 218 in this specific application may be limited to converter trials; the values above reflect production-scale cast film lines processing LLDPE in the 0.918–0.922 g/cm³ density range.

    What limits downgauging of food-contact cast web below 15 µm?

    When a food-contact cast web is downgauged to 15–25 µm for fresh-produce overwrap or flow-pack lamination, the governing limits are gel count, organoleptic performance, and heat seal stability. The resin must meet food-contact requirements under FDA 21 CFR 177.1520 and EU 10/2011. Overall migration under EU 10/2011 must not exceed 10 mg/dm² or 60 mg/kg for the intended food simulant. For fatty or acidic foodstuffs, converters should validate the final laminate because adhesive and ink layers may dominate migration. Slip and antiblock are adjusted to produce a kinetic coefficient of friction of 0.15–0.35 against stainless steel per ISO 8295:1995. Silica antiblock above approximately 3000 ppm raises haze and accumulates on the die lip; below approximately 1000 ppm, roll blocking may occur at winding tension above 250 N/m. Optical properties are controlled by polished chill roll finishing; haze below 5% per ASTM D1003 and 45° gloss above 85 GU per ASTM D2457 are common targets for direct overwrap. At gauge below 15 µm, draw resonance onset may occur near 250–300 m/min unless melt temperature is raised to 270–280 °C and the die gap is narrowed. Heat seal performance is characterized by ASTM F1921-12(2018) and seal strength by ASTM F88/F88M. PIB-based cling additives are generally avoided in direct food-contact overwrap unless a specific food-contact evaluation demonstrates compliance for the intended simulant.

    Application segmentCritical requirementTest method or regulationImplementation note
    Food-contact direct overwrapOverall migrationEU 10/2011≤ 10 mg/dm² or ≤ 60 mg/kg depending on food simulant
    Food-contact direct overwrapOlefin polymer complianceFDA 21 CFR 177.1520Validate extraction profile for intended food type
    Pallet stretch wrapPuncture resistanceASTM D5748-21Establish minimum from pre-stretch ratio and pallet corner type
    Lamination sealant webWetting tension after corona treatmentISO 8296:200338–42 mN/m before adhesive coating
    Hygiene backsheet laminationMachine-direction tensile strengthISO 527-3:2018Report MD and CD values; no universal minimum applies
    Silage cover filmAccelerated weathering screeningISO 4892-2Field validation mandatory; not a pass/fail standard

    For hygiene backsheet lamination, cast LLDPE webs at 18–30 µm are adhesive-laminated or thermal-laminated to polypropylene nonwovens. The polyethylene layer functions as the primary liquid barrier. The nonwoven face provides drape, tear propagation resistance, and hot-melt adhesive anchorage. Tensile strength and elongation at break are measured per ISO 527-3:2018; typical cast LLDPE webs in this segment show machine-direction tensile above 25 MPa and elongation above 500%, but published data for Braskem LH 218 in this specific laminate configuration is limited. Processability at 18 µm depends on low gel count and precise melt filtration. A backpressure increase across a 50 µm screen pack in continuous screen changers can indicate gel accumulation on long runs. Embossed chill rolls reduce blocking and adjust surface roughness. The coefficient of friction against nonwoven is maintained between 0.30 and 0.45 per ISO 8295:1995 to allow web tracking through converting lines. Pinhole and barrier integrity are not characterized by hydrostatic head alone; visual inspection under backlight or differential pressure decay is used for 20–30 µm cast webs. Converter-added masterbatches must be evaluated for REACH and RoHS compliance separately, because the base resin alone does not cover migrating substances from adhesive or additive packages.

    Draw resonance and edge neck-in are the controlling defects when cast LLDPE is used as the inner sealant web in PET/adhesive/PE or BOPP/adhesive/PE laminates. The cast web is produced at 25–40 µm and must deliver a seal plateau between 110 °C and 130 °C on vertical form-fill-seal machines. Hot tack and seal strength are measured per ASTM F1921-12(2018) and ASTM F88/F88M. A stable melt curtain at 300–500 m/min requires resin with low shear sensitivity and narrow molecular weight distribution. Neck-in at the die lip increases with draw ratio; without edge encapsulation or air pinning, total width loss can exceed 80 mm on a 1.8 m die. Corona treatment is applied in-line to raise surface energy to 38–42 mN/m for adhesive wetting, measured per ISO 8296:2003. The treated surface must retain 36 mN/m or higher before lamination; offline storage above 30 days at 25 °C and 50% RH may require retreatment. Coefficient of friction against metal guides is adjusted to 0.20–0.30 per ISO 8295:1995 to prevent drift in bag formers.

    When silage-sealing cast film operates at sub-zero puncture temperatures

    In silage sealing applications, cast LLDPE films at 20–30 µm are stretched over silage pit covers and round-bale wraps. Puncture from corn stalks and frozen forage is the dominant failure mode at temperatures below 0 °C. Puncture resistance is measured per ASTM D5748-21; tear propagation is measured per ASTM D1922-15 and ISO 6383-2:2004. Typical cast LLDPE silage wrap in this gauge band shows puncture force in the range of 1.5–2.5 N and machine-direction tear above 10 g, but published data for Braskem LH 218 in this specific agricultural configuration is limited. UV stabilization is mandatory for service beyond 6 months. HALS and UV absorber masterbatches are dosed by the converter because Braskem LH 218 is supplied as a base resin with limited outdoor weathering stability. Accelerated weathering per ISO 4892-2 is a screening tool only; field testing under real solar load is required for 12–18 month pit cover service. The film must retain sufficient cling to remain sealed on pit covers under wind load, but no universal wind speed threshold applies because pit geometry and cover anchoring dominate. Cast film orientation increases machine-direction tear resistance but reduces transverse tear; edge folds should be avoided during installation. Low-temperature flexibility below −20 °C is evaluated by dynamic mechanical analysis or practical bend tests, not only by room-temperature tensile elongation.

    Temporary surface protection for pre-painted aluminum coil or high-gloss stainless sheet requires controlled low peel adhesion and clean removal after heat ageing. The cast film is typically produced at 50–80 µm with a coextruded adhesive layer or a pressure-sensitive adhesive coating. 180° peel adhesion is measured per ISO 8510-2 or ASTM D3330; target values are usually 0.05–0.60 N/25 mm depending on substrate roughness. Ageing at 60 °C for 7 days must not increase peel force beyond removable limits or leave adhesive residue on the protected surface. Migratory additives such as erucamide, oleamide, or PIB cling agents are usually avoided in this segment because surface transfer may impair subsequent painting or coating. Processability demands a smooth cast surface on the substrate-contacting side; air-knife chatter and chill roll replication defects are direct visual defects on glossy metal sheet. Published data for Braskem LH 218 in UV-stable surface protection film is limited; converters should evaluate plate-out and peel stability on the intended substrate.

    Free Quote

    Competitive Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene is a butene-based linear low-density polyethylene supplied as pelletized feedstock for cast film converting. Manufacturer-published baseline specifications identify a nominal density of 0.918 g/cm³ determined in accordance with ASTM D792 and a melt flow rate of 2.5 g/10 min at 190 °C under 2.16 kg load, determined in accordance with ASTM D1238 or ISO 1133-1:2022. The butene comonomer introduces short-chain branching that reduces crystalline fraction relative to high-density polyethylene and broadens the frozen-film orientation balance. This designation is specific to cast film extrusion rather than blown film because the rheological profile supports high-speed drawdown and chill-roll cooling. Typical application areas include industrial overwrap, protective film, lamination webs, hygienic packaging, and automatic form-fill-seal packaging. The standard additive package reduces blocking tendency and stabilizes coefficient of friction after migration, but the exact additive loading is not disclosed in public datasheets; published data for the specific additive concentrations is limited.

    On a production cast film line equipped with a 75–120 mm single-screw extruder and an L/D ratio of 24:1 to 30:1, initial set-points are commonly ramped from 180 °C in the feed zone to 240 °C in the metering zone, with adapter and die temperatures held between 240 °C and 260 °C. Melt temperature should not remain above 280 °C for extended residence time because migratory slip additives can volatilize, oxidize, and create die-lip plate-out. For 20–30 µm film, chill-roll temperatures are typically set between 15 °C and 30 °C, the air gap is maintained between 15 mm and 50 mm, and the melt curtain is pinned by vacuum box, air knife, or electrostatic wire. Compared with LDPE of similar melt flow, LH 218 tends to produce higher head pressure at equivalent screw speed because the linear backbone has a shallower shear-thinning response. Published line-specific energy-consumption data for this exact grade is limited, and set-points require optimization against die width, throughput, and final film gauge.

    What Limits Draw-Down Stability in Thin-Gauge Cast Film?

    Draw-down stability for LH 218 is governed less by melt strength than by the interaction between die-lip shear, air-gap cooling, and contact geometry on the chill roll. The melt flow rate of 2.5 g/10 min indicates moderate viscosity compared with fractional-melt LLDPE grades, so film webs below 15 µm can be more sensitive to edge weave and air turbulence. This sensitivity is managed by reducing the air gap, increasing electrostatic pinning, and maintaining a uniform melt curtain from the coat-hanger die. The butene-based short-chain branching produces lower melt strength than hexene- or octene-based LLDPE formulations of similar density; that difference is advantageous for rapid drawdown but a limitation when ultra-thin film is run at high speed without vacuum assist. In cast coextrusion, LH 218 is typically placed in skin or core layers on multi-extruder lines, and edge trim levels of 5–15 % are common depending on die width and film thickness rather than resin quality alone.

    For 25 µm cast film, manufacturer-published typical values place tensile strength at break between 35 MPa and 45 MPa in the machine direction and between 25 MPa and 35 MPa in the transverse direction, as measured by ASTM D882. Elongation at break is typically above 600 % in both directions. Dart drop impact under ASTM D1709 Method A commonly falls between 60 g and 90 g. Elmendorf tear strength measured by ASTM D1922 is anisotropic, with transverse-direction values in the range 200–350 gf and machine-direction values in the range 100–180 gf. Haze at 25 µm is typically below 4 % under ASTM D1003, and 60° gloss is typically above 70 under ASTM D2457. These values are thickness-dependent, and converters should revalidate film properties at the final gauge because tear and impact can shift non-linearly below 20 µm.

    Typical PropertyTest MethodPublished Typical Range or Value
    DensityASTM D7920.918 g/cm³
    Melt flow rateASTM D1238 / ISO 1133-1:20222.5 g/10 min at 190 °C/2.16 kg
    Tensile strength at break, MDASTM D88235–45 MPa
    Tensile strength at break, TDASTM D88225–35 MPa
    Elongation at breakASTM D882above 600 %
    Dart drop impactASTM D1709 Method A60–90 g
    Elmendorf tear, MDASTM D1922100–180 gf
    Elmendorf tear, TDASTM D1922200–350 gf
    HazeASTM D1003below 4 %
    GlossASTM D2457above 70 at 60°

    Surface Friction and Additive Migration in High-Speed Converting

    Coefficient of friction for LH 218 is not a fixed value at the die; it reaches equilibrium after the migratory slip additive blooms to the film surface. Immediately after casting, kinetic coefficient of friction may be above 0.30, but after 24–48 h at 23 °C and 50 % RH the value typically falls into the range 0.10–0.25 under ASTM D1894. This time-dependent migration is critical for converters that print or laminate within hours of extrusion. In high-speed automatic packaging, the additive package also reduces blocking force during roll unwind and prevents film layers from sticking at storage temperatures up to 40 °C. Processing above 280 °C can degrade the slip additive and increase plate-out on the chill roll or downstream idler rolls. Pellets should be kept free of surface condensation before feeding; polyethylene has low moisture uptake, but cold pellets moved into a humid production hall can carry water that generates visual defects in cast film.

    Corona treatment is generally required for printing, adhesive lamination, or extrusion lamination. A neat polyethylene surface may measure below 38 mN/m; a treatment dose of 2–5 W·min/m² is often used to raise surface energy above 42 mN/m. Excessive treatment, however, can oxidize the surface, reduce heat-seal strength, and create odour precursors. Because LH 218 contains a migratory slip package, treated film should be converted within 48 h or monitored for surface-energy decay in ambient storage. In adhesive lamination, the slip additive can compete with polyurethane or acrylic adhesives for surface wetting if the film is stored beyond the specified treatment window. For extrusion lamination with molten LDPE or metallocene tie layers, an excessively oxidized skin can reduce interfacial bond strength; the optimal treatment level must be established by dyne solution evaluation and bond-peel testing according to ASTM F88 or equivalent internal methods.

    When Food Contact and Regulatory Compliance Documents Are Required

    Polyethylene grades intended for food packaging can be formulated to comply with FDA 21 CFR 177.1520 and EU Regulation 10/2011; however, the supplier conformity statement for LH 218 must be obtained from Braskem because additive package composition and production site practices determine final compliance status. Final articles require migration testing under EU 10/2011 Annex V and, where applicable, organoleptic evaluation. Slip and antiblock additives can contribute to overall migration and sensory effects if the film is used for hot or fatty food contact. Processors should not rely solely on the resin datasheet for food-contact declarations and should verify whether the grade is covered by dual-use or food-contact certifications in the production region.

    A Comparative Property Matrix Is Useful for Cast Film Resin Selection

    The selection of LH 218 rather than an LDPE or metallocene LLDPE depends on the balance among toughness, clarity, process stability, and additive package. The matrix below presents a qualitative and quantitative comparison based on published cast film values; exact values vary with gauge and line configuration.

    AttributeBraskem LH 218LDPE cast film resinmLLDPE cast film resin
    Comonomer / architectureButene LLDPEHigh-pressure LDPE with long-chain branchingHexene- or octene metallocene LLDPE
    Melt flow rate2.5 g/10 min2.0–4.0 g/10 min1.0–3.5 g/10 min
    Density0.918 g/cm³0.923–0.926 g/cm³0.902–0.918 g/cm³
    Hazebelow 4 %below 5 %below 2 %
    Dart drop impact60–90 g30–60 gtypically above 120 g
    Elmendorf tear, TD200–350 gf50–120 gftypically above 300 gf
    Drawdown capabilityHighModerateHigh, with higher melt pressure
    Melt strengthLower than LDPEHighLow to moderate
    Standard additive packageSlip and antiblockOften bare or slip onlyOften bare or slip/antiblock

    In direct comparison with LDPE cast film grades, LH 218 provides higher tensile strength and dart impact at equivalent film gauge because linear low-density polyethylene has fewer long-chain branches and a higher tie-molecule fraction. LDPE retains advantages in optical clarity and melt strength, particularly where thick film or high neck-in control is required. Against metallocene LLDPE, LH 218 generally has lower dart impact and lower tear resistance, but it is less demanding in extruder pressure and is often selected when a standard slip/antiblock package is required without external masterbatch addition. Hexene and octene LLDPE copolymers can outperform butene-based grades in toughness and puncture, but they may carry a higher raw-material price and can require tighter temperature control. The choice of LH 218 is therefore optimized for cast film converting where stable drawdown, low blocking, and acceptable optics are required in high-volume industrial film.

    Storage and handling constraints are operationally relevant. Pellets should be kept in clean, dry hoppers and conveyed with oil-free compressed air or vacuum systems to avoid contamination. Pre-drying at 60–70 °C for 2–4 h may be used only when cold pellets have been exposed to high humidity and surface condensation is visible. Avoid blending LH 218 with incompatible additive masterbatches containing high levels of peroxide, certain amine-based antistats, or unverified recycles, because such additions can shift slip migration, increase gel formation, and reduce film optics. Recycle from cast film edge trim can be reincorporated at levels of 15–25 % without major loss of mechanical properties, but higher recycle fractions may raise gel counts and reduce tear resistance. The material should be processed within the melt-temperature limits stated above, and prolonged hold-up at high temperature should be limited to retard oxidative degradation.

    Top