Braskem Lh 118 Lldpe Blown Film Extrusion Polyethylene

Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene

    • Product Name: Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 169611
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Applicationprocess Blown Film Extrusion
    Meltindex 1.0 g/10 min (190°C/2.16 kg)
    Density 0.918 g/cm³
    Meltingpoint 123 °C
    Vicatsofteningpoint 95 °C
    Crystallizationtemperature 105 °C
    Tensilestrengthatyield 10 MPa MD / 10 MPa TD
    Tensilestrengthatbreak 30 MPa MD / 25 MPa TD
    Elongationatbreak 600% MD / 700% TD
    Onepercentsecantmodulus 180 MPa MD / 200 MPa TD
    Dartdropimpact 120 g
    Elmendorftearstrength 200 g MD / 400 g TD
    Haze 12%
    Gloss45degree 60
    Coefficientoffriction 0.2
    Sealinitiationtemperature 105 °C
    Recommendedmelttemperature 190–220 °C

    As an accredited Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LH 118 LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for blown film extrusion.
    Container Loading (20′ FCL) 20′ FCL loaded with Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene, 25 kg bags, palletized, shrink-wrapped, secured for shipment.
    Shipping Braskem LH 118 LLDPE is a non-hazardous polyethylene resin in pellet form. It is typically shipped in 25 kg bags, bulk bags, or octabins, palletized and stretch-wrapped, or in bulk trucks/railcars. Keep dry, clean, and away from heat; no special dangerous goods classification required.
    Storage Store Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers or bags sealed, palletized off the floor, and protected from moisture, dust, and contamination. Rotate stock first-in, first-out and follow the manufacturer’s SDS and local regulations. Store at ambient temperature; avoid prolonged UV exposure.
    Shelf Life Shelf life is generally 12–24 months when stored unopened in original packaging, cool, dry, away from direct sunlight and contaminants.
    Application of Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene

    Why Heavy-Duty Sack Lines Operate Within a 2.0–3.0 Blow-Up Ratio Window

    Braskem LH 118, a butene-copolymer LLDPE with a nominal melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg and a nominal density of 0.918 g/cm³, is used on production-scale lines converting heavy-duty shipping sacks for mineral powders, fertilizer granules, and polymer pellets. The governing constraint is not tensile strength alone but bubble stability when the frost line is raised to increase machine-direction tear. A typical mono-layer or three-layer formulation uses 70–80 wt% LH 118-type butene LLDPE, 15–25 wt% high-pressure LDPE, and 2–5 wt% slip/antiblock masterbatch; the LDPE fraction contributes long-chain branching that raises melt tension and suppresses bubble breathing at a 2.0–3.0 blow-up ratio. Extruders run at melt temperatures between 190 °C and 230 °C through a 1.8–2.5 mm die gap, with the frost line positioned 2–5 die diameters above the die. On 90 mm die lines with internal bubble cooling, frost-line heights below 2 die diameters have been associated in converter trials with gauge bands of ±15% and reduced dart-impact consistency; high plant humidity can also increase blocking susceptibility when corona treatment is pushed above 45 mN/m. Compliance for non-food industrial sacks is governed by REACH and national packaging waste regulations; if food contact is specified, converters verify the olefin polymer under 21 CFR 177.1520 and EU 10/2011. Mechanical release testing anchors to ISO 527-3:2018 for tensile properties, ASTM D1709 Method A for falling dart impact, and ASTM D1922 for Elmendorf tear. Downstream conversion includes surface treatment to 38–42 mN/m, in-line gusseting, and bag making on side-weld or bottom-weld machines. Terminal products are valve sacks for cementitious powder, FIBC inner liners, gusseted fertilizer sacks, and heavy-duty rubble bags. The main processing boundary is that melt temperatures above 240 °C degrade bubble melt strength, and films above 150 µm may lose dart impact if the LDPE fraction falls below 15 wt%.

    PropertyTest methodCondition
    Tensile strength at breakISO 527-3:2018500 mm/min test speed
    Falling dart impactASTM D1709 Method A38 mm diameter dart
    Elmendorf tearASTM D1922Average of 5 specimens
    Corona treatment levelASTM D257838–42 mN/m

    Greenhouse covering film conversion with Braskem LH 118 as the core resin differs from industrial sack extrusion because the film must survive repeated UV exposure, condensation cycles, and wind-induced flexing without failing at the point of film-to-frame contact. In a standard three-layer agricultural structure, the core comprises 60–75 wt% LH 118-type butene LLDPE, 10–20 wt% LDPE for bubble support, and 10–15 wt% EVA or metallocene-enhanced polyethylene in the skin layers; UV stabilizer masterbatch is dosed at 0.5–1.5 wt% based on geographic UV load. Process conditions on 1.6–2.4 mm die gaps use melt temperatures of 195–225 °C, blow-up ratios of 2.2–2.8, and internal bubble cooling for films above 180 µm. The governing standard for European greenhouse covering is EN 13206:2017, which sets durability, optical, and dimensional requirements; where film is used in certified organic production, additive inputs must also comply with national organic-input lists and REACH. Terminal products include 150–200 µm greenhouse covers, low-tunnel films, and silage pit covers. An operational boundary appears with EVA-containing skins: at roll diameters above 600 mm and warehouse temperatures above 35 °C, blocking can cause film delamination during unwinding unless the skin anti-block dose is maintained at 2–4 wt%.

    Frozen-Food Laminates and the Onset of Low-Temperature Dart Impact Decline

    For frozen vegetable and seafood packs, Braskem LH 118 is generally incorporated in the sealant or core layer of two-layer and three-layer coextrusions, where low-temperature flexibility and seal formation through traces of condensation define the process. A representative sealant web blends 75–85 wt% LH 118-type butene LLDPE with 10–20 wt% LDPE and 3–8 wt% anti-block/slip masterbatch; the LDPE fraction improves hot-tack force but can reduce draw-down if its melt flow rate falls below 1.5 g/10 min. Coextrusion runs on blown-film lines with 1.2–2.0 mm die gaps, 2.0–2.8 blow-up ratio, and melt temperatures 185–220 °C. The downstream process includes in-line corona treatment to 38–42 mN/m and lamination of the LLDPE web to biaxially oriented polyester or polyamide. Compliance is anchored to 21 CFR 177.1520(c) for olefin polymers and EU 10/2011; overall migration is assessed by EN 1186, seal strength by ASTM F88, and film tensile by ISO 527-3. Terminal products are frozen vegetable pillow packs, seafood pouches, and ice-cream wrapper laminates. The critical limitation is that low-temperature dart impact falls as LDPE content exceeds 20 wt% and film thickness increases above 80 µm; published data for this specific configuration is limited, so converters generally run refrigerated drop tests before committing to high-speed vertical form-fill-seal lines.

    Pallet-load containment in ambient and cold-storage distribution centers has drawn blown-film stretch wrap produced with Braskem LH 118 where puncture resistance on irregular loads is more cost-sensitive than optical clarity. The formulation is typically 90–100 wt% LH 118-type butene LLDPE, 0–10 wt% metallocene LLDPE, and 1–3 wt% polyisobutylene-based cling additive; cling additive migration after extrusion is time-dependent and can produce uneven unwind force if rolls are stored more than 8 weeks above 30 °C. Blown stretch-film lines operate with a high-stalk bubble, 0.9–1.6 mm die gap, 2.0–2.5 blow-up ratio, and melt temperatures 200–240 °C, targeting 12–25 µm film. Testing follows ASTM D5458 for cling, ASTM D5459 for elastic recovery and permanent deformation, ASTM D1003 for haze, and ISO 527-3 for tensile properties. REACH and packaging waste legislation apply; food-contact compliance is not required unless the stretch film itself functions as a primary food wrapper. Terminal products are hand pallet wrap rolls and pre-stretched machine rolls. The central constraint is that blown-film stretch wrap has lower absolute machine-direction elongation than cast film; processors must verify that the pre-stretch ratio on wrapper carriages does not exceed the film's elastic recovery limit above 200% elongation.

    When Silage Wrap Replaces Three-Layer Stretch Film in High-Moisture Baling

    Round-bale silage wrapping is a more severe puncture and UV-resistance test for Braskem LH 118 than industrial packaging because the film must remain intact while stretched over sharp stalk ends and exposed to solar radiation for months. The standard blown-film formulation contains 85–95 wt% LH 118-type butene LLDPE, 5–10 wt% LDPE, and 3–5 wt% color/UV masterbatch; white or green pigment is used to reduce surface heating and UV penetration. Production uses 1.8–2.4 mm die gaps, 2.0–3.0 blow-up ratio, and melt temperatures 190–230 °C; closed-loop gauge systems reduce thickness variation in 25–40 µm rolls. For the European market, the relevant standard is EN 14932 for thermoplastic stretch films for wrapping round bales, which covers mechanical properties, oxygen permeability, and UV stability; REACH applies. Terminal products include 500 mm and 750 mm rolls for round balers and silage pit underlay films. The operational boundary is defined by film thickness and UV stabilizer loading: below 25 µm and below 0.5 wt% UV masterbatch, embrittlement can appear first along the bale shoulders; published data for this specific resin in high-UV southern European silage exposure is limited, so converters may require additional accelerated weathering evidence before switching suppliers.

    Stand-up pouch sealant webs for dry beverages, powdered nutrition, and pet-food lamination use Braskem LH 118 to obtain a balance between low seal initiation temperature and high hot-tack strength on high-speed form-fill-seal lines. In a three-layer coextrusion, the sealant layer contains 70–85 wt% LH 118-type butene LLDPE, 10–20 wt% LDPE, and 3–10 wt% anti-block/slip masterbatch; the outer skin may include metallocene LLDPE to improve interlayer adhesion to solventless or water-based laminating adhesives. Blown-film parameters are 1.2–2.0 mm die gap, 2.0–2.8 blow-up ratio, and 180–220 °C melt temperature; surface treatment is set to 38–44 mN/m before lamination to biaxially oriented polyester or polyamide. Food-contact compliance is verified against 21 CFR 177.1520 and EU 10/2011, with overall migration by EN 1186 and seal performance by ASTM F88 and ASTM F1921. Terminal products include stand-up pouches for dry foods, pet-food bag liners, and non-retort liquid pouch sealant films. The primary operational constraint is that storage beyond 12 months at ≤30 °C can reduce seal strength through additive migration; converters should avoid direct contact with aggressive fatty foods unless the final pouch passes specific migration tests for the exact food simulant under EU 10/2011.

    Free Quote

    Competitive Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LH 118 is a linear low-density polyethylene resin formulated for blown film extrusion. The grade is specified by its nominal density of 0.918 g/cm³ and nominal melt flow rate of 1.0 g/10 min when measured at 190 °C under a 2.16 kg load, in accordance with ASTM D1505 and ASTM D1238/ISO 1133-1. These values place the material in the thin-gauge LLDPE film category used for industrial liners, agricultural film, construction film, and overwrap. The resin is processed on mono-layer or coextruded blown film lines with conventional barrier screws having L/D ratios of at least 24:1, and is typically supplied without slip or antiblock additives unless post-added during conversion. The density and melt flow rate combination is intended to maintain puncture resistance, tear resistance, and bubble stability during stretch orientation; however, actual film performance is not fixed by resin density and melt index alone.

    What Resin Properties Govern Processing and Film Performance?

    The tabulated nominal values below are derived from the producer’s published product information for Braskem LH 118 and from general film-grade LLDPE behavior. Film mechanical values are test-condition sensitive and must be evaluated on a specific gauge, blow-up ratio, and frost line height. The melt flow rate of 1.0 g/10 min is selected to provide sufficient melt strength for stable bubble formation while retaining acceptable output on screw diameters from 40 mm to 90 mm.

    PropertyTest methodTypical value
    DensityASTM D1505 / ISO 1183-10.918 g/cm³
    Melt flow rate at 190 °C/2.16 kgASTM D1238 / ISO 1133-11.0 g/10 min
    DSC peak melting temperatureASTM D3418119–124 °C typical for film-grade LLDPE of 0.918 g/cm³ density
    Film tensile propertiesASTM D882 / ISO 527-3gauge-dependent; 25 µm laboratory film required for comparison
    Dart impact resistanceASTM D1709 / ISO 7765-1reported only at fixed gauge and quench conditions
    Elmendorf tear resistanceASTM D1922 / ISO 6383-2machine-direction/transverse-direction balance governed by blow-up ratio and die gap

    The low density reduces crystalline fraction and yields lower flexural modulus than high-density polyethylene. The 1.0 g/10 min melt flow rate, while common for film extrusion, should not be interpreted as an indicator of high shear-rate processability; fillers, processing aids, and temperature profiles must be matched to the selected screw geometry. Property values obtained from a 25 µm laboratory film are often used as a comparative baseline, but on production-scale lines the relationships among frost line height, air-ring cooling, and take-off speed can shift tear values by 10% or more under ASTM D1922 when the same resin grade is processed at different line speeds.

    In comparison to high-pressure LDPE of similar melt index, Braskem LH 118 typically requires greater extruder motor load because of the more shear-insensitive viscosity of linear polyethylene chains. Film produced from LLDPE at 0.918 g/cm³ generally exhibits higher dart impact resistance under ASTM D1709 and higher tensile strength at break under ASTM D882 than LDPE of equivalent gauge. LDPE commonly provides lower haze under ASTM D1003 and better bubble stability at low melt temperatures. Against a butene-based LLDPE of equal density and melt flow rate, the present grade may show improved tear resistance under ASTM D1922 and a broader hot-tack window under ASTM F1921; however, the magnitude of this difference depends on comonomer length, molecular weight distribution, and film fabrication conditions. Resin selection should not rely on density and melt index alone: two 0.918 g/cm³/1.0 g/10 min LLDPE resins can differ in output stability, seal strength, and optical clarity due to differences in short-chain branch distribution and catalyst system.

    Blown Film Extrusion Parameters Controlling Gauge Uniformity and Mechanical Balance

    On mono-layer blown film lines equipped with spiral mandrel dies of 200 mm to 300 mm diameter and single-lip air rings, Braskem LH 118 is typically processed at adapter and die temperatures between 200 °C and 230 °C, with die gaps of 1.8 mm to 2.5 mm. Blow-up ratios are commonly maintained between 2.0:1 and 2.8:1; higher blow-up ratios increase transverse-direction orientation and can reduce machine-direction Elmendorf tear under ASTM D1922. At fixed output, lowering the frost line below approximately 3 die diameters increases film haze under ASTM D1003 and may reduce modulus because smaller crystallites are formed during rapid quenching. A very high frost line above 8 die diameters can induce bubble palpitation and gauge bands visible at 5 µm to 10 µm thickness.

    The grade’s 1.0 g/10 min melt flow rate implies higher melt viscosity than a 2.0 g/10 min LLDPE. Head pressure depends on die diameter, die gap, screen pack condition, screw speed, and melt temperature. On a 60 mm extruder with 30:1 L/D and a clean screen pack, production-scale head pressures may range from 250 bar to 450 bar depending on output and die restriction; with fouled screens, pressure can exceed 500 bar and trigger alarms on lines without automatic screen changers. Screw speed should be adjusted to maintain bubble diameter and frost line height rather than fixed specific output, because die circumference and air-ring efficiency differ between lines. Stable operation is commonly achieved when the inflated bubble diameter is constant within ±2% during purging and when the frost line remains in the middle third of the stalk length.

    When Bubble Instability or Melt Fracture Restricts Throughput

    Linear low-density polyethylene with a melt flow rate of 1.0 g/10 min exhibits less strain hardening than high-pressure LDPE, which can narrow the stable bubble operating window. During start-up or rapid output increases, sharkskin melt fracture may appear as evenly spaced transverse ridges near the die exit. At the die lip, sharkskin onset in LLDPE is associated with wall shear stress in the range of 0.1 MPa to 0.3 MPa for common melt temperatures; the exact threshold varies with die metallurgy, die land length, and process aid concentration. On production-scale equipment, sharkskin is controlled by raising die temperature, reducing screw speed, opening the die gap, or adding a very small amount of fluoropolymer processing aid, which alters the die wall slip boundary condition without changing bulk rheology.

    In coextruded structures, Braskem LH 118 is commonly placed in the core or outer skin where its linear molecular architecture contributes to bubble stiffness. If run alone on a mono-layer line, blow-up ratios above 2.8:1 can amplify bubble flutter because LLDPE has lower melt elasticity than LDPE. A stable bubble cone requires coordinated adjustment of the air-ring damper and internal bubble air: the frost line should form within the middle third of the stalk, and the bubble diameter should not oscillate when the die is purged. Periodic die lip build-up is more likely at high melt temperatures and high back pressure; if die lip build-up appears, die-lip cleaning and screen pack replacement should be performed according to the line maintenance schedule rather than by increasing melt temperature beyond 250 °C, which can initiate oxidative degradation and introduce spec gels into thin film.

    Film produced from Braskem LH 118 is used in industrial liners, construction film, agricultural film, and overwrap where gauge reduction and puncture resistance are required. For liners, tear resistance is evaluated by ASTM D1922; for agricultural film, tensile properties are measured by ASTM D882; for waste-bag and heavy-duty sack applications, dart impact is assessed by ASTM D1709. Comparison of film mechanical performance across suppliers should be performed at a fixed gauge, typically 25 µm, and after conditioning for 40 h at 23 °C and 50% relative humidity. Published data for this specific grade in all possible formulations is limited; converters must generate film data on their own line configuration for final application approval.

    Heat Seal Initiation and Hot-Tack Requirements in Converting

    Where Braskem LH 118 is used in side-seal, bottom-seal, or vertical form-fill-seal applications, heat seal strength should be evaluated according to ASTM F88/F88M and hot-tack according to ASTM F1921. Linear low-density polyethylene generally provides a lower seal initiation temperature than LDPE of equivalent density because of its narrower melting distribution and absence of long-chain branching. At high packaging speeds, seal integrity depends on seal bar temperature uniformity, dwell time, and film gauge. Slip or antiblock masterbatch additions from 2 wt% to 5 wt% can reduce seal strength if they migrate to the film surface in excess; the sealant layer should be coextruded with a core of LDPE or HDPE when high hot-tack is required over a broad temperature range. Line converters should generate a heat seal curve for the exact film construction, gauge, and dwell time, because published generic seal data cannot replace lot-specific evaluation.

    Comparison parameterTest methodObserved trend for Braskem LH 118 film versus high-pressure LDPE
    Dart impact resistanceASTM D1709higher for LLDPE at equivalent gauge and frost line
    Elmendorf tear resistanceASTM D1922higher for LLDPE; machine-direction/transverse-direction ratio depends on blow-up ratio
    HazeASTM D1003LDPE or lower-density LLDPE typically gives lower haze
    Seal initiation temperatureASTM F88/F88Mlower for LLDPE due to lower melt enthalpy and narrower melting range
    Bubble stabilityline observationLDPE is generally more stable; LLDPE requires narrower blow-up ratio and frost line control

    Resin handling follows standard polyolefin practice. The product should be stored under dry conditions at ambient temperatures, and surface condensation should be avoided because moisture can produce spec gels and film bubble defects. No pre-drying is typically required at ambient relative humidity below 60%; if the resin has been exposed to water or if outdoor silo temperature swings are frequent, a desiccant hopper dryer set at 60 °C for 2 h may be used before start-up. Avoid blending with polyamide or EVOH unless interlayer adhesion and machine-direction tear have been evaluated on the target coextrusion line. For food contact applications, compliance with FDA 21 CFR 177.1520 and EU Regulation No. 10/2011 should be confirmed from the producer’s current regulatory statement for the exact grade.

    Top