| HS Code | 352652 |
| Manufacturer | Braskem |
| Productname | LF118 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) copolymer |
| Comonomer | Butene-1 |
| Application | Blown film extrusion |
| Physicalform | Pellets |
| Density | 0.918 g/cm³ |
| Meltindex | 1.0 g/10 min at 190°C/2.16 kg |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield | 10 MPa |
| Tensilestrengthatbreak | 25 MPa |
| Elongationatbreak | 700% |
| Dartdropimpact | 200 g |
| Elmendorftearstrengthmd | 300 g |
| Elmendorftearstrengthtd | 400 g |
| Haze | 8% |
| Gloss45 | 70 |
| Filmthickness | 25 µm (1 mil) typical |
As an accredited Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer packaged in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Braskem LF118 LLDPE blown film extrusion polyethylene copolymer in 25 kg bags, palletized and shrink-wrapped. |
| Shipping | Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer is shipped as generally non-hazardous solid pellets in 25 kg bags, 500–1000 kg supersacks, or bulk trucks/railcars. No special placards required. Store dry, away from heat, sunlight, moisture, and oxidizers. Follow SDS, local regulations, and use proper PPE. |
| Storage | Store Braskem LF118 LLDPE in a cool, dry, well-ventilated warehouse. Keep original containers sealed, palletized, and off the floor. Protect from direct sunlight, moisture, heat, sparks, and flames. Store away from oxidizing agents. Avoid contamination with dust, oils, or incompatible chemicals. Maintain stable ambient temperatures and follow the supplier’s SDS, local regulations, and FIFO stock rotation. |
| Shelf Life | Braskem LF118 LLDPE has a typical 12–24-month shelf life when stored unopened in original packaging, away from heat and sunlight. |
In three-layer machine-grade pallet stretch film production, Braskem LF118 with nominal density 0.918 g/cm³ per ISO 1183-1 and melt mass-flow rate 1.0 g/10 min per ISO 1133-1 is typically assigned to the core layer at 70–85 wt% when skin layers are compounded with metallocene polyolefin plastomer or ethylene-vinyl acetate at 10–20 wt% to control cling and puncture. The formulation may include polyisobutylene or hydrogenated tackifier at 1.0–2.5 wt% in the skin layer and slip/antiblock masterbatch at 1.0–3.0 wt%; the core layer is usually free of migratory cling additives to preserve modulus. Compliance for non-food industrial wraps references REACH EC No 1907/2006 and the Packaging and Packaging Waste Directive 94/62/EC, while optional food-contact use must follow FDA 21 CFR 177.1520(c) olefin polymer provisions and EU 10/2011 overall migration limits of 10 mg/dm². Extrusion is performed on a three-layer coextrusion blown-film line with die diameter 200–350 mm, die gap 1.8–2.4 mm, blow-up ratio 2.5–3.2, internal bubble cooling, frost line height 500–900 mm, and melt temperature 200–230°C. The winding section uses tapered tension of 10–30% and oscillating haul-off to distribute gauge bands. Machine stretch film is produced at 12–23 µm gauge; pre-stretched hand film at 6–10 µm; vented pallet wrap and extended-core rewind variants are also produced from the same line. Puncture resistance is assessed by ASTM D5748, machine-direction stretch recovery by ASTM D5459, and tensile elongation at break by ISO 527-3; at 23 µm, converters commonly specify machine-direction ultimate elongation above 400% and puncture energy at maximum load above 0.4 J, though published data for this specific configuration is limited and line trials are required to confirm additive interactions.
Frozen-food contact films using LF118 fall under EU 10/2011 with overall migration limit 10 mg/dm² and specific migration limits for slip and antiblock additives, and under FDA 21 CFR 177.1520(c) for olefin polymers when the applicable food-type extraction protocol is selected. The resin is typically formulated at 60–80 wt% LF118, 10–25 wt% low-density polyethylene for bubble stability, and 5–15 wt% metallocene LLDPE for low-temperature dart impact. Slip agent is added at 500–1,500 ppm, antiblock at 1,000–2,500 ppm, and fluoropolymer process aid at 200–600 ppm. Processing on monolayer or three-layer blown-film equipment uses die gap 1.2–2.0 mm, blow-up ratio 2.0–2.8, melt temperature 180–210°C, frost line height 300–600 mm, and internal bubble cooling; the lower melt temperature suppresses haze but increases die lip plate-out when high-slip masterbatch exceeds 1,500 ppm, shortening die cleaning intervals below 72 h. Finished types are pillow pouches, wicket bags for frozen vegetables, side-gusset seafood bags, and lidding film base webs in 25–80 µm gauge. Low-temperature dart impact is tested per ASTM D1709 Method A after 24 h conditioning at -20°C; tear propagation is measured per ISO 6383-2; and heat-seal strength is measured per ASTM F88, with typical target heat-seal strength above 15 N/25 mm at 130°C seal bar temperature for 0.3 s dwell.
High-stalk blown-film extrusion of heavy-duty industrial sacks using LF118 requires a die diameter between 200 mm and 500 mm and a die gap of 1.6–2.4 mm to balance gauge uniformity against shear heating. The formulation range is 75–100 wt% LF118, 0–20 wt% low-density polyethylene to modify melt strength, carbon black or titanium dioxide masterbatch at 2.0–5.0 wt% for opacity and ultraviolet opacity, and polymer processing aid at 200–800 ppm to delay melt fracture. Compliance is defined primarily by tensile properties per ISO 527-3, tear resistance per ISO 6383-2, dart impact per ASTM D1709 Method B, and heavy-metal limits under REACH EC No 1907/2006; where sacks are used as FIBC liners, converter specifications often reference ISO 21898 for filled bag handling tests. Processing on a high-stalk line uses blow-up ratio 2.2–2.8, melt temperature 200–230°C, internal bubble cooling set to maintain frost line height within ±50 mm of the nominal 600–1,200 mm position, and capacitive gauge scanning with a control tolerance of ±5%. At melt temperatures above 230°C, the melt strength of LF118 declines and bubble sag increases; below 200°C, die pressure near 350 bar may appear at high output with narrow die gap, producing shark-skin unless the process aid is maintained. Finished products include FIBC liner film in 80–150 µm, form-fill-seal heavy-duty sacks in 60–120 µm, industrial refuse sacks in 40–80 µm, and construction debris bags. Dart impact targets at 100 µm are commonly set above 400 g per ASTM D1709 Method B, but published data for this specific LF118 blend configuration is limited, so converter trials must confirm the effect of carbon black dispersion and high-stalk residence time on impact distribution.
Agricultural silage and greenhouse film formulations using LF118 place the resin at 65–85 wt% with low-density polyethylene at 5–15 wt%, carbon black masterbatch at 2.0–4.0 wt% for black/white or black/green silage covers, or hindered amine light stabilizer and UV absorber masterbatch at 1.0–3.0 wt% for clear greenhouse films. Processing involves wide-web blown-film extrusion with die diameter from 600 mm to 2,000 mm, die gap 2.0–2.6 mm, blow-up ratio 2.5–3.5, melt temperature 190–220°C, and internal bubble cooling with frost line height 800–1,500 mm to stabilize wide bubble geometry. Compliance is anchored to EN 13206:2017 for agricultural covering films, ISO 4892-2 for xenon-arc accelerated weathering, ISO 527-3 for tensile properties, and ISO 6383-2 for tear propagation. Finished types include bunker silo cover film in 100–150 µm, bale wrap film in 25–40 µm, greenhouse glazing film in 150–200 µm, and mini-tunnel mulch film in 25–50 µm. Retained elongation at break after 3,000 h xenon-arc exposure per ISO 4892-2 is typically specified at ≥50% for clear greenhouse film; for black silage film, cover durability is classified under EN 13206 by accelerated weathering and puncture resistance requirements, but because the specific stabilization masterbatch concentration interacts with LF118 comonomer distribution and film crystallinity, published data for this exact formulation is limited and outdoor exposure trials under local conditions are required.
For extrusion-laminated and adhesive-laminated flexible packaging structures, LF118 is introduced into the blown sealant web at 50–70 wt% with metallocene LLDPE or ethylene-vinyl acetate at 20–30 wt% to reduce heat-seal initiation temperature below 110°C under ASTM F1921 hot-tack test conditions and with low-density polyethylene at 5–10 wt% for neck-in control during subsequent extrusion lamination. The blown-film line operates at die gap 1.4–2.0 mm, blow-up ratio 2.0–2.5, melt temperature 190–220°C, and corona treatment at 38–42 mN/m to ensure adhesive anchorage. Compliance for food-contact pouches requires EU 10/2011 and FDA 21 CFR 177.1520(c), while overall packaging regulations include REACH EC No 1907/2006 and the Packaging and Packaging Waste Directive 94/62/EC; migration testing is conducted according to the EN 1186 series. Finished types are stand-up pouches, three-side-seal sachets, lidding films, and medical device overwrap when biocompatible additives are selected. Heat-seal strength per ASTM F88 at 130°C seal bar temperature and 0.3 s dwell is usually specified at ≥15 N/25 mm for a 70 µm web, while hot-tack strength per ASTM F1921 is specified only for high-speed vertical form-fill-seal applications. Corona treatment above 42 mN/m can reduce hot-tack performance by increasing surface polarity and seal initiation variability; therefore, inline surface tension monitoring is required.
Competitive Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer is a linear low-density polyethylene resin supplied as a butene copolymer for blown film extrusion. The resin is produced in a low-pressure catalytic polymerization process, which places short-chain branches along the polyethylene backbone. Nominal melt flow rate is 1.0 g/10 min at 190 °C under 2.16 kg load, determined by ASTM D1238 / ISO 1133, and nominal density is 0.918 g/cm³ by ASTM D1505 / ISO 1183. Industrial use is centered on monolayer and coextruded blown film for liners, consumer packaging, overwrap, and light industrial sacks. The butene-derived short-chain branching controls crystallization rate and directional solid-state deformation; this differentiates LF118 from high-pressure LDPE and from hexene- or octene-based LLDPE resins.
Nominal release-level properties are summarized below. Film values are not release targets; they depend on blow-up ratio, frost line height, die gap, and cooling configuration. Incoming resin quality is normally controlled by melt flow rate and density, while film mechanical data are generated on the target production line.
| Parameter | Test method | Nominal value |
|---|---|---|
| Melt flow rate, 190 °C / 2.16 kg | ASTM D1238 / ISO 1133 | 1.0 g/10 min |
| Density, 23 °C | ASTM D1505 / ISO 1183 | 0.918 g/cm³ |
| Melting peak temperature, DSC | ASTM D3418 / ISO 11357-3 | 120–126 °C |
| Vicat softening point, 10 N / 50 °C·h⁻¹ | ASTM D1525 / ISO 306 | 94–100 °C |
The additive formulation is designed for blown film extrusion and includes processing antioxidant; slip and antiblock additives may be present depending on the current product specification. Surface coefficient of friction is therefore checked on final film under ASTM D1894. The resin is not hygroscopic, but pellets stored below the local dew point can carry surface condensation into the feed throat. If pellet surface moisture is visible, a hopper dryer set at 50–60 °C for 2–4 h removes the condensed water but is not otherwise required. Food-contact status is not automatically conferred; the converter must verify the finished article under FDA 21 CFR 177.1520 and European Regulation EU 10/2011 for the specific layer structure, additive package, and end-use condition.
On blown film lines, LF118 is processed through a spiral mandrel die with a die gap of 0.9–1.2 mm. This wider gap, relative to the 0.5–0.75 mm gap commonly used for high-pressure LDPE, reduces melt fracture because the butene copolymer has lower melt strength and a narrower processing window at the die lip. Barrel temperatures are profiled from 170 °C in the feed throat to 200–215 °C in the metering zone, with adapter and die zones set at 190–210 °C. Melt temperature should not remain above 230 °C during extended start-ups; oxidative degradation accelerates above 240 °C and can produce gels, off-odor, and die-lip residue.
Screw selection affects melt-temperature uniformity and output stability. A barrier screw with L/D 24:1 to 30:1 and compression ratio 2.5:1 to 3.5:1 is recommended; a Maddock mixing section reduces the unmelted-particle fraction and improves melt homogenization. Screen packs at 40/80/40 mesh or 60/100/60 mesh increase back pressure and trap gel particles. Melt pressure before the screen pack is typically observed between 20 MPa and 35 MPa depending on output and melt temperature. A sudden pressure increase indicates screen blockage, while a sudden pressure drop can indicate screen rupture; both conditions require line shutdown because downstream film may contain gel defects or contamination.
Blow-up ratio is maintained between 2.0:1 and 3.0:1 to balance machine-direction and transverse-direction orientation. Frost line height is held at 5–10 die diameters; a short frost line generally increases transverse-direction tear but reduces bubble stability, while an excessive frost line lowers dart impact and promotes bubble sway. A dual-lip air ring is normally required for stable LLDPE bubble formation because single-lip designs common on LDPE lines do not generate sufficient contact force around the bubble. Internal bubble cooling can be used but requires closed-loop volume control; uncontrolled internal bubble cooling can induce bubble flutter, gauge bands, and frost line oscillation. On production lines, pinholes and instability are often traced to oxidized die lips, insufficient frost line height, or fouled air-ring outlets carrying low-molecular-weight waxes. Thickness uniformity for 25 μm film should be maintained within ±5% by die centering and air-ring adjustment; gauge variation above ±8% frequently reflects die-bolt heating imbalance or worn die lands.
In 25 μm monolayer blown film produced at BUR 2.2:1 and freeze-line height 6 die diameters, tensile yield strength under ASTM D882 is typically in the range 10–12 MPa in both machine and transverse directions. Elongation at break generally exceeds 600% under the same method. Dart impact measured by ASTM D1709A is commonly reported in the range 80–120 g; Elmendorf tear under ASTM D1922 usually falls between 120–190 gf in MD and 350–480 gf in TD. Haze measured by ASTM D1003 is commonly 12–18%, and 60° gloss under ASTM D2457 is typically 50–70. These ranges are representative for butene LLDPE of this density and are not incoming QC limits. Published data for this specific configuration is limited; final film properties must be generated on the target line because die gap, frost line, BUR, and additive package shift the values.
Comparison against high-pressure LDPE of equivalent melt index shows that LF118 has lower melt strength, which requires a wider die gap and a more effective air ring. Compared with hexene- and octene-based LLDPE, a butene copolymer of the same density and melt flow rate often exhibits lower dart impact and transverse-direction tear under ASTM D1709A and ASTM D1922. Metallocene-catalyzed LLDPE grades with narrow molecular weight distribution may provide lower seal initiation and better optical response under ASTM F1921 and ASTM D1003, but LF118 commonly consumes less drive energy because broader molecular weight distribution promotes shear thinning in the extruder. The resin is not intended for injection molding, cast film, or blow molding; the stabilization package and rheology are not optimized for those processes.
Blending LF118 with high-pressure LDPE changes melt rheology and film property balance. LDPE contributes long-chain branching that increases melt tension and enlarges the bubble stability window. Addition of 10–20 wt% LDPE is used on lines with marginal air-ring cooling or frequent bubble flutter. The trade-off is a reduction in dart impact and Elmendorf tear because LDPE-rich domains can initiate microcracks under rapid puncture. Conversely, blending with 10–15 wt% HDPE raises secant modulus and creep resistance but reduces optical clarity and low-temperature tear. In three-layer coextrusion, LF118 is frequently placed in the core or sealant layer; when used as a seal layer, seal initiation temperature should be characterized under ASTM F1921 or ASTM F88 with actual dwell time, temperature, and pressure conditions. Silo blends require mass-flow geometry to avoid pellet-size stratification; a funnel-flow bin can produce density and melt-flow excursions that appear as gauge bands and dart impact variation in the final film.