Braskem Lf0720 21af Blown Film Extrusion Linear Low Density Polyethylene

Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 740726
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800 %
    Flexural Modulus 250 MPa
    Elmendorf Tear Resistance Md 200 g
    Elmendorf Tear Resistance Td 400 g
    Dart Drop Impact 120 g
    Haze 12 %
    Gloss 45 60
    Coefficient Of Friction 0.20

    As an accredited Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LF0720/21AF Blown Film Extrusion LLDPE is packaged in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene loaded in 20′ FCL, palletized bags, securely braced for export transport.
    Shipping Braskem LF0720/21AF is a non-hazardous linear low density polyethylene resin supplied as pellets, typically packed in 25 kg bags or octabins. Ship in clean, dry, covered containers or trucks. Protect from moisture, heat, sunlight, and contamination. No special dangerous goods documentation required; follow standard industrial handling and local transport regulations.
    Storage Store Braskem LF0720/21AF LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed to prevent moisture and contaminant ingress. Protect from UV, static discharge, and strong oxidizers. Use pallets, avoid stacking damage, and clean spills promptly to prevent slipping. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months from manufacture when stored in original packaging, protected from direct sunlight, moisture, and heat.
    Application of Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene

    On a 70 mm single-screw blown-film extruder fitted with a 30:1 L/D barrier screw and a 350 mm monolayer die, Braskem LF0720/21AF is processed into heavy-duty form-fill-seal liners for 25 kg granular fertiliser sacks. The resin is a blown-film extrusion linear low density polyethylene with nominal density 0.920 g/cm³ (ASTM D792) and nominal melt flow rate 1.0 g/10 min (ASTM D1238, 190 °C/2.16 kg). A starting formulation for this sector is 75 wt% LF0720/21AF, 20 wt% high-pressure LDPE with MFR 0.3 g/10 min, and 5 wt% titanium dioxide masterbatch. The high-pressure LDPE phase raises bubble stability at elevated frost line positions, while the masterbatch lowers light transmission for fertiliser contact labelling. Die gap is set at 1.8 mm, blow-up ratio at 2.5:1, melt temperature at 205–215 °C, and frost line height at 8–10 die diameters. Film gauge is controlled at 60 µm. On this equipment, die pressure remains below 330 bar, and output is limited by bubble cooling rather than screw recovery. The terminal inner liner is pre-converted into tubular rollstock and sealed on vertical form-fill-seal equipment. Converter-side hot-tack and seal-strength checks are based on ASTM F1921; a minimum seal strength of 9 N/15 mm is commonly specified for pest-proof and moisture-tight wicket filling. Compliance for fertiliser contact is evaluated under applicable national packaging legislation, with REACH Regulation (EC) No 1907/2006 applying to European Union import. Batch-to-batch variance in dart impact at 60 µm is controlled by monitoring incoming resin MFR and density rather than relying on film appearance alone.

    What Limits Outdoor Service Life in Silage Cover Film?

    The service life of a bunker silo cover is controlled by UV stabiliser dispersion, film gauge, and mechanical damage during installation. Braskem LF0720/21AF is formulated as a black monolayer film at 125 µm with a starting blend of 96 wt% resin, 2 wt% carbon black masterbatch, and 2 wt% hindered amine light stabiliser masterbatch. The masterbatch carrier is selected to be compatible with LLDPE; incompatible carriers lower carbon black dispersion and create premature film fibrillation at fold lines. Processing is carried out on a 90 mm single-screw extruder with 30:1 L/D and a 450 mm die. Die gap is 2.0 mm, blow-up ratio is 2.8:1, melt temperature is 200–210 °C, and frost line height is 10–12 die diameters to stabilise the larger bubble. The finished bunker cover is perforation-free and is secured with sandbags or tires. Accelerated weathering is checked according to ASTM G154 Cycle 1; a common acceptance criterion is 70% retained elongation at break after 500 h, though published data for this specific formulation is limited. Compliance is industrial and agricultural, not food contact. Outdoor exposure beyond 12 months is not recommended unless gauge is increased above 150 µm, because continuous UV irradiation and silage acids embrittle the film near the soil interface.

    Coextruded frozen-food webs operating at −40 °C need sealant layers that retain impact resistance after surface frosting and distribution vibration. LF0720/21AF is placed in the sealant layer of a three-layer structure at 35 wt%, with a 45 wt% high-α-olefin LLDPE core and a 20 wt% high-pressure LDPE outer layer. The three-layer die measures 300 mm, with 1.6 mm die gap, 2.2:1 blow-up ratio, and 215 °C melt temperature across all layers; line output is held near 85 kg/h to control gauge profile. Finished film gauge is 50 µm. Cold-temperature dart impact is measured under ASTM D1709 Method A after conditioning at −18 °C for 24 h; a specification of 140 g or higher is frequently set for vegetable pillow pouches, but published data for this specific layer structure is limited and must be verified on the converter line. Heat seal initiation is tested on a laboratory jaw sealer at 0.7 N/mm² pressure and 1 s dwell; LLDPE sealant layers of this melt index typically initiate between 105 °C and 115 °C. Compliance is governed by FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² under simulated frozen-food conditions. The terminal article is a printed pillow pouch for free-flow frozen vegetables, where the sealant web provides low-temperature puncture resistance and controlled seal separation on packaging lines.

    Regulatory referenceApplication scenarioTest condition / limit
    ASTM D1238Incoming resin controlMelt flow rate 1.0 g/10 min at 190 °C/2.16 kg nominal
    ASTM D1709 Method AFrozen food and vapour barrier filmDart impact after conditioning; specification set by converter
    ASTM G154 Cycle 1Silage cover film500 h UV exposure; retained elongation ≥70% common
    ASTM E96 Method BCrawl-space vapour membrane23 °C, 50% RH; permeance below 0.15 perm target
    FDA 21 CFR 177.1520Frozen food sealant webOlefin polymer compliance for food contact
    EU Regulation (EU) No 10/2011Frozen food and lamination pouchesOverall migration below 10 mg/dm²

    Stretch Hood Tear Propagation Across Palletized Construction Materials

    Palletized construction materials create repeated low-speed puncture events at the bottom edges of the load. LF0720/21AF is used as the majority phase in a 180 µm monolayer stretch hood film blended with 15 wt% metallocene-catalysed LLDPE to lift puncture resistance without sacrificing elastic recovery. The line is a 100 mm extruder with 35:1 L/D and a 600 mm die. Die gap is 2.2 mm, blow-up ratio is 2.5:1, melt temperature is 215–225 °C, and the bubble is run in a high-stalk configuration to increase machine-direction orientation. Terminal stretch hoods are wound on 300 mm cores and applied on automatic pallet hooders. Tensile properties are checked according to ASTM D882, and tear propagation is measured by ASTM D1922; converters commonly define transverse-direction Elmendorf tear acceptance on a line-specific basis because tear anisotropy shifts with high-stalk frost line height. Compliance is industrial packaging; direct food contact is not claimed unless migration testing under EU Regulation (EU) No 10/2011 is completed by the converter. The operational boundary is cold stretching; at application temperatures below 5 °C, converter trials are required to set pallet hooder pre-stretch force and avoid film fracture at pallet corners.

    When a 150 µm Vapour Barrier Membrane Replaces LDPE in Crawl-Space Installation

    A 150 µm black membrane intended for crawl-space installation must combine low water vapour transmission with puncture resistance during aggregate placement. Braskem LF0720/21AF is formulated with 2.5 wt% carbon black masterbatch and 1 wt% processing aid masterbatch, then blown on a 75 mm extruder with 30:1 L/D, a 400 mm die, 2.0 mm die gap, 2.6:1 blow-up ratio, and 205 °C melt temperature. Water vapour permeance is measured by ASTM E96 Method B at 23 °C and 50% relative humidity; a 150 µm LLDPE film of 0.920 g/cm³ density typically reports permeance below 0.15 perm, but converter certification is required. Puncture resistance during installation is evaluated by ASTM D1709 Method A after film conditioning at 23 °C. The membrane is installed as a loose-laid sheet with 150 mm overlap; acrylic pressure-sensitive tape is recommended for lap seams. Compliance is building-code driven and may require ASTM E84 surface burning classification when the film is installed in a conditioned crawl space. LF0720/21AF contains no flame-retardant additive; a flame-retardant masterbatch can be introduced but commonly reduces tensile elongation and should be qualified with ASTM D882 before specification.

    Lamination Sealant Webs and Heat-Seal Strength Decay

    Lamination converters using solventless polyurethane adhesives require a sealant web that does not block at winding temperatures and maintains heat-seal strength after adhesive cure. LF0720/21AF is downgauged to 30 µm at 2.0:1 blow-up ratio and 1.2 mm die gap, with melt temperature 210 °C. The extruder is a 55 mm line with 28:1 L/D and a 250 mm die. No slip additive is added to this structure; antiblock is dosed at 0.15 wt% to avoid interference with ink adhesion after lamination. Seal strength is evaluated after lamination to 12 µm polyester film using ASTM F88 with a 25 mm strip at 180 °C, 0.5 s dwell, and 0.4 N/mm² pressure. The sealant web should reach stable peel strength above 12 N/25 mm after 48 h adhesive cure; early testing at 4 h can show reduced values due to undercured polyurethane. Compliance for dry food contact follows EU Regulation (EU) No 10/2011, with migration testing under test condition OM1. Terminal article is a stand-up pouch for powdered beverage mixes, in which the sealant layer provides burst resistance at the gusset corners.

    Free Quote

    Competitive Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LF0720/21AF is a blown-film-extrusion linear low-density polyethylene produced with butene-1 as the short-chain branching comonomer. The nominal density is 0.921 g/cm³ when measured under ASTM D1505-18; the nominal melt flow rate is 0.70 g/10 min at 190 °C and 2.16 kg load under ASTM D1238-20. These values place the grade in the low-MFR, medium-crystallinity window used for monolayer blown film, coextruded seal layers, and industrial film structures. The linear backbone and ethyl-type short-chain branches reduce melt elasticity relative to high-pressure low-density polyethylene, which alters die-lip shear stress, bubble stability, and the balance between tensile properties and tear resistance. The grade is supplied in pellet form and is intended for conventional single-screw blown-film lines. Published film property data for this exact Braskem configuration is limited in public sources; gauge-dependent mechanical values should be generated on finished film under ASTM D882, ASTM D1709, and ASTM D1922.

    What differentiates a butene-comonomer LLDPE at 0.921 g/cm³ from high-pressure LDPE?

    The defining structural difference is the absence of long-chain branching. High-pressure LDPE contains both short-chain and long-chain branches; LF0720/21AF contains a predominantly linear ethylene backbone with short-chain branches introduced by butene-1. This molecular difference changes the shear-thinning response. LDPE exhibits higher melt elasticity and greater bubble stability on low-pressure air-ring lines. LF0720/21AF requires a wider die gap or lower output to avoid surface melt fracture because the linear chains generate higher shear stress at the die lip. The linear backbone increases tensile strength and dart impact at equivalent gauge when measured under ASTM D882 and ASTM D1709. The narrower short-chain branching distribution shifts seal initiation upward compared with high-pressure LDPE but leaves it generally higher than many metallocene grades. For film converters, the practical consequence is that LF0720/21AF cannot always be run identically to an LDPE of the same melt flow rate; die geometry, air-ring settings, and temperature profile require separate adjustment.

    Nominal resin properties and film-test protocols

    ParameterMethodNominal value
    DensityASTM D1505-180.921 g/cm³
    Melt flow rateASTM D1238-200.70 g/10 min at 190 °C/2.16 kg
    Comonomer typeManufacturer technical summaryButene-1

    Film property values are thickness-dependent and should be generated on 25 µm or 50 µm blown film after conditioning at 23 °C and 50 % RH according to ASTM D618. Tensile yield and elongation are measured under ASTM D882 using film specimens cut in machine direction and transverse direction. Dart impact is evaluated under ASTM D1709, method A or B as determined by film thickness. Low-temperature toughness for frozen-food packaging may require ASTM D3420 or puncture testing under ISO 7765-1. Haze and gloss are measured according to ASTM D1003 and ASTM D2457. Published values for LF0720/21AF film tensile strength, elongation, tear, haze, and gloss are not uniform across public sources; converter-generated data on the actual gauge and layer structure is therefore preferred.

    Thermal transitions, crystallinity, and property development during air-ring quenching

    At a density of 0.921 g/cm³, the melting peak for butene-LLDPE class materials generally falls between 121 °C and 125 °C under ASTM D3418; the crystallization peak falls between 104 °C and 108 °C. These transitions define frost-line position and bubble shape. A higher frost-line height allows more molecular orientation before crystallization, increasing machine-direction tensile strength and potentially lowering transverse-direction tear resistance. On low-stalk bubble configurations with blow-up ratios near 2.0:1, bubble deformation occurs above the melt crystallization temperature, producing lower orientation and higher dart impact. On high-stalk configurations with internal bubble cooling, the same resin may develop more machine-direction orientation and more balanced shrink properties. Cooling rate also affects haze and gloss. Faster quenching in the frost line reduces crystallite size and improves clarity; slower cooling increases haze. Air-ring airflow should be set so the frost line remains stable and the bubble neck does not waver. Bubble instability often appears as vertical oscillation of the frost line, which creates gauge bands; adjusting lower-lip airflow and blow-up ratio frequently corrects this without changing melt temperature.

    The density value of 0.921 g/cm³ corresponds to a relatively low crystalline fraction compared with 0.935–0.960 g/cm³ high-density polyethylene, which is why the film remains flexible at freezer temperatures. The glass transition of polyethylene is below -100 °C, so frozen-food embrittlement is not generally governed by glass transition but by tie-molecule density and slow crack growth. Butene-1 incorporation produces ethyl branches; hexene-1 produces butyl branches. Longer branches are more efficient at creating tie molecules between crystal lamellae, which is why hexene LLDPE often provides better dart impact and tear than butene LLDPE at equal density. This comparative mechanism is documented in polymer science literature but does not replace film testing for LF0720/21AF.

    When a narrow die gap and low melt temperature produce sharkskin melt fracture

    Under production conditions, the main processing defect for this resin class is sharkskin melt fracture at the die exit. Shear stress rises when the die gap is reduced below 1.5 mm or when melt temperature falls below 190 °C. The defect appears as fine surface roughness perpendicular to extrusion direction and can carry through the nip at normal winding tension. On a conventional low-pressure blown-film line, melt temperature should be controlled in the 190–220 °C range; the die gap should remain at 1.5–2.5 mm. Blow-up ratios between 2.0:1 and 3.0:1 are typical, and the frost line is held between 1.5 and 3.0 die diameters when using a single-lip air ring. These settings are not proprietary to LF0720/21AF but follow from the melt elasticity of linear low-density polyethylene.

    Screw configuration contributes to output stability. Grooved-feed extruders with L/D ratios from 24:1 to 30:1 and barrier sections provide more uniform melt temperature for this MFR range; conventional three-zone screws may require lower screw speed to prevent unmelt or pressure variation. On 70 mm grooved-feed barrels, bubble pulsation is commonly reduced by raising adapter and die zones to 210–220 °C and by limiting backpressure spikes to 20–35 MPa. The stated backpressure range is an operational envelope observed in LLDPE film extrusion; actual values depend on screw wear, filter pack, and die size. Fine screen packs can increase backpressure and melt temperature; pressure before the breaker plate should be monitored for spikes.

    End-use placement for LF0720/21AF centers on blown-film structures requiring a balance of melt extensibility and seal performance. Typical uses include freezer films, agricultural sheeting, industrial liners, carrier bags, and coextruded seal layers for heavy-duty sacks. For food-contact applications, the base olefin polymer is covered under FDA 21 CFR 177.1520 when finished articles meet extractive limitations; European Union food-contact compliance requires migration testing under Regulation (EU) 10/2011. The grade is not a universal packaging resin: high clarity, high hot tack, or very low seal initiation may require a metallocene LLDPE or ionomer, and high stiffness or moisture-barrier targets may require blending with high-density polyethylene or a separate barrier layer.

    Moisture uptake below 60 % RH is negligible; if pellets are stored in uncontrolled warehouses or exposed to condensation, drying at 60–70 °C for 1–2 h prevents trapped moisture from generating bubble holes. Drying above 80 °C for extended periods is not recommended because pellets may agglomerate. Blending with high levels of high-density polyethylene raises density and reduces dart impact; blending with polypropylene is generally incompatible in film structures because of phase separation and optical degradation. Clean recycled LLDPE film streams can be incorporated, but melt flow rate shift and gel level must be controlled before release to the line.

    Is LF0720/21AF a direct substitute for metallocene-catalysed LLDPE in sealant layers?

    Sealant-layer substitution requires revalidation of seal strength and hot tack. Metallocene LLDPE grades typically exhibit lower seal initiation, broader hot-tack window, and lower extractables than butene-comonomer Ziegler-Natta LLDPE at comparable density. LF0720/21AF can seal at higher temperatures; seal strength per ASTM F88/F88M-21 and hot tack per ASTM F1921-12(2018) should be generated on the target film structure rather than inferred from resin density. The difference is most visible in high-speed vertical form-fill-seal lines, where a 10–15 °C increase in seal-bar set point may be required to achieve equivalent seal integrity. This range is not a published specification for LF0720/21AF; it is the typical shift reported for butene LLDPE relative to metallocene LLDPE. Compared with hexene LLDPE, LF0720/21AF may exhibit somewhat lower dart impact and tear at equal gauge because butyl branches in hexene grades are more effective tie-molecule contributors. Compared with high-pressure LDPE, LF0720/21AF generally provides higher tensile strength and puncture resistance but lower melt strength and less forgiving bubble stability.

    Published data for the complete specific configuration of LF0720/21AF is limited. Density and melt flow rate remain the most reliable specification anchors. All film-based values, including dart impact, tear, haze, and seal performance, should be treated as structure-dependent. Resin-to-resin substitution, layer ratio adjustment, or recycled-content addition without re-qualification under ASTM D882, ASTM D1709, ASTM D1922, and ASTM F88/F88M-21 can shift film performance outside customer limits. The product is intended for blown-film extrusion; cast-film, injection-molding, or blow-molding conversions are outside the normal processing envelope and require separate rheological characterization.