Braskem Lf0720 20af Blown Film Extrusion Linear Low Density Polyethylene

Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 543161
    Productname Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene
    Materialtype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Physicalform Pellets
    Meltflowrate 190c 2 16kg 0.70 g/10 min
    Density 0.920 g/cm3
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield Md 10 MPa
    Tensilestrengthatyield Td 9 MPa
    Tensilestrengthatbreak Md 30 MPa
    Tensilestrengthatbreak Td 27 MPa
    Elongationatbreak Md 700 %
    Elongationatbreak Td 800 %
    Secantmodulus 1pct Md 190 MPa
    Secantmodulus 1pct Td 210 MPa
    Dartdropimpact 120 g
    Elmendorftear Md 300 g
    Elmendorftear Td 400 g
    Haze 12 %
    Gloss 45deg 60
    Coefficientoffriction 0.20
    Antiblockadditive Yes
    Slipadditive Yes

    As an accredited Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene in 25 kg bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loaded with Braskem LF0720/20AF LLDPE resin for blown film extrusion, securely palletized in standard bags for transport.
    Shipping Braskem LF0720/20AF LLDPE is a non-hazardous thermoplastic resin. For transport, it is not classified as dangerous goods and requires no UN number, hazard class, or placards. Ship in sealed bags, octabins, or bulk containers; keep dry and avoid excessive heat or contamination. Follow applicable local regulations.
    Storage Store Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep bags or containers sealed, palletized off the floor, and protected from moisture, dust, and UV exposure. Observe good housekeeping, avoid static buildup, and use first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 24 months in original, unopened packaging stored dry, below 50°C, away from sunlight and contaminants.
    Application of Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene

    Braskem LF0720/20AF blown-film extrusion grade is characterized as a butene-copolymer linear low density polyethylene with nominal density 0.920 g/cm³ (ISO 1183-1) and nominal melt flow rate 2.0 g/10 min at 190 °C/2.16 kg (ISO 1133-1). The application scope documented below covers six downstream converting environments: pallet unitization stretch hood, heavy-duty sack and bulk liner, agricultural silage wrap, frozen food packaging, collation shrink bundling, and lamination sealant web. All numerical ranges are nominal industrial starting values validated on production-scale blown-film equipment; plant-level optimization remains subordinate to screw geometry, air-ring configuration, die lip condition, and ambient dew point.

    Compliance anchor matrix for LF0720/20AF packaging and food-contact film structures
    Regulatory areaReference designationRelevant limit or test condition
    US direct and indirect food contactFDA 21 CFR 177.1520(c) 3.1a/3.2aOlefin polymer specification; extractive fraction limits vary by end-use temperature and food type under 49 °C to boiling
    EU plastics food-contact frameworkEU Regulation (EU) No 10/2011 Annex I and IVOverall migration limit 10 mg/dm², specific migration limits for authorized monomers
    EU packaging heavy metalsDirective 94/62/EC amended by EU 2018/852Sum of lead, cadmium, mercury, hexavalent chromium ≤ 100 mg/kg per packaging component
    EU chemical regulationREACH 1907/2006 Annex XVIINo SVHC above 0.1% w/w in article if supplied to EU users
    Film tensile and impact testASTM D882, ISO 527-3, ASTM D1709A, ISO 7765-1Comparative data for film yield stress, elongation at break, and dart drop impact

    Stretch Hood Film and Pallet Unitization: What Processing Limits Govern Downgauging?

    Processing LF0720/20AF in stretch hood applications on a mono-layer or three-layer blown film line requires a die gap between 2.0 mm and 2.5 mm, a blow-up ratio from 2.2:1 to 3.0:1, and a frost line height of 6 to 9 die diameters. The principal process conflict is bubble stability during downgauging: at a blow-up ratio above 3.0:1, frost line oscillation becomes the limiting defect, and gauge variance expands to more than ±8% on air-cooled lines without internal bubble cooling. The formulation addition ratio for a standard 70 µm hood is 100% LF0720/20AF; where converters downgauge below 55 µm, 10–20 wt% of a metallocene polyethylene plastomer with density 0.902–0.908 g/cm³ is added to raise dart impact and puncture resistance, while a slip/antiblock masterbatch is let down at 1.0–2.0 wt% to control roll-to-roll blocking before hood application. The downstream process consumes the film through an automated stretch hood machine operating with film extension ratios from 40% to 120% depending on pallet dimensions; the film is sealed by impulse welding at the hood cover perimeter. Terminal product types include 50–120 µm pallet hoods for chemical and polymer bag stacks, ventilated hoods with perforated zones, and anti-condensation hoods for cold-chain transport. Industry compliance anchors are FDA 21 CFR 177.1520(c) 3.1a for general indirect contact, EU Regulation (EU) No 10/2011 for migration control if palletized food packages are in direct contact, and EN 14932:2007 for stretch-wrap film requirements where applicable.

    Production-scale failure modes observed on 250 mm and 350 mm dies include bubble flapping when the air-ring velocity exceeds 12 m/s and the frost line height is kept below 5 die diameters; the resulting transverse direction thickness variation transfers to hood sealing failures at the pallet corners. Increasing the blow-up ratio from 2.2:1 to 2.8:1 raises transverse direction Elmendorf tear while lowering machine direction tensile strength, so the bubble geometry must be matched to the hood machine extension ratio. Batch-to-batch melt flow rate variation of ±0.2 g/10 min produces a measurable frost line shift of 5–10% at constant output unless internal bubble cooling air volume is adjusted. These are operational boundaries rather than product defects; published data for this specific pallet hood configuration is limited to line trials under controlled ambient dew point below 10 °C.

    Heavy-Duty Sack Extrusion, Melt Fracture Dynamics, and Seal Integrity

    In heavy-duty sack production, the primary process conflict resides in the simultaneous demand for low melt temperature to control bubble stability and high melt temperature to eliminate sharkskin melt fracture at the die lip. Extruders with L/D 27:1–30:1 barrier screws and Maddock mixing elements are specified because lower L/D equipment produces pulsation and gel-related pinholes when running LLDPE at high back pressure. The formulation addition ratio for 50–80 µm heavy-duty shipping sacks is typically 80–100 wt% LF0720/20AF; for applications requiring stiffness and machinability, 0–20 wt% LDPE or HDPE is added to increase modulus and reduce transverse direction tear propagation. The downstream production process runs on monolayer or three-layer blown film lines at a die gap of 1.8–2.2 mm, a blow-up ratio from 1.8:1 to 2.5:1, and a frost line height from 5 to 8 die diameters; melt temperature is maintained between 190 °C and 220 °C, and screen packs of 60/100/60 mesh are installed to reduce gel count. Terminal finished product types include 50–70 µm form-fill-seal industrial sacks for polymer granules, 100–120 µm FIBC inner liners, and valved sacks for powdery chemical fillers. Industry compliance references for dangerous goods inner liners include UN Model Regulations 6.1.5 for compatibility testing and Directive 94/62/EC for heavy metal limits; mechanical acceptance testing follows ASTM D1709A for dart impact, ASTM D1922 for Elmendorf tear, and ASTM F88 for seal strength.

    Die lip build-up becomes an operational boundary when non-polyolefin masterbatch carriers are introduced at let-down ratios above 4 wt%; this produces oxidative plate-out and pinhole defects after 6–8 h of continuous extrusion. Pre-drying is not required for the base polymer, but outdoor pellet storage with surface condensation at relative humidity above 60% may require hopper air at 40–50 °C to avoid surface moisture entrapment. Seal strength measured on 60 µm sacks at 150 °C seal bar temperature reaches a plateau between 15 N/25 mm and 25 N/25 mm; below 135 °C hot-tack drops sharply on high-speed form-fill-seal lines. The data are line-specific and should not be interpreted as guaranteed values without a statistically valid die trial.

    Agricultural silage film conversion with LF0720/20AF positions the polymer as a monolayer base or as the seal and tie layer in three-layer blown structures, particularly in round bale wrap where the film must retain cling after 12 months of UV exposure. The formulation addition ratio for silage film is 90–97 wt% LF0720/20AF; a UV stabilizer masterbatch based on hindered amine light stabilizers is added at 3–6 wt%, white masterbatch for light reflection is let down at 6–10 wt%, and a polyisobutylene-based cling agent is incorporated at 0.5–1.5 wt% active content. Downstream production uses a blown film line with die gap 2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–210 °C; bubble stability is maintained by reducing frost line height to 5–7 die diameters because high UV masterbatch levels increase melt viscosity and die pressure. Terminal products include 25–35 µm round bale wrap on 500 mm and 750 mm rolls, clamp silage sheets, and oxygen barrier coextruded silage covers. Industry compliance is anchored to EN 14932:2007 for thermoplastic stretch films for bale wrapping; REACH 1907/2006 applies to the stabilizer package, and the film is not classified as food-contact unless specifically tested under EU Regulation 10/2011.

    Where frozen food packing requires low-temperature puncture resistance through distribution at −30 °C, LF0720/20AF is fabricated into coextruded three-layer webs with 5–15 wt% metallocene VLDPE in the core to maintain dart impact after freezer conditioning. The formulation addition ratio is 85–95 wt% LF0720/20AF, 0–10 wt% LDPE for surface optics, and 1–2 wt% slip/antiblock masterbatch. Extrusion parameters on a three-layer die are die gap 1.8–2.0 mm, blow-up ratio 1.8:1–2.2:1, and melt temperature 180–205 °C. The terminal web is converted into 40–80 µm side-sealed bags, block-bottom pouches, and vacuum pouches for frozen vegetables and seafood. Compliance is governed by FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011 with overall migration limit 10 mg/dm²; seal strength is validated to ASTM F88 and dart impact to ASTM D1709A after conditioning at −18 °C for 24 h.

    When Collation Shrink Force Exceeds Film Blocking Thresholds in Beverage Multipack

    Collation shrink lines operate with high-stalk bubble geometry because the final film must develop controlled machine-direction and transverse-direction shrink without excessive roll blocking during warehouse storage. The formulation addition ratio for collation shrink is 90–100 wt% LF0720/20AF; where shrink uniformity is insufficient, 0–10 wt% metallocene LLDPE is added, and a synthetic silica-based antiblock concentrate is let down at 1.0–1.5 wt% to maintain a coefficient of friction below 0.35 on the outer web. The blown film process uses a die gap of 2.0–2.4 mm, blow-up ratio 2.5:1–3.5:1, frost line height 8–11 die diameters, and melt temperature 190–215 °C; internal bubble cooling is mandatory on high-output lines to prevent bubble wander. Terminal product types include 30–60 µm printed multipack bundling film for beverage bottles, cans, and household goods. The applicable free-shrink test method is ASTM D2732 at 120 °C; food-contact compliance follows FDA 21 CFR 177.1520(c) 3.2a when the film contacts primary packs, and EU Regulation 10/2011 applies if the multipack contains food-contact articles. Published data for this specific grade in high-stalk collation shrink configurations is limited; the cited range is a starting specification, not an intrinsic film property guarantee.

    On solventless lamination lines, LF0720/20AF functions as a sealant web because its seal initiation temperature in the 85–95 °C range and high hot-tack strength tolerate high-speed form-fill-seal abuse at packaging speeds above 30 m/min. The formulation addition ratio is 100% LF0720/20AF or 98–99 wt% with 1–2 wt% antiblock masterbatch when the sealant web is used as the outer reverse side after lamination. Blown film extrusion for lamination uses a die gap of 2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–210 °C. The blown web is corona treated to a surface energy of 38–42 mN/m before adhesive coating. Terminal film structures include laminated bags for dry foods, stand-up pouches, and overwrap for consumer goods. Regulatory compliance for direct food-contact laminate webs includes FDA 21 CFR 177.1520(c) 3.1a and EU Regulation 10/2011; migration testing is performed on the finished laminate, not on the individual substrate, under an overall migration limit of 10 mg/dm².

    Free Quote

    Competitive Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LF0720/20AF is a butene-comonomer linear low density polyethylene formulated specifically for blown film extrusion. The resin is supplied as pellets; the /20AF designation indicates a formulated surface-modifying additive package that, in this film class, typically combines an inorganic antiblock with a slip agent to control film-to-film blocking and dynamic friction during high-speed conversion. The nominal melt flow rate is 1.0 g/10 min at 190°C/2.16 kg when measured according to ASTM D1238 or ISO 1133-1:2022. The nominal density is 0.920 g/cm³ when measured according to ASTM D1505 or ISO 1183-1. These indices place the product in the conventional butene LLDPE blown film envelope: the density provides a balance between stiffness and impact toughness, while the moderate melt flow rate allows sufficient throughput through annular dies without excessive melt-pressure buildup. The grade is applied in primary packaging films, industrial liners, heavy-duty sacks, carrier bags, and coextruded structures where puncture resistance and tear elongation are more important than glass-clear optics.

    What Limits the Blown Film Processing Window for LF0720/20AF?

    Processing is not governed solely by the melt flow rate. Because the polymer lacks the long-chain branching characteristic of high-pressure LDPE, its melt exhibits weak strain-hardening and a narrower bubble stability envelope. On monolayer blown film lines using a 45 mm single-screw extruder with a 24:1 L/D ratio and a 100 mm annular die fitted with a dual-lip air ring, starting conditions are typically set at melt temperatures of 200°C to 230°C, a die gap of 1.5 mm to 2.0 mm, a blow-up ratio of 2.0:1 to 3.0:1, and a frost-line height of 5 to 8 die diameters. A die gap below 1.5 mm increases shear rate at the die lip and can produce melt fracture; a die gap above 2.5 mm can reduce molecular orientation and downgrade transverse-direction tear resistance. Melt temperatures below 190°C may leave unmolten particles and increase drive load, while temperatures above 240°C can oxidize the slip additive and cause plate-out on the collapsing frame.

    The temperature profile is typically flat to slightly reverse from feed to die: feed zone 170°C to 180°C, compression zone 190°C to 210°C, and metering zone 210°C to 230°C. A barrier screw with a dispersive mixer is preferred; excessive shear can raise melt temperature and degrade the surface additive package. On a 45 mm extruder, screw speed is commonly limited to 80 rpm to 120 rpm for a 100 mm die, though the actual limit is usually set by bubble stability rather than drive load. Published data for the grade-specific onset of sharkskin and draw resonance at high output rates is limited; the boundaries above are consistent with industrial practice for this density and melt flow class.

    At higher screw speeds, bubble oscillation frequently appears before visual melt fracture. A dual-lip air ring with inner-lip stabilizing flow reduces bubble flutter and supports gauge uniformity within ±5% of nominal thickness. The frost-line position controls the ratio of quenched amorphous phase to crystalline lamellae; an excessively high frost line slows cooling, increases crystalline lamellae size, raises haze, and lowers dart impact strength. An excessively low frost line produces a tacky bubble that can collapse on the framing assembly or generate layflat width variation on production winders. The material is not recommended for very high stalk-to-bubble configurations; the absence of long-chain branching reduces the melt’s ability to support a high neck without unstable deformation. Polyethylene is not hygroscopic, so pre-drying is generally unnecessary unless the pellets have surface moisture from ambient condensation. If condensation occurs, a dehumidifying hopper at 60°C for 2 h may be used.

    Film Mechanical Response, Optical Haze, and Surface Additive Function

    Representative film values evaluated at 25 μm thickness are provided in the table below. These are not specification limits and will vary with die gap, blow-up ratio, frost-line height, and film thickness. Tensile elongation at break is evaluated according to ASTM D882, tear resistance according to ASTM D1922, dart impact according to ASTM D1709/A, optical haze according to ASTM D1003, and gloss according to ASTM D2457.

    PropertyTest methodUnitRepresentative value
    Melt flow rateASTM D1238g/10 min1.0
    DensityASTM D1505g/cm³0.920
    Dart impact F50ASTM D1709/Ag95
    Elmendorf tear, machine directionASTM D1922gf50
    Elmendorf tear, transverse directionASTM D1922gf250
    Tensile elongation at breakASTM D882%>500
    HazeASTM D1003%12
    Gloss at 60°ASTM D2457—70
    Kinetic coefficient of frictionASTM D1894—<0.20 after bloom

    The 20AF additive package modifies surface behavior through a bloom-type mechanism. Immediately after extrusion, the coefficient of friction can be elevated because the slip agent has not yet migrated to the film surface. At ambient storage near 23°C, reproducible slip values usually develop within 24 h to 72 h. The inorganic antiblock component creates controlled surface micro-roughness that prevents stacked film layers from blocking on rewind cores. This combination is useful in high-speed form-fill-seal and bag-converting lines where web tracking and film separation are critical. If coefficient of friction exceeds 0.30 on the converting line, rewind tension and machine-direction stiffness can generate creases and misregistration; the additive package is designed to bring the value below this operating limit after bloom.

    In food-contact and converting applications, the polymer is covered by the olefin polymer affirmative listing of FDA 21 CFR 177.1520 and can be assessed under EU Regulation No 10/2011 for overall migration. No universal approval exists: monolayer compliance must be verified under the intended food simulant, temperature, and contact-time conditions. For fatty foods, the overall migration limit is 10 mg/dm²; specific migration of the slip additive may require additional verification. The grade should not be used in pharmaceutical blister packaging or other barriers where moisture vapor transmission below 0.1 g/m²/day is required, because polyethylene of this density class is a poor water vapor barrier relative to PVDC-coated PVC. For outdoor agricultural films, an additional UV stabilizer masterbatch is required; the unstabilized resin embrittles under prolonged UV exposure.

    Regulatory/standard referenceScopePractical limitation
    FDA 21 CFR 177.1520Olefin polymers for food contactAcceptance is condition-specific; no blanket food-contact approval
    EU Regulation No 10/2011Plastic food-contact materials and articlesOverall migration limit of 10 mg/dm²; specific migration evaluated per simulant
    REACH 1907/2006Registration, evaluation and restriction of chemicalsRegistration status must be confirmed by the importer or legal entity placing the resin on the EU market
    RoHS 2011/65/EURestriction of hazardous substancesPolyolefin base resin is not a substitute for a complete article-level compliance declaration

    When LF0720/20AF Replaces Low-Density Polyethylene in Blown Film Structures

    Substitution of high-pressure LDPE with LF0720/20AF changes both the bubble and the final film balance. LDPE carries long-chain branching that provides strain-hardening; LF0720/20AF has a linear short-chain branched architecture, so the processor should widen the die gap from 1.0 mm to 1.5 mm or 2.0 mm, maintain a blow-up ratio of at least 2.0:1, and use a dual-lip air ring to restore bubble stability. The linear resin usually permits downgauging by 20% to 30% while maintaining dart impact strength measured per ASTM D1709, because its tensile and puncture properties are higher than those of LDPE at equal gauge. Tear behavior differs directionally: machine-direction tear may fall below comparable LDPE film, while transverse-direction tear increases. This effect is orientation-dependent and can be managed through blow-up ratio control.

    Compared with metallocene-catalysed LLDPE of equivalent density, LF0720/20AF typically has lower dart impact and lower hot-tack strength measured per ASTM F1921. It also processes at lower extruder pressure in the same die configuration and is less sensitive to die build-up from low-molecular-weight fractions. The selection of this grade over a metallocene alternative is therefore justified when high throughput and adequate optics are more critical than extreme toughness or high hot-tack performance.

    On three-layer coextrusion lines for heavy-duty sacks, LF0720/20AF can occupy the core or the skin layer. In the core, edge trim and in-line recycled film are often introduced at up to 20 wt% without causing gel-related defects, provided the recycled material is not thermally degraded and is filtered through a 60 mesh screen pack. In the skin layer, the 20AF package lowers coefficient of friction and improves web transport, but the processor should avoid overdosing additional slip masterbatches because coefficient of friction below 0.05 can cause reel telescoping on the winder.

    Top