| HS Code | 777137 |
| Polymer Type | Linear Low Density Polyethylene Copolymer |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 2.1 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 94 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 240 MPa |
| Elmendorf Tear Strength Md | 120 g |
| Elmendorf Tear Strength Td | 250 g |
| Dart Drop Impact | 120 g |
| Haze | 12% |
| Gloss 45 | 50% |
| Coefficient Of Friction | 0.20 |
As an accredited Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LF 118/21 LLDPE copolymer resin supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Braskem LF 118/21 LLDPE blown film extrusion polyethylene copolymer, 25 kg bags, palletized, shrink-wrapped, securely stowed. |
| Shipping | Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer ships as pellets in 25 kg moisture-resistant bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, avoiding heat, moisture, and direct sunlight. Non-hazardous; store cool and dry, following SDS guidelines. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed and palletized to prevent moisture, dirt, and contamination. Avoid contact with strong oxidizing agents. Maintain clean handling areas and follow good housekeeping to minimize dust and static. Refer to the manufacturer’s SDS for specific storage and safety requirements. |
| Shelf Life | Typically 24 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight. |
Municipal waste collection sacks in the 100 µm to 220 µm gauge range fail in service primarily by tear propagation from point punctures, not by tensile yield. The base resin is supplied with a density of 0.918 g/cm³ per ASTM D792 and a melt flow rate of 1.0 g/10 min at 190°C/2.16 kg per ASTM D1238. On high-stalk monolayer lines equipped with grooved-feed extruders at 30:1 L/D and die diameters from 400 mm to 800 mm, Braskem LF 118/21 is dry-blended at 60 wt% to 80 wt% with post-industrial LLDPE reclaim and 2 wt% to 4 wt% of a 40% carbon black masterbatch in an LLDPE carrier with melt flow rate below 1.0 g/10 min to minimize viscosity mismatch. The melt temperature at the die is maintained between 190°C and 225°C, the die gap between 1.8 mm and 2.5 mm, and the blow-up ratio between 2.0:1 and 2.8:1; a dual-lip air ring with air temperature controlled to 10°C to 18°C stabilizes the bubble, while frost line height is held at 2.0 to 3.0 die diameters to prevent gauge bands above ±4 µm at haul-off speeds above 80 m/min. Final film is converted on bottom-seal bag machines with impulse seal bars set at 165°C to 195°C, and seal strength is monitored according to ASTM F88/F88M-23. The 100 µm film is specified to survive a falling dart impact of at least 90 g per ASTM D1709-16A and an Elmendorf tear of 250 gf in the transverse direction per ASTM D1922-15; machine-direction tear is lower due to preferential machine-direction orientation and is compensated by increasing gauge rather than by adding more than 20 wt% LDPE, because LDPE dilution suppresses dart impact at blow-up ratios above 2.5:1. The end article is a compacted wheeled-bin liner or industrial can liner for construction and retail waste streams; the formulation is not intended for food contact, and the converter must verify that post-industrial reclaim meets local packaging waste regulations.
Greenhouse cladding film produced from LF 118/21 as a 70 wt% to 85 wt% base resin, with 10 wt% to 20 wt% of a 14% vinyl acetate EVA and a UV stabilizer package, is extruded on a three-layer blown film line with a 350 mm die diameter and 1.6 mm die gap. Barrel profiles below 190°C in the compression zone leave unmelted EVA domains that appear as periodic haze bands in the finished film, while melt temperatures above 240°C promote gel formation from EVA carboxylate degradation; therefore the melt temperature at the die is limited to 200°C to 215°C and the barrel profile is ramped from 175°C in the feed zone to 205°C in the metering zone. The formulation is stabilized with 0.6 wt% of a high-molecular-weight HALS and 0.25 wt% of a benzotriazole UV absorber, both pre-dispersed in an LLDPE carrier through a 50:1 co-rotating twin-screw masterbatch line; 1.2 wt% glycerol monostearate is added as an anti-fogging agent, and the slip/antiblock package consists of 0.15 wt% erucamide and 0.10 wt% silica. The bubble is run at a blow-up ratio of 2.5:1 and a frost line height of 800 mm to 1,000 mm to balance transverse tear and machine-direction tensile strength. After 3,000 h of QUV exposure under ASTM G154-23, the 150 µm film is specified to retain 70% of initial elongation at break measured by ISO 527-3; total luminous transmittance for photosynthetically active radiation is measured by ISO 13468-1:2019 and is specified above 85% for clear film, while haze is limited to 20% by ISO 14782:2021. The finished tunnel and gutter-connected greenhouse cover is expected to survive three to five growing seasons in temperate zones; exact service life depends on UV radiation dose, sulfur dioxide exposure, and condensation management.
In pallet unitization lines operating at 40 to 70 loads/hour, blown stretch hood film is transported from a gusseted roll to a stretching frame, where it is expanded by 50% to 80% in the transverse direction before being released over a palletized load; the critical downstream requirement is recovery force retention after 24 h at 45°C and 60% relative humidity. LF 118/21 is extruded at 190°C to 215°C through a die with a 1.8 mm gap and run at a blow-up ratio of 3.0:1 to 3.5:1 with a high stalk height of 6 to 10 die diameters to generate transverse orientation and raise dart impact. The formulation contains 65 wt% LF 118/21, 25 wt% of an octene metallocene LLDPE with density 0.912 g/cm³ and melt flow rate 1.0 g/10 min, and 10 wt% of a high-pressure LDPE with density 0.923 g/cm³ and melt flow rate 0.3 g/10 min; the LDPE component increases melt tension and bubble stability, but additions above 15 wt% cause a measurable drop in machine-direction tear propagation resistance. Film thickness is held between 50 µm and 80 µm, and the specified minimum transverse elongation at break is 600% per ASTM D882, with a dart impact above 120 g per ASTM D1709-16A for 50 µm film. After slitting, the film is welded into tubular hoods by ultrasonic sealing at 20 kHz with amplitude of 55 µm to 65 µm; seal area temperature is controlled to avoid burn-through. The finished stretch hood is used for palletized construction materials, block pavers, and appliances; ultraviolet exposure is limited to outdoor storage periods shorter than six months unless an additional UV stabilizer package is incorporated.
Frozen-food flexible packaging uses LF 118/21 as a 20 µm to 40 µm sealant web laminated to PET or BOPP print webs with a solventless polyurethane adhesive. The sealant web is blown on a monolayer line with a 1.5 mm die gap and a blow-up ratio of 2.2:1 to 2.8:1, then corona treated to 38 mN/m to 42 mN/m before lamination; film melt temperature is held at 190°C to 215°C and the line is operated with chilled air to maintain low web tensions. Seal initiation is observed at 105°C, and the plateau seal strength at 140°C is reached within 0.5 s dwell on standard vertical form-fill-seal machines; the relevant test method is ASTM F88/F88M-23, with a specified average seal strength of 5.0 N/15 mm for 40 µm film after 12 months at −25°C. The cold-temperature seal performance is governed by the density of 0.918 g/cm³ and the narrow molecular weight distribution of the grade, but the converter must limit total slip and antiblock additive loadings to 0.15 wt% because erucamide bloom becomes crystalline at −25°C and deposits on seal jaws, causing intermittent seal leaks. The olefin polymer is covered by FDA 21 CFR 177.1520(c) for food contact olefin polymers, and the finished laminate is subject to European Union Regulation EU 10/2011 Annex I Table 1 with an overall migration limit of 10 mg/dm² using EN 1186-1:2002 extraction; REACH Regulation EC 1907/2006 Annex XVII restrictions apply to the additives and adhesive. The terminal package is used for IQF vegetables, frozen fruit, and frozen meat; seal integrity is additionally verified by dye penetration per ASTM F3039-23 after thermal shock from −25°C to 40°C.
| End-use segment | Standard designation | Test method or clause |
|---|---|---|
| Heavy-duty refuse sacks | ASTM D1709-16A | Falling dart impact for 100 µm film |
| Greenhouse cladding | ASTM G154-23 | QUV exposure 3,000 h, 70% elongation retention |
| Frozen-food laminate | ASTM F88/F88M-23 | Heat seal strength after −25°C storage |
| Food contact resin | FDA 21 CFR 177.1520(c) | Olefin polymer extractive limits |
| EU food contact | EU 10/2011 Annex I | Overall migration 10 mg/dm² |
| Construction vapour barrier | ASTM E96/E96M-22 | Procedure B water vapour transmission |
Produced in monolayer form at 50 µm to 120 µm, temporary containment enclosures and concrete curing films fail in service predominantly by puncture propagation from rebar ends and thermal expansion stress after dark-coloured films absorb solar radiation. LF 118/21 is run at 100 wt% or with 5 wt% of a UV-stabilized LDPE carrier containing carbon black at 3 wt% for opacity; the film is extruded through a die with a 2.0 mm gap at 200°C, with a blow-up ratio of 2.0:1 to 3.0:1, and is edge-folded in-line to produce a continuous sheeting layout. Slip and antistatic additive loadings are maintained below 0.05 wt% because surface contamination reduces tape adhesion at seam overlaps; seam adhesion is verified by a 180° peel test at 23°C per ISO 29862:2018. Water vapour transmission is measured by ASTM E96/E96M-22 Procedure B at 23°C and 50% relative humidity; for a 100 µm film the permeance is typically specified below 3.0 g/m²·24 h, but the converter must generate the value from the exact formulation because dust and carbon black content affect the vapour path. Puncture propagation resistance is tested by ASTM D5748-95(2019) using a 0.25 kg dart; the required breakout height is set by the site-specific containment protocol and is not a universal resin property. The end product is used as temporary building enclosure film, concrete curing cover, and lead-abatement barrier; flame-spread classification is outside the scope of the raw resin and must be established on the fabricated film according to regional building codes.
When coextruded silage bale wrap is stretched over a 1.2 m diameter round bale at 55% to 70% extension, the outer layer must resist UV degradation while the core layer maintains cling and puncture resistance against stalk ends and frozen forage. LF 118/21 is extruded as the core layer in a three-layer 25 µm to 35 µm film, with skin layers containing 2.5 wt% polyisobutylene tackifier and 0.5 wt% HALS UV stabilizer; the core layer is run at 100% LF 118/21 or blended with 10 wt% of an octene metallocene LLDPE to raise dart impact. The three-layer line uses a 400 mm die, a 1.5 mm die gap, a blow-up ratio of 2.8:1, and a melt temperature of 200°C to 220°C; film is wound with differential slip additives to avoid blocking in storage at 40°C. Pre-stretch ratio is limited by transverse creep of the butene copolymer; at extension above 70%, the film exhibits stress relaxation after 24 h that reduces bale compression and increases oxygen ingress. Retained cling is measured after 7 days at 40°C and 50% relative humidity by a modified 180° peel test based on ASTM D5458-20, with a specified minimum of 0.8 N/cm between the tackified skin layers; puncture resistance is verified by ASTM D5748-95(2019) on the 25 µm film. The finished wrap is used for round bale silage, haylage, and stalky crop bales; the film is not designed for direct food contact and must be disposed or recycled according to local agricultural plastics collection schemes.
Competitive Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem LF 118/21 is a butene-based linear low density polyethylene copolymer intended for blown film extrusion. The resin is supplied in pellet form with antioxidant stabilization and has a nominal melt flow rate of 1.0 g/10 min measured at 190°C under a 2.16 kg load in accordance with ASTM D1238, and a nominal density of 0.918 g/cm³ measured in accordance with ASTM D1505. The polymerization route yields a linear backbone with short-chain branching derived from butene incorporation; this molecular architecture places the resin between high-pressure low density polyethylene and higher-alpha-olefin LLDPE grades in melt relaxation and extensional response. Industrial converting lines typically process the resin on single-screw extruders with barrier or Maddock mixing screws, die gaps in the 1.6 mm to 2.3 mm range, and blow-up ratios between 2.0:1 and 3.0:1. Within this envelope, the grade is directed toward general-purpose packaging films, lamination base webs, liners, and sack applications where puncture resistance, tensile strength, and optical clarity are balanced.
Die gap selection controls shear rate, die pressure, and the onset of melt fracture. Because butene LLDPE exhibits lower shear thinning than high-pressure LDPE at equivalent melt index, narrowing a die from 2.0 mm to 1.2 mm raises die pressure and increases shear heat generation; on process lines equipped with 30:1 L/D single-screw extruders, the resulting melt temperature rise can require downward adjustment of barrel profiles by 5°C to 8°C to avoid surface oxidation and gel accumulation. Screw designs with barrier flights and spiral Maddock mixing sections should be operated at screw speeds that maintain melt temperature below 225°C; extended residence time above this threshold accelerates antioxidant depletion and can generate gel particles visible as pinhole defects in films thinner than 25 μm. Published data for LF 118/21 in specific narrow-die configurations is limited, but production-scale behavior on comparable butene LLDPE grades indicates that output rate is more often limited by bubble cooling capacity than by screw recovery. When die gap is reduced below 1.4 mm, shark-skin melt fracture typically appears first at the die lip; adjustments to die temperature, die lip geometry, or processing aid addition become necessary. Fluoropolymer processing aids are occasionally used at addition levels from 200 ppm to 800 ppm to suppress melt fracture without shifting film coefficient of friction.
Bubble geometry influences the division of orientation between machine direction and transverse direction. A high-stalk configuration is preferred for LF 118/21 because the butene-based linear backbone exhibits limited strain hardening; extending the stalk length delays crystallite formation until after biaxial orientation is imposed, improving bubble stability and gauge uniformity. Internal bubble cooling should be used when line speed exceeds approximately 60 m/min on a 200 mm die, but exhaust air must be controlled below the dew point to prevent condensation on the inner bubble surface; condensation produces chatter marks and local thickness variation. Frost line height is maintained between 200 mm and 500 mm above the die face depending on gauge and ambient airflow. High chilled-air velocities at the lower bubble perimeter increase transverse orientation and reduce haze, but excessive airflow can trigger bubble instability in thin films below 30 μm. Gauge uniformity, measured with a capacitance gauge, should remain within ±5% of target thickness; excursions beyond this range alter tear propagation and sealing behavior because LLDPE films exhibit anisotropic mechanical properties after orientation. For exact dart drop impact, Elmendorf tear, and haze values, the converter should request current certificate of analysis data because these values shift with film thickness, blow-up ratio, frost line height, and annealing history.
On production-scale lines, bubble instability frequently appears when drawdown ratio exceeds 5:1 or when frost line height is moved above 600 mm without increasing cooling-air pressure. The resulting thickness variation can be detected as repeating gauge bands in wound rolls; this condition is not reversible by downstream processing and must be corrected by adjusting internal bubble cooling exhaust flow, external air ring pressure, and bubble deresonance. For monolayer film structures at thicknesses between 25 μm and 80 μm, radial gauge variation is commonly held to ±5% by rotating dies or oscillating haul-offs; on fixed dies, the variation may be larger and can affect print registration and heat-seal transfer.
Substitution on an existing LDPE line is not direct. LF 118/21 has lower melt strength and narrower molecular weight distribution than high-pressure LDPE; therefore the bubble shape, die gap, and temperature profile must be re-established. The die gap should be widened, melt temperature reduced, and the die lip temperature increased to reduce melt fracture and improve surface smoothness. Torque increases relative to LDPE at the same screw speed because the more linear structure has lower shear thinning, so extruders with 24:1 L/D or lower may become torque-limited. When LF 118/21 replaces a hexene LLDPE of equivalent density and melt index, the butene comonomer produces shorter ethyl branches and fewer tie-chain linkages between crystals; the result is generally lower dart drop impact and lower tear resistance at equivalent film gauge, although optical clarity and stiffness may remain comparable. Compared with metallocene-catalyzed LLDPE, LF 118/21 has a broader molecular weight distribution and is generally more easily extruded at conventional die gaps, though metallocene grades may exhibit superior impact and clarity. These differences are class-level expectations; specific property comparisons require parallel film trials on the production line using identical die gap, blow-up ratio, and cooling air settings.
Slip and antiblock additives are not universally incorporated in LF 118/21 base shipments; converters typically dose masterbatches at the throat to achieve kinetic coefficient of friction values below 0.35 on filled packaging lines. Erucamide-based slips migrate to the film surface over 24 h to 72 h; full development of slip performance is temperature-dependent and may not be complete immediately after winding. High-shear dispersion of antiblock particles is necessary to prevent lensing and haze; synthetic silica with a median particle size of 3 μm to 5 μm is usually dispersed at letdown ratios corresponding to 1000 ppm to 5000 ppm active content. Incompatibility with amine-containing additives should be avoided because acidic residuals from blown film oxidation can react with amines and cause discoloration. For clean-room or low-haze structures, additive packages are minimized and downstream handling conditions must control roll-to-roll surface contact.
Food-contact suitability is governed by FDA 21 CFR 177.1520 in the United States and EU Regulation 10/2011 in the European Union. Compliance with these frameworks is not determined solely by the base resin; the final film must be tested for overall migration and specific migration under the intended temperature, time, and food simulant conditions. LF 118/21 contains antioxidant stabilization, but the addition of slip, antiblock, or polymer processing aids by the converter can modify organoleptic and migration properties, and these additives must be evaluated separately. REACH obligations under EC 1907/2006 should be confirmed against the current safety data sheet. RoHS Directive 2011/65/EU applies to electrical and electronic equipment articles rather than the resin as supplied; therefore, film converters supplying E&E applications must verify that all intentional additives meet restricted substance limits.
| Standard or regulation | Designation | Relevance and limit to verify |
|---|---|---|
| ASTM D1238 | Melt flow rate | 190°C/2.16 kg; nominal value 1.0 g/10 min |
| ASTM D1505 | Density | Nominal value 0.918 g/cm³ |
| FDA 21 CFR 177.1520 | Olefin polymers | Final film migration limits apply |
| EU Regulation 10/2011 | Plastic food-contact materials | Overall migration limit 10 mg/dm² subject to simulant |
| REACH EC 1907/2006 | Registration and safety data sheet | Confirm supplier status |
| RoHS 2011/65/EU | Homogeneous material limits | Cadmium 100 ppm; lead 1000 ppm; mercury 1000 ppm; hexavalent chromium 1000 ppm |
Thermal and oxidative stability are affected by processing temperature. At melt temperatures above 250°C, the antioxidant package is consumed rapidly and film edge trim may show yellowing or gel. The resin should be kept dry; although polyethylene is not hygroscopic, surface moisture on pellets can generate steam bubbles at the die and form pinholes in film below 30 μm. Silos and hoppers should be purged with dry air in environments where relative humidity exceeds 70% to prevent condensation during overnight shutdown.
Thickness-dependent properties require in-line and off-line verification. Dart drop impact, Elmendorf tear, and tensile elongation are measured after conditioning at 23°C ± 2°C and 50% ± 5% relative humidity per ASTM D618; these values shift with film thickness, and a single data sheet value cannot be extrapolated to all gauges. Seal initiation behavior should be evaluated on a film-specific basis using standard heat-seal testers because seal strength depends on comonomer distribution, surface additives, and dwell time. For adhesive lamination, the film surface should be corona treated to a minimum wetting tension of 38 mN/m to 42 mN/m immediately before coating; treatment decay occurs over hours to days and is faster in high-humidity environments. If exact film performance values are required for a new application, published data for this specific configuration is limited, and parallel film trials on the production line are recommended.