| HS Code | 392419 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) Copolymer |
| Comonomer Type | Butene-1 |
| Melt Index 190 C 2 16 Kg | 1.2 g/10 min |
| Density | 0.918 g/cm³ |
| Melt Flow Ratio I21 I2 | 28 |
| Melting Temperature | 123 °C |
| Vicat Softening Temperature | 94 °C |
| Tensile Strength At Yield Md | 10 MPa |
| Tensile Strength At Break Md | 28 MPa |
| Elongation At Break Md | 600% |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Dart Drop Impact | 120 g |
| Haze | 12% |
| Gloss 45 | 50 |
| Coefficient Of Friction | 0.20 |
As an accredited Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer is packaged in 25 kg moisture-resistant polyethylene bags, palletized and stretch-wrapped for shipping. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Braskem LBH0120PBS LLDPE blown film extrusion polyethylene copolymer: palletized 25 kg bags, stretch-wrapped and secured. |
| Shipping | Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer is shipped as non-hazardous solid resin pellets, typically in 25 kg bags, bulk bags, or bulk trucks. Palletized loads are stretch-wrapped. Transport and store in dry, clean, covered conditions, away from heat, moisture, sunlight, and contamination. Not regulated for standard transport. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packaging closed and palletized to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain moderate ambient temperatures, do not store outdoors, and use first-in, first-out inventory. Follow the manufacturer’s SDS and local regulations for safe handling. |
| Shelf Life | Braskem LBH0120PBS LLDPE copolymer resin has a recommended shelf life of 24 months when stored unopened, dry, and away from heat and sunlight. |
Heavy-duty shipping sack extrusion targets high dart-impact and tear-propagation resistance without excessive blocking on the winder. Butene-copolymer LLDPE tolerates greater bubble deformation than metallocene grades before melt fracture, but its lower melt tension makes frost-line position the primary control for gauge uniformity. Converters running tubular-quench lines with die diameters of 200–300 mm and die gaps of 2.0–2.4 mm usually set blow-up ratio at 2.5:1 to 3.0:1 and maintain melt temperatures between 215 °C and 230 °C. A 90 mm single-screw extruder with 30:1 L/D can sustain outputs of 180–250 kg/h in this process window, with die pressure typically held at 300–400 bar through screen-pack selection. Silica antiblock at 2,000–4,000 ppm and erucamide slip at 500–1,000 ppm are metered in; beyond 5,000 ppm silica, dart impact for 50 µm film can drop from the 80–120 g range typical of this polymer class toward 60–80 g because antiblock particles act as stress concentrators. Dart impact is measured under ASTM D1709 Method A, Elmendorf tear under ASTM D1922, tensile modulus and elongation under ASTM D882, and coefficient of friction under ASTM D1894. The main quality failure mode is a low machine-direction tear value relative to transverse direction, which appears when the frost line is too high and molecular orientation relaxes in the machine direction; operators restore the ratio by lowering the air-ring chiller setpoint and increasing blow-up ratio within the upper limit. Industrial sacks are subject to heavy-metal limits under EU 94/62/EC Annex II and U.S. CONEG model legislation. Terminal articles include valve sacks, open-mouth shipping sacks, bag-in-box inner liners for industrial fills, and industrial form-fill-seal bags.
On high-speed collation-shrink lines for beverage multipacks, the blown-film converter shifts from puncture resistance toward controlled shrink, low blocking, and consistent shrink force. The web must pass through a hot-air tunnel at line speeds above 30 m/min and shrink around cans or bottles without tearing at corner geometries. Film is produced at 45–70 µm with a die gap of 1.6–2.0 mm, a blow-up ratio of 3.0:1, and a frost line height held between 450 mm and 700 mm. The high hoop orientation obtained at this BUR is necessary to reach transverse free-shrink levels above 60% under ASTM D2732 at 130 °C; machine-direction shrink is kept below 45% to avoid tall-pack distortion. Shrink force and release stress are measured under ASTM D2838 to control tunnel dwell time. Erucamide slip is reduced to 300–600 ppm to prevent lubricant bloom from reducing shrink force, and antistatic masterbatch is added at 500–1,500 ppm to assist collation laning. A frost-line height above 3 die diameters allows molecular relaxation and lowers transverse shrink; an excessively low frost line increases blocking and uneven shrink force across the width. Secondary packaging for beverage multipacks is not direct food contact but must meet EU 94/62/EC Annex II heavy-metal limits and REACH SVHC disclosure for EU supply. Terminal articles are collation shrink bundling film, shrink sleeve bundling for PET bottles, and multipack wrap for beverage cans.
Frozen food overwrap reaches a low-temperature seal-strength and puncture-resistance boundary where frost-line position relative to die diameter is the critical process variable. If the frost line falls below 3 die diameters, the quenched bubble retains excessive orientation and may become brittle at freezer temperatures; if it rises too high, optical haze increases and seal initiation widens. Blown-film lines running 25–50 µm overwrap use extruder L/D of 25:1 to 30:1, die gap 1.6–2.0 mm, BUR 2.5:1, and melt temperature 200–225 °C. Slip and antiblock loadings are lower than industrial sacks: erucamide 400–800 ppm and synthetic silica 1,500–3,000 ppm maintain machinability while preserving heat-seal strength. Low-temperature brittleness is measured under ASTM D1790, seal strength under ASTM F88, puncture resistance under ASTM D5748, and dart impact under ASTM D1709. Food-contact compliance requires FDA 21 CFR 177.1520(c) for olefin polymers and EU 10/2011 migration testing with aqueous and fatty simulants appropriate to the intended frozen-food types. Published data for this specific configuration is limited; converters should conduct seal-strength and migration testing on the final structure at sub-zero storage temperatures, particularly for high-fat frozen products where simulant D2 or vegetable-oil substitutes are specified. Terminal articles include frozen vegetable bags, freezer film, frozen seafood overwrap, and carton-overwrap film for frozen food.
Lamination-grade sealant webs for PET/aluminium/LLDPE pouches require a surface that reaches and holds a corona treatment level of 38–42 dyn/cm under ASTM D2578 while retaining a low coefficient of friction after winding. The sealant web is produced as a monolayer or coextruded layer at 25–50 µm, with die gap 1.6–2.0 mm, BUR 2.2:1 to 2.6:1, and melt temperature 205–225 °C. Erucamide slip is kept to 300–700 ppm, synthetic silica antiblock at 1,000–2,500 ppm, and polymer processing aid at 200–600 ppm to delay melt fracture during thin-gauge extrusion. The principal process conflict occurs during corona treatment: oxidation raises surface energy for adhesive lamination but can degrade migratory slip molecules on the treated surface, raising kinetic coefficient of friction by more than 0.10 in ASTM D1894 sled tests if the treater power is too aggressive. Seal initiation temperature and heat-seal strength are measured under ASTM F88, hot-tack under ASTM F1921, and surface treatment under ASTM D2578. Direct food-contact compliance for the final laminate is evaluated under FDA 21 CFR 177.1520(c) and EU 10/2011; REACH SVHC declarations are required for EU supply. Terminal articles include stand-up pouches, coffee-bag lamination, snack-food laminates, and non-retort pouch structures where the LLDPE sealant layer provides seal integrity below 100 °C.
Industrial liner films extruded without internal bubble cooling rely entirely on the external air ring for melt solidification; this restricts heat-transfer rate and makes frost-line position the limiting factor for output and gauge uniformity at heavy thickness. For liners of 100–200 µm used inside fibre drums, corrugated boxes, and FIBC inserts, the process typically starts with a single-screw extruder of 30:1 L/D, a die diameter of 250–400 mm, die gap 2.0–2.4 mm, BUR 2.0:1 to 2.5:1, and melt temperature 210–235 °C. Without internal bubble cooling, raising output above the air-ring capacity generates a high frost line and causes web wander; lowering output to stabilise the bubble increases residence time and can over-degrade the slip additive if melt temperature is not reduced concurrently. Erucamide slip at 700–1,000 ppm and silica antiblock at 2,500–5,000 ppm are used to achieve low insertion force into boxes and drums, with coefficient of friction monitored under ASTM D1894. Industrial liners do not normally require food-contact registration unless the filled product is food; heavy-metal limits under EU 94/62/EC Annex II and the U.S. CONEG model apply. Mechanical acceptance tests include dart impact under ASTM D1709, Elmendorf tear under ASTM D1922, tensile properties under ASTM D882, and conditioning under ISO 291. Terminal articles include FIBC liners, fibre-drum liners, corrugated-box liners, and chemical bag liners.
The compliance matrix below consolidates the principal regulatory anchors and test methods for the downstream contexts described above.
| Application context | Regulatory anchor | Key test methods | Typical additive constraint |
|---|---|---|---|
| Agricultural silage cover | EN 13206:2017, REACH SVHC | ISO 527-3, ISO 6383-2, ASTM D1709, ASTM G154 | HALS 2,500–6,000 ppm, silica 2,000–4,000 ppm |
| Heavy-duty shipping sack | EU 94/62/EC Annex II, CONEG | ASTM D1709, ASTM D1922, ASTM D882, ASTM D1894 | Silica 2,000–4,000 ppm, erucamide 500–1,000 ppm |
| Collation shrink film | EU 94/62/EC Annex II, REACH SVHC | ASTM D2732, ASTM D2838 | Erucamide 300–600 ppm, antistatic 500–1,500 ppm |
| Frozen food overwrap | FDA 21 CFR 177.1520(c), EU 10/2011 | ASTM D1790, ASTM F88, ASTM D5748, ASTM D1709 | Erucamide 400–800 ppm, silica 1,500–3,000 ppm |
| Lamination sealant web | FDA 21 CFR 177.1520(c), EU 10/2011, REACH SVHC | ASTM D2578, ASTM F88, ASTM F1921, ASTM D1894 | Erucamide 300–700 ppm, silica 1,000–2,500 ppm |
| Industrial liner film | EU 94/62/EC Annex II, CONEG | ASTM D1709, ASTM D1922, ASTM D882, ASTM D1894, ISO 291 | Erucamide 700–1,000 ppm, silica 2,500–5,000 ppm |
Competitive Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
For converters evaluating blown film LLDPE for gauge-critical liners, carrier bags, overwrap, and agricultural film, Braskem LBH0120PBS is a butene-comonomer linear low-density polyethylene copolymer with a nominal density of 0.920 g/cm³ per ASTM D1505 and a nominal melt index of 1.0 g/10 min per ASTM D1238 at 190 °C/2.16 kg. The resin is designed for monolayer and coextruded blown film extrusion. The PBS designation is associated with a formulated slip/antiblock surface package intended to reduce film-to-film coefficient of friction and blocking in high-speed converting lines. Published data for the exact additive concentration in the public datasheet is limited; the property values in Table 1 are representative values reported for the grade family and should be verified against the current Braskem certificate of analysis before lot-specific conversion.
| Property | Nominal value | Test method |
|---|---|---|
| Melt index | 1.0 g/10 min | ASTM D1238, 190 °C/2.16 kg |
| Density | 0.920 g/cm³ | ASTM D1505 |
| Tensile strength at yield, MD/TD | 11 / 11 MPa | ASTM D638 |
| Tensile strength at break, MD/TD | 40 / 32 MPa | ASTM D638 |
| Elongation at break, MD/TD | 750 / 850 % | ASTM D638 |
| Secant modulus at 1% strain, MD/TD | 230 / 250 MPa | ASTM D638 |
| Elmendorf tear, MD/TD | 420 / 500 gf | ASTM D1922 |
| Dart impact strength, F50 | 130 g | ASTM D1709A |
| Haze | 15 % | ASTM D1003 |
| Gloss at 45° | 55 | ASTM D2457 |
| Kinetic coefficient of friction | 0.10 | ASTM D1894 |
| Vicat softening temperature | 101 °C | ASTM D1525 |
The butene comonomer architecture produces a linear backbone with short-chain branching distribution that differs from high-pressure LDPE and from hexene/octene metallocene LLDPE. Molecular weight distribution and comonomer placement influence extensional viscosity, tear propagation, and seal initiation. Density and melt index alone are insufficient to predict orientation behavior, dart puncture energy, or optical uniformity in the finished film. The grade is therefore positioned as a conventional Ziegler-Natta blown film resin for processors seeking a balance between rupture resistance and processability rather than maximum low-temperature impact or clarity.
A melt index of 1.0 g/10 min places the resin in a higher-viscosity segment of the blown film LLDPE range. On a 40 mm to 75 mm extruder with L/D 24 to 30 and a barrier or Maddock mixing screw, the melt temperature is generally held between 190 °C and 220 °C. Die adaptor pressure depends on output, die diameter, and die gap, but for a 50 mm line operating at 90–120 kg/h, adaptor pressure commonly falls in the 180–260 bar range. Exceeding 230 °C is not recommended because oxidative degradation may increase gel counts and reduce film tear resistance, particularly at high screw speed.
Bubble stability is managed through die gap selection of 1.5–2.5 mm and blow-up ratios of 2.0:1–3.0:1. Narrow die gaps increase shear and can improve gauge uniformity, but excessive shear may approach the critical shear stress for sharkskin melt fracture, commonly reported for LLDPE in the 0.14–0.20 MPa range. In such conditions, the preferred corrective action is to increase die gap or melt temperature rather than reduce output alone. A frost line height of 6–10 die diameters is typical for this resin. Higher frost lines can reduce internal haze by allowing slower crystal nucleation, while lower frost lines improve bubble stability and throughput but may raise haze and gauge scatter.
Processors operating internal bubble cooling with the 1.0 g/10 min melt index report sufficient melt strength to sustain 2.5:1 BUR at 50 µm gauge without bubble flutter, provided the air ring is not over-tightened. When down-gauging below 20 µm, bubble respiration, edge curl, and die-lip oxidation increase. A dual-lip air ring, internal bubble cooling, and melt temperature within the 190–220 °C band are typically required. Slip additive migration can also produce lip plate-out over extended runs; periodic lip cleaning and purge with LDPE or LLDPE purge compounds reduce die-streak formation.
Gauge variation on automatic thickness control lines can be maintained within ±5% at 50 µm, while manual systems frequently show ±8–10%. The variation is influenced by die eccentricity, cooling air distribution, and ambient air movement. Motor load for the 1.0 g/10 min LLDPE is generally lower than for a high-pressure LDPE of equivalent melt index because of reduced long-chain branching, but higher than for a 2.0 g/10 min LLDPE of similar density. Extruder drives should be sized for sustained operation near the upper end of the recommended output range rather than for short-term peak output.
The branching architecture of butene-copolymerized LLDPE differs from hexene and metallocene-catalyzed grades. Butene comonomer produces shorter chain branches and generally broader molecular weight distribution in conventional Ziegler-Natta products. This yields processability advantages on smooth-bore extruders but lower dart puncture energy and lower Elmendorf tear than hexene grades of similar density and melt index. In comparative film tests, dart impact by ASTM D1709A may be lower by 10–30% relative to hexene/octene metallocene grades, although published data for this specific configuration is limited and must be confirmed by side-by-side converter trials.
Relative to high-pressure LDPE, the linear structure raises elongation at break and dart impact at equivalent gauge, but reduces melt strength in high-stalk bubble configurations. The 0.920 g/cm³ density provides a balance between stiffness and seal initiation temperature. Seal initiation for LLDPE of this density is typically in the 95–110 °C range under 0.5 s dwell, but converter validation is required because seal bar pressure, dwell time, and film surface slip modify heat transfer at the seal interface. Hot tack strength is lower than for high-pressure LDPE blends; form-fill-seal operations may require blending with 20–30% LDPE to extend the heat-seal plateau.
The PBS surface formulation distinguishes this grade from unmodified LLDPE of the same base density. In high-speed converting, film-to-film kinetic coefficient of friction measured per ASTM D1894 is typically below 0.20 for the slip package, while unmodified film can exceed 0.60. Blocking force per ASTM D3354 is reduced, permitting roll naps and side-gusseted bags to unwind without web breaks. However, the antiblock component raises haze by a measurable amount; the trade-off must be evaluated in clarity-critical packaging where gloss and see-through appearance control consumer rejection rates.
Slip migration is time-dependent. Coefficient of friction decreases over 24–72 h after extrusion at 23 °C as the slip additive migrates to the film surface. In cold storage below 10 °C, migration slows and coefficient of friction may remain elevated during the first days of storage. Antiblock performance is also gauge-dependent. Thick films above 100 µm may require higher antiblock levels than thin films, and the standard PBS formulation may not be sufficient for all applications. When recycled LLDPE is introduced, gel count, density drift, and slip/antiblock dilution must be monitored because they alter bubble stability, coefficient of friction, and optical properties.
In food-contact and regulatory review, the grade is positioned under the olefin polymer provisions of FDA 21 CFR 177.1520 and EU Regulation 10/2011, provided the final article meets migration limits and use conditions. For EU food-contact compliance, overall migration should not exceed 10 mg/dm² under the selected food simulant. Specific migration of heavy metals is governed by EU 94/62/EC, with a combined lead, mercury, cadmium, and hexavalent chromium limit of 100 mg/kg by weight. REACH compliance under EC 1907/2006 depends on batch-specific SVHC declarations; processors should request a certificate of compliance because additive packages may vary by production site.
| Regulatory dimension | Standard / clause | Typical limit or condition |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520 | Olefin polymer provisions for food-contact use |
| EU food contact | EU Regulation 10/2011 | Overall migration ≤ 10 mg/dm² |
| Packaging heavy metals | EU 94/62/EC | Sum Pb, Hg, Cd, Cr(VI) ≤ 100 mg/kg |
| REACH | EC 1907/2006 | SVHC content < 0.1 % w/w per article |
| RoHS recast | Directive 2011/65/EU | Pb ≤ 1000 mg/kg, Cd ≤ 100 mg/kg where applicable |
| Service temperature | Derived from Vicat softening | Continuous use below 80 °C; not for retort or autoclave |
The product is not recommended for retort, autoclave, or continuous service above 80 °C, because the Vicat softening temperature of 101 °C per ASTM D1525 indicates dimensional softening under elevated thermal load. Although polyolefins are not hygroscopic, pellet surface moisture at relative humidity above 60% should be removed by hopper drying at 60–80 °C for 1–2 h to avoid steam bubbles in the melt film. Do not melt blend with polymers that release acidic volatiles such as PVC, because the slip package may be deactivated and die-lip deposits may increase. Purging should be performed with LDPE or LLDPE purge materials; combination with amine-containing polyamide purge compounds can produce odor and color shifts. In applications where high clarity is the acceptance criterion, a non-antiblock grade should be evaluated instead.