Braskem In34 Lldpe Injection Molding Polyethylene Copolymer

Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer

    • Product Name: Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 260394
    Density 0.924 g/cm³
    Melt Index 34 g/10 min
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 10 MPa
    Elongation At Break 700%
    Flexural Modulus 260 MPa
    Notched Izod Impact Strength 80 J/m
    Vicat Softening Temperature 90 °C
    Melting Temperature 122 °C
    Brittleness Temperature < -70 °C
    Shore D Hardness 50
    Mold Shrinkage 1.5-2.0%
    Thermal Expansion Coefficient 2.0e-4 /°C
    Volume Resistivity > 1e15 ohm·cm
    Dielectric Constant At 1 Mhz 2.3
    Dissipation Factor At 1 Mhz 0.0005

    As an accredited Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem IN34 is supplied in 25 kg polyethylene-lined bags, palletized; bulk bags and bulk trucks are also available.
    Container Loading (20′ FCL) 20′ FCL loading: Braskem IN34 LLDPE injection molding polyethylene copolymer, 25 kg bags, palletized; typically 18–20 MT per container.
    Shipping Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer is non-hazardous and not regulated for transport. It is typically shipped in 25 kg moisture-barrier bags, octabins, or bulk trucks/railcars. Keep dry and away from heat, sunlight, and contamination. Follow local regulations and the SDS.
    Storage Store in a cool, dry, well-ventilated warehouse. Keep material in original sealed bags or packaging, palletized and off the floor. Protect from direct sunlight, heat, moisture, and contamination. Avoid prolonged high temperatures, open flames, and ignition sources. Maintain good housekeeping and prevent dust accumulation. Store away from incompatible materials. Use first-in, first-out stock rotation. Inspect containers regularly for damage. Follow manufacturer SDS and label instructions.
    Shelf Life Braskem IN34 LLDPE has a typical shelf life of 12–24 months when stored unopened in a cool, dry, ventilated area.
    Application of Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer

    Where Thin-Wall Dairy Container Moulding Departs From Conventional LLDPE Processing

    In thin-wall dairy container production, IN34 is processed only after food-contact status is confirmed against FDA 21 CFR 177.1520 for olefin polymers and Commission Regulation (EU) No 10/2011 for plastics intended to come into contact with food. The finished article is evaluated for overall migration at 10 mg/dm²; fatty dairy products require simulant D2 under the intended contact time and temperature, while aqueous products are assigned simulant A at 10% ethanol and acidic products simulant B at 3% acetic acid, with migration testing carried out according to EN 1186. Before production, melt mass-flow rate is verified using ISO 1133-1:2022 and density using ASTM D792-20; lot-to-lot variation outside the datasheet tolerance alters fill pressure and screw recovery time in multi-cavity tooling. The compound is run at 100 parts by weight IN34 with 2–4 wt% polyolefin-based colour masterbatch; external demolding aids are excluded because silicone or amide release agents can raise global migration after repeated use. Downstream processing is thin-wall injection moulding on high-speed electric or hydraulic toggle machines with clamp forces between 150 and 350 t. Melt temperature is held at 190–230°C, mould surface temperature at 10–30°C, and injection velocity is profiled at 150–300 mm/s to minimize gate blush at the side or diaphragm gate. Holding pressure is set at 40–65 MPa and switched to holding at 95–98% screw position. Vent depth is maintained at 0.02–0.04 mm, draft angle above 1.5°, and cooling time is calculated from the thickest cross-section. The principal process failure observed on production lines is gate freeze followed by sink in the container base, corrected by shortening the gate land to 0.5–1.0 mm and increasing pack pressure while maintaining a screw cushion above 2–6 mm. If the container includes an integral hinge, cyclic flexing performance must be validated on the actual part; published IN34-specific hinge life data is limited. Terminal finished product types include yogurt cups, dairy spread tubs, margarine packs, deli salad containers, and corresponding flat lids.

    Which Closure Markets Can Use IN34 Without Sacrificing Torque Retention?

    Closure applications require a controlled balance between environmental stress-crack resistance under oil or wetting agents and dimensional stability at the tamper-evident band. IN34 is appropriate for non-carbonated closures where oxygen barrier is not the limiting requirement; it should not replace polypropylene in high-pressure carbonated beverage closures unless the closure geometry has been reinforced. Compliance is established under FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011 with migration testing by EN 1186, and, where child-resistant function is required, ISO 8317 or 16 CFR 1700. The compound is run at 100 parts by weight IN34; colour masterbatch is added at 2–4 wt%, and slip or antiblock masterbatch is added at 0.3–0.8 wt% only when cap stacking requires reduced surface friction. Processing aid additions above 0.2 wt% are avoided because they can lower screw friction and reduce torque retention at the tamper band. Downstream processing is closure injection moulding on 120–250 t high-speed machines with single-cavity or multi-cavity hot-runner tooling and thermal or valve gates. Melt temperature is set at 200–235°C, mould temperature at 10–35°C, and injection velocity at 80–180 mm/s to control turbulent filling at the centre gate. Pack pressure is held at 35–55 MPa for 1.5–3 s, followed by post-mould cap cooling on a water or air conveyor for 4–8 s and liner insertion where specified. The limiting failure mode is creep of the tamper-evident band after torque application, and published IN34-specific creep data under food-oil exposure is limited; torque retention therefore requires validation on the actual filling line using cap tightness measurement according to the end-user specification. Terminal finished product types include snap lids, dispensing flip caps, tamper-evident screw caps for dairy, sauces, dry foods, and non-carbonated beverages.

    Refrigerator storage boxes and kitchen tool handles moulded from IN34 present a thicker-wall processing regime than thin-wall packaging, which changes solidification rate and sink-mark control. Compliance for repeated food-contact kitchenware is based on FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011; in Germany, BfR Recommendation III for polyethylene provides an additional verification path for household contact at refrigerator and room temperatures. The compound is run at 100 parts by weight IN34 with 2–4 wt% food-approved polyolefin colour masterbatch; anti-static, nucleating, or filler additions are not normally used because they disturb the low-warpage characteristic of the copolymer. Downstream processing on 150–350 t injection moulding machines uses a melt temperature of 190–220°C, mould temperature of 15–40°C, and two-stage injection speed: the initial stage fills the hinge region at 70–120 mm/s, and the second stage completes the sidewall at 100–180 mm/s. Holding pressure is set at 30–50 MPa for 5–10 s depending on wall thickness, and gate seal is confirmed by screw position stability rather than timer only. Deep-draw refrigerator boxes require vent depths of 0.02–0.04 mm and core draft angles of at least 1.5° to avoid ejection-pin penetration because LLDPE parts remain flexible at demolding temperature. Terminal finished product types include refrigerator storage containers, modular freezer boxes, kitchen drawer dividers, serving trays, and utensil handles where soft-touch overmolding is not specified.

    Toy Structural Parts and Heavy-Element Migration Compliance

    Toy component moulding with IN34 requires the compound to pass heavy-element extraction limits even when coloured masterbatches are used, because pigment carriers and metal compounds may be extracted from the polymer matrix. The governing standards are EN 71-3:2019+A1:2021 for migration of arsenic, cadmium, chromium, lead, mercury, antimony, barium, and selenium; ASTM F963-23 for heavy-element solubility in accessible toy parts; and REACH Regulation (EC) No 1907/2006 Annex XVII for restricted substances, although phthalate plasticizers are not required in this polyethylene. The formulation is set at 100 parts by weight IN34 with 2–3 wt% colour masterbatch whose pigment components carry EN 71-3 certificates. Antimony-based white pigments are not used unless the antimony extraction result remains below the 60 mg/kg limit; no external plasticizer or low-molecular-weight processing oil is added because such components can contribute to organic extractables. Downstream processing uses multi-cavity tools on 120–280 t machines with melt temperatures of 190–220°C, mould temperature of 10–35°C, and fill speeds of 60–150 mm/s. Gate locations are placed on non-visible surfaces to prevent flow lines on small structural parts. Because toy parts have minimum wall thicknesses of 0.8–1.5 mm and multiple bosses or snap fits, the packing phase is set at 30–45 MPa and cooling time is determined by the thickest section using 10–15 s for a 2 mm wall; ejection is assisted by core pulling rather than high ejector force. Terminal finished product types include miniature vehicle bodies, building block bases, role-play kitchen accessories, and board game structural components.

    Medium-duty stack/nest crates, bread trays, and industrial totes impose long flow paths and ribbed bases that require wide gates and programmed holding pressure rather than elevated melt temperature. The applicable compliance framework is REACH Regulation (EC) No 1907/2006 for general industrial articles; when the crate is used for direct contact with dry foods, Commission Regulation (EU) No 10/2011 applies, and for export to North America FDA 21 CFR 177.1520 applies if the article is sold as food contact equipment. The compound is run at 100 parts by weight IN34 with 2–5 wt% colour masterbatch; outdoor-weatherable articles add 0.2–0.5 wt% hindered amine light stabilizer masterbatch and 0.05–0.15 wt% antioxidant masterbatch, but these additions must be reduced or eliminated for direct food-contact crates. Downstream processing is performed on 350–800 t injection moulding machines with sequential valve-gated multi-gate tooling to avoid knit lines along the base grid and handle areas. Melt temperature is held at 190–220°C, mould temperature at 10–30°C for cycle-time control, and injection speed at 40–120 mm/s; speeds above 200 mm/s create flow marks on flat sidewalls. Packing pressure is set at 45–65 MPa with 8–15 s hold time, and the screw cushion is maintained above 2–6 mm to prevent sink on the ribbed bottom. Failures observed on industrial lines are predominantly gate blush at valve pin marks and warpage caused by non-uniform cooling; multi-zoned mould thermolators controlled to ±2°C reduce warpage. Tensile strength and impact resistance are verified by ASTM D638-14 and ASTM D256 at 23°C. Terminal finished product types include stackable distribution totes, bread trays, mushroom harvesting crates, dairy transport boxes, and warehouse storage bins.

    When Zero-Burr Moulding of Appliance Internal Parts Requires Low-Temperature Ductility

    Internal appliance components such as defrost drain trays, blower wheel covers, and detergent dispenser bodies require the moulded part to survive low-temperature impact and mechanical assembly without burr or flash. IN34 can be considered when the part does not require continuous service above 70–80°C and when the electrical safety requirement is limited to UL 94 HB under IEC 60695-11-10; appliance end-product standards such as EN 60335-1 govern the component through the final product certification. Compliance includes RoHS Directive 2011/65/EU, REACH Regulation (EC) No 1907/2006, and UL 94 HB where the part is a non-flame-retardant functional internal component. The compound is run at 100 parts by weight IN34 with 2–4 wt% appliance-grey or white masterbatch; where UL 94 V-2 or V-0 performance is required, a halogen-free flame-retardant masterbatch at 20–30 wt% may be necessary, but published data on IN34 compounded at that loading is limited, so mechanical properties must be reconfirmed by ASTM D638-14 and ASTM D256. Downstream processing is injection moulding on 180–350 t machines with precision shut-off nozzles. Melt temperature is set at 190–220°C, mould temperature at 10–35°C, injection speed at 50–120 mm/s, and holding pressure at 35–55 MPa. Venting depth of 0.015–0.03 mm is critical because the low melt viscosity of the grade can produce fine flash at parting lines if clamping force is below 4 kN/cm² of projected area. Demolding is assisted by draft angles of 1–2°; forced ejection of hot parts below the heat deflection temperature produces white stress marks, so cooling time is set by the thickest cross-section. Terminal finished product types include washing machine detergent dispenser housings, refrigerator defrost trays, dishwasher internal water management components, and appliance cable carrier parts.

    Free Quote

    Competitive Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem IN34 is a linear low-density polyethylene injection molding copolymer characterized by a nominal melt flow rate of 30 g/10 min when measured at 190 °C under a 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022. The nominal density is 0.934 g/cm³ as determined by ASTM D1505 or ISO 1183-1:2019. The material is a butene-1 copolymer, and the inclusion of ethyl short-chain branches reduces crystallite thickness relative to high-density polyethylene. The result is a resin positioned at the upper density boundary of the LLDPE category, with melt fluidity approximately one order of magnitude higher than typical blown-film LLDPE. This attribute makes the grade suitable for injection molding of thin-wall parts, while the comonomer content provides a ductility profile different from high-flow HDPE injection grades. Because the product is not a film-extrusion resin, spiral-flow behavior, gate-freeze characteristics, and mold release behavior are more relevant design inputs than blown-film bubble stability or haul-off tension.

    What Processing Advantages Emerge from the 30 g/10 min Flow Class?

    The 30 g/10 min flow classification does not define a single viscosity; it indicates that the material has a relatively low weight-average molecular weight and a comparatively narrow molecular weight distribution for injection molding. On a capillary rheometer operating at 190 °C, the apparent shear viscosity of a 30 g/10 min linear low density polyethylene at 100 s⁻¹ is typically lower than that of a 10–20 g/10 min injection molding grade, but the melt remains shear-thinning because of the short-chain branching and chain entanglements. This non-Newtonian behavior reduces energy input during plastication and permits shorter screw-recovery times on general-purpose reciprocating screws with L/D ratios of 20:1 to 24:1.

    On horizontal injection molding machines with clamp forces from 800 kN to 4000 kN, the grade is commonly processed at melt temperatures between 180 °C and 230 °C, with mold temperatures between 10 °C and 40 °C. The lower temperature boundary is controlled by viscosity rise; below 180 °C, frozen-layer formation at the flow front can increase filling pressure and produce short shots in wall sections thinner than 1.0 mm. The upper temperature boundary is controlled by thermo-oxidative chain scission; above 230 °C, yellowness index and odor-active volatiles may increase if melt residence time is not tightly controlled. The usable processing window is therefore narrower than that of many HDPE injection grades, and production conditions should be verified by measuring actual melt temperature in the nozzle rather than relying solely on barrel set-points.

    Process control on high-cavitation tools benefits from the high MFR because pressure drop through hot-runner manifolds and narrow gate diameters is reduced. However, high melt fluidity increases the risk of flash on worn parting lines and can permit jetting if gate velocities are not controlled by sequential valve-gate sequencing. Cavity-pressure transfer from velocity-controlled filling to pressure-controlled packing is typically set in the range 30–50 MPa for thin-wall food packaging; lower transfer pressures can produce sink marks at rib intersections, while higher transfer pressures can increase molded-in stress and warpage after ejection. These operating boundaries are derived from general high-flow LLDPE injection practice; the resin supplier’s process datasheet and mold-flow simulation inputs should be used to establish lot-specific setpoints.

    Molecular architecture separates IN34 from HDPE and from LLDPE film grades in terms of crystallinity, density, and mechanical response. The butene-1 comonomer substitutes ethyl branches along the polyethylene backbone; these branches interrupt lamellar ordering and reduce density to 0.934 g/cm³. A high-density polyethylene injection grade of comparable melt flow rate would normally have a density above 0.952 g/cm³, and would exhibit higher flexural modulus but lower environmental stress-cracking resistance when exposed to surfactants, oils, and fatty acid solutions. The LLDPE film resin with melt flow rates below 2 g/10 min offers high melt strength for blown film, but its viscosity during mold filling is too high for sprues, runners, and thin-wall cavities with wall thickness below 1.2 mm. IN34 occupies a narrow formulation space in which melt fluidity is raised to injection-molding levels while density remains low enough to preserve ductility and stress-cracking resistance.

    In comparison with random copolymer polypropylene, the IN34 grade has lower flexural modulus and lower heat deflection temperature but greater resistance to stress whitening and lower density. The tensile modulus of injection-molded LLDPE of 0.934 g/cm³ density is typically in the range 350–500 MPa, whereas random copolymer polypropylene often exceeds 900–1200 MPa. This difference affects part removal, capping, living-hinge behavior, and stack-load deformation. Polyethylene is not used for living hinges because it undergoes stress whitening and permanent deformation under repeated flexural loading, but the lower modulus is advantageous for snap-fit covers and closures that must tolerate multiple assembly cycles.

    Specification Data and Certificate of Conformance Parameters

    The following table compiles commonly listed physical property values for injection-molded specimens of Braskem IN34. These values are typical and should not be interpreted as contractual lot-release limits; the certificate of conformance for a specific lot applies only to the parameters listed on that document.

    PropertyTypical ValueTest Method
    Nominal melt flow rate30 g/10 minASTM D1238, 190 °C/2.16 kg
    Nominal density0.934 g/cm³ASTM D1505
    Tensile strength at yield15 MPaASTM D638
    Tensile elongation at break>800%ASTM D638
    Flexural modulus, 1% secant450 MPaASTM D790
    Notched Izod impact, 23 °C5.0 kJ/m²ASTM D256
    Vicat softening point110 °CASTM D1525
    Hardness, Shore D56ASTM D2240

    Lot-level release testing on injection molding grades typically includes melt flow rate and density only. Mechanical properties in the table are determined from specimens injection-molded under defined conditions, and values can shift with gate type, packing pressure, mold temperature, and cooling time. When comparing IN34 with other products, one should not substitute datasheet values for end-use testing; properties such as weld-line strength, frozen-in orientation, and post-mold dimensional change depend on tool geometry and processing.

    On a 1500 kN toggle-clamp machine with a 24:1 L/D screw and 32-cavity hot-runner tool, the high MFR of IN34 allows short fill times in applications such as dairy container lids and thin-wall food storage boxes. Process monitoring frequently focuses on screw-recovery time and melt cushion consistency; lot-to-lot variation in melt flow rate can appear as changes in recovery time, dosing stroke, and injection pressure at the same barrel temperature. A sustained increase in screw-recovery time above 10% of the baseline can indicate a lower-MFR lot, contaminated feed, or worn check-ring leakage, and should trigger melt flow verification by ASTM D1238 on retained samples.

    Failure modes observed in injection molding of high-flow LLDPE include jetting, gate blush, and sink marks caused by insufficient packing. Jetting is more likely when the melt passes through small submarine gates or pinpoint gates at high velocity, while gate blush can be mitigated by reducing injection velocity at the beginning of fill and by using larger gate diameters with land lengths appropriate for the part thickness. Sink marks in boss and rib areas are controlled by packing pressure and packing time rather than by material change alone; because IN34 has a high MFR, the packing window is shortened by rapid gate freeze. The part and runner system must be designed so that the gate remains open long enough for volumetric shrinkage compensation before solidification of the gate region.

    When Thin-Wall Food Contact and Closure Applications Require Ductility

    For food storage containers with nominal wall thickness below 1.5 mm, IN34 is specified where low-temperature ductility, low warpage, and acceptable organoleptic properties are required. Injection-molded lids and closures produced from this grade are tested for dimensional stability after 48 h of post-molding crystallization at 23 °C; the density of 0.934 g/cm³ results in greater crystalline shrinkage than low-density polyethylene but less than HDPE. Shrinkage anisotropy is influenced by flow-induced orientation; the use of mold temperatures below 40 °C accelerates skin solidification and can increase in-plane orientation and post-mold warpage. For round lids, processing adjustments such as reduced injection velocity near the end of fill and uniform cooling layout reduce out-of-roundness.

    Regulatory clearances for food-contact applications must be verified on the specific formulation and lot. Polyethylene homopolymers and copolymers are covered by FDA 21 CFR 177.1520, but the applicable paragraph depends on density, extraction limits, and intended food type. The resin supplier’s food-contact declaration should be reviewed for migration limits under 21 CFR 177.1520(c) and for compliance with applicable European Union plastics regulations. Heavy metal and substance restrictions under REACH and RoHS should be validated through supplier declarations or third-party testing for each finished article, because downstream colorants and processing aids can alter final compliance status.

    Thermal and Chemical Resistance Boundaries Are Set by the LLDPE Backbone

    The upper service temperature of IN34 is lower than that of polypropylene and far lower than semicrystalline engineering resins. The Vicat softening point near 110 °C does not allow continuous use at boiling-water temperatures; hot-fill applications should be validated under hydrostatic load and closure torque because softening can reduce seal force. The material resists many aqueous detergent solutions, dilute acids, and alkalis, but it is susceptible to swelling and stress cracking in contact with aromatic hydrocarbons, chlorinated solvents, and unsaturated fatty esters. Oxidative degradation during melt processing can be controlled by maintaining melt temperature below 230 °C; if regrind is used, the fraction should be limited to maintain consistent viscosity and to avoid cumulative thermal stabilizer depletion. No hydrolysis drying is required because polyethylene does not undergo hydrolytic chain scission, but surface moisture on pellets stored at relative humidity above 60% can cause splay and must be managed with covered hoppers or predrying at 70–80 °C for 1–2 hours in a desiccant dryer.

    Outdoor weathering is not an intended performance attribute of unfilled IN34. If articles are exposed to UV radiation, a UV stabilizer masterbatch should be compounded into the resin at the press or purchased as a pre-compounded variant, and retention of mechanical properties after exposure should be evaluated by ASTM G154 or ISO 4892-2. Chemical compatibility testing should follow ASTM D543 or equivalent, with the specific service chemical, stress condition, and exposure temperature. Published data for this specific grade under aggressive chemical and UV exposure are limited; end-use testing is therefore required before production release.

    Top