Braskem If33 Lldpe Injection Molding Polyethylene Copolymer

Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer

    • Product Name: Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 777072
    Melt Flow Rate 33 g/10 min (190°C/2.16 kg)
    Density 0.924 g/cm³
    Comonomer Butene-1
    Melting Point 122 °C
    Vicat Softening Temperature 94 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 12 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Shore D Hardness 50
    Notched Izod Impact At 23 C 80 J/m
    Notched Izod Impact At 20 C 40 J/m
    Environmental Stress Crack Resistance >1000 h (10% Igepal, 50°C)
    Mold Shrinkage 1.5-2.0%
    Thermal Expansion Coefficient 1.5E-4 /°C

    As an accredited Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer is packaged in 25 kg polyethylene bags, palletized for industrial bulk handling.
    Container Loading (20′ FCL) Container loading (20′ FCL): 25 kg bags, palletized, stretch-wrapped, secured; approximately 18–22 MT net Braskem IF33 LLDPE copolymer for injection molding.
    Shipping Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer is shipped as non-hazardous solid pellets in moisture-barrier bags, octabins, or bulk trucks/railcars. No special placarding is required. Keep containers dry, cool, and protected from moisture, heat, UV light, and contamination. Store in a cool, dry, well-ventilated area during transport.
    Storage Store Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer indoors in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, ignition sources, and strong oxidizers. Use closed original containers or lined bins, palletized, clean, and dry. Prevent moisture, contamination, and excessive stacking. Maintain stable temperatures to avoid softening or pellet blocking. Follow SDS, local regulations, and first-in, first-out stock rotation.
    Shelf Life Braskem IF33 LLDPE typically has a 12-month shelf life when stored in original packaging, cool, dry, and protected from sunlight.
    Application of Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer

    Thin-wall injection moulding of IF33 for dairy spread cups, delicatessen packs, freezer-tray inserts, and snap-on lids places the resin’s flow-length-to-wall-thickness behaviour at the centre of tooling decisions. In high-cavitation tooling, IF33 is processed as 100% natural pellets or as a dry blend of 85–95 wt% IF33 with 5–15 wt% LDPE where improved pin-hole tear and hinge flexibility are required. Colour masterbatch is dosed at 2–4 wt%, and slip/antiblock masterbatch at 1.0–2.0 wt%, depending on denesting force and lid-to-tub release behaviour. Melt temperature is held at 220–235 °C, mould temperature at 15–30 °C, injection velocity at 180–260 mm/s, and cavity pressure during pack at 35–55 MPa; screw decompression before recovery is kept below 5 mm to avoid nozzle drool in hot-runner valve-gated tools. A general-purpose polyolefin screw with L/D 20:1–24:1 and compression ratio 2.5:1–3.0:1 is sufficient for homogenization. The primary process conflict is shear heating in the hot runner and valve gate: excessive melt temperature at the gate produces odour and organoleptic drift in dairy applications, while insufficient temperature causes flow marks and cavity-to-cavity weight variation. Food-contact compliance is assessed under FDA 21 CFR 177.1520 and EU Regulation 10/2011, with overall migration testing according to EN 1186 parts 1 and 14. Terminal converted articles include heat-sealed dairy cups, deli packs, freezer-tray inserts, and snap-on lids; seal-peel performance is not controlled by the resin alone but by the interface between the moulded edge and the lid film, and tool maintenance controls gate vestige below 0.10 mm.

    Where the finished article is sold into retail food service, the following compliance matrix applies:

    Compliance domainStandard / clauseParameter / limitTest condition
    US FDA food contactFDA 21 CFR 177.1520Olefin polymer specificationFood-type extraction end tests
    EU food contactEU Regulation 10/2011OML 10 mg/dm²EN 1186 migration series
    REACHEC 1907/2006 Annex XVIISVHC communication 0.1% w/wArticle-level declaration
    RoHS2011/65/EU Annex IIPb 1000 ppm, Cd 100 ppmXRF and wet chemistry

    What Limits ESCR Retention in IF33 Closure Blends When Melt Temperature Exceeds 230 °C?

    Closure injection tooling running IF33 in the 20–40 wt% blend band for HDPE-based tamper-evident caps demonstrates a measurable improvement in environmental stress crack resistance under ASTM D1693, but only when the melt is not overheated. The addition ratio is reversed in flexible dispensing closures, where IF33 can be used at 70–100 wt% with HDPE or LDPE at 0–30 wt% to tune hinge memory and squeeze recovery. Melt temperature for closure moulding is normally set between 190 °C and 220 °C; exceeding 230 °C for prolonged residence above 6 min accelerates thermo-oxidative chain scission, causing cap skirts to fail under applied torque and reducing environmental stress crack resistance. Multi-cavity closure tools operate with valve-gated hot runners, nozzle shut-off, and screw decompression below 3 mm; injection speed is aligned to fill the cap tether before gate freeze, typically 120–180 mm/s, with pack pressure 40–60 MPa and mould temperature 10–25 °C. For food-contact closures, the finished article must meet FDA 21 CFR 177.1520 and EU Regulation 10/2011, including organoleptic evaluation on the converted article. Terminal articles include tamper-evident dairy caps, condiment orifice caps, sports caps, and flush-cut dispensing closures for personal-care tubes. The primary production failure mode is hinge whitening in flip-top designs when the hinge is packed too long or the mould is too cold; the second is skirt ovality due to uneven cooling in non-concentric gates.

    In low-unit-cost houseware conversion, the controlling process variable is retained core heat rather than thin-wall frozen-layer formation. Storage crates, foldable baskets, drawer modules, and garment hangers are moulded from IF33 in conventional single-face tools with wall thicknesses of 2.5–4.0 mm; the copolymer is dosed at 100 wt% or blended with 15–25 wt% post-industrial LLDPE regrind where closed-loop scrap handling is available. Melt temperature is kept at 190–215 °C, mould temperature at 15–35 °C, injection pressure at 60–90 MPa, and hold time is set by gate-freeze rather than cosmetic finish. Compliance for this segment is commercial rather than food-contact: REACH Article 33 SVHC communication and RoHS Directive 2011/65/EU Annex II heavy-metal limits apply when the articles enter electrical or electronic equipment packaging. Terminal product types include injection-moulded crates, foldable storage boxes, drawer organisers, garment hangers, and refuse-bin bases. Published peel-strength or ESCR data for these specific geometries is limited; processors rely on in-house drop tests and visual stress-whitening checks, not on laboratory tensile values alone.

    Low-Temperature Impact Retention in High-Volume Pail and Materials-Handling Moulding

    Five-litre to 25 L injection-moulded pails produced from IF33-modified HDPE or from 100% IF33 use the copolymer’s low-temperature impact retention where standard HDPE grades can show brittle failure below −20 °C. The blend ratio is typically 60–80 wt% IF33 with 20–40 wt% HDPE for open-head pails requiring stacking stiffness, or 100% IF33 for low-stiffness pails and collapsible buckets; colour masterbatch is kept at 1.5–2.5 wt% to limit modulus loss. Melt temperature is 200–230 °C, and the mould wall is maintained at 10–20 °C to extract heat from the 3.0–4.5 mm wall section; cooling time, not fill time, dominates the cycle. Pack pressure is ramped from 50 MPa to 30 MPa over 6–10 s to prevent core voids at the pail handle pinches. Transport packaging compliance for dangerous goods is assessed under the UN Model Regulations Chapter 6.1 drop and stack provisions, with drop testing carried out to ASTM D5276 on loaded containers at −18 °C or 23 °C. Terminal articles include open-head pails, tamper-evident paint pails, industrial waste bins, and stackable materials-handling tubs. The critical process boundary is the slab-like handle pinch: if pack pressure is released too early, frozen-layer separation at the core creates a void that later initiates brittle failure under drop load; if the melt temperature exceeds 240 °C, surface gloss improves but low-temperature impact falls due to molecular weight reduction.

    When the Mould Cycle Must Stay Below 18 Seconds for Diagnostic Packaging Trays

    Diagnostic packaging trays, transport-box lids, and non-fluid-path analyser components moulded from IF33 are produced in electric injection machines with cavity pressure monitoring where the cycle window is compressed to 15–18 s. The resin is used at 100% virgin; if closed-loop regrind is permitted in a quality-control plan, rework is capped at 20 wt% and segregated by lot. Melt temperature is set at 210–225 °C, mould temperature at 20–35 °C, and fill speed is limited to 140–180 mm/s to prevent jetting around mould inserts. Cleanroom production under ISO 14644-1 Class 8 is common, and packaging operations for terminally sterilized devices are controlled under ISO 11607-1:2019; the quality system is evaluated to ISO 13485:2016. No statement of biocompatibility is made for IF33 in primary blood-contact or implantable applications; if such use is evaluated, ISO 10993-1 biological risk assessment and USP Class VI testing would be required on the finished device, not on the resin alone. Terminal products include diagnostic analyser tray bases, specimen transport tube carriers, non-fluid-path lids, and laboratory benchtop organizers. The main rejection mode in this class is contamination from black specks and carbonized resin; screw and barrel wear, back pressure above 10 MPa, and long residence time are the dominant causes.

    Toy Compliance Does Not End at EN 71 Mechanical and Element Migration Testing

    Under the EN 71 test regime, injection-moulded IF33 components for building blocks, playset figures, ball-pit shells, and push-along toys must satisfy mechanical and element-migration requirements before colour masterbatch is approved. The resin is processed at 100% or blended with 10–20 wt% LDPE where a softer hinge or lower gloss is required; colour masterbatch addition is 2–3 wt%, and only REACH-compliant pigments are allowed. Melt temperature is 190–220 °C, mould temperature 15–30 °C, injection speed 80–120 mm/s, and pack pressure 30–50 MPa; thick bosses and snap-fit features require gate sizes above 1.5 mm to prevent sink marks. The relevant regulatory set includes EN 71-3 for migration of elements, REACH Annex XVII entries 51 and 52 for phthalates, and ASTM F963 where North American distribution is intended. Terminal product types include construction blocks, figurine components, push-along toy bodies, ball-pit spheres, and indoor play modules. The operational boundary is not mechanical but chemical: switching to a non-approved phthalate-containing masterbatch can pass visible inspection and still fail total phthalate screening above 0.1 wt% per plasticized material. Because IF33 itself is an unplasticized polyolefin, the contamination risk is almost entirely introduced by pigment and slip masterbatches or by cross-contamination in shared silos.

    Free Quote

    Competitive Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem IF33 is a linear low-density polyethylene copolymer injection molding grade supplied as pelletized resin. Manufacturer-published typical values identify a melt flow rate of 33 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238 and a density of 0.925 g/cm³ according to ASTM D1505. The grade belongs to the high-flow LLDPE injection segment, not to high-density polyethylene or low-density polyethylene film resins. Target applications include thin-wall kitchenware, closures, caps, housewares, and general-purpose injection molded parts requiring rapid mold filling without the stiffness of HDPE. The copolymer architecture provides a combination of ductility, low-temperature toughness, and processability. The following table presents manufacturer-typical physical property data; these values are not specification limits.

    PropertyTest methodTypical value
    Melt flow rate, 190 °C/2.16 kgASTM D123833 g/10 min
    DensityASTM D15050.925 g/cm³
    Tensile strength at yieldASTM D63811 MPa
    Elongation at breakASTM D638>800%
    Flexural modulus, 1% secantASTM D790260 MPa
    Vicat softening temperatureASTM D152588 °C
    Shore hardnessASTM D224055 Shore D
    Low-temperature brittlenessASTM D746< −76 °C

    Because the melt flow rate is 33 g/10 min, the low-shear viscosity is lower than in conventional LLDPE injection grades with 20 g/10 min or 25 g/10 min melt flow. This reduces injection pressure in thin sections but limits melt strength in blow molding or cast-film processes. The density of 0.925 g/cm³ places the material below HDPE densities and above typical LDPE film densities; the result is a balance of stiffness, elongation, and stress-crack resistance. The tensile yield strength of 11 MPa is low relative to polypropylene and HDPE, but the elongation at break above 800% indicates ductile failure under short-term tensile loading. The yield strength should not be used as a long-term allowable stress; polyethylene creeps under continuous load, and the creep modulus can fall below 50% of the short-term flexural modulus after 1000 h at 23 °C depending on stress level. Published creep data for this specific product configuration is limited, so sustained-load parts require prototype testing under actual service temperature and stress.

    What Distinguishes IF33 from Ethylene Homopolymer Injection Resins?

    Against LDPE injection grades, the linear-low-density polyethylene architecture of IF33 provides a higher concentration of tie molecules and higher tensile yield strength at comparable density. Environmental stress cracking resistance is characteristically improved relative to branched LDPE, although product-specific ESCR data for IF33 should be requested from the supplier under ASTM D1693 or ASTM D2561. In bent-strip tests with 10% Igepal CO-630, LLDPE injection grades can exceed LDPE by 2 to 5 times in failure time, but actual IF33 performance depends on molded-in stress, part thickness, and the specific stress-cracking fluid. Liquid dishwashing agents, mineral oil, and certain silicone-based lubricants can reduce ESCR; compatibility testing with the intended service fluid is required.

    Against HDPE injection grades, IF33 shows lower flexural modulus and lower Vicat softening. The published typical value of 260 MPa secant flexural modulus is approximately one-fourth to one-sixth of the values common for HDPE injection grades. The trade-off is improved low-temperature ductility and reduced mold shrinkage anisotropy. Processors replacing HDPE with IF33 must redesign for lower service temperature, lower creep resistance, and higher elongation under continuous load. HDPE grades with density near 0.955 g/cm³ often exhibit flexural modulus near 1100 MPa, whereas IF33 is reported at 260 MPa. The following table summarizes general comparative ranges for injection molding polyethylene families.

    AttributeIF33 typicalLDPE injection rangeHDPE injection range
    Density (g/cm³)0.9250.917–0.9240.950–0.965
    Melt flow rate (g/10 min)3310–404–40
    Flexural modulus (MPa)260150–250900–1500
    Vicat softening (°C)8880–95120–130
    Mold shrinkage (%)1.5–2.01.5–2.51.5–3.0

    The comparative ranges are general industry values for injection molding grades, not Braskem product data except for IF33. They illustrate why IF33 is not a direct substitute for HDPE in high-stiffness applications. The lower flexural modulus and lower Vicat softening imply lower load-bearing capability at elevated temperature. The elongation at break and low-temperature brittleness below −76 °C provide improved ductility in cold impact.

    The molecular weight distribution and comonomer distribution determine the shear-thinning behavior of IF33. The grade is designed for injection molding rather than extrusion. At shear rates above 100 s⁻¹, the effective viscosity decreases sharply, characteristic of linear polyethylenes with a narrow-to-medium molecular weight distribution. Oscillatory rheology data for IF33 are not commonly provided in standard product documentation; process interpretation therefore relies on injection pressure, cavity pressure transducers, and part-weight stability. The low-shear melt flow rate of 33 g/10 min is an index of molecular weight; it does not by itself define the high-shear viscosity relevant to injection filling.

    Cavity Filling, Shrinkage, and Warpage Control

    On reciprocating-screw injection machines with L/D ≥ 20:1 and compression ratio 2.5:1–3.5:1, the recommended melt temperature window is 180 °C to 230 °C, with mold temperatures of 10 °C to 40 °C. For thin-wall parts with wall sections below 1.2 mm, higher melt temperatures within the window reduce pressure loss; however, temperatures above 230 °C can increase gate-to-gate viscosity variation in hot-runner systems and produce surface streaking. Clamp force requirements generally fall between 3.0 kN/cm² and 5.0 kN/cm² of projected area, depending on flow length and wall thickness. Gate freeze-off is faster than in lower-MFR LLDPE grades; pack pressure and hold time should be established by part-weight stability rather than fixed timer settings. Back pressure of 0.5–1.0 MPa and screw speed below 100 rpm are typical starting points for LLDPE injection grades. Excessive screw speed can cause air entrainment and splay. Screw recovery time should be shorter than cooling time; if screw recovery exceeds cooling time, melt quality may suffer. A shut-off nozzle is recommended to prevent drooling from the high-flow resin during mold-open time.

    Mold shrinkage for injection molded plaques is typically reported in the 1.5% to 2.0% range under ASTM D955, with flow-direction shrinkage somewhat higher than transverse shrinkage. Differential shrinkage in flat lids and shallow containers is a common source of warpage. Cooling uniformity, gate placement, and pack pressure history influence warpage more than the resin alone. Multi-cavity tools with unbalanced runner systems can produce batch-to-batch part weight variation of 0.5% to 1.5%; hot-runner manifold temperature should be profiled to avoid thermal gradients exceeding 5 °C across nozzles. The high flow rate of IF33 produces orientation in the flow direction that can increase directional shrinkage differences. For a shallow rectangular container, flow-direction shrinkage may be approximately 1.8% and transverse shrinkage 1.5%, producing corner lift if cooling is asymmetric. Tooling designed for HDPE may not be directly reusable because the lower density and lower crystallinity of IF33 produce less post-ejection contraction but greater compliance in the solid state.

    In production-scale multi-cavity tools, venting deficiencies produce burn marks when injection velocity exceeds 300 mm/s and vent depth is below 0.02 mm. The low melt elasticity of IF33 permits rapid cavity filling, so the cavity must be adequately vented before flow-front arrival. Short-shot defects in thin-wall containers often appear as incomplete rim formation; increasing fill speed without correcting gate geometry can raise internal stress and reduce impact performance at sharp corners. Gate locations and weld lines are common failure initiation sites in cold impact. Impact performance can be improved by reducing melt and mold temperatures within the processing window, increasing pack pressure to reduce oriented skin stress, and avoiding high injection velocity at the end of fill.

    When Elevated Melt Flow Is Needed Without HDPE-Level Flexural Modulus

    IF33 is assigned to injection molding applications where lower-MFR LLDPE grades cannot fill multi-cavity tooling within available injection pressure. The melt flow rate of 33 g/10 min provides a practical processing advantage in flow length-to-wall thickness ratios above 150:1, a condition common in thin-wall food packaging. The trade-off is that melt strength is lower than in 20 g/10 min injection grades; therefore the grade is not suitable for blow molding, film, or open-discharge extrusion. For caps and snap-fit closures, the lower flexural modulus of 260 MPa permits undercut ejection with lower ejection force than HDPE; however, if the closure requires high stacking strength or torque retention under load, a density above 0.950 g/cm³ HDPE is the appropriate alternative. The lower flexural modulus also reduces ejection force in textured or undercut molds, but the soft surface may drag on rough tool steel; a draft angle of 0.5° to 1° is generally required. Ejector pins should have sufficient area to avoid surface puncturing when parts are ejected above 60 °C.

    Regrind from sprues and runners can be incorporated into IF33 at levels up to 20% to 30% by mass without significant loss of short-term mechanical properties, provided the regrind is free of contamination and thermally degraded. Higher regrind fractions increase the risk of black specks and flow variation; the melt flow rate may increase due to molecular weight reduction during repeated extrusion. For food-contact articles, regrind use must comply with the applicable regulatory conditions.

    Hot-runner systems with internally heated nozzles may produce stagnation zones if the resin residence time exceeds 10 min. The high-flow grade is less sensitive to viscosity increase than lower-MFR polyethylenes, but long residence at high temperature still leads to discoloration. Flush the hot-runner system with a purging polyolefin after shutdown to prevent carbonized deposits. Batch-to-batch variation in MFR may be controlled by the producer within a specified range. A shift from 30 g/10 min to 36 g/10 min can change fill pressure and part weight; processors should monitor melt index via ASTM D1238 and adjust shot size or holding pressure accordingly.

    Observed Processing Boundaries in Production-Scale Injection Molding

    Polyethylene is not hygroscopic, so pre-drying is not normally required. Condensation on cold pellets taken from outdoor storage can cause surface splay; a dehumidifying or dry-air hopper at 60 °C for 1 h removes surface moisture without adversely affecting stabilizers. Melt temperatures above 280 °C should be avoided due to thermal oxidation and generation of low-molecular-weight degradation products. Outdoor service without UV stabilization is not recommended. Polyethylene is susceptible to photo-oxidation; for outdoor use, a UV stabilization masterbatch at 2% to 5% by mass is commonly added, with the exact let-down ratio depending on part thickness and exposure severity. Carbon black at 2% to 2.5% provides long-term UV protection for articles that do not require a natural color.

    Food-contact status for IF33 should be confirmed from the supplier’s lot-specific certificate. Polyethylene copolymer grades of this type are covered as olefin polymers under FDA 21 CFR 177.1520(c) when extractables limitations are met. European users should confirm compliance with Regulation (EU) No 10/2011 and its amendments for the intended food simulant and time–temperature condition. REACH and RoHS declarations are typically supplied in the product regulatory documentation, but additive packages may vary by production site; verification against the Safety Data Sheet is required before use in toys, medical devices, or drinking-water components. The grade should not be assumed compliant for infant formula packaging or medical devices without explicit supplier written confirmation.

    The commercial stabilization package typically includes a phenolic antioxidant and a phosphite processing stabilizer. The resin may be supplied with or without slip or antiblock additives depending on the final application; users should confirm whether the supplied grade contains a slip agent because slip can reduce print adhesion and lid-seal torque. Certain amine-containing color concentrates can shift the stabilization balance and cause yellowing at high processing temperatures; compatibility with the base resin stabilizer package should be verified by the masterbatch supplier. The grade should not be combined with pro-oxidant additives unless the final article is intended for degradable service, because such additives can prematurely reduce molecular weight during processing and shorten service life.