Braskem Hf3712 Extrusion Linear Low Density Polyethylene

Braskem HF3712 Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem HF3712 Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 152635
    Gradename HF3712
    Materialtype Linear Low Density Polyethylene
    Processingmethod Extrusion
    Comonomer Butene-1
    Form Pellets

    As an accredited Braskem HF3712 Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem HF3712 Extrusion Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, with 1,000 kg jumbo bag options.
    Container Loading (20′ FCL) 20′ FCL container loading for Braskem HF3712 Extrusion Linear Low Density Polyethylene; securely stowed, dry, sealed, and documented for export.
    Shipping Braskem HF3712 Extrusion Linear Low Density Polyethylene typically ships as non-hazardous resin pellets in 25 kg polyethylene bags, stacked on pallets and stretch-wrapped, or in bulk trucks/railcars. During transport, store in a dry, cool area away from direct sunlight, heat, and moisture. No special DOT hazards.
    Storage Store Braskem HF3712 Extrusion Linear Low Density Polyethylene in original, sealed bags or containers in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, and ignition sources. Keep away from strong oxidizers. Avoid dust accumulation and spills to prevent slipping. Electrostatic hazards may exist; use proper grounding and bonding. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Braskem HF3712 LLDPE shelf life: two years from manufacture, stored in original packaging, dry, ambient conditions, away from direct sunlight.
    Application of Braskem HF3712 Extrusion Linear Low Density Polyethylene

    When Braskem HF3712 is specified for three-layer blown film structures in food-contact packaging, the grade is typically assigned to the sealant layer or to a core layer between an LDPE skin and an mLLDPE abuse layer. The principal regulatory path is FDA 21 CFR 177.1520 for olefin polymers, supplemented by EU 10/2011 overall migration testing under EN 1186-1 and incoming melt-flow verification under ISO 1133-1:2022. In production-scale trials on a 90 mm single-screw extruder with 30:1 L/D barrier screw and 250 mm spiral mandrel die, the recommended barrel profile is 180 °C, 200 °C, 210 °C, 210 °C, 215 °C, with die zones held at 215 °C and melt temperature at die entry not exceeding 220 °C. Die gap is set between 1.8 mm and 2.2 mm; blow-up ratio is controlled between 2.2:1 and 2.8:1; frost line height is maintained at 6–8 die diameters to limit haze below 7% when measured by ASTM D1003. Formulation addition ratios for the sealant web are typically 70–80 wt% HF3712, 15–25 wt% LDPE with a 0.25–0.35 g/10 min melt index, 5–8 wt% anti-block masterbatch containing 15–20% synthetic silica, and 0.03–0.08 wt% fluoroelastomer processing aid to suppress melt fracture at high screw speeds. When a lower heat-seal initiation temperature is required, a butene LLDPE with lower melting peak is added at 10–15 wt% to bring seal initiation to 85–95 °C. Downstream conversion involves extrusion through a spiral mandrel die, internal bubble cooling, primary nip collapse, in-line corona treatment to 38–42 mN/m, and slitting to wound rolls. Terminal product types include frozen food pouch films, bakery bread bags with antifog inner surfaces, side-gusset liquid packaging inner webs, and dry food laminates for confectionery overwrap. The limiting operational boundary is regrind fraction: regrind above 20 wt% increases gel counts and visible fish-eye defects, while ambient relative humidity above 60% can introduce moisture-induced additive agglomeration that disrupts film appearance.

    Why Is Neck-In and Air-Gap Melt Curtain Stability the Defining Constraint in Extrusion Coating of Kraft Paperboard?

    Melt curtain stability in extrusion coating of bleached kraft paperboard and aluminum foil depends on the relationship between melt temperature, air gap, and polymer melt strength. Food-contact status relies on FDA 21 CFR 177.1520 for the polyolefin and FDA 21 CFR 176.170(c) for contact with aqueous and fatty foods through uncoated paperboard, with EU compliance under Regulation (EU) No 1935/2004 and good manufacturing practice under Regulation (EC) No 2023/2006. A typical coating formulation uses 70–85 wt% HF3712, 10–25 wt% LDPE with a melt index of 4–8 g/10 min to reduce neck-in, and 2–5 wt% ethylene-vinyl acetate or ethylene-methyl acrylate copolymer as an adhesion promoter to aluminum foil and polypropylene. On a 120 mm single-screw extruder with 33:1 L/D and feedblock-fed slot die having a deckle width of 2,400 mm, barrel temperatures are profiled from 200 °C to 315 °C, with die temperature at 305 °C and melt temperature at 305–315 °C. The air gap is set between 150 mm and 250 mm; longer gaps increase neck-in beyond 60 mm per side, while shorter gaps reduce adhesion due to insufficient surface oxidation. Coating weight is controlled between 12 g/m² and 25 g/m² at line speeds from 150 m/min to 300 m/min. Chill roll temperature is maintained at 10–18 °C with mirror or matte surface, and nip pressure is set between 4 N/mm² and 6 N/mm². Terminal products include aseptic gable-top carton liners, sandwich packaging paper, aluminum foil lidding membranes, and release paper coatings for pressure-sensitive adhesive laminates. The documented failure mode is edge tear at the die lip or melt curtain sagging when melt index falls below 0.9 g/10 min, which forces excessive melt temperature and accelerates gel formation. Incoming substrate moisture above 6 wt% causes steam blow-out at the nip and pinholes in the coating layer.

    Flexible geomembrane lines running HF3712 at thicknesses above 0.75 mm require continuous verification of oxidative induction time and carbon black dispersion because both variables control long-term hydraulic barrier integrity. The product must be formulated with a UV-stabilized carbon black masterbatch, and compliance is assessed under ASTM D3350 cell classification, GRI-GM17 for linear low-density polyethylene geomembranes, ASTM D6693 tensile properties, ASTM D4833 puncture resistance, ASTM D5884 tongue tear, ASTM D5397 notched constant tensile load, and ISO 13438 oxidative induction time. The addition ratio is typically 72–82 wt% HF3712, 10–18 wt% single-site mLLDPE, 2.2–3.0 wt% carbon black masterbatch yielding a carbon black content of 2.0–2.5 wt%, and 0.1–0.3 wt% hindered phenolic/phosphite antioxidant masterbatch. In flat die sheet extrusion on a 150 mm single-screw extruder with 30:1 L/D and a 5,000 mm coat-hanger die, melt temperature is kept between 210 °C and 235 °C; excursions above 240 °C consume antioxidant and can reduce oxidative induction time below the 100 min threshold at 200 °C imposed by many mining pond specifications under ISO 13438. The polishing stack is operated at 70–90 °C to control surface gloss and minimize internal stress; calendered sheet thickness ranges from 0.75 mm to 2.5 mm, and line speed is limited to 4–8 m/min at the upper thickness. Terminal product types include landfill temporary covers, heap leach pond liners, agricultural water storage reservoirs, and secondary containment membranes for chemical tank farms. The field-relevant processing bottleneck is edge bead formation when die lip opening is not corrected after thickness changes; edge trim levels above 8% indicate die bolt adjustment error rather than resin deficiency. Weld-seam peel strength in hot-wedge seams depends on carbon black dispersion; dispersion below 2.0 on the microscope rating scale creates shear-thinning variation and weak seam fusion.

    Cast Stretch Film: Chill Roll Haze, Cling Additive Migration, and Puncture Propagation

    A cast stretch film line running at 600 m/min imposes specific limits on melt temperature and chill roll condensation because both factors directly influence optical haze and cling uniformity. HF3712 is used primarily in the core layer because its 0.918 g/cm³ density limits haze development and its melt index supports high draw rates without draw resonance. The applicable mechanical requirement is ASTM D5748 puncture resistance, with cling force measured by ASTM D5458 and tensile by ISO 527-3; migration into food is not typically claimed unless an over-wrap product is tested under EU 10/2011. A three-layer A/B/C structure is used: the cling layer contains 2–5 wt% polyisobutylene tackifier, 0.5–1.5 wt% slip agent, and 88–95 wt% lower-density mLLDPE; the core layer contains 65–80 wt% HF3712, 15–25 wt% mLLDPE, and 5–8 wt% LDPE; the release layer contains 0.8–1.5 wt% erucamide slip and 95–99 wt% LLDPE. The cast film process uses a slot die with automated lip adjustment, primary chill roll at 20–25 °C, secondary chill roll at 15–20 °C, vacuum box edge pinning, and in-line thickness scanning with feedback to die bolts. Pre-stretch ratios on downstream pallet wrapping lines are set between 200% and 300%. Terminal products include machine pallet wrap with 15–23 μm thickness, hand wrap, agricultural bale film, and bundling film. The most frequent field failure is cling-transfer blocking caused by tackifier migration when storage exceeds 35 °C for more than 48 h; this is mitigated by lowering tackifier to 2–3 wt% in hot-climate formulations. A measured boundary is chill roll condensation at relative humidity above 70%, which produces optical defects described as pinhead haze.

    Where Continuous Extrusion of Thin-Wall Drip Tape Demands Melt Fracture Suppression

    Sharkskin and emitter weld fusion rather than tensile strength determine whether HF3712 can be processed into thin-wall drip tape without excessive fluoropolymer processing aid. Product compliance for irrigation laterals is anchored to ISO 9261 emission uniformity, ISO 8779 polyethylene pipes for irrigation, and ASTM D3350 cell classification for PE pipe materials. The formulation addition ratio for a drip tape wall thickness of 0.15–0.25 mm is 80–90 wt% HF3712, 5–10 wt% HDPE or mLLDPE to raise stiffness, 2.0–2.5 wt% carbon black masterbatch, and 0.03–0.08 wt% fluoropolymer processing aid. On a 60 mm single-screw extruder with 30:1 L/D and barrier screw, melt temperature is limited to 190–215 °C because higher temperatures reduce melt viscosity and destabilize emitter welding. Die pressure at the screen changer is maintained between 20 MPa and 35 MPa; pressure spikes above 37 MPa indicate filter blockage and cause localized sharkskin. The downstream process involves continuous tube extrusion through a crosshead or in-line emitter insertion, vacuum calibration at 15–25 °C water, laser or mechanical slit formation, and winding at 60–150 m/min. Terminal product types include integral drip tape with flat emitters, round micro-irrigation laterals, and sprinkler dropper tubing. Field-reported failure includes burst at seam welds when carbon black dispersion rating exceeds 3 according to ISO 18553; fused emitter detachment occurs when melt temperature drops below 185 °C due to insufficient penetration into the emitter substrate.

    Heavy-duty sack converters evaluate HF3712 primarily by dart impact at the gusset crease and by coefficient of friction after flexographic printing. HF3712 is selected because its butene branch structure retains impact strength at film thicknesses between 80 μm and 200 μm. Compliance for the semi-finished film is tested under ASTM D1709 dart impact, ASTM D882 tensile properties, ASTM D1922 Elmendorf tear, and ASTM D1894 coefficient of friction. For finished flexible intermediate bulk containers, ISO 21898 governs cyclic lift and drop performance, while ISO 7023 applies to shipping sacks. The formulation addition ratio for a three-layer blown film is 70–80 wt% HF3712, 10–20 wt% HDPE with a melt index below 0.5 g/10 min to increase modulus, 5–10 wt% LDPE, and 1.0–2.0 wt% antiblock/slip masterbatch containing 5–10% silica and 1–2% erucamide. On a 90 mm grooved-feed extruder with 30:1 L/D and a 400 mm dual-lip air-ring die, blow-up ratio is held between 1.5:1 and 2.2:1 to maintain machine-direction tear balance; melt temperature is set between 190 °C and 215 °C. Frost line height is raised to 8–10 die diameters to reduce frozen-in orientation and improve dart impact. Downstream conversion includes gusseting, inline corona treatment to 40–44 mN/m, flexographic solvent-based or water-based printing, and sewing or thermal sealing. Terminal product types include fertilizer sacks with side gussets, FIBC inner liners, polymer granule shipping bags, and sand/cement valve bags. The production bottleneck is dart impact loss at the gusset crease; when crease radius is below 0.2 mm, splitting initiates at 120–160 g dart impact even though flat film exceeds 400 g, requiring gusset bar adjustment rather than resin reformulation.

    Application segmentRelevant standardsFormulation addition windowCritical processing boundary
    Food packaging blown filmFDA 21 CFR 177.1520, EU 10/2011, ASTM D100370–80 wt% HF3712, 15–25 wt% LDPE, 5–8 wt% anti-block masterbatchMelt temperature above 220 °C creates bubble instability
    Extrusion coating of kraft paperboardFDA 21 CFR 176.170(c), EU 1935/2004, EN 1186-170–85 wt% HF3712, 10–25 wt% LDPE, 2–5 wt% EVA/EMAAir gap above 250 mm raises neck-in beyond 60 mm per side
    Flexible geomembrane linersGRI-GM17, ASTM D6693, ISO 1343872–82 wt% HF3712, 10–18 wt% mLLDPE, 2.2–3.0 wt% carbon black masterbatchMelt temperature above 240 °C reduces oxidative induction time
    Cast stretch filmASTM D5748, ASTM D5458, ISO 527-365–80 wt% HF3712 in core layer, 2–5 wt% PIB tackifier in cling layerStorage above 35 °C for 48 h induces cling-transfer blocking
    Drip tape irrigationISO 9261, ISO 8779, ASTM D335080–90 wt% HF3712, 5–10 wt% HDPE, 2.0–2.5 wt% carbon black masterbatchMelt temperature below 185 °C prevents emitter weld fusion
    Heavy-duty sacks and FIBC linersISO 21898, ISO 7023, ASTM D170970–80 wt% HF3712, 10–20 wt% HDPE, 5–10 wt% LDPEGusset crease radius below 0.2 mm triggers dart impact failure
    Free Quote

    Competitive Braskem HF3712 Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem HF3712 is identified in the manufacturer’s product line as an Extrusion Linear Low Density Polyethylene. The grade is supplied as free-flowing pellets for blown film and cast film conversion, with a nominal density of 0.918 g/cm³ determined in accordance with ASTM D1505 and a melt flow rate of 1.0 g/10 min when measured at 190 °C under a 2.16 kg load in accordance with ASTM D1238. Manufacturer lot-release windows for density are typically 0.916 g/cm³ to 0.920 g/cm³, while melt flow rate ranges from 0.85 g/10 min to 1.15 g/10 min; values outside these ranges are considered non-conforming to the release specification. The designation does not encode the comonomer identity, but product literature describes the resin as a conventional butene-based linear low density polyethylene with a processing profile suited to moderate-stiffness film structures. The material should be distinguished from high-pressure low density polyethylene, which contains long-chain branching and provides higher melt strength at the expense of tensile toughness.

    What processing window is required on blown-film lines?

    On single-screw extruders with a length-to-diameter ratio of 24:1 to 30:1 and barrier screws equipped with Maddock mixing elements, the recommended melt temperature is 190 °C to 230 °C. Die lip gaps of 1.8 mm to 2.5 mm are used to maintain sufficient shear stress for melt fracture avoidance, and blow-up ratios from 2.0:1 to 3.0:1 produce balanced machine-direction and transverse-direction tensile properties. Bubble stability is maintained through dual-lip air rings; internal bubble cooling is required when film thickness is reduced below 25 µm because the low melt strength of a linear resin can allow bubble sway at high film line speeds. A frost line height of 6 to 8 die diameters is typical. Lower frost lines increase quench rate and reduce haze, but excessive cooling can raise machine-direction shrinkage when winder tension exceeds 4 N/mm². At die shear rates up to 800 s⁻¹, the resin does not exhibit severe sharkskin melt fracture provided the die land length-to-gap ratio is greater than 10:1. Published data for maximum output on specific 75 mm or 90 mm grooved-feed extruders is limited; converters should establish melt pressure, screw speed, and melt temperature limits through instrumented line trials.

    Surface moisture on pellets stored in silos with relative humidity above 80% should be reduced by a hopper dryer set at 40 °C to 65 °C for 2 to 4 hours. Polyethylene does not undergo hydrolytic degradation, but condensate at the feed throat can produce pin holes, gel-like defects, and unstable melt pumping. Pneumatic conveying systems should be fitted with dew-point monitoring when ambient absolute humidity exceeds 12 g/kg dry air.

    Mechanical property benchmarks for 25 µm monolayer film

    At a nominal film thickness of 25 µm, blown film converted from Braskem HF3712 on a 45 mm single-screw line with 30:1 L/D and 2.5 mm die gap typically exhibits the property windows shown in the comparative matrix below. Dart drop impact is measured by ASTM D1709 Method A; reducing film thickness to 12 µm lowers dart impact by approximately 3.5 to 4.0 times, not linearly, due to concentration of impact energy over a smaller cross-section. Tensile properties are measured by ASTM D882 with a jaw separation of 50 mm and crosshead speed of 500 mm/min.

    Property HF3712 typical window High-pressure LDPE comparison Hexene LLDPE comparison Test method
    Density 0.918 g/cm³ 0.923 g/cm³ 0.918 g/cm³ ASTM D1505
    Melt flow rate 1.0 g/10 min 1.9 g/10 min 1.0 g/10 min ASTM D1238
    Dart drop impact 110 g to 170 g 75 g to 95 g 180 g to 250 g ASTM D1709 Method A
    Elmendorf tear MD 150 g to 190 g 100 g to 140 g 220 g to 300 g ASTM D1922
    Elmendorf tear TD 380 g to 460 g 150 g to 210 g 480 g to 560 g ASTM D1922
    Tensile strength at yield MD 10 MPa to 12 MPa 9 MPa to 11 MPa 9 MPa to 11 MPa ASTM D882
    Ultimate tensile strength MD 34 MPa to 42 MPa 20 MPa to 26 MPa 38 MPa to 48 MPa ASTM D882
    Elongation at break MD 600% to 750% 300% to 450% 700% to 850% ASTM D882
    Haze 7% to 12% 5% to 8% 5% to 9% ASTM D1003

    When butene comonomer selection affects puncture and tear

    The butene-based chemistry of HF3712 differentiates it from hexene- and octene-based linear low density polyethylene grades through the short-chain branching distribution. Butene introduces ethyl branches, while hexene introduces butyl branches; the longer branch in hexene-based grades increases tie-molecule concentration and yields higher dart impact and Elmendorf tear at equivalent density and melt flow rate. This is visible in the property matrix: hexene LLDPE at 0.918 g/cm³ and 1.0 g/10 min typically shows dart impact values 20% to 40% higher than butene grades. High-pressure LDPE exhibits long-chain branching and therefore has lower ultimate tensile strength and lower tear resistance, but greater melt strength and improved bubble stability on air-cooled blown film lines. In three-layer coextruded structures, HF3712 is commonly placed in the core layer at 30 wt% to 60 wt% to increase stiffness and reduce raw-material cost while the skin layers provide sealing or slip properties. It is not the first choice where maximum puncture resistance or organoleptic purity is the primary requirement.

    On cast film lines with air knife pinning and chill-roll temperatures between 15 °C and 25 °C, the low melt flow rate of HF3712 requires lower die temperatures than typical cast-film LDPE to avoid haze increase from surface irregularities. In extrusion coating, the resin may be blended with high-pressure LDPE at 20 wt% to 40 wt% to improve seal initiation and tear resistance, but neck-in increases as LDPE content decreases; the processing window should be verified on the actual line because published data for this specific configuration is limited.

    Regulatory and compositional boundaries in food-contact use

    The resin is manufactured to meet olefin polymer requirements of FDA 21 CFR 177.1520(c), paragraphs 3.1 and 3.2, with conditions of use specified by the appropriate food type table. European food-contact compliance is typically supported by Regulation (EU) No 10/2011 as amended, with overall migration below 10 mg/dm² when tested under OM2 or OM5 conditions depending on the intended temperature profile. The grade is supplied without intentionally added slip or antiblock; converters must formulate masterbatch additions at the hopper to achieve the required coefficient of friction. Typical erucamide slip addition is 500 ppm to 1,500 ppm, and synthetic silica antiblock addition is 1,000 ppm to 5,000 ppm, depending on film gauge and blocking tendency. The following matrix summarizes the principal compliance and characterization methods applied to this grade.

    Standard or regulation Scope Method or clause
    FDA 21 CFR 177.1520(c) Olefin polymers for food contact Paragraphs 3.1 and 3.2
    Regulation (EU) No 10/2011 Plastic materials in food contact Overall migration 10 mg/dm²
    REACH EU registration of substances EC 1907/2006
    RoHS Restriction of hazardous substances Directive 2011/65/EU Annex II
    ISO 1183-1 Density measurement ISO 1183-1:2019
    ASTM D1238 Melt flow rate ASTM D1238-20
    ASTM D882 Thin film tensile properties ASTM D882-18
    ASTM D1709 Dart impact of film ASTM D1709-15ae1

    What differentiates HF3712 from metallocene-catalyzed LLDPE and high-pressure LDPE?

    The principal differences are molecular weight distribution and melt elasticity. Metallocene-catalyzed LLDPE grades typically exhibit a polydispersity index below 3.0 and lower hexane extractables; conventional butene-based LLDPE grades such as HF3712 have broader molecular weight distribution, which increases die lip build-up but improves processing at high back pressure. At equivalent density, metallocene grades can yield haze values below 5%, while conventional butene grades are typically in the 7% to 12% range at 25 µm. Organoleptic performance also differs: conventional LLDPE can produce higher hexane extractables than metallocene grades, so applications requiring 0.5% or lower hexane extractables should not use HF3712 without verification. Compared with high-pressure LDPE, HF3712 provides higher dart impact, higher Elmendorf tear, and higher elongation at break, but lower melt strength and narrower bubble stability. The selection of HF3712 is therefore appropriate for gauge-reduced films where toughness and draw-down capacity are critical, while high-pressure LDPE remains necessary for very high stalk heights, heavy-duty shrink structures, or maximum melt strength in extrusion coating.

    Operational boundaries include maximum sustained melt temperature of 260 °C to avoid oxidative gel formation. Prolonged storage at ambient temperatures above 40 °C, particularly with direct sunlight exposure, should be avoided because oxidation induction time decreases with thermal history. The resin should not be combined with high levels of peroxide masterbatch or aggressive metal stearate lubricants without evaluating interaction at the intended processing temperature, as excessive peroxide can initiate premature chain scission and shift melt flow rate beyond the release window.

    Top