Braskem Hf2007 Blown Film Extrusion Linear Low Density Polyethylene

Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 287597
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 11 MPa
    Tensile Strength At Yield Td 11 MPa
    Tensile Strength At Break Md 35 MPa
    Tensile Strength At Break Td 30 MPa
    Elongation At Break Md 700 %
    Elongation At Break Td 800 %
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 500 g
    Haze 12 %
    Gloss 45 50
    Coefficient Of Friction 0.2

    As an accredited Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem HF2007 Blown Film Extrusion LLDPE is supplied in 25 kg moisture-resistant bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Braskem HF2007 Blown Film Extrusion LLDPE, 25 kg palletized bags, shrink-wrapped, securely stowed for ocean transport.
    Shipping Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene is shipped as non-hazardous polyethylene resin pellets in moisture-barrier bags or bulk containers. Palletized, stretch-wrapped, and labeled. Store in cool, dry conditions away from heat. No special DOT/IMDG/ADR hazard classification. Handle with standard PPE and avoid dust generation. For industrial use only.
    Storage Store Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and ignition sources. Keep bags or containers closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking, protect from ultraviolet light and static buildup, and follow the supplier’s SDS and local regulations. Use first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 24 months when stored cool, dry in unopened original packaging, away from direct sunlight and moisture.
    Application of Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene

    Heavy-duty industrial liners in the 100 µm–200 µm gauge range are produced from Braskem HF2007 on a 75 mm grooved-feed single-screw blown film extruder with L/D 30:1 and a 400 mm diameter low-pressure spiral die. The resin has nominal density 0.918 g/cm³ and melt index 1.0 g/10 min at 190°C/2.16 kg under ASTM D1238. Melt temperature is held between 195°C and 215°C at the adapter. Die gap is set at 2.0 mm. Blow-up ratio is maintained between 2.5:1 and 3.0:1. Frost line height is fixed at 8 to 10 die diameters. For bubble stability on high-speed winders, HF2007 is blended with 15–20 wt% high-pressure LDPE having melt index below 0.30 g/10 min. The blend provides improved melt strength and reduced bubble flutter but dart impact measured under ASTM D1709 declines if LDPE exceeds 25 wt%. The film is converted into side-gusseted FIBC inner liners, drum liners and bulk box liners. Seams are impulse heat sealed at 125°C–140°C and seam strength is evaluated by ASTM F88. Compliance for non-food industrial use relies on REACH 1907/2006 Article 33 and EU Directive 94/62/EC heavy-metal concentration below 100 mg/kg in packaging components. Pre-drying is not required, but surface condensation from cold warehouse transfer must be avoided because free moisture on pellets can generate bubble instability at the die. On lines without automatic air ring control, ambient air temperature swings above 10°C can shift frost line height and create gauge variation exceeding 5%.

    Compliance and test matrix for Braskem HF2007 blown film applications
    StandardDesignationApplication area
    FDA 21 CFR 177.1520(c) 3.2aOlefin polymers for food contactFood packaging films
    EU No 10/2011Overall migration and specific migration limitsFood packaging films
    REACH 1907/2006 Article 33SVHC disclosureIndustrial and agricultural films
    EU Directive 94/62/ECPackaging heavy metalsAll packaging
    ASTM D1238Melt flow rateIncoming resin QC
    ASTM D882Tensile properties of thin plastic sheetingFrozen food and industrial films
    ASTM D1709Dart impact resistanceIndustrial liners, refuse sacks
    ASTM D1922Elmendorf tear resistanceSilage film, industrial liners
    ASTM D1894FrictionVFFS packaging
    ISO 1133-1:2022Melt mass-flow rateIncoming resin QC
    ASTM F88Seal strengthFlexible packaging
    ASTM F1921Hot tackVFFS packaging
    ASTM D3985Oxygen transmission rateSilage film, barrier lamination
    ASTM D2578Surface wetting tensionLamination sealant web

    How Does Seal Initiation Temperature Shift in 30 µm Frozen Food Packaging Films?

    In mono-layer frozen food packaging produced on a 55 mm extruder with L/D 24:1 and a 150 mm die, Braskem HF2007 is processed at 190°C–205°C melt temperature with die gap 1.8 mm and blow-up ratio 2.2:1 to 2.5:1. The melt index of 1.0 g/10 min under ASTM D1238 supports stable bubble formation. A 5–10 wt% addition of high-pressure LDPE further stabilises the bubble at line speeds above 80 m/min. Food-contact qualification is performed under FDA 21 CFR 177.1520(c) 3.2a and EU No 10/2011. Overall migration testing for frozen aqueous food uses 10% ethanol simulant at 20°C for 10 days. The blown web is converted into pillow pouches and side-seal bags for IQF vegetables and frozen meat portions. Seal initiation on VFFS jaw is controlled by heat transfer through the web; the low melt index reduces thin-down at the seal edge, but seal bar temperature must be raised by 5–10 K compared with high-slip blown LDPE grades. Hot tack is measured by ASTM F1921 and seal strength by ASTM F88. The film’s low density of 0.918 g/cm³ maintains flexibility at freezer temperatures; published data for this exact configuration is limited and should be confirmed by ASTM D882 tensile testing at -20°C. Film with gauge below 25 µm risks pinholing in draw-down after frost line, and should be produced only with automatic gauge control and cold air ring at 10°C to 15°C.

    Silage Film Oxygen Permeability and Tear Retention in a 150 µm Coextruded Structure

    Agricultural bale wrap in 150 µm thickness uses a three-layer coextrusion die with skin layers carrying 2–4 wt% HALS/UV masterbatch and a core layer containing Braskem HF2007 blended 70/20/10 with high-pressure LDPE and a metallocene LLDPE. Melt temperature is kept at 200°C–220°C. Die gap is set at 2.4 mm. Blow-up ratio is held between 2.5:1 and 3.0:1. The collapsing frame is positioned to minimise surface tension wrinkles. Oxygen transmission rate is measured by ASTM D3985 at 23°C and 0% RH. Processors use an internal reference of 4,000 cm³/m²·day·atm at 50 µm, but this value must be confirmed because OTR scales inversely with thickness only when the web is free of pinholes. Tear retention after 12 months of weathering is monitored by ASTM D1922 in machine direction. A loss below 50% of initial tear indicates UV stabiliser depletion. The finished blown bale wrap tube is slit to 750 mm widths for round-bale wrappers. Regulatory compliance for non-food agricultural film does not require FDA food-contact clearance; REACH 1907/2006 Article 33 and EN 13206 are the relevant references. High UV masterbatch loadings above 6 wt% can reduce bubble stability due to carrier resin incompatibility and should not be entered without stabilizer compatibility testing. In multi-layer structures, the core layer remains unstabilised if the skin layers provide complete UV shielding; incorrect layer distribution below 15% core can expose HF2007 to UV and accelerate embrittlement.

    Because post-consumer PE recyclate at 30–40 wt% reduces bubble strength and narrows the HF2007 processing window on a 55 mm extruder, refuse sack producers lower melt temperature to 185°C–200°C and install a 100/80/60/100 mesh screen pack upstream of the die. The recyclate fraction is a washed and regranulated blown film fraction with melt index between 0.7 g/10 min and 1.5 g/10 min. Drawn film gauge is 20 µm to 30 µm. Die gap is set at 1.2 mm. Blow-up ratio is held at 2.0:1 to 2.5:1. The finished sacks are star-sealed or drawstring sealed and must meet EN 13592 for household refuse sacks. Dart impact is tested under ASTM D1709 and Elmendorf tear under ASTM D1922. Compliance follows REACH 1907/2006 Article 33 and EU Directive 94/62/EC. Screen pack gel capture must be balanced against melt temperature rise; excessive head pressure above 350 bar can degrade the recyclate fraction and form gel streaks in the bubble. Batch-to-batch variation in recyclate melt index above 0.5 g/10 min can require die gap adjustment or output reduction to maintain film gauge.

    When 50 µm Film Enters Vertical Form-Fill-Seal Lines for Pulses and Cereals

    At 50 µm thickness, mono-layer HF2007 web is slit to 350 mm and converted on vertical form-fill-seal machines running 60–90 packages per minute. The coefficient of friction is controlled with slip additive masterbatch at 0.5–1.0 wt% added at the extruder throat. Target kinetic COF under ASTM D1894 is 0.15–0.30. Film is processed at 190°C–210°C melt temperature, with die gap 1.8 mm and blow-up ratio 2.0:1 to 2.4:1. Bubble cooling air at 15°C improves gauge uniformity to ±8% or better. Compliance for dry food contact requires FDA 21 CFR 177.1520(c) 3.2a and EU No 10/2011. The selected erucamide or oleamide slip masterbatch must satisfy the applicable specific migration limit in EU No 10/2011 Annex II. Terminal products include 1 kg pulse pillows and 500 g breakfast cereal pouches. Seal strength after filling is measured by ASTM F88 and hot tack by ASTM F1921. Dusty product fines on the seal area require positive air purge at the jaw; otherwise accumulated fines can create a continuous dust layer and lower seal strength. Gauge bands outside ±8% produce seal jaw pressure variation; if seal pressure drops below 0.3 MPa, bottom seal failures increase in high-speed drop filling.

    Pallet Hooder Holding Force Decay at Sub-Ambient Temperatures

    Stretch hood film in 90–120 µm gauge is produced from HF2007 with a 10–20 wt% addition of high-toughness mLLDPE or high-pressure LDPE to increase melt strength and elongation at break. The film is drawn over pallets at 55–70% pre-stretch on elastic recovery equipment. Elastic recovery is measured by ASTM D5459 and holding force by machine-specific instrumentation. At -10°C warehouse conditions, elastic recovery must remain above 90% at 70% stretch to prevent pallet load shift. If more than 30 wt% high-pressure LDPE is used, loss of recovery may exceed 15% after 24 h. Processing on a 65 mm extruder with L/D 30:1 uses melt temperature 200°C–215°C, die gap 2.2 mm, blow-up ratio 2.5:1–3.0:1, and double-bubble air ring configured for high frost line 10 die diameters. The terminal product is a tubular hood film sealed at the top with axial seals, used for pallets of cement, paper rolls, beverage cans and white goods. Compliance is limited to REACH 1907/2006 Article 33 and RoHS 2011/65/EU for non-consumer goods. No food-contact declaration is made unless the specific structure is qualified. At warehouse temperatures above 35°C, holding force decay accelerates; film rolls stored in direct sunlight may show width shrinkage above 2%.

    Evaluating Sealant Web Bond Strength in Extrusion Lamination

    Following corona treatment to 42–46 mN/m measured under ASTM D2578, blown HF2007 film at 30–60 µm is used as a sealant web in duplex or triplex laminates for liquid and dry food sachets. The web is combined to aluminum foil or PET through a 15 g/m² LDPE extrusion tie layer at 320°C. Lamination bond strength is measured by ASTM F904. The sealant layer must maintain heat seal strength above 15 N/25 mm after 0.5 s dwell at 140°C. If sealant web is stored above 40°C or exposed to sunlight, corona treatment decay reduces bond strength. Processing of the sealant web itself uses die gap 1.8 mm, blow-up ratio 2.0:1, melt temperature 190°C–210°C, and inline slitting to 650 mm rolls. Compliance is governed by FDA 21 CFR 177.1520(c) 3.2a and EU No 10/2011. For fatty food simulant D2, overall migration must remain below 10 mg/dm². Finished terminal products include stand-up pouches for sauces and stick packs for drink powders. High extrusion lamination temperatures can retract the sealant web at the nip if line speed drops below 50 m/min; thermal shrinkage is measured by ASTM D2732.

    Free Quote

    Competitive Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem HF2007 is a linear low density polyethylene produced for blown film extrusion with a nominal density of 0.920 g/cm³ and a nominal melt flow rate of 1.0 g/10 min when determined at 190 °C under a 2.16 kg load following ASTM D1238. The resin is a butene-1 copolymer; the comonomer introduces short-chain branches that disrupt crystallinity and produce the density level required for flexible film toughness. The grade is supplied as pelletized reactor product with antioxidant and processing-stabilizer packages, but publicly available technical literature does not disclose exact additive loadings. Film property values for Braskem HF2007 are not fixed resin constants. They vary with blow-up ratio, frost line height, die gap, melt temperature, and screw design. The material is used in monolayer and multilayer blown film structures, including frozen food packaging, collation shrink film, industrial liners, consumer films, and agricultural film. In these applications, the resin is selected for a balance of melt processing stability, low-temperature ductility, and sealing behavior rather than for maximum dart impact or optical clarity.

    What Limits Bubble Stability When Butene-LLDPE Is Processed at Low Melt Temperatures?

    Bubble stability in Braskem HF2007 depends on melt strength and the rate of strain-hardening in the tubular film. When melt temperature falls below 180 °C, insufficient melting of the pellet core can produce unmelted gel particles, and the bubble can become sensitive to air drafts and uneven air-ring flow. The butene-1 comonomer provides a more linear backbone than long-chain-branched LDPE, so zero-shear viscosity and melt strength are lower at equivalent melt index. As a result, the frost line is normally maintained at a greater distance from the die than would be used for high-pressure LDPE to allow the film to stabilize. Melt temperatures from 190 °C to 220 °C are commonly used for this density and melt flow rate, while die temperatures are held 10 °C to 20 °C above the last barrel zone. Blow-up ratios between 2.0:1 and 3.0:1 provide a favorable balance between machine-direction and transverse-direction tear strength. At blow-up ratios below 1.8:1, machine-direction orientation increases, and transverse-direction Elmendorf tear drops. At blow-up ratios above 3.5:1, bubble curvature becomes difficult to control, and gauge variation can increase on lines without automatic air-ring control. The absence of long-chain branching means that Braskem HF2007 does not exhibit the same extensional hardening as LDPE, which must be considered when the resin is substituted into a high-stalk LDPE application.

    On single-screw blown film lines with L/D values between 24:1 and 30:1, barrier screws with a Maddock mixing section are used to homogenize the melt and avoid temperature gradients. Die gaps from 1.5 mm to 2.5 mm are typical for film gauges between 20 µm and 150 µm. A narrower die gap increases shear rate and raises melt temperature, which can improve optical quality but also increase die pressure. A wider die gap reduces die pressure but can lower melt homogeneity and create film bands if the screw is not designed for the lower shear. The extruder backpressure should be monitored continuously; screw surging caused by pellet bridging in the feed throat can lead to gauge variation and inconsistent frost line position. Hopper temperature should not exceed 45 °C to avoid pellet softening and feed instability. Published data for this specific configuration is limited, but the process limits are established by standard blown film practice for 0.920 g/cm³ butene-based LLDPE grades.

    When HF2007 Is Coextruded with LDPE Skin Layers in Frozen Food Structures

    Coextrusion is used to separate the toughness contributed by LLDPE from the melt strength and seal performance supplied by other resins. In frozen food packaging, Braskem HF2007 may be placed in the core or a sub-skin layer of a three-layer A/B/A film where LDPE or a lower-melting ethylene copolymer forms the seal layer. The LDPE skin improves bubble stability and reduces splitty tear behavior, while the LLDPE core contributes tensile strength and low-temperature impact resistance. The blend ratio must be controlled because addition of more than 30 wt% LDPE can reduce dart impact and Elmendorf tear below the values required for frozen-food handling. Conversely, less than 10 wt% LDPE may not adequately correct bubble instability on older low-output blown film lines. Seal initiation temperature and hot-tack strength are not determined only by HF2007; they are governed by the sealant resin and are measured according to ASTM F88 and ASTM F1921. Surface treatment for lamination or printing typically targets 38 mN/m to 42 mN/m corona treatment level. The treatment decay rate can increase when amide-based slip additives bloom to the surface, so additive packages and storage conditions should be controlled for downstream conversion.

    For heavy-duty industrial liners and agricultural film, the film gauge is often increased to 100 µm or more, and puncture resistance becomes the controlling property. Braskem HF2007 is converted on the same tubular blown film equipment used for commodity LLDPE, but the output rate and gauge uniformity are influenced by die size, air-ring design, and internal bubble cooling capability. A production line with a 65 mm single-screw extruder and a 1.5 mm die gap can process the resin at screw speeds that maintain melt temperature within the recommended range; screw speed should not be increased beyond the point where melt temperature exceeds 230 °C, because oxidative degradation at the screw root can generate gel particles and odor. If the line uses internal bubble cooling, the internal air temperature and exchange rate should be stable enough to avoid frost line fluctuations of more than ±10 mm. Frost line fluctuation is a direct indicator of bubble instability in butene-LLDPE grades, and it correlates with gauge variation and film roll profile defects.

    Tensile properties are measured according to ASTM D882 on specimens cut in the machine and transverse directions. Dart drop impact is determined by ASTM D1709 Method A, Elmendorf tear by ASTM D1922, and haze and gloss by ASTM D1003 and ASTM D2457. These test methods are not interchangeable with ISO equivalents when reporting commercial specifications; ASTM D882 uses a different specimen grip separation and strain rate than ISO 527-3. The reported values for Braskem HF2007 depend on film thickness. A 40 µm monolayer film produced at a 2.5:1 blow-up ratio and a 1.5 mm die gap will not have the same dart impact or tear values as a 100 µm film. Therefore converter specifications should be based on production trial data and not on a single supplier datasheet value.

    Table 1: Nominal resin characteristics for Braskem HF2007
    PropertyStandard methodNominal value
    DensityASTM D15050.920 g/cm³
    Melt flow rateASTM D1238 at 190 °C/2.16 kg1.0 g/10 min
    Melting peakASTM D3418122 °C
    Vicat softening pointASTM D1525100 °C
    Comonomer typeIR spectroscopybutene-1

    The table values are nominal resin characteristics from supplier-published technical literature. They do not constitute a specification for every lot; lot-to-lot variation and test uncertainty must be applied when certifying film for commercial use. Film property values are omitted because they are line-dependent and cannot be stated as an intrinsic property of the resin without specifying the exact film fabrication conditions.

    On form-fill-seal lines, film made from Braskem HF2007 is converted at seal bar temperatures that are typically 10 °C to 20 °C higher than those used for LDPE-rich films because the linear ethylene backbone has a higher melting point and lower melt flow under low shear. Hot-tack strength is measured by ASTM F1921, and seal strength by ASTM F88. For frozen food bags, the film must maintain seal integrity through -20 °C temperature cycles; the density of 0.920 g/cm³ provides a balance between stiffness at freezer temperatures and impact resistance. In collation shrink film, the film is oriented in the machine direction and then shrunk in a hot tunnel; the butene-LLDPE contributes high film toughness, but the shrink tension and shrinkage percentage depend on the orientation ratio and the addition of LDPE or mLLDPE.

    Agricultural greenhouse and mulch films require UV stabilization; Braskem HF2007 does not contain high levels of UV stabilizers as supplied, so converters add a UV masterbatch during extrusion. The dispersion of the masterbatch must be verified because poor dispersion creates localized film weakness and premature failure under solar radiation. Film for silage or bale wrap is stretched and wrapped under tension; Elmendorf tear and puncture resistance at the edges must be tested according to ASTM D1922 and ASTM D5748. The grade is also suitable for consumer overwrap and light-duty pallet films when the correct orientation and additive levels are applied, but it is not equivalent to a high-performance hexene- or octene-LLDPE stretch film in terms of ultimate elongation and load retention.

    Processing Line Limits and Pellet Handling Behavior

    Field experience with butene-LLDPE grades on single-screw extruders with L/D 28:1 indicates that pellet feed stability is as important as screw design for gauge control. Pellet bridging can occur when hopper temperature is too high or when regrind with high fines content is mixed into the feed. Fines content above 5 wt% can disturb solids conveying and produce melt pressure oscillations. If regrind is used, the particle size distribution should be matched to virgin pellets, and the feed throat should be purged with dry air when ambient relative humidity exceeds 60%. Although polyethylene does not require predrying in the same manner as polar hygroscopic resins, surface moisture on pellets can introduce bubbles or surface defects in thin films. The use of an air-cooled feed throat is preferred for high-output lines because it prevents premature pellet melting and feed blockages. The resin should not be combined with amine-based antistatic or certain nitrogen-containing additives at levels that cause discoloration or promote oxidative degradation; compatibility should be tested because additive interactions can alter film color and organoleptic performance.

    When Braskem HF2007 is used in applications requiring low odor and taste, the converter should monitor the extrusion temperature profile. Melt temperatures above 230 °C increase the rate of thermo-oxidative degradation, and degradation products can produce odor and off-taste in food packaging. The temperature profile should therefore be optimized to stay below 230 °C while still ensuring melt homogeneity. The use of nitrogen blanketing on the hopper or reduced screw speed may be necessary on lines with long residence time. The operational boundary is not solely a function of the resin; it is also influenced by the antioxidant package, the extruder screw design, and the amount of regrind. Published data for this specific configuration is limited, and validation on the target line is required.

    The Regulatory Framework Does Not Replace Lot-Specific Certification

    For food contact use, Braskem HF2007 is generally evaluated under the olefin polymer framework of FDA 21 CFR 177.1520 and under the European Union plastics regulation 10/2011. These frameworks establish migration limits and permitted monomers, but the final film must be tested or supported by a supplier declaration because processing aids, blending resins, and surface treatment can alter overall compliance. For industrial and electrical packaging, the converter may also need to demonstrate conformity to REACH SVHC restrictions and RoHS Directive 2011/65/EU heavy metal limits. The table below lists the applicable frameworks and standard designations, but it does not substitute for a lot-specific certificate of analysis from the resin supplier or a declaration of conformity from the film converter.

    Table 2: Compliance frameworks commonly applied to Braskem HF2007 film
    FrameworkClause or directiveApplication boundary
    US FDA21 CFR 177.1520Olefin polymers for food contact
    European UnionRegulation 10/2011Plastic materials and articles intended to contact food
    REACHSVHC candidate listSubstances of very high concern
    RoHSDirective 2011/65/EURestricted heavy metals in electrical/electronic equipment

    Braskem HF2007 differs from high-pressure LDPE in that its linear backbone provides higher tensile strength at equivalent density and melt flow rate, but it requires more attention to bubble stability because strain hardening is lower. The resin differs from c6- and c8-LLDPE grades in that its butene comonomer produces a more pronounced decline in dart impact and Elmendorf tear at equivalent density, but the lower comonomer cost and broader availability make it suitable for less extreme packaging demands. It differs from metallocene LLDPE in that its molecular weight distribution is generally wider and its seal initiation temperature is higher, but extrusion pressures are typically lower and the resin can be processed on conventional smooth-bore single-screw machines without the same high-pressure filtration constraints. These differences are mechanical and thermodynamic, not cosmetic; they decide film gauge distribution, bubble stability, and converter efficiency on specific production lines.