Braskem Hf0131 Blown Film Extrusion Linear Low Density Polyethylene

Braskem HF0131 Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem HF0131 Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 616776
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Density 0.918 g/cm³
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Yield Td 10 MPa
    Tensile Strength At Break Md 30 MPa
    Tensile Strength At Break Td 25 MPa
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Dart Drop Impact 120 g
    Elmendorf Tear Resistance Md 150 g
    Elmendorf Tear Resistance Td 300 g
    Haze 12 %
    Gloss 45 50
    Coefficient Of Friction 0.2

    As an accredited Braskem HF0131 Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem HF0131 LLDPE is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for blown film extrusion use.
    Container Loading (20′ FCL) Braskem HF0131 blown-film extrusion LLDPE resin is bagged, palletized, and loaded into 20′ FCL containers for secure ocean shipment.
    Shipping Braskem HF0131 Blown Film Extrusion LLDPE is non-hazardous and not regulated for transport. Ship in sealed 25 kg bags or bulk containers on pallets, stretch-wrapped and labeled. Keep dry, cool, and out of direct sunlight. Avoid contamination and spills; spilled pellets are slippery. No special placards required.
    Storage Store Braskem HF0131 LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Stack pallets securely and avoid excessive height. Protect from UV exposure and rodents. Observe good housekeeping and first-in, first-out stock rotation. Follow the manufacturer’s SDS for detailed requirements.
    Shelf Life Braskem HF0131 typically has a 24-month shelf life when stored dry, unopened, at ambient temperature, away from direct sunlight.
    Application of Braskem HF0131 Blown Film Extrusion Linear Low Density Polyethylene

    In high-output monolayer liner production on 90 mm to 120 mm grooved-feed extruders with 30:1 L/D ratios, Braskem HF0131, a butene copolymer blown film LLDPE with nominal density 0.918 g/cm³ under ASTM D1505 and nominal melt index 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg, is blended at 60 wt% to 85 wt% with clean post-industrial LLDPE/LDPE reclaim and, where stiffness is required, 15 wt% to 30 wt% of an HDPE having nominal density between 0.945 g/cm³ and 0.955 g/cm³. The extruder temperature profile is ramped from 180 °C at the feed throat to 210 °C at the adapter and die. The annular die gap is maintained at 1.8 mm to 2.5 mm because narrower gaps at high screw speeds can amplify melt pressure behind the screen pack above 250 bar. A blow-up ratio of 2.2:1 to 3.0:1 is used, with a frost line height of 2 to 3 die diameters for balanced machine-direction and transverse-direction tear values under ASTM D1922. High stalk machines can operate toward the lower end of that range, while low stalk lines with dual-lip air rings can approach 3.0:1 if internal bubble cooling is available. The film is converted into waste collection sacks, construction debris liners, and industrial bulk packaging. For non-food industrial packaging, European Packaging Directive 94/62/EC Article 11 heavy metal limits apply, and REACH Regulation (EC) No 1907/2006 Annex XVII restricts substances in articles. Color concentrates based on carbon black at 2 wt% to 5 wt% are common for UV stability in outdoor storage, but carbon black agglomerates above 20 µm can initiate pinholes at 25 µm film thickness.

    Why Silage Film Lines Run a Three-Layer Butene LLDPE Core?

    Silage film converters running three-layer lines with 800 mm to 1,200 mm annular dies tend to position HF0131 in the core layer at 60 wt% to 70 wt% because the grade contributes puncture resistance during high-density bale wrapping without raising melt pressure excessively. The outer white layer is usually 15 wt% to 20 wt% of LLDPE or LDPE containing titanium dioxide at 6 wt% to 10 wt%, a hindered amine light stabilizer package at 0.2 wt% to 0.5 wt%, and a UV absorber at 0.1 wt% to 0.3 wt%. The inner cling layer is often 10 wt% to 15 wt% of EVA with vinyl acetate content between 9 wt% and 14 wt% plus polyisobutylene cling additive. The melt temperature at the die is held between 190 °C and 220 °C, and the blow-up ratio is increased to 2.8:1 to 3.2:1 to balance tear resistance. The frost line is raised to 4 to 6 die diameters to reduce transverse-direction orientation and improve tear propagation resistance under ISO 6383-2. Process conflict arises because excessive frost line height above 6 die diameters can induce bubble back and increase gauge variation beyond ±8% at 1,200 mm die widths. EN 13207 specifies mechanical properties for thermoplastic silage films; converters should verify that the final three-layer film meets the tensile and tear requirements of EN 13207 before use. The end products are round bale wrap, silo cover, and temporary greenhouse film.

    At film conversion temperatures below -20 °C, the ductile-to-brittle transition of a butene LLDPE sealant layer becomes the controlling variable for frozen food package integrity. In three-layer coextruded structures, HF0131 is typically compounded in the sealant layer at 70 wt% to 80 wt%, with a metallocene plastomer or low-density polyethylene at 20 wt% to 30 wt% to lower seal initiation temperature. The outer layer is usually high-density polyethylene or a stiffer LLDPE for surface hardness and moisture vapor transmission control. The die gap is held between 1.6 mm and 2.0 mm, and the blow-up ratio is kept at 2.0:1 to 2.5:1 to preserve machine-direction strength. Heat-seal dwell time is set between 0.3 s and 0.8 s at seal bar temperatures from 105 °C to 130 °C, with hot tack force measured according to ASTM F1921. The film must comply with FDA 21 CFR 177.1520 for olefin polymers and with European Regulation (EU) No 10/2011 Annex I and Annex II for food contact materials. Specific migration of constituents must be verified under the intended time and temperature conditions of frozen storage. Films are converted into pillow bags for IQF vegetables, poultry overwrap, and barrier-free frozen seafood pouches. Published data for this specific HF0131 formulation under commercial deep-freeze distribution is limited; converter trials are required to establish dart impact and tear values on the target line.

    When Form-Fill-Seal Sealant Layers Require a 1.0 g/10 min Melt Index

    Vertical form-fill-seal operations converting granular dry mixes place simultaneous demands on sealant layer hot tack, bubble stability, and roll unwind tension. HF0131 is introduced into the sealant layer at 20 wt% to 40 wt% of the total film structure, with a metallocene LLDPE or LDPE to shift seal initiation below 110 °C. The outer layer contains HDPE at 30 wt% to 50 wt% of the total structure for stiffness and moisture resistance. The core layer may contain the remaining LLDPE plus process regrind. A three-layer blown film die with gap 1.5 mm to 2.0 mm and a low blow-up ratio of 1.8:1 to 2.3:1 is used to increase machine-direction orientation and reduce gauge variation before bagmaking. The frost line is maintained at 3 to 5 die diameters to avoid low hot tack in the sealant. Hot tack strength is measured with ASTM F1921, and seal initiation is determined with a gradient heat sealer at 0.5 s dwell time and 0.3 N/mm² seal pressure. For food contact, the sealant layer must meet FDA 21 CFR 177.1520 and European Regulation (EU) No 10/2011, including overall migration below 10 mg/dm² under simulated dry food conditions. End products include pillow pouches for rice, dry pet food bags, and sealed pouches for powdered drink mixes.

    End-use segmentRegulation or standardClause or methodCondition assessed
    Frozen food packagingFDA 21 CFR 177.1520Olefin polymer specificationFood contact suitability
    Frozen food packagingEU Regulation 10/2011Annex I and Annex IIOverall and specific migration
    Industrial liners94/62/ECArticle 11Heavy metal limits
    Industrial linersREACH 1907/2006Annex XVIISubstance restrictions in articles
    Silage filmEN 13207Mechanical property clausesTensile and tear resistance
    Dangerous goods linersUN packaging requirementsLiquid class test provisionsLiner integrity under fill and transport

    Collation Stretch Film: Die Gap, Blow-Up Ratio, and Low-Temperature Puncture

    On blown stretch-film lines with 50 mm to 75 mm grooved-feed extruders, HF0131 is processed at melt temperatures of 195 °C to 225 °C and die gaps of 1.8 mm to 2.5 mm. The blow-up ratio is set between 2.5:1 and 3.5:1 to generate balanced stretch force in both directions; internal bubble cooling is normally required above 3.0:1 to maintain bubble stability. A polyisobutylene tackifier is added at 1 wt% to 3 wt% for cling in pallet unitization, while a slip agent may be omitted to avoid loss of peel force. The film gauge is typically 17 µm to 35 µm, and puncture resistance is measured according to ASTM D5748 or ISO 7765-2. Low-temperature performance is checked at -10 °C because cold-chain pallet handling can expose the film to embrittlement risks. The films are converted on center-fold or single-wound rewinders into hand and machine pallet wrap, beverage collation film, and freezer-grade stretch wrap. For non-food industrial packaging, REACH Regulation (EC) No 1907/2006 applies to the tackifier and polymer additives, and the finished article should be evaluated for mechanical recyclability under a suitable collection stream.

    Blown Film Threading on Industrial Liquid Packaging Lines

    Coextruded industrial liquid packaging structures typically split HF0131 into the outer and core layers at 50 wt% to 70 wt%, with an ethylene-vinyl alcohol copolymer barrier layer at 5 wt% to 10 wt% and tie resins at 5 wt% to 10 wt%. The die gap is maintained at 1.8 mm to 2.2 mm, and the blow-up ratio is limited to 2.0:1 to 2.6:1 to reduce barrier-layer thinning during bubble inflation. Melt temperatures at the die are kept at 200 °C to 220 °C, and the EVOH layer must be processed within the supplier's specified temperature window to avoid degradation and gel formation. The resulting film is fabricated into liners for non-hazardous liquid chemicals, IBC liners, and box-in-box liquid packaging. For dangerous goods packaging, the fabricated liner must be tested under the applicable UN packaging requirements for the specific liquid class, and the outer carton must meet the corresponding freight classification.

    Free Quote

    Competitive Braskem HF0131 Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem HF0131 is a blown film extrusion grade of linear low density polyethylene. The product is supplied as a butene-based copolymer with a nominal density of 0.918 g/cm³ measured by ASTM D1505 and a nominal melt flow rate of 1.0 g/10 min measured at 190°C/2.16 kg by ASTM D1238. The grade is intended for tubular blown film lines producing general-purpose liners, sacks, and packaging films. Melt flow rate is a single-point quality control parameter and does not describe the molecular weight distribution or the shear response required to predict bubble stability; lot-specific datasheets should be consulted for current typical film property values.

    Published typical polymer property values
    PropertyMethodTypical value
    Nominal densityASTM D15050.918 g/cm³
    Melt flow rateASTM D1238 (190°C/2.16 kg)1.0 g/10 min
    Comonomer type—Butene

    Storage and handling prior to conversion require control of surface moisture rather than bulk moisture absorption. Polyethylene does not undergo hydrolytic degradation; however, condensation on cold pellets transferred into a warm conversion hall can produce surge feeding and bubble defects. If the pellet surface temperature is below the ambient dew point, a hopper dryer set at 60°C for 2 h removes surface condensation. Storage at temperatures above 50°C or extended exposure to direct sunlight can reduce additive performance and shift film color; bags should remain sealed and protected from UV radiation.

    How does HF0131 differ from autoclave LDPE and octene-based LLDPE in tubular extrusion?

    Compared with an autoclave LDPE of equivalent melt index, HF0131 exhibits lower melt tension and reduced strain hardening because the linear backbone contains a low concentration of long-chain branches. On a 60 mm grooved-feed extruder with 30:1 L/D and a 100 mm spiral mandrel die at 1.8 mm die gap, the linear resin typically requires higher motor torque per kg/h and generates higher die lip pressure at constant melt temperature because the viscosity at typical die shear rates decreases less rapidly with shear than that of a branched LDPE. Capillary rheometry curves for a 1.0 g/10 min LLDPE show a less shear-thinning response between 100 s-1 and 1,000 s-1 than LDPE of the same melt index. Existing LDPE extruders may require a wider die gap, higher melt temperature, or reduced screw speed when HF0131 is introduced.

    When HF0131 is compared with an octene-based LLDPE of the same density, film made from HF0131 typically shows lower dart impact values under ASTM D1709 and lower Elmendorf tear propagation under ASTM D1922 at equal gauge, particularly below 25 µm. The shorter butene short-chain branch length alters tie-chain formation and crack propagation resistance relative to the longer octene branch length. For less demanding liner and sack constructions, the butene grade provides a lower comonomer-cost position; for low-temperature toughness or high abuse resistance, an octene grade or a blend should be evaluated on the same blown film line.

    Film property development is sensitive to blow-up ratio and frost line height. At a 2.5:1 blow-up ratio and a frost line height of 5–8 die diameters, the film tends to develop balanced machine-direction and transverse-direction tear resistance while maintaining bubble stability on a conventional single-lip air ring. Running with a low stalk and a frost line below 3 die diameters may improve clarity by reducing spherulite size but can increase blocking and reduce dart impact because solidification occurs under higher melt stress. The effect is more pronounced in LLDPE than in LDPE because of the absence of strain-hardening long-chain branches and the faster crystallization behavior.

    When the die gap is set below 1.6 mm at high output

    Die gap selection controls shear rate at the die lip and molecular orientation before bubble expansion. For HF0131 on a 250 mm die with a 2.0 mm gap, a melt temperature between 195°C and 215°C generally keeps die pressure within the normal envelope for spiral mandrel tooling. If the die gap is reduced below 1.6 mm without a throughput reduction, die shear rate increases and sharkskin melt fracture may appear on the film surface. Raising the die temperature by 5°C to 10°C or reducing screw speed can restore a smooth surface; however, increasing temperature may raise oxidation risk if residence time exceeds 20 min. The frost line should then be lowered by 1–2 die diameters to compensate for the higher melt temperature and maintain bubble symmetry.

    Typical starting conditions for HF0131 on a 60 mm grooved-feed extruder with 30:1 L/D and 100 mm die
    ParameterTypical value
    Barrel zone 1175°C
    Barrel zones 2–4185–200°C
    Adapter/die temperature200–210°C
    Melt temperature195–215°C
    Die gap1.8–2.5 mm
    Blow-up ratio2.2:1–2.8:1
    Frost line height5–8 die diameters

    These values are starting points and not lot-specific instructions. The actual profile should be adjusted to keep the melt pressure below the die manufacturer’s maximum limit and to keep the extruder drive motor within its continuous torque rating. The melt temperature must be confirmed with a needle probe at the die exit, not inferred from barrel set points.

    Heavy-duty shipping sacks and industrial liners can be produced from HF0131 at thicknesses from 25 µm to 100 µm. The resin is frequently dry-blended with 10–30% by mass of an autoclave LDPE to increase melt tension and improve bubble stability on lines originally built for LDPE. The blend ratio must be confirmed by measuring dart drop according to ASTM D1709 and tear propagation according to ASTM D1922 on the actual film because the property response is not linear with LDPE content. In agricultural silage film, puncture resistance should be measured under ASTM D5748; published data for HF0131 in this specific configuration are limited, and controlled trials at 2.5:1 blow-up ratio and 50 µm gauge are required before commercial substitution.

    Transitioning from a general-purpose LDPE to HF0131 without purging can produce incompatibility defects if dissimilar resin remains in the screw and die. A purge with a fractional-melt LDPE or a dedicated LLDPE purge compound is run at 10–15°C above the previous resin’s melt temperature until no visible splay or melt fracture remains. The die gap should be opened to 2.5 mm during purging to reduce die pressure. Published purge time data for specific extruder configurations are limited; the endpoint is judged by film surface inspection rather than by a fixed time interval.

    Optical haze, gloss, and surface roughness after antiblock addition

    Natural HF0131 without slip or antiblock additives produces film whose haze depends on cooling rate, die gap, and frost line height. Haze is measured under ASTM D1003, and 60° gloss is measured under ASTM D2457. When an antiblock masterbatch is added at 2–5% by mass, surface roughness reduces blocking but can raise haze and reduce gloss. Rapid cooling at a low frost line can reduce spherulite size and improve haze, but excessive cooling reduces bubble stability in this butene-based LLDPE. The coefficient of friction is measured under ASTM D1894 after conditioning for 40 h at 23°C/50% RH. Slip additive migration is time-dependent; measurements taken immediately after winding will understate the final coefficient of friction.

    Food-contact films made from HF0131 require confirmation of compliance with FDA 21 CFR 177.1520(c) for olefin polymers and any applicable food-type restrictions. The final article must also meet overall migration limits under Regulation (EU) No 10/2011 where European Union food contact is intended. Compliance depends on the complete formulation and processing aids; the converter should obtain a compliance letter from the resin supplier and evaluate the finished article under EN 1186-1 or the relevant national standard.

    Film surface quality on a 70 mm extruder can deteriorate when the die lip temperature is maintained below 200°C and throughput is high. Oxidized material can accumulate at the die lip and transfer to the film as dark specks. Raising the die lip temperature to 205–215°C and using a screw geometry designed for LLDPE reduces dwell time and stagnation. Published data for this specific configuration are limited, but the failure mode is consistent with thermal-oxidative degradation at stagnant flow boundaries.

    Compared with metallocene-catalyzed LLDPE film grades, HF0131 generally has a broader comonomer distribution and lower dart impact at equivalent density. Metallocene grades may offer lower extractables and better low-temperature impact, but they can require tighter temperature control and may exhibit lower melt strength. The comparison should be confirmed by ASTM D1709 and ASTM D1922 on the same blown film line.

    Coextruded structures using HF0131 as a core layer with LDPE skins are used in heavy-duty liners. On a three-layer die with a 250 mm die diameter and 2.0 mm gap, the melt temperature difference between the core and skin should be maintained below 10°C to avoid viscosity mismatch and interfacial wave patterns. The layer distribution must be confirmed by thickness profiling because optical gauges cannot always distinguish individual layers. Published data for this specific configuration are limited.

    Frozen food films require low-temperature dart impact rather than high-temperature seal strength. HF0131 should be evaluated for dart impact at -20°C using ASTM D1709 Method A or Method B depending on gauge. Results from ambient dart testing do not predict cold-temperature performance; published data for HF0131 at this condition are limited.

    Corona treatment of HF0131 film should be verified by wetting tension measured under ASTM D5946 or ISO 8296. A surface energy of 38–42 mN/m is typically required for solvent-based lamination; the required level depends on ink chemistry and storage time. Published data for this specific configuration are limited.

    Stretch hood films and silage films require resistance to puncture and creep. In these applications, HF0131 is typically blended with a linear low density polyethylene of higher density or with LDPE to increase modulus; the blend ratio is not fixed and must be confirmed by measuring secant modulus under ASTM D882 and puncture resistance under ASTM D5748. On a high-stalk LLDPE line, bubble stability of a blend is not predictable from the melt indices of the components alone; the converter should measure melt pressure variation and gauge distribution at 2.5:1 BUR before committing to a formulation.

    Top