Braskem Green Pe Sll318 Blow Film Extrusion And Cast Film Extrusion Linear Low Density Polyethylene

Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 950858
    Meltflowrate 3.2 g/10 min (190°C/2.16 kg)
    Density 0.918 g/cm³
    Meltingpoint 123 °C
    Vicatsofteningpoint 94 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 800%
    Flexuralmodulus 240 MPa
    Hardnessshored 50
    Dartimpact 120 g
    Elmendorftearmd 200 g
    Elmendorfteartd 300 g
    Haze 10%
    Gloss45 80
    Coefficientoffriction 0.2
    Biobasedcarboncontent 100%

    As an accredited Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Green PE SLL318 is supplied in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL loaded with Braskem Green PE SLL318 LLDPE, 25 kg bags, palletized, shrink-wrapped, and secured for blow/cast film extrusion.
    Shipping Braskem Green PE SLL318 is shipped as non-hazardous polyethylene pellets in 25 kg bags, octabins, or jumbo bags, palletized and stretch-wrapped. Transport in clean, dry trucks, containers, or railcars. Store cool, dry, away from UV; avoid contamination and static buildup. Handle per SDS.
    Storage Store Braskem Green PE SLL318 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags/packaging tightly closed, off the floor, and protected from moisture, dust, and contamination. Avoid prolonged high temperatures or UV exposure. Maintain clean handling to preserve resin quality. Use first-in, first-out stock rotation.
    Shelf Life Two years when stored in original packaging, in a dry, cool, ventilated area, away from direct sunlight and ignition sources.
    Application of Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    In frozen spinach, IQF shrimp, and bakery bread bag production, SLL318 is converted as a monolayer blown web in thicknesses from 25 µm to 60 µm on single-screw grooved-feed extruders with screw diameter 60-90 mm and L/D 30, coupled to spiral-mandrel dies of 150-250 mm diameter and 1.4-2.0 mm die gap. The barrel profile from feed throat to die is typically set at 175 °C, 185 °C, 195 °C, 200 °C, and 200 °C, while melt temperature at the die lip is held below 210 °C to reduce gel formation during extended runs. A blow-up ratio of 2.2:1 to 2.8:1 and frost line height of 8-12 die diameters are maintained to balance dart impact and tear propagation. When film gauge drops below 40 µm, the frost line height is narrowed to 8-10 die diameters because additional machine-direction orientation raises dart impact but reduces transverse tear. The polymer is processed at 100% or in an 85/15 blend with high-pressure LDPE when bag stiffness must be increased on vertical form-fill-seal lines. For pouches below 35 µm, silica anti-block is added at 1000-2000 ppm and erucamide slip at 500-1200 ppm to maintain coefficient of friction between 0.20 and 0.35 as measured by ASTM D1894-23. Compliance for direct food contact is established under 21 CFR 177.1520 for olefin polymers and EU Regulation (EC) No 1935/2004 with EU No 10/2011; overall migration testing is performed according to EN 1186-1 and EN 13130-1 with aqueous and fatty simulants. Bio-based carbon content is reported by ASTM D6866-22 Method B. Low-temperature performance is verified using dart impact ASTM D1709-16a method A at -18 °C and Elmendorf tear ASTM D1922-15 in machine and transverse directions. Finished articles include frozen vegetable pouches of 40 µm, IQF seafood pillow packs of 60 µm, and bakery bread bags of 25 µm.

    Application requirementStandardRelevant output
    Olefin polymer food contact21 CFR 177.1520Direct food contact, all food types under conditions of use
    EU plastic food contactEU No 10/2011Overall migration limit 10 mg/dm²
    Biogenic carbon fractionASTM D6866-22 Method BReported as modern carbon percentage
    Dart impact at frozen temperatureASTM D1709-16aMethod A, -18 °C

    What limits on-machine retention force when SLL318 is cast as pre-stretch pallet film?

    Pre-stretch pallet film is converted at 12-25 µm on cast lines equipped with a 75-120 mm extruder with L/D 30, a flat die of 2.0-3.5 m working width, a vacuum box with edge pinning, and a matt chrome chill roll controlled at 18-25 °C. SLL318 is let down with a high-pressure LDPE at 10-25 wt% to lower melt elasticity and with a low level of polyisobutylene from a 5 wt% active masterbatch at 3-6 wt% letdown, giving final tackifier content between 0.15 wt% and 0.30 wt%. Melt temperature at the die lip is maintained between 220 °C and 240 °C; excessive temperature above 245 °C produces smoke generation and die-lip deposit formation that reduces film clarity and increases break rate. Air gap is set at 15-30 cm, with an air knife pressure of 3-5 kPa to reduce edge neck-in below 8%. Retention force is measured after 24 h on a standard A-4 load cell according to ASTM D5458-95(2020), and unstretched film elongation at break is characterized by ASTM D882-18. On-machine failure is most frequently observed when chill roll temperature drifts above 28 °C, producing post-crystallization that reduces pre-stretch uniformity at 250% elongation. For EU industrial packaging, REACH SVHC content below 0.1 wt% is verified by supplier certification. Products include hand wrap and machine film for pallets of beverage cans, corrugated boxes, and white goods.

    Agricultural greenhouse film with HALS and EVA three-layer blown structures

    For three-season greenhouse covers and low-tunnel cladding, SLL318 is coextruded in 150-200 µm three-layer structures on lines with three extruders of 45/60/45 mm feeding a 250 mm spiral die at total output of 250-400 kg/h. The core layer contains 50-70 wt% SLL318 to provide tear resistance and down-gauging capacity; the outer layers contain EVA with 12-18% vinyl acetate for thermal retention and anti-drip wetting. UV stabilization is achieved with HALS at 0.3-0.8 wt% and benzophenone or triazine UV absorber at 0.1-0.3 wt%, with phenolic antioxidant at 0.05-0.15 wt%. Blow-up ratio is set at 2.5:1 to 3.5:1, die gap at 2.0-2.5 mm, and frost line height is raised to 600-900 mm above the die to increase transverse orientation. Internal bubble cooling air temperature is held at 8-15 °C with air flow of 5000-8000 m³/h for a 250 mm die. Anti-fog additives are incorporated in the outer EVA layer at 0.5-1.5 wt%; insufficient anti-fog loading permits condensation droplets that can reduce light transmission by up to 25%. The web is measured against EN 13206:2017 for covering films for agriculture; tensile retention after artificial weathering is assessed by ISO 4892-2 cycles and ISO 527-3 tensile test. The bio-based carbon content of SLL318 does not confer soil biodegradation and this structure must be disposed through mechanical recycling or energy recovery, not EN 13432 composting. Halogen-based fumigants should be avoided because they deactivate HALS stabilizers and accelerate crack formation. Finished products include three-season greenhouse covers, low tunnels for strawberry production, and silage bunker covers where oxygen barrier is not the primary specification.

    For liquid pouch lamination sealant webs, the standard cast film configuration uses a 90 mm single-screw extruder with L/D 30, a 2.5-3.0 m flat die with 0.8-1.2 mm die gap, and a primary chill roll held at 15-20 °C. Corona treatment is applied in-line to reach surface energy of 38-42 mN/m as measured by ASTM D2578-23, enabling bond strength after lamination to 12 µm PET, 18 µm OPP, or 9 µm aluminum foil with solventless adhesives. Formulation includes SLL318 at 97.0-99.0 wt%, silica anti-block at 0.5-1.5 wt%, and erucamide slip at 0.2-0.6 wt%. Heat-seal strength is characterized by ASTM F88-23 at a seal bar temperature of 125 °C, dwell time 0.5 s, and pressure 275 kPa; seal initiation temperature below 115 °C is typical for the grade. Food-contact compliance follows 21 CFR 177.1520 and EU No 10/2011 for fatty food simulants. The main process conflict in this application is the interaction between high slip additive levels and lamination bond strength; additions above 0.6 wt% erucamide can reduce bond strength by more than 20% after 72 h storage. Web thickness variation is maintained within ±5% by online gauge and spot checks under ISO 4593. End uses include liquid detergent refill pouches, edible oil pouches as the inner sealant layer in triplex laminates, and condiment sachets.

    When down-gauging heavy-duty industrial liners exposes melt-fracture limits

    On high-output blown film lines producing construction aggregate liners, SLL318 is blended at 60-80 wt% with 20-40 wt% post-industrial recycled LDPE and blown at 80-150 µm through a 200-350 mm die with die gap 2.0-2.8 mm. The extruder is typically 75-100 mm with L/D 30 and internal bubble cooling is used to sustain output above 150 kg/h. The recycled fraction is restricted to clean in-house trim to avoid gel disruption. Polymer processing aid is added at 0.03-0.08 wt% when die pressure exceeds 350 bar or when sharkskin melt fracture appears at output rates above 180 kg/h. The bubble is run at blow-up ratio 2.5:1 to 3.2:1, frost line height 5-8 die diameters, and melt temperature 195-215 °C. Heavy-duty performance is verified by tensile strength ASTM D882-18, Elmendorf tear ASTM D1922-15, and dart impact ASTM D1709-16a. When the recycled LDPE fraction exceeds 40 wt%, dart impact can drop by more than 30%, and gels larger than 600 µm increase film break frequency. For EU industrial packaging, REACH SVHC content below 0.1 wt% is confirmed by supplier declaration, and RoHS Directive 2011/65/EU restrictions on lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE apply to pigments in masterbatches rather than to the resin itself. End products include 100 µm chemical salt liners, 120 µm mineral wool bag liners, and 150 µm construction debris sacks.

    Free Quote

    Competitive Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem Green PE SLL318 is a butene-copolymer linear low-density polyethylene derived from sugarcane ethanol via ethylene dehydration. The grade is specified for blown film extrusion and cast film extrusion where a renewable-feedstock alternative must perform as a drop-in replacement for fossil-derived LLDPE. Published identification values list a density of 0.918 g/cm³ measured under ASTM D792 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg under ASTM D1238 or ISO 1133-1:2022. The comonomer is butene; short-chain branches produced by comonomer incorporation govern dart impact, Elmendorf tear, seal initiation, and melt fracture behavior in monolayer and coextruded film structures. Because the ethylene is obtained from ethanol dehydration and polymerized without introducing polar functionality, the finished polymer is chemically equivalent to fossil-derived LLDPE and is not biodegradable.

    Applications reported for this viscosity class include agricultural stretch film, collation shrink film, lamination substrates, heavy-duty shipping sacks, and general packaging webs. The grade is also positioned for food-contact films when the finished article complies with FDA 21 CFR 177.1520 and applicable migration limits under EU 10/2011. Published SLL318-specific case studies and converter trial data are limited; end-users should qualify seal strength, coefficient of friction, optical haze, and gauge uniformity on each film line.

    Molecular architecture in SLL318 is linear with short-chain branching. The density and melt flow rate place it between rubbery and stiff film LLDPE grades; the polymer retains enough crystallinity for tensile strength while maintaining tear and puncture resistance. Intermolecular comonomer distribution is not uniform; species with lower short-chain branching crystallize earlier, producing a broad melting range. This breadth aids heat-seal performance but can reduce hot-tack if the sealant layer is not formulated with lower-density resins. Published data for the exact molecular weight distribution and rheological spectrum of SLL318 is limited; lot-specific certificates of analysis should be reviewed for gel count, melt flow ratio, and density before high-speed conversion.

    Why Is the Renewable Carbon Fraction of SLL318 Not an Indicator of Biodegradability?

    Carbon-14 measurement under ASTM D6866 distinguishes fossil carbon from biogenic carbon. Commercial Braskem Green PE grades typically report renewable carbon fractions in the 80–95% range, with exact values shown on the certificate of analysis. The residual fossil carbon may arise from process auxiliaries, additives, or allocation boundaries. SLL318 does not contain hydrolytically cleavable ester or amide linkages; it will not compost. The environmental advantage is limited to feedstock sourcing and potential life-cycle greenhouse gas reductions, not end-of-life degradation. Recyclability in LDPE/LLDPE recovery streams is retained because melt rheology and density are comparable to fossil LLDPE. This is the primary difference from biodegradable polymers and the primary similarity to conventional polyolefins.

    Downstream converting lines do not require requalification based solely on feedstock origin. Corona treaters, flexographic presses, slitters, and pouch machines respond to surface energy, tensile modulus, and heat-seal parameters, all of which are governed by the polymer structure. The use of bio-based ethylene does not alter coefficient of friction unless slip and antiblock masterbatches are changed. A written supplier declaration should be obtained for renewable content, REACH registration, and EU 10/2011 food-contact compliance.

    On a production-scale blown film line equipped with a 70 mm single-screw extruder at 30:1 L/D, Maddock mixing section, and 40/60/100 mesh screen pack, SLL318 typically enters the processing window at melt temperature 210–230 °C. Die gap is commonly set at 1.5–2.5 mm, blow-up ratio 2.0:1 to 3.5:1, and dual-lip air ring with frost-line height 4–8 die diameters. Setpoints below 190 °C can increase back pressure and initiate sharkskin melt fracture on a plain die; setpoints above 250 °C increase oxidative gel formation and edge oxidation in thin-gauge webs. These are general starting parameters for butene-copolymer LLDPE of 0.918 g/cm³ density and 1.0 g/10 min melt flow rate; published SLL318-specific temperature data is limited and line-specific thermal profiling remains necessary.

    In cast film extrusion, a 75 mm barrier-screw extruder with die gap 0.5–0.8 mm, chill roll temperature 15–25 °C, and air gap 20–60 mm is a standard reference. Edge trim can be reincorporated at 20–30 wt% when granulation and feeding are consistent. Cast film from SLL318 develops lower haze and better thickness uniformity than blown film; blown film offers higher transverse-direction tear and puncture resistance. These differences are not unique to SLL318 but follow from the processing route and molecular orientation.

    Starting process references for SLL318 in blown and cast film
    Parameter Blown film Cast film Unit
    Melt temperature 210–230 230–260 °C
    Die gap 1.5–2.5 0.5–0.8 mm
    Blow-up ratio 2.0–3.5 Not applicable ratio
    Air gap Not applicable 20–60 mm
    Chill roll temperature Not applicable 15–25 °C
    Frost-line height 4–8 die diameters Not applicable die diameters

    Comparative Positioning: SLL318, Fossil LLDPE, and Low-Density Polyethylene

    Processors substituting SLL318 for fossil butene LLDPE with equivalent density and melt flow rate do not need to replace screw or die geometry. Extruder pressure, shear heating, and draw-down behavior are controlled by molecular architecture rather than feedstock origin. The differentiation is in feedstock attribution, life-cycle accounting, and renewable carbon certification, not in motor load or melt temperature. Compared with high-pressure LDPE, SLL318 has lower melt strength and narrower molecular weight distribution. This creates more neck-in in cast film and less bubble stability in blown film. Blending 10–30 wt% LDPE is a common remedy when draw resonance or bubble chatter limits line speed. Compared with hexene-copolymer LLDPE of the same density, the butene comonomer type in SLL318 generally provides lower dart impact and Elmendorf tear but may offer an economic advantage in medium-duty film. Comparative values must be verified by ASTM D1709 dart drop and ASTM D1922 tear testing on target film gauge.

    Within coextruded structures, SLL318 is used in core layers where toughness and stiffness are required, while metallocene LLDPE, plastomer, or EVA may be used in sealant skins. Absence of long-chain branching means the product should not be expected to deliver autoclave LDPE-type shrink force or melt strength. Shrink film formulations may include LDPE to control machine-direction and transverse-direction shrink. The use of SLL318 alone in high-shrink collation film may produce insufficient shrink force; converter trials should quantify shrink percentage under 120–140 °C hot-air tunnels or 150 °C oil baths.

    When High-Speed Cast Film Demands Reduction in Neck-In and Melt Fracture

    Cast film converters running above 150 m/min may observe neck-in and edge thickening amplified by the linear structure of butene-copolymer LLDPE. Narrowing the air gap to 20–40 mm and increasing melt temperature toward 240–250 °C reduces elastic recovery but increases oxidation risk when residence time is long. A die gap of 0.7 mm with a draw ratio near 2.0:1 is a starting reference; draw resonance appears as periodic gauge bands and can be corrected by raising melt temperature, reducing air gap, or adding LDPE. Processing above 260 °C is not recommended without flood-cooled extruder and rapid purging schedules. Cross-contamination with polypropylene, polyester, and nylon should be avoided; incompatibility creates optical defects and mechanical weak spots in thin films.

    The product should not be predried for normal processing unless moisture exposure has created surface condensation. If stored at relative humidity above 60%, a hopper dryer at 60–70 °C for 1–2 h is sufficient to remove surface moisture, but polymer degradation must be prevented by limiting residence time. SLL318 is not hygroscopic; the drying step addresses surface water, not internal moisture.

    Seal Initiation Temperature, Mechanical Limits, and Regulatory Boundaries in Converted Food Film

    Seal initiation for butene-copolymer LLDPE with density 0.918 g/cm³ typically falls between 90 °C and 105 °C, depending on seal jaw pressure, dwell time, and layer thickness. Published SLL318-specific seal curves should be requested from the supplier for thermal-transfer packaging; SLL318 generally is not the sole sealant layer when low-temperature sealing below 90 °C is required, but it can be blended with metallocene LLDPE or plastomer to reduce seal temperature. Mechanical properties of films are evaluated by ASTM D882 for tensile strength and elongation, ASTM D1709 for dart impact, and ASTM D1922 for tear. Puncture resistance is often measured under ASTM D5748. The table below summarizes test and compliance designations relevant to SLL318.

    Test and compliance designations relevant to Braskem Green PE SLL318
    Designation Application Unit or value
    ASTM D792 Density 0.918 g/cm³
    ASTM D1238 Melt flow rate 1.0 g/10 min at 190 °C/2.16 kg
    ASTM D6866 Renewable carbon fraction 80–95%
    ASTM D882 Tensile properties of film MPa / % elongation
    ASTM D1709 Dart impact g
    ASTM D1922 Elmendorf tear g
    FDA 21 CFR 177.1520 Olefin polymer food-contact Compliance condition
    EU 10/2011 Plastic materials and articles in contact with food Migration limits

    Because published data for SLL318-specific tensile, tear, and optical values is limited, the numerical ranges in this document are supplied as process-engineering starting references for the viscosity and density class. The film producer retains responsibility for qualified performance, migration compliance, and renewable-content documentation.

    Top