Braskem Green Pe Sll218 21 Blow Film Extrusion And Cast Film Extrusion Linear Low Density Polyethylene

Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 477959
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Recommended Processing Temperature C 180-220

    As an accredited Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Green PE SLL218/21 pellets are supplied in 25 kg moisture-resistant bags, palletized and stretch-wrapped for safe transport.
    Container Loading (20′ FCL) 20′ FCL container loading: palletized, shrink-wrapped Braskem Green PE SLL218/21 LLDPE bags for blow and cast film extrusion.
    Shipping Braskem Green PE SLL218/21 is shipped as solid polyethylene pellets, typically in 25 kg moisture-barrier bags or bulk bags, palletized and stretch-wrapped. Keep in a cool, dry, ventilated area away from direct sunlight, heat, ignition sources, and contamination. Non-hazardous; comply with local transport regulations.
    Storage Store Braskem Green PE SLL218/21 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, palletized, and off the floor to prevent moisture uptake, dust, and contamination. Use first-in, first-out stock rotation and avoid excessive stacking. Ground handling equipment to control static discharge. Do not store outdoors. Inspect packaging regularly.
    Shelf Life Shelf life is typically 24 months from production when stored in original, unopened packaging under cool, dry conditions, away from sunlight.
    Application of Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    On high-speed vertical form-fill-seal lines converting 40–70 µm blown film into dried food pouches, the sealant web performance of SLL218/21 is governed less by bulk tensile properties than by the interaction of jaw temperature, dwell time, and heat-transfer lag through the film cross-section. The grade has a nominal melt flow rate of 2.1 g/10 min at 190°C/2.16 kg when measured under ASTM D1238 and a nominal density of 0.918 g/cm³ when measured under ASTM D792. These values place the material in the standard butene-copolymer LLDPE envelope used on grooved-feed blown film extruders with screw L/D of 30:1 and die gap settings between 1.6 mm and 2.4 mm. The renewable ethanol feedstock used to produce the ethylene does not alter melt rheology; processors should apply conventional LLDPE temperature profiles and screw design guidelines, with bio-based carbon claims verified separately under ASTM D6866. Sealing is not a fixed temperature event. A 50 µm web passing over a serrated jaw at 40 packages/min requires more thermal energy than a 35 µm web on flat sealing bars at the same speed, because the polymer-air interface and the crystalline melting front both retard heat penetration. Hot tack under ASTM F1921 determines whether the bottom seal can survive product-drop loading before cooling. Operators should track the hot tack window between 115°C and 140°C only as a starting range, since sealing through dust or product fines shifts the window upward. Seal strength under ASTM F88 should be recorded after the seal has reached 23°C. The failure mode must be noted: cohesive failure in the sealant layer indicates adequate interdiffusion, while delamination indicates oil or moisture contamination on the sealing jaw. Published data for exact SLL218/21 seal-initiating curves on specific commercial jaw profiles is limited; converter trial runs remain the only reliable source for package-specific settings. Food-contact qualification must be verified against FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 for the intended condition of use. Addition of external slip or antiblock concentrates above the supplier-recommended letdown can lower hot tack and interfere with sealant interdiffusion because additive migration to the seal interface creates a weak boundary layer. Therefore, masterbatch additions should be qualified by seal strength and hot tack measurements before production, not by melt flow alone.

    Compliance matrix for food-contact and bio-based carbon claims associated with the application scenarios below.

    Application segmentStandard or regulationCritical verification
    Dry food pouchesFDA 21 CFR 177.1520, Regulation (EU) No 10/2011Overall migration < 10 mg/dm²
    Frozen food packagingFDA 21 CFR 177.1520Sub-ambient seal integrity under ASTM F88
    Agricultural silage filmRegulation (EC) No 1907/2006 (REACH)SVHC content < 0.1 wt%; UV additive compliance
    Bio-based carbon claimASTM D6866 or ISO 16620-2Carbon-14 content documentation from Braskem certification

    What limits downgauged stretch film retention force at 23°C and 50% RH?

    When SLL218/21 is converted on cast film lines for machine stretch pallet wrap, the process window shifts from blow-up ratio control to chill roll quenching and web gauge uniformity. Cast line configurations typically use a coat hanger or flex-lip die with a die gap of 0.65–0.80 mm, a primary chill roll temperature of 18–24°C, and a secondary cooling roll temperature of 15–20°C. Melt temperature is usually held between 225°C and 245°C for this density and melt index, but the selection is linked to screw design and back pressure rather than to the resin alone. The central property for pallet stretch is not ultimate tensile strength but retained force after pre-stretch. Under ASTM D5459, a 20 µm cast film elongated by 200% and then held at 23°C and 50% RH will relax over time through molecular orientation recovery and chain disentanglement. Load retention is routinely logged at 1 h, 24 h, and 7 days. At 250% pre-stretch, gauge uniformity becomes the limiting variable. Any thickness band deviating more than 1.5% from the web mean concentrates stress and can initiate a tear path parallel to the machine direction. Tear propagation under ASTM D1922 in the machine direction indicates whether the web can tolerate the localized defects generated by die lines or chill roll deposits. The resin is not self-cling. Engineered cling is provided by a coextruded or blend-mixed layer containing polyisobutylene or a polyolefin plastomer, and the outer surface coefficient of friction should be held between 0.3 and 0.5 under ASTM D1894 to prevent telescoping on high-speed wrapping arms. Published numerical retention-force curves for SLL218/21 across all pre-stretch ratios are limited in public datasheets, because cling additive chemistry, chill roll temperature, and winder taper tension all shift the relaxation response. Operators should avoid excessive melt temperature above 250°C, because thermal degradation of the slip additive package can generate volatile condensation on the chill roll, reducing web tack and increasing scratch defects. Pre-stretch ratios beyond 300% with a 12 µm gauge are outside the typical validated range for butene-LLDPE cast stretch film without coextruded metallocene layers. Such constructions often fail by edge tear before pallet load convergence.

    Blown film towers configured with internal bubble cooling and low-pressure die geometry for freezer-grade packaging often process SLL218/21 into film gauges from 40 µm to 80 µm at a blow-up ratio of 2.2:1 to 2.8:1. The frost line height is set high enough to reduce film curvature and gauge variance but low enough to maintain bubble stability. Production-scale machines generally run a frost line between 6D and 10D above the die, where D is the die diameter. Low-temperature ductility is the main reason for selecting a butene-copolymer LLDPE in frozen vegetable or seafood bags, but sub-ambient property data for SLL218/21 is limited in publicly available summaries. Converters commonly evaluate freezer films at -18°C using in-house drop tests modeled on ASTM D1709 and measure tensile elongation under ASTM D882 after conditioning the specimen in a cold chamber for at least 4 h. The film should not be considered a high-clarity freezer web. Haze measured under ASTM D1003 on blown film depends on die gap, blow-up ratio, and melt temperature, and butene-LLDPE typically exhibits greater haze than metallocene-catalyzed ethylene-hexene copolymers with similar density. If the bag is printed, the surface wetting tension after corona discharge should be at least 38 mN/m when checked with test fluids under ASTM D2578. Seal integrity at low temperatures still depends on the sealing jaw parameters rather than the film storage temperature. The sealant interdiffusion governed by ASTM F88 is similar to ambient sealing. Moisture conditioning is not required, but condensation on film surfaces should be avoided during warehouse transfer because ice crystal formation at the seal area can reduce seal strength at startup.

    Agricultural silage film oxygen transmission and puncture resistance

    Silage film made from SLL218/21 on blown film lines is typically extruded at 25–50 µm gauge and applied as a covering web over bunker silos or wrapped over round bales, where oxygen transmission and puncture resistance determine fermentation quality. Oxygen transmission under ASTM D3985 at 23°C and 0% RH is a function of film density and thickness for LLDPE, and the 0.918 g/cm³ density of this grade gives a moderate barrier. Operators should not position this resin as a barrier layer without a coextruded EVOH or nylon core. Puncture resistance is influenced by gauge, orientation, and additive loading. The relevant test is ASTM D5748 for stretch wrap films or a plant-specific slow-puncture method based on ASTM D3420; published results for SLL218/21 in silage applications are limited. The resin does not inherently provide UV stabilization for prolonged outdoor exposure. A UV masterbatch containing hindered amine light stabilizers or benzotriazole absorbers must be qualified using accelerated weathering under ASTM D5208 cycle A, because unmodified LLDPE loses mechanical integrity through chain scission and embrittlement after seasonal solar exposure. The processing window requires stable bubble geometry at a BUR of 2.0:1 to 2.5:1. Excessive blow-up ratio combined with low melt temperature below 195°C can generate melt fracture and localized thinning. Air speed from the external cooling ring should be adjusted to keep frost line height consistent, because frost line oscillation causes gauge bands that later fail under bale wrapping tension. Inorganic antiblock can reduce cling in silage film and must be kept below the minimum required for unwinding; excessive levels will increase haze and reduce the film’s extensibility under winding stress.

    Heavy-duty sack extrusion demands a broader molecular weight distribution than typical butene-LLDPE

    For industrial liners and sacks used in construction waste, chemical intermediates, and bulk powders, SLL218/21 can be processed on high-output blown film lines with die gaps up to 2.5 mm and film thicknesses up to 150 µm, but the mechanical requirements must be validated rather than assumed from density and melt index. The elongation at break under ASTM D882 for butene-LLDPE generally decreases with increasing molecular orientation, and heavy-duty sacks often depend on coextrusion with high-density polyethylene to raise modulus. Puncture and slow tear are the limiting properties. Dart impact under ASTM D1709 and Elmendorf tear under ASTM D1922 should be measured on machine-direction and transverse-direction specimens, because blown film orientation makes tear anisotropic. A sack that passes a 50 kg drop test at 23°C may fail at -10°C if the film develops microcracks at fold lines; low-temperature performance should be tested on the finished sack, not predicted from resin datasheet values. The melt flow rate of 2.1 g/10 min is suitable for thin-gauge film, but high-speed conversion above 250 kg/h on an extruder with screw diameter above 75 mm may require optimized temperature profiles to avoid shear-induced overheating. Additive packages containing high levels of stearate slip can reduce interlayer friction and cause roll telescoping on jumbo winders; slip level should be controlled by coefficient of friction measurements under ASTM D1894 on both surfaces. For stored chemical powders, the film must be evaluated against the specific chemical’s aggressive species, because LLDPE is not a barrier to aromatic solvents, ketones, or chlorinated hydrocarbons. Published data for SLL218/21 in chemical-contact service is limited; qualification requires immersion testing under realistic temperature and stacking load, using weight change and tensile retention after exposure as acceptance criteria.

    Because cast-film gauge uniformity affects shrink force generation in collation bundling, the use of SLL218/21 for beverage multipack shrink film requires measurement of unrestrained linear shrinkage under ASTM D2732 or ISO 11501 at the exact hot air tunnel settings. Cast film exhibits a high machine-direction orientation compared with the transverse direction; at a hot air temperature of 130°C, the machine-direction shrinkage typically exceeds the transverse-direction shrinkage by a factor of 2:1 to 3:1. That anisotropy is acceptable only if the pack dimensions, film layflat, and tunnel air flow are aligned to produce controlled bundle compression without edge curl. The film should be tested for shrink force as a function of temperature, not just percentage shrinkage, because the spring-like recovery force determines whether the film can hold bottle caps and neck rings under transit vibration. Standard practice uses a hot oil bath or hot air oven with force transducer; the data are process-specific rather than resin-specific. SLL218/21 can serve as the base layer, but the formulation must incorporate sufficient slip and antiblock to allow high-speed film feeding through the bundler. The coefficient of friction under ASTM D1894 should be established on corona-treated film if in-line printing is used. Treatment should not be below 38 mN/m under ASTM D2578. The cast film line’s winding unit must maintain controlled web tension, because loose edges at the winder produce baggy film that wanders in the shrink tunnel. For printed collation film, the ink adhesion depends on surface energy and the absence of external slip additive migration; an excessive slip level can reduce ink bond strength and create print skipping at high press speeds.

    When lamination replaces coextruded sealant layers in dry food pouches

    In adhesive lamination, SLL218/21 is extruded into 25–50 µm blown or cast film and then laminated to oriented polyester, biaxially oriented polypropylene, or metallized substrates. The resin acts as the sealant and puncture-resistant backside of the pouch, while the oriented substrate provides stiffness and print surface. Seal performance under ASTM F88 and hot tack under ASTM F1921 become the controlling criteria because the pouch must survive product drop testing immediately after vertical form-fill-seal. The film should be corona-treated to a minimum wetting tension of 38 mN/m under ASTM D2578 on the lamination side to ensure adhesive wet-out. Laminators often specify a solventless or solvent-based adhesive with an application weight of 1.5–2.5 g/m²; the adhesive must be cured at 40–50°C for 24–48 h unless a high-solids solventless system is used. Because film-grade LLDPE contains migrating processing stabilizers common to the polymer class, lamination bond strength should be measured after cure using ASTM F904 or ASTM D1876 T-peel to detect weak boundary layer formation. If bond strength falls below 1.5 N/15 mm on a standard laminate, the converter should verify that the film surface has not been overslipped or contaminated by roll handling. The restriction on additives is similar to that in form-fill-seal applications: external slip or antiblock migration to the lamination surface creates a low-energy interface that can cause delamination under high-temperature retort or hot-fill conditions. SLL218/21 is not suitable as the sole substrate for retort pouches above 110°C, because the crystalline melting region and sealant geometry do not provide the same creep resistance as a higher density sealant resin. Published bond strength data for SLL218/21 on specific laminating adhesives is limited; a laboratory T-peel series on the production film is required before commercial runs.

    Free Quote

    Competitive Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem Green PE SLL218/21 is a renewable linear low density polyethylene designated for blown film extrusion and cast film extrusion. The grade is produced from ethylene derived from sugarcane ethanol by dehydration followed by low-pressure coordination polymerization; the resulting polymer is chemically identical to fossil-derived linear low density polyethylene and contains no ester, amide, or ether backbone linkages. Product literature lists a nominal density of 0.918 g/cm³ by ASTM D1505 and a melt flow rate of 2.1 g/10 min at 190°C under 2.16 kg load by ASTM D1238. The SLL218/21 designation identifies a film extrusion grade in the general-purpose LLDPE range. The material is not biodegradable and does not meet compostable plastics standards such as ASTM D6400 or EN 13432. Renewable carbon content is measurable by ASTM D6866-22 or ISO 16620-2, but the resin should be regarded as a drop-in polyethylene rather than a chemically distinct biopolymer.

    The linear low density architecture is obtained by copolymerizing ethylene with a short-chain alpha-olefin. A density of 0.918 g/cm³ corresponds to a medium level of short-chain branching and crystallinity. This degree of crystallinity provides a balance between flexibility and modulus. Compared with lower-density polyethylene grades, SLL218/21 has a higher crystalline fraction and therefore greater temperature resistance but lower clarity and impact. Compared with higher-density grades, it has lower stiffness and a lower melting point, which broadens the heat-sealing window in coextruded film structures. Potential converter applications include flexible packaging films, liners, lamination films, and general-purpose blown or cast structures where a 0.918 g/cm³ density and 2.1 g/10 min melt flow rate are appropriate. The resin is not formulated for high-clarity retort films or high-stiffness heavy-duty sacks requiring HDPE-like modulus.

    What distinguishes SLL218/21 from fossil-derived LLDPE film resins?

    The practical distinction is limited to carbon sourcing and the life-cycle inventory attached to the ethylene monomer. The mechanical, rheological, and thermal properties of the polymer are controlled by density, melt flow rate, molecular weight distribution, and comonomer distribution. For SLL218/21, the 0.918 g/cm³ density positions the resin in the medium-crystallinity LLDPE range, while the 2.1 g/10 min melt flow rate balances extruder torque against bubble stability. Compared with high-alpha-olefin LLDPE grades based on 1-hexene or 1-octene, a butene-comonomer product of similar density usually shows lower dart impact and lower tear strength but can exhibit reduced melt pressure at the die and easier screw conveyance. Compared with LDPE, the linear backbone of SLL218/21 requires higher shear stress at a given melt flow and does not provide the same degree of strain hardening during bubble expansion. The drop-in nature arises because the polymer chain is chemically identical to fossil LLDPE; the renewable ethylene introduces no oxygen-containing or hydrolyzable linkages that would alter melt stability or recyclability.

    Processors switching from a fossil SLL218/21 to the Green PE version do not need to alter barrel temperature profiles, die geometry, or corona treatment settings solely because of the renewable carbon source. The polymer’s critical shear stress for melt fracture onset, die swell, and air-cooling behavior remain governed by the same average molecular weight, comonomer content, and polydispersity as the fossil analogue. However, antioxidant packages and slip/antiblock masterbatches can differ between production campaigns. When a line previously ran a non-renewable grade, the first 30–60 min of operation should be monitored for die-lip buildup and film blocking. The renewable grade is not hygroscopic in the sense of polyamide or PET, but condensed surface moisture at relative humidity above 60% can create gel-like defects and bubble instability in blown film.

    Blown film conversion of SLL218/21 on a conventional line should maintain a die gap of 1.8–2.4 mm to reduce die-lip shear stress. At stock temperatures below 185°C, sharkskin melt fracture is the most commonly observed defect on 45–60 mm single-screw extruders equipped with 24–30 L/D barrier screws and spiral mandrel dies. Raising the die zone to 200–220°C and keeping the screen-pack differential within the extruder manufacturer’s limit usually eliminates the defect. Bubble stability is maintained at blow-up ratios of 2.0:1 to 3.0:1 and a frost line height of 5–10 die diameters; internal bubble cooling and dual-lip air rings reduce bubble chatter and gauge irregularity at high output. Unlike high-density polyethylene, a linear low density film of this melt flow does not require high melt temperatures for homogenization. Excessive temperature above 230°C accelerates antioxidant consumption and can increase die-lip oxidation.

    Output limitations in blown film arise from the balance between die shear rate and bubble cooling. With a 200 mm spiral mandrel die and 2.5:1 blow-up ratio, maximum stable output on a 60 mm extruder is typically limited by air ring capacity rather than melt temperature. Increasing screw speed without increasing cooling air leads to a high frost line and bubble oscillation. Internal bubble cooling is particularly effective for LLDPE of 2.1 g/10 min because the strain hardening of linear chains is lower than that of LDPE, making the bubble more sensitive to cooling and air pressure changes. A field-observed failure mode is helical gauge variation at high screw speed, which can be traced to poor melt temperature homogenization in the spiral mandrel. The correction is to increase adapter and die set points or reduce screw speed until the melt stream at the die lip is uniform.

    When cast film conversion is selected, quench dynamics replace bubble stretching as the primary property lever

    Cast film lines using SLL218/21 generally run with melt temperatures at the feedblock of 220–250°C, a flat die gap of 0.4–0.8 mm, and a chill roll temperature of 15–30°C. Rapid quenching against the chill roll gives lower haze and higher gloss than slow air-cooled blown film of the same gauge, but it imposes a uniaxial orientation gradient. The resulting film is typically stronger in machine-direction tensile strength and weaker in transverse-direction Elmendorf tear than blown film of the same resin and thickness. Draw resonance is the dominant process instability for cast LLDPE; it appears as periodic thick-thin bands and becomes more likely when draw ratio is too high, air knife velocity is too low, or melt temperature at the die is below 215°C. Reducing die-to-chill-roll distance, increasing melt temperature to 230–240°C, or increasing air knife pressure can suppress the oscillation. Published data for the exact cast film configuration of SLL218/21 is limited; converter trials should establish line-specific gauge, haze, and coefficient of friction values.

    The processing window of SLL218/21 is bounded at low temperature by melt fracture and at high temperature by stabilizer depletion and oxidative odor. Blown film melt temperatures above 230°C and cast film die temperatures above 250°C should be avoided unless required by a specific die or lamination configuration. The resin should not be processed with polar barrier polymers without adhesive tie layers, and pellet surface condensation should be removed by drying at 50–60°C for 2–4 h only when the resin has been exposed to high humidity. Routine predrying is not required under clean dry storage. The grade is not designed for rotational molding, injection molding of thick structural parts, or profile extrusion requiring high melt strength.

    Specification parameters and normalized test methods

    Table 1 lists the principal characterization methods applicable to SLL218/21 film. Test values should be generated on film of the intended production gauge because LLDPE properties are thickness-dependent.

    PropertyMethodCondition / specimen
    Melt flow rateASTM D1238-20 / ISO 1133-1:2022190°C, 2.16 kg
    DensityASTM D1505-18 / ISO 1183-1:201923°C, solid state
    Tensile strength at break and elongationASTM D882-18 / ISO 527-325 µm film, 500 mm/min
    Elmendorf tearASTM D1922-15MD/TD, 25 µm
    Dart drop impactASTM D1709-22 Method A25 µm, F50
    HazeASTM D1003-2125 µm
    Gloss at 60°ASTM D2457-2125 µm
    Biogenic carbon fractionASTM D6866-22 / ISO 16620-2bulk resin

    Mechanical property comparisons between the renewable grade and a fossil-derived SLL218/21 analogue generally fall within normal lot-to-lot variation because the fundamental chain structure is unchanged. The more relevant differences in a converter’s operation arise from stabilizer and slip/antiblock packages. When SLL218/21 is used in coextrusion, it is melt-compatible with polyethylene skin layers and tie resins, but it does not directly adhere to polyamide, EVOH, or PET without an adhesive tie layer. For printing and lamination, corona treatment should raise surface energy to 38–42 mN/m, with readings taken no earlier than 24 h after treatment to account for decay.

    Table 2 lists typical process settings for both conversion methods. The values are starting points, not product specifications, and must be adjusted for die diameter, output rate, and film gauge.

    ParameterBlown film SLL218/21Cast film SLL218/21
    Melt temperature at die entry190–220°C220–250°C
    Die gap1.8–2.4 mm0.4–0.8 mm
    Chill roll temperaturenot applicable15–30°C
    Blow-up ratio2.0:1–3.0:1not applicable
    Frost line height5–10 die diametersnot applicable

    Batch-to-batch variance in film extrusion is often observed as shifts in melt pressure and die-lip deposit rather than changes in density or melt flow. If the melt flow rate varies within the allowed specification band, screw speed and temperature profiles may need adjustment. Catalyst residues and additive hydrolysis products can increase die-lip deposit, especially on long blown film campaigns exceeding 48 h; die cleaning frequency should be established with the supplier’s technical data.

    For food-contact applications in the United States, the base olefin polymer falls under FDA 21 CFR 177.1520 when the finished article meets the prescribed conditions of use and migration limits. In the European Union, plastic articles intended for food contact are assessed under (EU) No 10/2011; the overall migration limit and any specific migration limits for additives must be verified on the final film. REACH registration obligations rest with the supplier of the polymer and with downstream converters for imported articles. The renewable carbon claim is substantiated by ASTM D6866-22 or ISO 16620-2 and must not be extended to imply biodegradability or compostability. The resin is not certified under ASTM D6400 or EN 13432.