| HS Code | 373316 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Bio Based Carbon Content | 100% renewable carbon |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 92 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 24 MPa |
| Elongation At Break | 900% |
| Dart Drop Impact | 110 g |
| Elmendorf Tear Strength Md | 230 g |
| Elmendorf Tear Strength Td | 330 g |
| Haze | 11% |
| Gloss 45 | 65% |
| Recommended Processing | Blow film extrusion and cast film extrusion |
As an accredited Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packaged in 25 kg moisture-resistant bags, palletized and stretch-wrapped, with 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Braskem Green PE SLL118 LLDPE resin, 25 kg bags, palletized, sealed, for blow/cast film extrusion. |
| Shipping | Braskem Green PE SLL118 is shipped as non-hazardous, bio-based LLDPE pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/containers. Packages are palletized, stretch-wrapped, and labeled. Transport in clean, dry equipment; avoid heat, moisture, and contamination. Store in a cool, dry area. Follow local transport regulations. |
| Storage | Store Braskem Green PE SLL118 in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, and flames. Keep in sealed original packaging, elevated off the floor, to prevent moisture, dust, and contamination. Avoid incompatible substances and extreme temperatures. Maintain clean, stable conditions and follow the supplier’s safety data sheet and local regulations. |
| Shelf Life | Shelf life: 24 months from production when stored unopened in a cool, dry, well-ventilated area, away from sunlight and heat. |
Pallet-unitization stretch film extrusion on high-output cast lines constitutes a demanding downstream path for Braskem Green PE SLL118 because the resin is drawn from a 0.5–0.9 mm die gap across an air gap of 10–40 mm onto a chill roll set at 15–25 °C, producing films at line speeds up to 600 m/min. At the nominal melt index of 1.0 g/10 min (190 °C/2.16 kg, ASTM D1238-20) and density of 0.918 g/cm³ (ASTM D1505-18), the polymer retains sufficient melt strength to limit draw resonance while permitting draw-down to 12–23 µm machine-grade film. The formulation for monolayer cast stretch film is typically 85–100 wt% SLL118, with 0–15 wt% LDPE added only when edge trim viscosity falls outside the target range and a cling masterbatch based on polyisobutylene or an ultra-low-density ethylene-olefin copolymer added at 1–4 wt% to control unwind peel force and roll-to-roll noise. Compliance for exported film rolls references REACH Regulation (EC) No 1907/2006, Article 33, with SVHC content below 0.1 wt%, and renewable carbon fraction can be reported through ASTM D6866-21 under ISO 14067 carbon footprint documentation. Terminal product types include hand stretch wraps, machine stretch wraps, and pre-stretched rolls for automated pallet wrappers.
In three-layer blown coextrusions for quick-frozen seafood and vegetable packaging, SLL118 is placed in the sealant layer where the bubble stability limit becomes measurable when total film thickness drops below 35 µm and the sealant layer falls below 8 µm; at that point, oscillating melt pressure across the screen pack and die can couple with low melt strength to produce gauge bands and transverse thickness variation. The sealant-layer formulation is typically 55–75 wt% SLL118, 25–45 wt% metallocene-catalyzed ethylene-octene plastomer, and 0.5–1.5 wt% of a slip/antiblock masterbatch containing 5–10 wt% erucamide and 15–25 wt% synthetic silica. Processing is conducted on a grooved-feed blown-film extruder with L/D 30:1–33:1, die gap 1.8–2.4 mm, BUR 2.2:1–3.0:1, melt temperature 190–220 °C, and frost line height 200–350 mm; quality control includes ASTM D1709-15a dart impact and ASTM D1922-15 Elmendorf tear. For food-contact uses, the resin falls under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with the overall migration limit of 10 mg/dm² applied to the finished sealant web. Terminal products include frozen vegetable pillow bags, seafood pouches, and zipper freezer bags.
| Compliance reference | Parameter | Converter control measure |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer food-contact resin | Supplier lot certification and condition-of-use confirmation |
| Regulation (EU) No 10/2011, Annex I, Table 2 | Overall migration limit | 10 mg/dm² |
| Regulation (EU) No 10/2011, Article 11 | Supporting documents for compliance declaration | Batch-specific masterbatch and resin traceability |
| ASTM D6866-21 | Renewable carbon fraction | Bio-based carbon traceability for packaging claims |
Greenhouse and silage film formulations based on SLL118 use a three-layer blown structure in which the SLL118-rich layers account for 70–85 wt% of the total structure and an EVA core layer is added at 10–20 wt% to improve infrared retention and light diffusion. A hindered amine light stabilizer masterbatch is dosed at 0.4–0.8 wt%, with an antioxidant at 0.05–0.15 wt% and an anti-drip additive at 0.8–1.5 wt%; because the anti-drip additive is thermally sensitive, the metering-zone temperature is capped at 215 °C. Compliance for agricultural coverings references EN 13206:2017 for mechanical and weathering requirements, and Regulation (EC) No 1907/2006 for SVHC content below 0.1 wt%. The blown film line operates at die gap 1.8–2.5 mm, BUR 2.4:1–3.2:1, melt temperature 190–215 °C, and film thickness 150–200 µm; after extrusion, the web is surface-treated to 38–42 dyn/cm for antifog coating adhesion. Published data for high-altitude greenhouse exposure of this specific grade is limited; pre-qualification weathering trials are required. Terminal products include greenhouse covers, low tunnels, and silage clamp barriers.
A monolayer or two-layer blown film format is used for heavy-duty industrial shipping sacks, where the formulation is 100 wt% SLL118 with a slip/antiblock masterbatch at 1.0–2.5 wt% total loading and, for outdoor-stabilized sacks, a carbon-black UV masterbatch at 0.5–1.0 wt%. Extrusion uses a grooved-feed screw with L/D 30:1–33:1, die gap 1.6–2.2 mm, BUR 2.0:1–2.8:1, melt temperature 200–230 °C, and corona treatment to 38–42 dyn/cm before flexographic printing. Compliance references ASTM D4976-21 for polyethylene materials and Regulation (EC) No 1907/2006 Annex XVII; when converted sacks carry dangerous goods, qualification shifts to UN packaging performance tests under ADR/RID Chapter 6.1 for sacks or Chapter 6.5 for IBC inner liners, not to the resin standard. Terminal products include valve sacks, FIBC inner liners, and powder transport sacks.
When the converter targets increased transverse shrink force for bottle or can collation, the formulation moves from neat SLL118 to a blend of 55–75 wt% SLL118 and 25–45 wt% LDPE, with an optional HDPE fraction of 0–8 wt% to increase stiffness without eliminating shrink recovery. Shrink force is generated by high transverse orientation on a blown film line, typically 3.0:1–4.0:1 BUR, die gap 1.2–1.8 mm, melt temperature 185–210 °C, and frost line height set at 1.5–2.5 die diameters; shrink tension is measured according to ASTM D2732-14 in a heated oil bath at 120 °C. Compliance for packaging is tied to EU Packaging and Packaging Waste Directive 94/62/EC, Article 11, where the sum of lead, cadmium, mercury, and hexavalent chromium in the packaging material must not exceed 100 ppm, and to Regulation (EC) No 1907/2006. Terminal products include bottle collation shrink bundles, canned goods multipacks, and shrink hoods.
Unlike ordinary lamination webs, liquid packaging sealant webs made from SLL118 require a seal initiation temperature low enough to avoid damaging barrier layers during high-speed form-fill-seal, typically below 110 °C; the sealant layer is therefore blended with 20–40 wt% metallocene-catalyzed ethylene-octene plastomer in a 60–80 wt% SLL118 sealant layer. The web is cast-extruded at melt temperature 240–270 °C, die gap 0.6–0.8 mm, air gap 15–30 mm, and chill roll 18–25 °C, then corona-treated to 44–48 dyn/cm before lamination to aluminum foil or paperboard. Food-contact compliance is documented under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration limit 10 mg/dm²; seal strength after lamination is tested according to ASTM F88/F88M-21. Terminal products include bag-in-box liners, aseptic carton sealant webs, and liquid pouch spout films.
Competitive Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Green PE SLL118 is a sugarcane-derived linear low density polyethylene specified for both blown film extrusion and cast film extrusion. The resin is a butene-copolymer LLDPE with a nominal melt flow rate of 1.0 g/10 min when measured according to ASTM D1238 at 190 °C under a 2.16 kg load, and a nominal density of 0.918 g/cm³ determined by ASTM D1505. The ethylene monomer is produced by dehydration of sugarcane ethanol and then polymerised into a polyethylene backbone that is chemically equivalent to fossil-derived LLDPE but contains renewable carbon measurable by ASTM D6866. The grade suffix 118 follows conventional polyethylene nomenclature: the first digit indicates a nominal melt index of 1.0 g/10 min and the last two digits indicate a nominal density of 0.918 g/cm³. Standard film variants are pelletised with an antioxidant package and an antiblock/slip additive combination. The resin is intended for thin-gauge industrial, agricultural, overwrap, and lamination film applications, but is not biodegradable or compostable; it belongs to polyethylene recovery streams under the same conditions as fossil-derived LLDPE.
On production-scale blown film lines with 60 mm to 90 mm single-screw extruders and 24:1 to 30:1 L/D barrier screws, SLL118 is normally started with barrel zones of 180 °C to 220 °C, adapter and die zones of 210 °C to 230 °C, and a melt temperature of 205 °C to 235 °C at the head. Die gaps between 1.6 mm and 2.4 mm are typical, with blow-up ratios of 2.0:1 to 3.0:1 and frost line heights of 6 to 8 die diameters. The lower melt strength of 0.918 g/cm³ butene LLDPE becomes visible when take-off speeds exceed 120 m/min; bubble instability then appears as a vertical or helical oscillation of the frost line, generating gauge bands of ±5 % or more on capacitance or beta-ray thickness profilers. Raising melt temperature toward 235 °C and reducing the frost line to 5 die diameters can stabilise the bubble, but melt temperature above 250 °C accelerates gel formation in high-shear zones. Die pressure on a 90 mm extruder with a 2.0 mm die gap and 2.5:1 blow-up ratio is generally in the range of 200 bar to 320 bar; pressure variation of more than 10 bar at fixed screw speed indicates feed starvation, screen pack fouling, or resin degradation. Fluoropolymer processing aid at 200 ppm to 500 ppm is used on some lines to suppress sharkskin melt fracture when the film die lip shear rate exceeds 400 s⁻¹. Field data from conventional blown film lines at 120 kg/h on 75 mm extruders show specific energy consumption of 0.25 kWh/kg to 0.32 kWh/kg. When compared with metallocene LLDPE, die pressure is typically lower by 10 % to 18 % at the same output and melt temperature, a result of the broader molecular weight distribution.
Agricultural use of SLL118 is typically specified at film thicknesses of 80 µm to 150 µm for greenhouse and tunnel covers. Tear propagation resistance is measured by ASTM D1922, and puncture resistance is measured by ASTM D5748. UV stabiliser masterbatch addition in the range of 0.3 % to 1.0 % by mass is required depending on service life; the base resin alone does not provide UV resistance. Published data for SLL118 greenhouse film lifetimes without UV additive is limited. The broad molecular weight distribution supports high melt strength at low shear rates, but the film can develop high line-direction orientation when the drawdown ratio exceeds 4:1; drawdown ratios below 4:1 are therefore typical.
Cast film conversion of SLL118 on chill-roll lines commonly uses 90 mm to 150 mm extruders with barrier feed sections, 100 µm to 250 µm screen packs, and automatic die-bolt gauge control. Melt temperatures are set between 240 °C and 260 °C to reduce neck-in, improve die-lip wetting, and maintain gauge uniformity at the edge beads. Typical starting conditions include die gaps of 0.5 mm to 0.8 mm, air gaps of 20 mm to 40 mm, and chill-roll temperatures of 20 °C to 35 °C. Edge trim fractions of 8 % to 12 % are routine in cast LLDPE operations. On lines with online capacitance gauges, film thickness variation at 25 µm nominal thickness is typically held below ±2 %, although published data for SLL118-specific neck-in coefficients under draw ratios above 200 % is limited. For stretch-wrap applications, the standard slip package can reduce peel cling measured by ASTM D4649; processors often add a cling-agent masterbatch to achieve the required unwind force, and the resulting film is then tested on high-speed wrappers at 40 % to 300 % pre-stretch settings. The grade is also used for overwrap and lamination films, where corona treatment levels of 38 mN/m to 42 mN/m according to ASTM D2578 are maintained for ink and adhesive bonding.
Table 1 reports representative nominal values obtained on 40 µm blown film produced at a melt temperature of 190 °C, blow-up ratio of 2.0:1, die gap of 1.6 mm, and frost line height of 5 die diameters. These values are drawn from manufacturer technical literature and are not lot-release maxima or minima. Lot-to-lot variation can occur due to additive package, film thickness, gauge uniformity, and orientation.
| Property | Test method | Typical value |
|---|---|---|
| Density | ASTM D1505 | 0.918 g/cm³ |
| Melt flow rate (190 °C/2.16 kg) | ASTM D1238 | 1.0 g/10 min |
| Melting temperature | ASTM D3418 | 122 °C |
| Vicat softening temperature | ASTM D1525 | 102 °C |
| Secant modulus at 1 % strain MD/TD | ASTM D882 | 190/210 MPa |
| Tensile strength at break MD/TD | ASTM D882 | 36/32 MPa |
| Elongation at break MD/TD | ASTM D882 | 750/850 % |
| Dart impact F50 | ASTM D1709 Method A | 100 g |
| Elmendorf tear MD/TD | ASTM D1922 | 120/350 g |
| Haze | ASTM D1003 | 6.5 % |
| Gloss at 45° | ASTM D2457 | 85 |
Compared with high-pressure LDPE of density 0.923 g/cm³, SLL118 gives higher elongation at break and dart impact, but lower melt strength and lower bubble stiffness. Compared with a metallocene-catalysed hexene LLDPE of similar melt index, SLL118 typically shows broader molecular weight distribution, lower extrusion head pressure at equivalent output, and higher shear sensitivity, but may produce higher haze and lower dart impact. The comparative difference is measured by ASTM D1238 pressure-displacement rheology, ASTM D1709 Method A, and ASTM D1003. Film using SLL118 is not recommended where optical clarity is the sole acceptance criterion because the butene copolymer backbone and standard antiblock particle package can raise haze relative to metallocene grades. Conversely, the grade is suitable for heavy-duty sacks and industrial liners where tear propagation resistance and extrusion throughput are more important than optical clarity. Because the standard antiblock package is designed for thin-gauge film, thick film above 150 µm may exhibit visible haze and reduced gloss. For cast film below 20 µm, gauge uniformity is limited by die-lip geometry and air gap rather than by resin lot variation.
Because the ethylene monomer is purified to polymerisation-grade specification before insertion into the polyethylene chain, the bio-based origin does not alter the short-chain branching distribution or molecular weight distribution of SLL118. The butene comonomer content and reactor conditions control crystallisation, not the feedstock source. Differential scanning calorimetry under ASTM D3418 shows a peak melting endotherm near 122 °C, equivalent to fossil-derived butene LLDPE at the same density. The bio-based carbon fraction does not change lamella thickness distribution or film crystallinity after orientation.
Seal initiation temperature on 40 µm film measured according to ASTM F88 typically falls between 100 °C and 110 °C. Hot-tack and contamination-seal behaviour are governed by gauge, corona treatment level, additive bloom rate, and heat-seal jaw profile rather than by renewable carbon content. The main analytical distinction from fossil LLDPE is the 14C concentration determined by ASTM D6866, which detects biogenic carbon through radiocarbon analysis. Conventional hydrocarbon analysis by FTIR, GPC, and DSC cannot distinguish Green PE from fossil-derived LLDPE because the molecular repeat unit is identical.
This distinction has regulatory and life-cycle consequences but not conversion-lane consequences. Films produced from SLL118 can be introduced into established polyethylene recycling streams. The material is not biodegradable, compostable, or oxo-degradable. If a downstream application requires industrial compostability, SLL118 is not an appropriate substitute for aliphatic-aromatic copolyesters or PLA.
Food-contact evaluation for SLL118 follows FDA 21 CFR 177.1520 for olefin polymers. The bio-based feedstock does not change the regulatory status of the polymer; the finished article must still meet the conditions of use in the regulation, including thickness, temperature, and food-type restrictions. For European food-contact applications, compliance is assessed under Commission Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² for plastic materials and articles. Specific migration of the antioxidant and slip/antiblock package must be confirmed with the final film structure. Braskem maintains REACH registration for the resin; downstream processors remain responsible for any additives or masterbatches introduced on the production floor. Renewable carbon content is documented by ASTM D6866, and Braskem technical literature reports bio-based carbon values above 85 % for the bio-based polyethylene portfolio. The resin is not formulated with intentionally added phthalates. RoHS restrictions do not apply to polyethylene packaging unless the finished article is incorporated into electrical or electronic equipment and is subject to downstream substance restrictions.
Changeover to SLL118 does not require screw, die, or winder modification when the incumbent resin has a similar melt flow rate and density. The melt pump and screen changer remain within normal pressure limits; however, the standard slip and antiblock package can shift the coefficient of friction measured by ASTM D1894, and downstream tension, web tracking, and roll hardness should be revalidated after each lot change. Corona treatment levels of 38 mN/m to 42 mN/m are typical for lamination and print adhesion, measured by ASTM D2578. The resin should not be held above 280 °C melt temperature for extended periods because oxidative chain scission can generate gel defects and dark specks. Pre-drying is not required at ambient relative humidity below 60 %; storage above 70 % RH may require drying at 60 °C for 2 h to prevent surface moisture defects on cast film. Regrind addition up to 20 % is acceptable when the regrind is clean and free of PVC, high-acid copolymers, or peroxide residues. The material is not compatible with high levels of amine-based antifog additives unless compatibility testing is performed because additive interactions can raise haze and reduce slip performance. Processors should verify final film properties against ASTM D882 tensile and ASTM D1709 dart impact values to establish lot conformity.