| HS Code | 533252 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.1 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 22 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 10% |
| Gloss | 60% |
| Coefficient Of Friction | 0.2 |
| Bio Based Carbon Content | 100% |
| Renewable Source | Sugarcane ethanol |
As an accredited Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem Green PE SLL118/21 LLDPE is supplied in 25 kg polyethylene bags, forty bags per pallet, totaling 1,000 kg net. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Braskem Green PE SLL118/21 Linear Low Density Polyethylene for blow film and cast film extrusion. |
| Shipping | Braskem Green PE SLL118/21 LLDPE is shipped as non-hazardous polyethylene pellets in 25 kg bags or 1,000 kg octabins, palletized and stretch-wrapped. Transport in clean, dry trucks/containers away from heat, moisture, and ignition sources. Not regulated for transport; store below 50°C, follow local regulations/SDS. Handle with care; use original packaging. |
| Storage | Store Braskem Green PE SLL118/21 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed, clean, and palletized off the floor to prevent moisture pickup. Avoid prolonged UV exposure and static buildup. Follow manufacturer SDS and local regulations for safe handling and storage. |
| Shelf Life | Recommended shelf life is 12 months from production when stored in original unopened packaging, dry, cool, away from direct sunlight. |
In blown film conversion of Braskem Green PE SLL118/21 for silage covers and mulching sheets, the polymer is processed on high-output blown film towers equipped with grooved-feed extruders of 30:1 to 35:1 L/D ratio, spiral mandrel dies of 250 mm to 400 mm diameter, and dual-lip air rings with internal bubble cooling. The resin has a nominal density of 0.918 g/cm³ and a melt flow rate of 1.0 g/10 min measured at 190 °C under 2.16 kg according to ISO 1133-1. A die gap of 1.8 mm to 2.4 mm and a blow-up ratio of 2.2:1 to 2.8:1 are maintained because the film is drawn down to 25 µm to 200 µm depending on service exposure. Frost line height is set between 8 and 12 die diameters to stabilize the bubble. Excessive stalk height in this resin produces transverse direction tear anisotropy, while an overly low frost line reduces layflat and aggravates blocking during winder nip accumulation. For silage cover applications, the UV stabilization package is introduced as a masterbatch containing hindered amine light stabilizers combined with a UV absorber, typically at 0.5 wt% to 1.2 wt% in the final film, although the exact loading is adjusted to target service life under ISO 4892-2 accelerated weathering. The film is coextruded with a metallocene LLDPE skin or an EVA-rich skin to improve puncture resistance and weldability. Tensile properties are evaluated according to ISO 527-3 or ASTM D882, tear resistance according to ISO 6383-2 or ASTM D1922, and dart impact according to ASTM D1709 Method A. Mulching films made from SLL118/21 require carbon black or titanium dioxide opacifiers; the choice of opacifier changes the infrared absorption profile and influences soil temperature control, but published data for this specific configuration is limited.
Cast stretch film production with SLL118/21 on high-speed chill-roll lines exposes the resin to elongational deformation rates that can initiate draw resonance at high draw ratios. The melt is extruded through a flat die with a die gap of 0.5 mm to 0.8 mm onto a chill roll maintained at 20 °C to 30 °C, with air knife pressure and vacuum box settings used to pin the web and minimize neck-in. Melt temperatures are typically held at 240 °C to 260 °C, and the film is drawn in the machine direction to a final thickness of 12 µm to 30 µm. Edge tear resistance depends on transverse direction orientation; if the die lip temperature profile is non-uniform, edge beads form and initiate tearing during pre-stretch at 150 % to 300 % on power pre-stretch units. Cling is generated by adding a low-molecular-weight polyisobutene or a dedicated cling masterbatch, while slip additives in the opposite skin control unwind force. The coefficient of friction is measured according to ISO 8295, and puncture resistance according to ASTM D5748. Migration of the cling agent to the film surface is time- and temperature-dependent; storage above 35 °C can cause excessive surface tack and blocking in reel form. Published data for this specific configuration is limited, but industrial practice for LLDPE cast film uses additive loadings in the 0.5 wt% to 2.0 wt% range in the skin layer.
Vertical form-fill-seal equipment running 40 µm to 70 µm monolayer frozen vegetable bags from SLL118/21 requires seal integrity through moisture, starch dust, and low-temperature product impact. The film is produced by the blown process with a blow-up ratio of 2.0:1 to 2.5:1, then corona-treated to a wetting tension of 38 mN/m to 42 mN/m for ink adhesion. Seal strength is measured according to ASTM F88/F88M, and hot tack force according to ASTM F1921/F1921M at dwell times below 0.5 s, because filler speeds exceed 60 packs/min. Low-temperature dart impact is tested at -20 °C under ASTM D1709 Method A; the film must resist brittle failure when filled product is dropped from the sealing jaws to the takeaway conveyor. Food-contact status for the resin in the United States is established under FDA 21 CFR 177.1520(c), and in the European Union under Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² as specified in Article 12. Organoleptic performance is monitored by sensory panel testing using DIN 10955 and related standard procedures. Additive selection is restricted to slip and antiblock concentrates whose specific migration limits are listed in EU 10/2011 Annex II; excessive antiblock loading above 3,000 ppm reduces film clarity and can create visible haze on frozen product packages.
| Application | Requirement | Standard or method |
|---|---|---|
| Frozen food VFFS film | Overall migration limit | EU 10/2011 Article 12 |
| US food-contact film | Olefin polymer compliance | FDA 21 CFR 177.1520(c) |
| Bio-based carbon content | Carbon-14 determination | ASTM D6866 |
| Melt flow rate | MFR at 190 °C/2.16 kg | ISO 1133-1 / ASTM D1238 |
| Dart impact | Impact failure mass | ASTM D1709 Method A |
| Heat seal strength | Force at seal failure | ASTM F88/F88M |
| Heavy-duty industrial liners | SVHC content declaration | Regulation (EC) No 1907/2006, Article 33 |
Lamination sealant webs convert SLL118/21 into a low-sealing-temperature layer for snack and dry food structures. The cast web is produced at 25 µm to 40 µm, then laminated to BOPP or BOPET with a solventless polyurethane adhesive. The sealant layer is the reverse side, while the printed BOPP or BOPET face provides stiffness and gloss. Seal initiation temperature is measured by making seals at 0.5 s dwell and 0.3 N/mm² jaw pressure, then testing seal strength according to ASTM F88/F88M. A lower seal initiation permits higher packaging speeds because the jaw temperature can be reduced without sacrificing seal strength. Hot tack measured by ASTM F1921/F1921M is critical on vertical and horizontal form-fill-seal lines where the seal is loaded immediately after sealing. The coefficient of friction of the sealant surface is adjusted with slip additives to a kinetic value below 0.30 under ISO 8295 to support reliable flow through forming collars. Additives must not exceed migration limits specified in EU 10/2011 Annex II. Primary aromatic amines from the laminating adhesive are monitored under EU 10/2011 Annex II with a detection limit of 0.01 mg/kg. The Green PE sealant web retains the bio-based carbon attribution measured by ASTM D6866; however, the laminated structure's overall bio-based content is diluted by the fossil-based BOPP or BOPET facestock.
Blown film lines producing 100 µm to 200 µm heavy-duty industrial liners from SLL118/21 operate with a high-stalk bubble configuration to maximize machine direction tear strength and puncture resistance. Die diameters of 350 mm to 600 mm and blow-up ratios of 1.8:1 to 2.2:1 are common, with die gaps of 2.0 mm to 2.5 mm to control melt fracture and maintain output stability. The liners are filled with fertilizers, resins, or mineral powders. Seal-through-dust performance requires heat-seal settings that displace product contamination from the seal area, and seal strength is measured according to ASTM F88/F88M. Film tear resistance is evaluated by ASTM D1922 and ISO 6383-2, while puncture resistance is tested according to ASTM D5748. A fluoropolymer processing aid at 200 ppm to 500 ppm is added to delay shark-skin melt fracture when line speed exceeds 80 m/min; loading above this range does not improve surface quality and can increase die-lip deposit formation. Film blocking is controlled with an antiblock masterbatch based on synthetic silica at a final film concentration of 1,000 ppm to 3,000 ppm, but excessive antiblock reduces tear strength and creates stress concentration points at seal corners.
Stretch hood packaging uses a tubular blown film of SLL118/21 that is stretched over a loaded pallet and allowed to recover, requiring higher elastic recovery than machine-direction cast pallet wrap. The film is blown at a thickness of 100 µm to 180 µm, a blow-up ratio of 1.5:1 to 2.0:1, and a frost line height adjusted to balance tensile strength and snap-back recovery. The film is stretched by a forming head that opens the tube; recovery force holds the pallet load under transit vibration. Puncture resistance is tested according to ASTM D5748, and slow puncture by ISO 7765-2 may be specified for sharp corner protection. Elastic recovery after 50 % elongation is measured using a tensile test method derived from ISO 527-3; the film must recover enough to maintain load stability but not so much that it crushes fragile cartons. SLL118/21 is coextruded with a high-pressure LDPE layer in some stretch hood structures to increase melt strength and improve bubble stability. UV stability is required when the wrapped pallet is stored outdoors; a UV masterbatch designed for polyethylene film is added at the film producer's specified loading for the intended exposure period. Published data for this specific configuration is limited, so converter trials must establish the relationship between blow-up ratio, frost line height, and recovery force for the pallet dimensions being wrapped.
Competitive Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene is a renewable linear low-density polyethylene produced from sugarcane-derived ethylene. The grade is designed for monolayer and coextruded film structures manufactured by blown film extrusion or cast film extrusion. Nominal density is 0.918 g/cm³ measured according to ASTM D792, and melt flow rate is 1.0 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238. The polymer backbone is a linear ethylene–alpha-olefin copolymer, and the renewable ethanol feedstock does not require a dedicated polymerisation reactor separate from hydrocarbon ethylene routes after dehydration. The renewable carbon fraction is verified by ASTM D6866; lot-specific chain-of-custody documentation supplies the controlling value rather than a fixed single average. The product is supplied in pellet form with antioxidant and processing stabiliser additions for film extrusion. Because the melt flow rate is lower than many cast film grades, die pressure and torque response must be managed when the material is run outside blown film settings.
Melt temperature is the principal variable governing bubble stability in blown film extrusion. A practical starting profile on a single-screw extruder with 25:1 to 30:1 L/D and a barrier screw places the feed zone at 150–170 °C, the compression zone at 170–190 °C, the metering zone at 180–210 °C, and the die body at 190–220 °C. Die lip melt temperature should be held between 180 °C and 220 °C. Operation below 180 °C increases melt viscosity, raises screen pack differential pressure, and can initiate melt fracture in the spiral mandrel die. On production lines running LLDPE of 1.0 g/10 min MFR, lowering barrel temperature toward 160 °C has been observed to increase head pressure by more than 8–10 MPa depending on throughput and screen condition. Operation above 240 °C accelerates thermo-oxidative degradation at the die lip and produces gel particles and optical defects. A 60/100/60 mesh screen pack is a common starting point for blown film; continuous head pressure logging should be established, and filter replacement should occur when pre-screen pressure increases by 8–10 MPa above clean-line baseline.
The blow-up ratio should be limited to 2.0:1 to 2.5:1 for this linear polyethylene. Blow-up ratios above 3.0:1 reduce bubble stability because the grade has lower melt strength than autoclave LDPE. Frost line height is normally held between 6 and 10 die diameters above the air ring; a frost line that is too low raises quench-induced orientation and a frost line that is too high can increase blocking force. On-line capacitance thickness measurement combined with ISO 4593 laboratory sampling should be used to confirm gauge uniformity. Film tensile properties require converter-run capability studies because gauge, blow-up ratio, quench rate, and masterbatch dilution override single-point data sheet values.
Selected specification parameters are summarised below. Film tear, dart impact, haze, and coefficient of friction are not fixed material constants for this grade; they are dependent on gauge, extrusion temperature, cooling rate, and additive package. Published data for this specific configuration is limited when the converter uses modified die gaps or unusual layer structures.
| Property | Test method | Nominal or controlling value |
|---|---|---|
| Density | ASTM D792 | 0.918 g/cm³ |
| Melt flow rate | ASTM D1238 | 1.0 g/10 min at 190 °C/2.16 kg |
| Renewable carbon fraction | ASTM D6866 | Lot-specific certificate value |
The density of 0.918 g/cm³ places the resin in the low-density linear range, providing higher dart impact and Elmendorf tear than stiffer medium-density linear grades while retaining sufficient modulus for industrial packaging. The melt flow rate of 1.0 g/10 min is moderate and suited to blown film; for cast film, the lower flow raises die pressure relative to cast film grades at 2.0–4.0 g/10 min. Melt temperature can be increased inside the permissible window to reduce viscosity, but screw speed should not be used as the only compensation because shear heating may exceed the set-point temperature.
In cast film extrusion, SLL118/21 is processed through a slot die with a die lip gap between 0.5 mm and 0.8 mm. Die melt temperature is typically raised to 200–240 °C to support thin-gauge draw and to reduce head pressure. The air gap between die exit and chill roll is maintained between 20 mm and 80 mm; a shorter air gap improves melt curtain stability but may increase surface haze if quench is too abrupt. Chill roll surface temperature is set between 15 °C and 30 °C. Higher quench rates improve optics but can increase internal stress and splitty tear behaviour. Edge pinning is required, and edge trim is recycled in-line. Recycled edge trim addition should be limited to approximately 15–20% unless converter-run data demonstrate acceptable gel levels and colour drift.
For gauges below 25 µm, draw resonance can appear as cyclic machine-direction thickness variation. Mitigation includes reducing the air gap, increasing melt temperature, raising chill roll temperature toward 25–30 °C, or reducing line speed. Because SLL118/21 has a melt flow rate of 1.0 g/10 min, cast film extruders should verify drive torque and die pressure before sustained high-speed operation. A barrier screw with 25:1 L/D can process the grade, but torque will be higher than with a 2.5 g/10 min cast film resin. Die lip heater zones should be balanced to avoid cold-edge bands that cause thickness variation and subsequent wound roll deformation.
Applications for SLL118/21 are established in industrial liners, heavy-duty sacks, non-food packaging films, and laminating webs where blown or cast films require toughness and drawability. Dart drop impact and Elmendorf tear should be measured according to ASTM D1709 and ASTM D1922; for heavy-duty sacks at 40–80 µm, gauge uniformity frequently controls impact performance more than the base polymer. For outdoor agricultural film, the neat resin requires a separate UV stabiliser masterbatch because the base stabiliser package is not designed for prolonged weathering. In lamination films, surface treatment is required before adhesive application; a minimum wetting tension of 38–42 mN/m measured according to ASTM D2578 or ISO 8296 is a typical control point after corona treatment. The product is not supplied as a controlled sealant resin; seal initiation temperature and hot tack must be measured under ASTM F1921 and ASTM F2029 if the grade is placed in a sealant layer. Food-contact status for the final article must be verified by the converter under FDA 21 CFR 177.1520 or EU Regulation 10/2011; the base resin certificate alone does not establish compliance for all converted structures.
When SLL118/21 is substituted for a petroleum-derived linear low-density polyethylene of equivalent density and melt flow rate, the primary measurable distinction is renewable carbon fraction rather than polyethylene backbone structure. Density, melt flow rate, and extrusion behaviour remain within the same processing envelope, provided the additive package is equivalent. Converters replacing fossil LLDPE can retain the existing temperature profile, screw speed, die gap, and corona treatment settings, but should perform incoming raw material identification with ASTM D6866. Physical pellets and standard ASTM D1238 and ASTM D792 values may not distinguish renewable from fossil polyethylene.
Differences become more pronounced when SLL118/21 replaces high-pressure LDPE rather than fossil LLDPE. Autoclave LDPE has branched long-chain architecture and higher melt strength, allowing blow-up ratios above 3.0:1. SLL118/21 will show lower bubble stability at those ratios and should be run at 2.0:1 to 2.5:1. In cast film, the linear structure yields narrower thickness variability after quenching, but die lip adjustment requires tighter control to maintain edge flatness. Compared with high-MFR cast film grades, the 1.0 g/10 min melt flow rate creates higher die pressure; the compensation is higher die temperature rather than excessive screw speed. If slip or antiblock additives are introduced by masterbatch, coefficient of friction should be re-qualified under ASTM D1894, and blocking force should be checked because additive response is lot-dependent and cannot be inferred from base resin data alone.
Incoming material controls for SLL118/21 should include melt flow rate, density, visual pellet inspection, and lot-specific renewable carbon documentation. Polyethylene is not hygroscopic in the manner of polyamide or polyester, but condensation on cold pellet surfaces can produce surface defects in film. If pellets are moved from unheated storage into a warm production hall at relative humidity above 60%, a hopper air sweep at 50 °C for 1 hour may be applied before extrusion. Material should be stored below 50 °C and protected from direct ultraviolet radiation. Shutdown with LLDPE requires purging with a lower-MFR LDPE or a designated purge compound before cooling to prevent oxidised polymer from solidifying in the die and screen pack. Purchase orders should specify density tolerance, melt flow rate tolerance, and renewable carbon certificate requirements so that incoming lots remain within the converter’s process capability window.