Braskem Green Pe Slh118 Blow Film Extrusion And Cast Film Extrusion Linear Low Density Polyethylene

Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 692371
    Grade SLH118
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Hexene
    Renewablesource Bio-based polyethylene from sugarcane ethanol
    Density 0.918 g/cm³
    Meltflowrate 190c 2 16kg 1.0 g/10 min
    Meltingpoint 120 °C
    Vicatsofteningpoint 94 °C
    Tensilestrengthatbreak Md 30 MPa (typical)
    Tensilestrengthatbreak Td 25 MPa (typical)
    Elongationatbreak Md 600% (typical)
    Elongationatbreak Td 700% (typical)
    Dartimpactstrength 120 g (typical)
    Elmendorftearstrength Md 200 g (typical)
    Elmendorftearstrength Td 300 g (typical)
    Haze 12% (typical)
    Gloss 70 (typical)
    Coefficientoffriction 0.2 (typical)
    Processingmethods Blow Film Extrusion and Cast Film Extrusion

    As an accredited Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Green PE SLH118 supplied in 25 kg polyethylene bags; 55 bags (1,375 kg) per shrink-wrapped pallet.
    Container Loading (20′ FCL) 20′ FCL loading: Braskem Green PE SLH118 LLDPE in 25 kg bags, palletized, shrink-wrapped, moisture-protected, and secured for ocean transport.
    Shipping Braskem Green PE SLH118 is generally shipped as non-hazardous LLDPE resin pellets in 25 kg polyethylene bags or bulk sacks, palletized and stretch-wrapped. Transport in clean, dry trucks or containers at ambient temperature. Keep away from moisture, heat, sunlight, and strong oxidizers. Follow applicable local transport and safety regulations.
    Storage Store Braskem Green PE SLH118 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep bags or containers tightly closed to prevent contamination. Use clean handling equipment and avoid damaging packaging. Stack securely on pallets to prevent falls. Observe good housekeeping and follow the manufacturer’s safety data sheet and local regulations.
    Shelf Life Store in original packaging in a dry, ventilated area away from direct sunlight and heat; shelf life typically 12 months.
    Application of Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    For dry-food pouches and cereal liners, blown film lines running Braskem Green PE SLH118 operate with a die gap of 1.8–2.3 mm, a blow-up ratio of 2.2–3.0:1, and melt temperatures between 185°C and 210°C. Frost-line height is maintained at 6–8 die diameters when internal bubble cooling airflow is set to hold bubble diameter variation below ±5%. Under these conditions, the converter meters a food-contact slip/antiblock masterbatch into the main resin at 1.5–4.0 wt%, leaving 96.0–98.5 wt% SLH118 in the finished web. Closed-loop trim refeed up to 15 wt% can be used in non-food contact layers of a coextruded structure, but monolayer food packages built under 21 CFR §177.1520(c) must restrict post-consumer reclaim to 0 wt% unless the source polymer meets the same food-contact specification and migration data support its use. Compliance documentation for EU markets is framed by Commission Regulation (EU) No 10/2011, Annex I and Annex III, with an overall migration limit of 10 mg/dm² for simulants selected under the intended food type. Tensile and elongation data for quality release should be generated against ASTM D882 and ISO 527-3; seal initiation measurements are not a strength requirement for dry fill but are relevant for vertical form-fill-seal operations. Static and kinetic coefficients of friction are measured under ASTM D1894; packaging lines running above 80 bags/min require kinetic COF below 0.30 to avoid jaw drag. Because SLH118 is produced from renewable ethylene, converters may verify the bio-based carbon fraction using ASTM D6866 Method B; the exact fraction is grade-specific and should be taken from the supplier’s technical documentation rather than inferred from fossil LLDPE databases. Terminal articles produced under this configuration include dry-cereal liners, sugar and salt pouches, bakery overwrap, candy twist wrap base film, and dry soup sachets.

    What Restricts Cast Film Line Speed in Pallet Stretch Wrap from SLH118?

    To suppress draw resonance and edge instability in pallet stretch film, a three-layer A/B/A construction places SLH118 in the core layer at 70–85 wt% of the total structure. The skin layers are metered with cling masterbatch at 0.8–1.5 wt% on the unwind side and slip/release additive at 0.5–1.2 wt% on the opposite skin; the core may contain 5–15 wt% of a lower-density LLDPE or ULDPE grade to suppress draw resonance. The constraint on line speed is not the extruder capacity but the onset of edge instability driven by insufficient melt strength at high draw ratios, typically above 220 m/min when the air gap is 100–150 mm and the chill-roll temperature is 18–24°C. Published data for the exact critical draw ratio of SLH118 in production-scale cast lines is limited; the operational boundary is identified in real time by a rise in film thickness variation above ±3% across the gauge scanner. Melt temperature at the die is held at 220–260°C, and the flex lip gap is set to 0.5–0.8 mm. Before extrusion, incoming resin is released against ISO 1133-1:2022 at 190°C and 2.16 kg; batch-to-batch variation larger than ±0.2 g/10 min requires adjustment of barrel zone 2 and die temperature to keep edge encapsulation stable. Compliance testing for pallet stretch films does not require food-contact clearance unless the article is used in secondary packaging with indirect food contact; in that case Commission Regulation (EU) No 10/2011 may apply to the outer surface. Mechanical release criteria typically reference ASTM D5459 for elastic recovery and stress retention, ASTM D5748 for puncture resistance, and ASTM D882 for tensile strength. Terminal products include machine-grade stretch wrap for automatic pallet wrappers, hand-held stretch rolls, and thin-gauge logistics bundling film.

    Cling development is evaluated by ASTM D5458 for peel cling, and the target unwind force is often specified at 1.5–3.0 N per 50 mm width. The core layer of SLH118 must not contain slip masterbatch above 2.0 wt% because surface slip can suppress the necessary unwind force. During pre-stretching above 200%, film must be free of gel particles larger than 200 µm; gel contamination causes pinholes and breaks on automated pallet wrappers. Filter screens at the extrusion breaker plate are specified at 80–120 mesh for the core layer.

    Gas Transmission in Silage Film Is Controlled by Carbon Black Loading and Freeze-Line Height

    During silage film conversion of SLH118, simultaneous control of oxygen transmission and photothermal stability is required; the resin contributes low-temperature flexibility but is not converted into agricultural film without stabilizer loading. The addition ratio for a typical monolayer silage film is 94–96 wt% SLH118, 3–5 wt% carbon black masterbatch, and 1–2 wt% HALS/UV stabilizer masterbatch; for bale wrap, a white or black masterbatch may be used at 4–6 wt% depending on surface reflectivity requirements. Blown film processing uses a die gap of 2.0–2.5 mm and a BUR of 2.5–3.0:1 to produce a final gauge of 25–50 µm for silage bale wrap and 50–150 µm for silo bag liners. Bubble stability is maintained with high-stalk extrusion when the frost-line height is set at 8–10 die diameters; that configuration raises MD/CD tear balance and is less sensitive to ambient air drafts. The relevant product standard is EN 13206, while weathering retention is evaluated according to ISO 4892-2 with tensile retention measured after xenon arc exposure. Terminal articles include silage bale wrap, silo bag liners, greenhouse cover film, mulch film for row-crop vegetable production, and temporary grain storage covers.

    Secondary multipack overwrap fabricated from a blend of 65–80 wt% SLH118 and 20–35 wt% high-pressure LDPE is blown at a BUR of 1.8–2.2:1 to a gauge of 45–70 µm; free shrink is verified under ASTM D2732 at 120°C, the shrink tunnel is operated at 140–160°C, and the resulting wrap is used for bottled water multipacks, carbonated soft drink bundles, and canned goods overwrap.

    Fold-Crease Tear Resistance in Filled Sack Liners

    At filled weights above 20 kg, heavy-duty sack films from SLH118 are run at a die gap of 2.2–2.6 mm, a BUR of 2.0–2.5:1, and melt temperature of 195–215°C to generate films from 100–200 µm. The formulation for export sacks and FIBC liners is 96–98 wt% SLH118, 1.5–3.0 wt% carbon black masterbatch, and 0.5–1.0 wt% antioxidant/processing aid masterbatch; no post-industrial reclaim is added in primary liners for hygroscopic granular chemicals. If reclaim is used, it is restricted to the outer non-contact layer of a coextruded structure and must not reduce tear resistance below the release limit. Mechanical compliance uses ISO 6383-2 for Elmendorf tear, ASTM D1709 for falling dart impact, and ISO 527-3 for tensile. The fold-crease failure mode is the main release barrier; filled liners folded before insertion show lower tear resistance when conditioned at −10°C than at 23°C, which is why the minimum gauge is set at 100 µm for granular chemical sacks. For non-hazardous granular fill, the relevant article standard is ISO 21898 for FIBCs and their liners. Terminal articles include heavy-duty shipping sacks for granular chemicals, FIBC liners, construction aggregate sacks, and resin export bags.

    When Frozen Storage Touches −25°C, Dart Impact and Seal Initiation Take Priority

    Flexible packaging for frozen vegetables and ice cream requires the film to retain falling dart impact under ASTM D1709 after conditioning at −25°C, a condition in which the change in low-strain modulus induces brittle puncture in non-toughened polyolefins. SLH118 is used at 93–97 wt% in a formulated web with 1–2 wt% slip masterbatch and 1–2 wt% antiblock masterbatch; in a coextruded structure the seal layer may be a lower-melt-initiation ethylene copolymer while SLH118 forms the external abuse layer at 60–80 wt% of the structure. The film is processed on a blown line with a die gap of 1.8–2.2 mm, a BUR of 2.2–2.8:1, and melt temperature of 190–205°C, yielding a gauge of 40–70 µm. Seal initiation is measured on a laboratory heat sealer with 0.5 N/mm² jaw pressure and 0.5 s dwell, using ASTM F88/F88M; converters commonly release frozen food webs only when seal strength is no lower than 4 N/15 mm. Food-contact compliance is established under 21 CFR §177.1520(c) and Commission Regulation (EU) No 10/2011, with overall migration testing according to Annex III and Annex V time-temperature combinations selected for frozen food. Terminal article types are printed frozen vegetable bags, ice cream pouches and sleeves, frozen seafood liners, and shrink-seal overlap film for frozen poultry cartons.

    Free Quote

    Competitive Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem Green PE SLH118 is a linear low-density polyethylene grade derived from sugarcane ethanol and supplied for blown film extrusion and cast film extrusion. The grade is identified by a nominal density of 0.918 g/cm³ and a melt flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238. Renewable carbon content is batch-verified by ASTM D6866; typical certificates report renewable carbon fractions above 80% depending on additive package and feedstock allocation. The resin is used in monolayer and coextruded flexible film structures where an LLDPE toughness envelope, seal response, and renewable-carbon claim are required in the same material. Compared with conventional fossil LLDPE of similar density and melt flow rate, SLH118 is positioned as a drop-in bio-based alternative, but converter trials are required to confirm backpressure, bubble stability, and seal plateau shifts on a specific film line.

    What rheological and density specifications define the SLH118 grade boundary?

    The resin is specified by density and melt flow rate as primary lot-release parameters. Density is measured on compression-moulded plaques according to ASTM D792 or ISO 1183-1:2019; the grade normally falls within 0.916 g/cm³ to 0.920 g/cm³. Melt flow rate is determined under 190 °C/2.16 kg conditions using ASTM D1238 procedure A or technically equivalent ISO 1133-1:2022 procedure B. The nominal value is 1.0 g/10 min, with a typical commercial control window of approximately ±0.2 g/10 min. Melt flow rate below 0.8 g/10 min increases extruder backpressure and may reduce output on shallow-channel cast-film screws, while values above 1.2 g/10 min reduce bubble mechanical stability and lower dart impact in blown film. Renewable carbon fraction is assessed by accelerator mass spectrometry according to ASTM D6866 Method B. Batch certificates commonly report values between 80% and 96%; the exact value varies with the bio-ethylene allocation, catalyst residues, and the presence of mineral-based processing additives.

    PropertyTest methodTypical value or range
    DensityASTM D7920.916–0.920 g/cm³
    Melt flow rateASTM D1238, 190 °C/2.16 kg1.0 ± 0.2 g/10 min
    Renewable carbon contentASTM D6866 Method B80–96%
    Dart impact, 25 µm blown filmASTM D1709A60–120 g
    Elmendorf tear, transverse directionASTM D1922250–400 g
    Haze, 40 µm blown filmASTM D10038–16%

    The values in the table are manufacturer-published typical data and are not batch release limits. Film mechanical properties shift with gauge, blow-up ratio, frost-line height, and additive package; converter-specific testing under ASTM D882 for tensile properties and ASTM D1894 for coefficient of friction is required to establish control limits for a given film structure.

    Blown-film die gap, frost line, and bubble stability thresholds

    On blown-film lines, bubble stability is the principal processing constraint. Converters operating smooth-bore or grooved-feed extruders with 24:1 to 30:1 L/D and barrier screws report stable bubble geometry at melt temperatures from 190 °C to 220 °C. Die gaps of 1.5 mm to 2.5 mm are used for SLH118; narrower gaps reduce melt-fracture onset but increase shear heating and may limit output. The recommended blow-up ratio is 2.0:1 to 3.0:1. Below 2.0:1, film flatness improves but tear balance shifts toward the machine direction; above 3.0:1, edge tension rises and frost-line movement becomes sensitive to ambient air fluctuations. Frost-line height should be maintained within ±5 °C of the set melt temperature using chilled air-ring stabilisation. A fluctuating frost line above 8 die diameters generally indicates insufficient cooling capacity or excessive haul-off speed. On a 45 mm grooved-feed extruder, maximum output is frequently limited by bubble pressure rather than resin feed; specific output may reach approximately 0.5 kg/h per mm die circumference in monolayer configurations, but published data for this specific configuration is limited at high ambient humidity above 60% RH.

    Surface melt fracture appears as sharkskin at the die exit when die exit shear stress exceeds roughly 0.14 MPa. The standard corrective sequence is to lower output, increase die gap, or raise die lip temperature within the 200–220 °C range. Sustained melt temperatures above 230 °C accelerate oxidation and raise carbonyl index; this degradation mechanism reduces heat-seal strength and increases gel count. Free-radical peroxide masterbatches should not be dry-blended without rheology validation, because long-chain branching can increase melt tension and destabilise bubble geometry. Slip and antiblock masterbatches are typically used at 1–3 wt%; above 3 wt%, haze increases sharply and coefficient of friction may fall below 0.15, raising the risk of roll telescoping in subsequent conversion.

    Cast film processing of SLH118 uses a different set of operating limits. The die gap is typically 0.3 mm to 0.5 mm, and melt temperature is held at 200 °C to 230 °C to avoid draw resonance. Chill roll temperatures between 15 °C and 30 °C are used to control film density, clarity, and blocking; lower chill roll temperatures increase film clarity but raise condensation risk above 60% RH. Neck-in and edge trim are controlled by die-to-roll distance, air knife pressure, and electrostatic pinning. Because the resin has an MFR of 1.0 g/10 min, its drawdown is lower than cast-film grades with MFR values near 2.7 g/10 min. Line speeds above 120 m/min may require a wider die gap and higher melt temperature; published data for SLH118 cast film above 150 m/min is limited. Surface additives should be introduced via pre-compounded masterbatch rather than direct dry blending to avoid agglomerates that form gel defects and lens distortion in thin cast webs.

    When film optics and seal response separate SLH118 from conventional LLDPE

    SLH118 differs from low-density polyethylene, conventional fossil LLDPE, and high-density polyethylene in measurable processing and property terms. First, the linear backbone with short-chain branching provides higher tensile strength and dart impact than LDPE of equivalent melt index, but lower melt strength and higher neck-in on cast-film lines. The optical haze of a 40 µm blown film may be 1.5 to 2 times higher than an LDPE-rich blend when measured by ASTM D1003, because the linear-low molecular architecture produces larger surface roughness and higher crystallinity than a branched LDPE control. Second, compared with fossil LLDPE grades of equivalent density and melt flow rate, the bio-based origin does not create a separate mechanical property class; however, lot-to-lot rheology can show a wider band because of bio-ethylene feedstock variability and catalyst response. Third, compared with high-density polyethylene grades above 0.940 g/cm³, SLH118 has lower flexural modulus measured by ASTM D790 and lower Vicat softening point measured by ASTM D1525; it is therefore selected for flexible film rather than rigid packaging or blow moulding.

    Seal initiation temperature on co-extruded films is measured by ASTM F1921; typical values for SLH118 fall in the 100–110 °C range but vary with sealing pressure, dwell time, and total film gauge. Heat-seal plateau strength should be confirmed under ASTM F88 across the desired sealing range. In coextruded structures where SLH118 is used as a core layer beneath an ethylene vinyl acetate or polyolefin plastomer sealant layer, the presence of renewable LLDPE can shift the observed seal plateau by 2–5 °C relative to fossil LLDPE controls. This shift is not necessarily a failure, but it must be captured in packaging line validation and seal window documentation.

    Compliance documentation is required before substitution in food-contact films

    Food-contact use is not established by resin grade alone. Converters must verify the final film under the applicable regulatory framework, such as 21 CFR 177.1520 for olefin polymers in the United States or Commission Regulation (EU) No 10/2011 Annex I for plastic materials intended to contact food. Braskem Green PE grades are generally supported by migration and organoleptic data, but the additive package, conversion residues, and coextruded layer composition in the finished article must be assessed for the complete film. For biobased claims, renewable carbon measurement follows ASTM D6866. For supply-chain verification of bio-ethylene mass balance, converters may request ISCC PLUS certification. Specific migration limits for slip agents, antioxidants, and processing aids should be confirmed with the supplier, because additive levels in one film structure do not automatically transfer to a different multilayer construction.

    RequirementReference standard or certification
    US olefin polymer food-contact compliance21 CFR 177.1520
    EU plastic food-contact complianceEU 10/2011 Annex I
    Biobased carbon measurementASTM D6866 Method B
    Melt flow rate testASTM D1238 / ISO 1133-1:2022
    Density measurementASTM D792 / ISO 1183-1:2019
    Film tensile propertiesASTM D882
    Dart impact testASTM D1709A
    Elmendorf tear testASTM D1922
    Seal initiation and heat-seal strengthASTM F1921 / ASTM F88
    Mass-balance supply-chain verificationISCC PLUS

    Closed-container storage below 40 °C is recommended. Surface condensation is the relevant moisture-related failure mode when cold pellets are transferred into a warm high-humidity area above 60% RH; dry-air purging for 2–4 h at 50–60 °C can remove surface moisture before extrusion. Direct blending with peroxide masterbatch is an incompatibility because free-radical modification can raise long-chain branching, reduce drawdown, and destabilise bubble geometry. In cast and blown film operations, film defect counts should be monitored with laser scanning systems; gels larger than 500 µm in 40 µm film are cause for line intervention because they compromise seal integrity and optical quality in packaging-grade webs.

    Top