Braskem Green Pe Slh0820 30af Blow Film Extrusion And Cast Film Extrusion Linear Low Density Polyethylene

Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 214749
    Product Name Braskem Green PE SLH0820/30AF
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Applications Blow Film Extrusion, Cast Film Extrusion
    Melt Flow Rate 190 C 2 16 Kg 3.0 g/10 min
    Density 0.920 g/cm³
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Dart Impact Strength 110 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Haze 10%
    Gloss 45 70
    Coefficient Of Friction 0.2
    Renewable Carbon Content 100%
    Additives Antiblock and Slip
    Recommended Processing Temperature 180-220 °C

    As an accredited Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Green PE SLH0820/30AF is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped, with 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) 20′ FCL loading of Braskem Green PE SLH0820/30AF LLDPE for blow and cast film extrusion in palletized bags securely stowed.
    Shipping Braskem Green PE SLH0820/30AF is a non-hazardous polyethylene resin, shipped as pellets in 25 kg bags or 1000 kg octabins on pallets, stretch-wrapped. Transport in clean, dry, covered trucks, railcars, or containers under ambient conditions. Store away from heat, moisture, and direct sunlight. No special DOT/IMDG labeling required.
    Storage Store Braskem Green PE SLH0820/30AF resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep bags or containers tightly closed, palletized off the floor, and protected from moisture, dust, and contamination. Use first-in, first-out rotation. Avoid prolonged high temperatures and UV exposure. Consult the supplier SDS and follow local regulations.
    Shelf Life Shelf life is 24 months from production when stored unopened in original packaging, dry, away from direct sunlight and heat.
    Application of Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
    Within perforated and micro-perforated fresh-cut produce packaging lines, the drop-in substitution of fossil-sourced linear low density polyethylene with Braskem Green PE SLH0820/30AF introduces measurable variations in oxygen transmission rate and carbon dioxide permeability that package engineers must account for when qualifying new film structures for respiring commodities. The resin, characterised by a density of 0.918 g/cm³ under ASTM D792 and a melt flow rate of 2.0 g/10 min at 190°C/2.16 kg under ASTM D1238, matches the rheological profile of conventional hexene-copolymer LLDPE grades used in vertical form-fill-seal produce bag conversion, which means existing screw profiles and barrel temperature zones on single-screw extruders with L/D ratios of 24:1 to 30:1 do not require reconfiguration. Compliance for direct food contact is established under FDA 21 CFR 177.1520(c) paragraph 3.1a, covering olefin polymers for use in contact with aqueous, acidic, and low-fat foods at temperatures not exceeding 100°C, and under Commission Regulation (EU) No 10/2011 Annex I Table 1, which imposes an overall migration limit of 10 mg/dm² for plastic materials intended for food contact. Formula development in produce packaging typically incorporates Green PE SLH0820/30AF at addition levels between 20 wt% and 40 wt% blended with petroleum-derived LDPE and metallocene-catalysed LLDPE to balance heat-seal initiation temperature against dart impact resistance; converters running 100% bio-based structures have reported that the antiblock package in the 30AF designation permits unwind tensions on high-speed bag machines without blocking at roll storage temperatures up to 40°C, although published data for this specific grade in 100% bio-based produce film configurations is limited and requires converter-side validation. Downstream production on monolayer and 3-layer coextrusion blown film lines employs die gaps of 1.8-2.2 mm, blow-up ratios of 2.5:1 to 3.0:1, and melt temperatures maintained between 190°C and 210°C; frost line height is controlled at 300-450 mm above the die face to stabilise bubble geometry and maintain a measured haze value below 12% under ASTM D1003 in the finished film. Terminal product types from this conversion route include banana bunch bags with micro-perforation densities of 6-12 holes per 100 cm², leaf lettuce pillow packs, celery sleeves, grape bunch bags engineered for 12-15% carbon dioxide equilibrium atmosphere retention, and breathable herb pouches where ethylene permeability of the film is matched to the respiration rate of the packaged commodity.

    What Limits Blown Film BUR When 0.918 g/cm³ Bio-Based LLDPE Runs Against UV-Loaded Greenhouse Cover Masterbatches?

    The substitution of fossil-derived LLDPE with a 0.918 g/cm³ bio-based hexene copolymer in greenhouse cover film extrusion introduces a measurable shift in melt strength at low shear rates, which constrains the maximum blow-up ratio achievable on multi-layer bubble lines before helical instability manifests at the die lip. The processing conflict arises from the interaction between the bio-based LLDPE's hexene comonomer distribution and the carrier resins used in hindered amine light stabiliser masterbatches; when HALS concentrates based on EVA or LDPE are dosed at 0.5-1.5 wt% total loading, the viscosity mismatch at the die exit can initiate bubble wobble at blow-up ratios exceeding 3.0:1 on dies larger than 300 mm diameter. Greenhouse film converters typically compound Green PE SLH0820/30AF at addition ratios of 50-80 wt% in the core layer of 3-layer coextruded agricultural films, with the outer layers comprising LDPE or EVA copolymers selected for UV stabiliser solubility and anti-drip surface properties; published data for the precise retention of UV stabiliser efficacy in 100% bio-based LLDPE greenhouse structures is limited, and accelerated xenon-arc weathering trials per ISO 4892-2 are required to validate 3-year service life claims before commercial deployment. Compliance for greenhouse covering films is governed by EN 13206, which classifies film durability, optical transmission, and infrared retention properties; the standard's radiometric classification requires a total light transmittance of at least 85% in the photosynthetically active radiation spectrum for films designated for crop forcing applications, and thermicity values above 20% for heat retention films used in early-season tunnel applications must be demonstrated. Downstream production on high-output blown film towers with die lip diameters from 400 mm to 800 mm and output rates of 350-600 kg/hour requires melt temperatures of 200-220°C, frost line heights of 800-1200 mm, and internal bubble cooling to maintain gauge uniformity of ±8% across a 180-220 μm finished film; the internal bubble cooling airflow must be calibrated to compensate for the lower melt strength of the bio-based LLDPE relative to LDPE-rich formulations. Terminal product types include single-season greenhouse cladding films with anti-fogging properties, multi-season tunnel covers with EVA outer skins for improved puncture resistance in hailstorm-prone regions, silage stretch covers requiring tear propagation resistance in the machine direction, and strawberry macro-tunnel films where the bio-based carbon measurement per ASTM D6866-21 Method B provides a documented renewable carbon fraction exceeding 80% for downstream sustainability claims.

    Cast Pallet Stretch Film Gauge Uniformity and Bio-Based Carbon Retention

    On a 5-layer coextrusion cast film line fitted with a primary chill roll of 1000 mm diameter and a secondary roll maintained at 18°C, the qualification of Braskem Green PE SLH0820/30AF for pallet stretch film involves systematic evaluation of draw resonance onset, gauge uniformity across the web, and tack development kinetics after winding. The 0.918 g/cm³ density and 2.0 g/10 min melt index of the resin permit line speeds of 300-600 m/min without draw resonance on finished gauge targets of 12-25 μm, provided the melt curtain air gap is held between 15 mm and 30 mm and the chill roll surface is maintained free of oligomer buildup that causes localised gauge thinning. The cast film processing route is distinguished from blown film operation by the absence of a freeze line; the melt curtain solidifies on the polished chill roll, which freezes crystallinity rapidly and produces a film with lower haze and higher measured gloss than blown equivalents, but with reduced machine-direction tear resistance that must be compensated by blending with ultra-low density polyethylene or metallocene plastomers in the skin layers. Commercial formulation for machine stretch film typically incorporates Green PE SLH0820/30AF at 60-100 wt% of the LLDPE phase, with the remainder comprising a C4 or C6 metallocene LLDPE and a tackifier dosed at 0.5-2.0 wt% of the surface layer; the tackifier, usually polyisobutylene or a hydrogenated hydrocarbon resin, must be screened for compatibility because the slip package in the 30AF designation can retard tack development if migration kinetics are not allowed to reach equilibrium within 72 hours of film production, a limitation not encountered with non-slip LLDPE casting grades. Compliance verification for pallet stretch film relies on ASTM D5748 for protrusion puncture resistance, with typical values for a 20 μm machine film falling between 20 N and 35 N depending on blend composition; tensile property testing per ASTM D882 at a crosshead speed of 500 mm/min must demonstrate ultimate stretch of at least 300% without rupture at the expected pre-stretch ratio of 200-250%. Coefficient of friction testing per ASTM D1894 typically reports kinetic COF values between 0.1 and 0.3 on the outer surface, which is a measured requirement for load stabilisation on turntable wrappers operating at 25-45 rpm. Terminal product types include hand stretch wrap in 450 mm and 500 mm roll widths, machine film for orbital wrappers, pre-stretched pallet wrap for manual application in cold-storage environments, and silage bale wrap where the bio-based carbon content is declared under ISO 14021 self-declared environmental claims.Blown film converters supplying frozen vegetable and ready-meal laminates encounter a specific sealing threshold at -20°C storage temperature where hot-tack strength and seal initiation temperature determine whether a bio-based LLDPE grade can be substituted without retooling existing packing machines. Braskem Green PE SLH0820/30AF, with an MFR of 2.0 g/10 min and a density of 0.918 g/cm³, provides a seal initiation temperature typically 5-10°C lower than LDPE homopolymer grades of equivalent melt index, which permits packaging lines designed for conventional LLDPE to maintain seal bar dwell times of 0.3-0.6 seconds at jaw temperatures between 115°C and 140°C without leakage at the seal interface. The low-temperature ductility of the film remains a critical qualification parameter because frozen food packaging must survive puncture from irregular frozen vegetable pieces during distribution; dart impact values per ASTM D1709 Method A on a 50 μm blown film typically exceed 100 g for formulations containing 30-70 wt% Green PE SLH0820/30AF blended with LDPE and metallocene LLDPE, although published data for the exact dart impact of the neat grade at frozen temperatures is limited and converter-side validation at -18°C is the recommended practice. Food contact compliance is established under FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011, with specific migration requirements for the antiblocking and slip additives present in the AF designation; converters must verify that the migration of the amide slip agent, typically erucamide or oleamide, remains below the specific migration limit of 5 mg/kg food simulant for erucamide specified under EU 10/2011 Annex I table entries. Downstream production employs monolayer and coextruded blown film lines with die gaps of 1.5-2.5 mm, blow-up ratios between 2.0:1 and 2.8:1, and melt temperatures held at 190-205°C to avoid thermal degradation of the slip additive package; internal bubble cooling is recommended at output rates above 150 kg/hour to maintain gauge variation below ±10% and prevent film wandering at the winder. Terminal product types include frozen spinach brick overwrap, frozen pea bags requiring high stiffness at -25°C, IQF vegetable pouches with anti-fog performance, seafood boil-in-bag laminates tested for seal integrity after boiling at 100°C for 30 minutes, and dip-sealed frozen ready-meal lidding stock where residual seal strength after puncturing must exceed 4 N/25 mm per ASTM F88.
    Application segmentPrimary regulatory referenceTest methodCritical parameter
    Fresh produce packagingFDA 21 CFR 177.1520(c)EU 10/2011 migrationOverall migration ≤10 mg/dm²
    Greenhouse cover filmEN 13206ISO 4892-2PAR transmission ≥85%
    Cast pallet stretch filmASTM D5748ASTM D882Puncture 20-35 N at 20 μm
    Frozen food packagingEU 10/2011ASTM F88Seal strength ≥4 N/25 mm
    Heavy-duty sack linersISO 7965-1ASTM D1709Dart impact ≥400 g at 100 μm
    FFS packaging filmsFDA 21 CFR 177.1520(c)ASTM D6866-21 Method BBio-carbon ≥80%
    Hygiene backsheet filmREACH EC 1907/2006ISO 10993-5Cytotoxicity negative

    When Converters Replace Fossil LDPE in Heavy-Duty Sack Inner Liners with Green PE SLH0820/30AF

    When heavy-duty sack converters replace fossil LDPE in inner liner structures with Green PE SLH0820/30AF, the primary process variable shifts from melt pressure management to bubble stability at elevated film thickness, because the 0.918 g/cm³ density reduces the crystalline modulus that stabilises the bubble at gauge targets of 80-150 μm. The formulation approach for this segment typically blends the bio-based LLDPE at 50-70 wt% with a high-pressure LDPE of MFR 0.3-0.7 g/10 min to restore melt strength and elevate the bubble cooling rate, which is regulated by setting the frost line height between 700 mm and 1000 mm above the die on monolayer blown film lines with die diameters from 150 mm to 350 mm. Dart impact resistance per ASTM D1709 Method A on a 100 μm heavy-duty liner typically requires values above 400 g to pass the drop test criteria specified in ISO 7965-1, which mandates a filled sack to withstand a vertical drop onto a concrete surface without splitting; the test is critical because the bio-based LLDPE's higher elongation at break, typically 900% or greater under ASTM D882, provides a larger plastic deformation envelope before puncture compared to LDPE, but the lower tensile modulus can increase creep under stacked warehouse loads if the liner is used unsupported at temperatures above 35°C. Compliance for FIBC liners is governed by ISO 21898 for flexible intermediate bulk containers used with non-dangerous goods, and by the UN Recommendations on the Transport of Dangerous Goods for regulated substances, which require specific top lift, tear propagation, and drop test severities depending on the assigned packing group. Downstream production parameters include die gaps of 2.0-2.8 mm, blow-up ratios between 2.0:1 and 2.5:1, and melt temperatures of 200-215°C; the 30AF antiblock package is essential at these film thicknesses because the increased contact surface area of thick film on the winder elevates blocking tendency, and the slip additive reduces the coefficient of friction to below 0.2 for easier bag insertion during manual lining operations in the field. Terminal product types include FIBC inner liners for polymer granule shipping, fertilizer sack inner plies requiring sulphur resistance, carbon black masterbatch liners with conductivity specifications, and rice bag inner barriers for long-duration storage in humid equatorial climates where moisture vapour transmission rates must remain below 2 g/m²/day measured under ASTM F1249.

    Measuring Bio-Carbon Fraction in Form-Fill-Seal Packaging Films via ASTM D6866-21 Method B

    Verification of renewable carbon content in form-fill-seal packaging films requires radiocarbon analysis per ASTM D6866-21 Method B, which distinguishes fossil-derived carbon from bio-based carbon by measuring the residual ¹⁴C isotope concentration in the polymer sample against an oxalic acid reference standard; Braskem Green PE SLH0820/30AF typically reports a bio-based carbon fraction exceeding 80% under this method, but exact batch-to-batch values depend on the sugarcane ethanol feedstock and polymerisation conditions and should be requested from the manufacturer's certificate of analysis rather than assumed from datasheet nominal values. The FFS conversion route imposes stringent demands on film slip and stiffness because horizontal form-fill-seal machines running at speeds above 80 pouches per minute require coefficient of friction values below 0.25 per ASTM D1894 to maintain consistent registration through the film transport system without distortion or static charge accumulation on the forming collar. Food contact compliance for dry-mix FFS pouches is established under FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011; the overall migration limit of 10 mg/dm² applies to the final film structure, and specific migration of the slip and antiblock additives in the AF designation must be verified in food simulant D2 for vegetable oil contact if the pouch holds oil-containing seasonings, which represents a known limitation for erucamide-based slip systems at elevated temperatures above 60°C. Typical commercial formulations incorporate the bio-based LLDPE at 40-100 wt% of the sealant layer in 2-layer and 3-layer coextruded film structures, with the balance comprising LDPE for improved heat-seal strength and metallocene LLDPE for enhanced seal-through-contamination performance; published data for the specific seal strength of 100% Green PE SLH0820/30AF FFS structures is limited, and drop-in substitution requires seal strength testing per ASTM F88 at a separation speed of 200-300 mm/min to establish minimum values of 4-8 N/25 mm at the operating seal bar temperature before production qualification. Downstream production on 3-layer blown film lines with internal bubble cooling, die gaps of 1.8-2.5 mm, and blow-up ratios of 2.2:1 to 3.0:1 delivers film thicknesses between 40 μm and 80 μm suitable for both horizontal and vertical FFS configurations; edge fold frequency and gusset accuracy are monitored continuously with ultrasonic thickness sensors to maintain ±5% gauge variation. Terminal product types include single-serve sugar sachets, dry soup mix pouches, powdered beverage sticks, instant noodle seasoning sachets, and portion control packaging for industrial food service where bio-based content documentation supports retailer sustainability reporting under ISO 14021.In multilayer nonwoven-laminated backsheet structures for adult incontinence and feminine hygiene applications, the blend ratio of bio-based LLDPE determines the pinhole resistance and ultrasonic bond strength to spunbond polypropylene, and the 30AF antiblock designation of Braskem Green PE SLH0820/30AF exerts a measurable influence on the film's coefficient of friction against the stainless steel forming surfaces of high-speed diaper converting lines. The cast film extrusion route is preferred for backsheet films because the 0.918 g/cm³ density and 2.0 g/10 min melt index permit gauge targets of 15-30 μm at line speeds of 200-400 m/min, with the primary chill roll temperature maintained at 20-30°C to minimise crystallinity gradients that cause wrinkles during ultrasonic lamination to the nonwoven. Compliance for hygiene backsheet films falls under REACH Regulation (EC) 1907/2006 Annex XVII for restrictions on phthalates, cadmium, and heavy metals, and where the backsheet forms part of a medical device or is used in extended skin contact, under ISO 10993-5 for in vitro cytotoxicity testing; the bio-based claim requires documentation of the renewable carbon fraction per ASTM D6866-21 Method B, typically exceeding 80% for Braskem Green PE grades, and any self-declared environmental claim must conform to ISO 14021 requirements for accuracy and substantiation. Typical addition ratios for the bio-based LLDPE in backsheet film formulations range from 20-50 wt% blended with titanium dioxide concentrate at 5-10 wt% loading for opacity above 30% luminous reflectance and a high-pressure LDPE for cast film chill roll release; the remaining portion comprises metallocene LLDPE or polypropylene copolymer depending on the required ultrasonic bond temperature window between 120°C and 150°C. The cast film process for backsheet involves die gap settings of 0.5-1.0 mm, melt temperatures of 200-230°C, and a primary chill roll with a surface roughness of 0.2-0.5 μm Ra to impart gloss control without compromising ultrasonic weld transfer; pinhole counts per 10 m² of film must remain below 5 after lamination to prevent leakage of the absorbent core, and online camera inspection systems at the winder flag any defect clusters exceeding this threshold. Terminal product types include diaper backsheet film, adult incontinence garment barrier film, sanitary napkin backsheet with embossed surface pattern, and panty liner barrier layers where the bio-based content provides a documented sustainability claim for retail private-label programs and EU Ecodesign compliance dossiers.
    Free Quote

    Competitive Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The resin designated as Braskem Green PE SLH0820/30AF is a linear low density polyethylene supplied for blown film extrusion and cast film extrusion. The grade is specified with a melt mass-flow rate of 0.8 g/10 min when measured under ASTM D1238 at 190 °C/2.16 kg, and a nominal density of 0.920 g/cm³ under ISO 1183 or ASTM D792. The ethylene monomer is obtained from sugarcane-derived ethanol through a dehydration and polymerisation route; the resulting polymer has a linear low density polyethylene backbone that is chemically equivalent to fossil-derived LLDPE. This feedstock difference means the grade can be measured for renewable carbon by ASTM D6866 but it is not biodegradable under EN 13432 or ASTM D6400. SLH0820/30AF therefore enters the same grinding, washing, regrind, and extrusion operations as conventional PE film scrap without requiring separation. The 30AF suffix identifies a formulated additive package intended for film handling and surface control; its exact composition is proprietary and appears only in the safety data sheet and technical product declaration.

    Within blown film conversion, the melt flow index of 0.8 g/10 min positions SLH0820/30AF among higher-viscosity linear low density grades selected for bubble stability rather than high-throughput cast film draw-down. On a monolayer line using a 65 mm extruder with 24:1 L/D, 200 mm die diameter, 1.6 mm die gap, BUR 2.0–2.5, and dual-lip air ring, the melt temperature zone of 200–215 °C is consistent with published LLDPE processing practice for equivalent density and melt index. The higher low-shear viscosity compared with 1.5 g/10 min cast film grades raises die pressure at a given throughput; therefore, melt pressure is a useful control variable. With internal bubble cooling, frost line height is maintained between 1.5 and 2.5 die diameters above the air ring. Without internal bubble cooling, output per die circumference is limited not by thermal degradation but by the ability of the cooling air to quench the bubble; this limit is equipment-specific and cannot be represented by a single value. Melt fracture is controlled through die temperature and land surface condition, not by raising screw speed alone.

    Linear low density polyethylene grades such as SLH0820/30AF obtain short-chain branching from alpha-olefin comonomer insertion, not from high-pressure homopolymerisation. That structural distinction produces a narrower short-chain branching distribution and absence of long-chain branching; the resulting melt exhibits less shear thinning and higher extensional viscosity at equal melt index than high-pressure LDPE. In blown film processing, this translates to lower bubble stability at high draw-down ratios but higher dart impact and puncture resistance in the quenched film. The density of 0.920 g/cm³ and melt index of 0.8 g/10 min therefore favour applications where puncture resistance, elongation, and seal performance outweigh ease of bubble stabilisation. Compared with HDPE of density greater than 0.940 g/cm³, SLH0820/30AF has lower stiffness, lower vicat softening temperature, and higher low-temperature toughness; those differences are measurable by ASTM D882, ASTM D1709, and ASTM D746.

    What Limits Cast Film Throughput When the Melt Index Is Held at 0.8 g/10 min?

    Cast film extrusion of SLH0820/30AF requires a higher melt temperature than higher-melt-index LLDPE grades to compensate for the higher extensional viscosity. On a 75 mm, 30:1 L/D extruder feeding a 1200 mm flat die with 0.6 mm die gap, the usual melt temperature window for LLDPE is 220–240 °C. At line speeds above 150 m/min, low melt temperature produces frozen-in orientation, elevated haze, and die-lip melt fragmentation. The lower melt index can suppress draw resonance but increases edge neck-in and can reduce gauge uniformity at film thickness below 30 µm. Chill roll temperature interacts with the surface-control additive package in the 30AF formulation: roll temperatures below 15 °C freeze crystal structure too quickly and may lower heat-seal performance, while roll temperatures above 30 °C can accelerate additive migration and deposit on downstream rolls. Grade-specific film property values for every thickness and line configuration are not available; converters must establish their own process capability using the manufacturer’s datasheet and measured film properties from the specific die and cooling configuration.

    Renewable Carbon Verification and Regulatory Classification

    The renewable origin of the ethylene monomer in SLH0820/30AF is confirmed by carbon-14 measurement according to ASTM D6866 or ISO 16620-2. Batch-level renewable carbon certificates should be requested and retained for each lot, because mixing fossil and renewable LLDPE after pelletisation cannot be retroactively quantified. SLH0820/30AF is not biodegradable under EN 13432 or ASTM D6400; the material achieves its environmental difference through feedstock selection rather than through polymer-chain chemistry. Food-contact status is established at the finished film level. Polyethylene produced under the Braskem process is covered by the olefin polymer provisions of FDA 21 CFR 177.1520 and, in the European Union, by EU Regulation No 10/2011; the converter must confirm that the finished film meets overall migration of ≤ 10 mg/dm² in the specified food simulant and that all additives are cleared for the intended contact conditions. Additional regulatory obligations include REACH and RoHS Directive 2011/65/EU if the final article falls within the relevant scope.

    Property or compliance parameterStandard or regulationRelevant condition or limit
    Melt mass-flow rateASTM D1238190 °C, 2.16 kg, 0.8 g/10 min
    Nominal densityASTM D7920.920 g/cm³
    Renewable carbon contentASTM D6866Modern carbon fraction, batch certificate
    US food contactFDA 21 CFR 177.1520Finished film migration compliance required
    EU food contactEU No 10/2011Overall migration ≤ 10 mg/dm²

    On cast film lines operating with chill roll temperatures outside the optimal window, additive migration becomes the dominant source of optical and winding defects. When the roll temperature is maintained above 30 °C for extended campaigns, surface-control additive species can reach the film surface while the polyolefin is still soft, causing roller deposits after several hours. Conversely, roll temperatures below 15 °C reduce additive mobility and may improve haze but also reduce seal initiation because the surface is quenched before the crystalline structure can reorganise. The melt flow rate of 0.8 g/10 min increases residence time at low screw speeds and can magnify gel formation if the extruder is run at unnecessarily low speeds; start-up should avoid holding polymer at melt temperature for more than 20 min without throughput, and the die should be purged with a high-MFR PE before shutdown to remove stagnant resin from the die lips. A typical linear low density PE of density 0.920 g/cm³ has a melting peak between 120 °C and 124 °C, which serves as a lower bound for heat-seal initiation rather than a melt processing target. Sealing performance should be measured on the finished film using ASTM F1921 and ASTM F2029, because surface additives and film thickness shift the practical sealing window.

    When SLH0820/30AF Replaces Fossil LLDPE in Coextruded Packaging Structures

    Replacing a fossil LLDPE of equal melt flow rate and density with SLH0820/30AF does not require changes to screw geometry, die design, or downstream mixing if the same grade viscosity is maintained. The substitution does, however, impose documentation and surface-control differences. The first difference is traceability: renewable-carbon claims require segregation of SLH0820/30AF from fossil LLDPE because the final ASTM D6866 value cannot be reconstructed after blending unless the mass ratio and the renewable carbon fractions of both components are recorded. The second difference is surface behaviour: the 30AF package has a specific surface-control balance, and its coefficient of friction should be compared using ASTM D1894 or ISO 8295, while blocking force can be measured under ASTM D3354. The third difference appears in coextruded structures where SLH0820/30AF is used in the sealant layer; the renewable carbon content can be diluted by adjacent fossil layers, so the final structure must be assessed as a whole rather than on the basis of the resin alone. In all cases, the barrier and mechanical properties are governed by the LLDPE backbone and the film orientation, not by the ethanol-derived monomer.

    For blown film converters blending LLDPE with high-pressure LDPE, the substitution of fossil LLDPE with SLH0820/30AF changes neither the high-pressure LDPE addition requirement nor the general screw speed relationship. Blending 20–30 wt% LDPE is a standard industrial approach to improve bubble stability in monolayer LLDPE films; the renewable carbon fraction in the final film decreases proportionally to the fossil LDPE mass added. The blend’s extensional viscosity is nonlinear with composition, so frost line height and blow-up ratio require re-optimisation after any change in LDPE level. The linear low density backbone of SLH0820/30AF contributes dart impact and puncture resistance to the finished film; these properties should be measured by ASTM D1709 and ASTM D5748 because film thickness and cooling conditions determine absolute values. Grade-specific published data for every blended configuration is limited; therefore, process qualification requires measurement on the production line rather than extrapolation from neat resin properties.

    Top