Braskem Fp33 Lldpe Blown Film Extrusion Polyethylene Copolymer

Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 156136
    Grade Braskem FP33
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.921 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Break Md 30 MPa
    Tensile Strength At Break Td 25 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Drop Impact F50 150 g
    Elmendorf Tear Strength Md 150 g
    Elmendorf Tear Strength Td 300 g
    Haze 12%
    Gloss 45 70
    Coefficient Of Friction 0.2

    As an accredited Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loading: Braskem FP33 LLDPE blown film extrusion polyethylene copolymer in 25 kg bags, palletized and stretch-wrapped; approx. 18–22 MT payload.
    Shipping Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer is shipped as non-hazardous resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep containers dry, closed, and away from heat, sunlight, and contamination. No special transport labels required; store in a cool, ventilated area.
    Storage Store Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or packaging sealed, clean, and elevated on pallets. Avoid moisture, dust, static buildup, and prolonged UV exposure. Maintain ambient temperature, avoid excessive stacking, and follow manufacturer/SDS guidance and local regulations.
    Shelf Life Shelf life: typically 12 months from production date if stored sealed in original packaging, dry, away from heat and sunlight.
    Application of Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer

    Why Does Blown Film Puncture Resistance Fall Off at High Cling Additive Loadings?

    In pallet wrap lines converting Braskem FP33 at blown film thicknesses from 12 µm to 25 µm, the conflict between surface cling and puncture resistance is controlled by the concentration of polyisobutylene or specialty tackifier masterbatch. FP33 is a butene-LLDPE blown film copolymer with a nominal density reported in the range of 0.920 g/cm³ to 0.922 g/cm³ and a nominal melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. It is processed on single-layer or three-layer lines with a die gap of 2.0 mm to 2.5 mm, a blow-up ratio of 2.0:1 to 2.5:1, and a melt temperature of 190 °C to 220 °C. At cling additive loadings above 3 wt%, the tackified surface layer behaves as a lubricating stratum that lowers the energy required for crack initiation under protrusion puncture, while also plasticizing the amorphous interlamellar region and reducing the ability of tie chains to absorb impact energy. Puncture resistance is tested under ASTM D5748-23, peel cling under ASTM D5458-21, and tensile properties under ASTM D882-18. Extended warehousing after winding allows migration of low-molecular-weight tackifier to the film surface; at ambient storage above 30 °C, the outer film face may lose extensibility and the differential coefficient of friction between the inside and outside of the web can exceed automatic stretch-wrapper tolerances. Roll telescoping after 72 h of warehouse conditioning is commonly corrected by reducing tackifier masterbatch let-down by 0.5 wt% to 1.0 wt% and verifying that core-layer melt temperature at the die exit remains below 220 °C.

    Extrusion line behaviour under high cling additive loadings differs from neat polyethylene because low-molecular-weight PIB can exude at the die lip and deposit on air ring surfaces. This deposit disturbs local cooling and creates thickness bands around the bubble circumference, which are detected as gauge profiles outside ±10% of nominal. On lines equipped with internal bubble cooling, chilled air temperatures below 8 °C can condense volatile fractions from tackifier masterbatch and produce die-lip streaks. The preferred practice is to hold cooling air above 10 °C and to inspect die lips after every 8 h shift. Screw geometry influences additive dispersion: single-flighted barrier screws with L/D ratios of 28:1 to 30:1 produce lower melt temperature and fewer fused gel particles than general-purpose screws with L/D ratios below 24:1. At melt temperatures above 230 °C, oxidative degradation of unsaturated cling modifiers can generate gels that appear as optical defects and weaken dart impact under ASTM D1709-24. Melt pressure before the screen changer should be logged continuously; an increase of 15% to 20% across a 100 µm mesh pack indicates excessive unmelts or gel accumulation and mandates line shutdown to prevent screen pack deformation or bubble rupture.

    Crop silage covers and greenhouse films converted from FP33 are generally run at higher thickness, from 120 µm to 200 µm, with hindered amine light stabilizers added for multi-season exposure. The processing window moves to a lower blow-up ratio of 1.8:1 to 2.2:1 to preserve machine-direction tear strength, while frost line height is held at 4 to 6 die diameters to balance dart impact and optical haze. Agricultural film specifications usually quote ASTM D1709-24 dart impact, ASTM D1922-23 Elmendorf tear, and ISO 527-3:2018 tensile properties before and after 2,000 h of accelerated weathering under ISO 4892-2:2013. Because butene comonomer grades generally produce lower interlamellar tie-molecule density than hexene or octene LLDPE, low-temperature crack propagation resistance must be supplemented with stabilizer and pigment loadings that do not exceed the solubility limit of the polyethylene matrix. Silage leachate with pH from 3.5 to 4.5 does not chemically attack polyethylene, but repeated abrasion from corn stover and soil particulate creates micro-cracking in the film skin. A coextruded outer skin containing HDPE or metallocene LLDPE is therefore used on many agricultural lines to raise abrasion resistance, while FP33 remains in the sealable inner layer. Anti-fogging surfactants may be added at 1.5 wt% to 2.5 wt% to reduce condensation on greenhouse covers; surface bloom of these additives should not exceed 3 wt% because excessive exudation lowers the coefficient of friction below winding tension limits and interferes with corona treatment for later print adhesion. Published data for the specific additive lot effect of FP33 on anti-fog bloom rate is limited; converters are required to perform condensation chamber testing and optical evaluation under ASTM D1003-21.

    The same agricultural structures require careful control of film bubble stability when a high concentration of processing aid is not used. Polyprocessing aid addition between 400 ppm and 800 ppm suppresses melt fracture and improves gauge uniformity on high-output lines running at extrusion rates above 250 kg/h. However, fluoropolymer processing aids can interact with anti-fogging agents, causing surface haze development after 30 days of storage. In such cases the processing aid masterbatch must be evaluated by surface energy measurement and optical microscopy for additive incompatibility. Greenhouse films are further tested for tensile retention after contact with sulphur vapor from crop protection; polyethylene is generally inert to sulphur, but the bromine and chlorine species liberated by certain fumigation chemicals can reduce HALS effectiveness and accelerate carbonyl formation at the film surface. For this reason, agricultural converters frequently specify thermo-oxidative stabilizers in addition to light stabilizers when the final film is intended for enclosed fumigated structures. This field-operating constraint is sometimes omitted from standard data sheets and must be documented through end-use field trials.

    Heavy-Duty Open-Mouth Sack Film: LDPE Dilution and Sealing Window

    When 10 wt% to 30 wt% LDPE is added to FP33 for heavy-duty open-mouth sack film, the blend lowers bubble incidence and permits stable operation at higher line speed, but it also shifts the seal initiation temperature upward and reduces hot-tack at a given sealing bar setpoint. The blend is normally extruded at 200 °C to 220 °C through a die gap of 1.8 mm to 2.2 mm, with a blow-up ratio of 2.0:1 to 2.4:1. Fractional-melt LDPE increases tubular bubble stiffness and improves gauge control on lines without automatic air-ring regulation, but it can also raise extruder backpressure and reduce melt elongation at high draw. Seal strength is measured by ASTM F88/F88M-21, while hot-tack is tested under ASTM F1921-12(2018); published data for FP33 hot-tack at specific blend ratios is limited, so the converter must generate a sealing matrix for each film thickness. On form-fill-seal equipment running 50 to 80 bags per minute, seal bar setpoints are typically observed between 105 °C and 125 °C, and the seal jaw must provide uniform pressure across the full sack width. Seal strength in LLDPE/LDPE blends generally plateaus between 100 °C and 130 °C; above this band the sealant layer may extrude from the jaw and produce stringing that contaminates the fin seal zone.

    Dart impact of heavy-duty sacks under ASTM D1709-24 is controlled mainly by the LLDPE phase. As LDPE content rises above 20 wt%, the ductile-to-brittle transition temperature increases, making the sack more vulnerable to puncture in cold storage or outdoor winter handling. Elmendorf tear resistance measured by ASTM D1922-23 is directionally dependent; blown film orientation normally yields higher transverse-direction tear than machine-direction tear, and this anisotropy must be considered when specifying minimum values for side-gusset integrity. For 80 µm to 120 µm sacks used in resin, mineral, and dry bulk packaging, the blend ratio is commonly kept at 15 wt% LDPE to retain dart impact while allowing stable bubble size. Published data for this specific configuration is limited. If the converter introduces recycled trim above 10 wt%, gel contamination from degraded PIB, printing ink, or paper fibre can produce pinholes in the sack wall. Melt filtration through 80 mesh or finer, combined with gravimetric dosing accuracy of ±1%, is standard practice on heavy-duty sack lines. A weight-fed hopper system rather than volumetric blending is required because the bulk density difference between LLDPE granules and LDPE pellets is sufficient to cause let-down drift during long production campaigns.

    If FP33 Is Specified for Frozen Bag Conversion, Low-Temperature Seal Integrity Demands Emulsion-Free Polymer Melt

    When FP33 is converted into freezer film at thicknesses from 40 µm to 70 µm, the primary process risk is not extrusion pressure but the presence of moisture droplets on pellet surfaces, which generate steam bubbles in the melt film and reduce seal continuity after filling. Drying is unnecessary for neat polyethylene under normal storage, but when resin has been stored in unheated warehouses at relative humidity above 60%, surface condensation must be removed by passing the material through a dehumidified hopper dryer at 70 °C to 80 °C for 2 h. Blown film lines should operate with a die gap of 2.0 mm to 2.5 mm, frost line height of 5 to 7 die diameters, and melt temperatures below 210 °C to limit formation of low-molecular-weight oxidation products at the die exit. Low-temperature dart impact is measured on specimens preconditioned at -18 °C and tested under ASTM D1709-24 or ISO 7765-2:2022. Butene-LLDPE has a lower concentration of load-bearing tie molecules than octene-based LLDPE, so brittle failure in frozen bags is often initiated by heavy-gauge fish-eyes or gel particles rather than uniform film thinning. Seal integrity after frost conditioning is tested under ASTM F88/F88M-21; edge delamination of the seal under freezer conditions indicates either additive exudation at the sealant surface or seal bar temperature below the final melting point of the polymer.

    FP33 should not be used as an oxygen barrier layer in frozen food packaging. Polyethylene exhibits high oxygen transmission measured by ASTM D3985-17 or ASTM F1927-20, and oxygen-sensitive products such as IQF seafood, fatty fish, and certain vegetables require gas flushing or coextrusion with EVOH or PVDC. When FP33 is coextruded as a sealant skin with EVOH, the melt temperature must remain below 220 °C to avoid EVOH thermal degradation, and the adhesive tie resin should be selected so that its melting range lies within 10 °C of the FP33 sealant layer. Continuous exposure of polyethylene film to high-fat frozen products above 0 °C for extended periods can plasticize the polymer through fat absorption, lowering seal strength after thawing. Food-contact compliance must be verified under Regulation (EU) No 10/2011, with food simulant selection determined by the actual frozen storage and reheating conditions of the final article. If the bag is used for microwave reheating, the converter must also evaluate the migration behaviour of surface additives under fatty food simulant D2 at the maximum package temperature, not merely at frozen storage temperature.

    High-clarity lamination film for confectionery and snack packaging is converted from FP33 at thicknesses of 18 µm to 35 µm, where haze development is determined less by the base resin itself than by die-lip deposits, film cooling rate, and post-extrusion handling. The use of a die gap of 1.5 mm to 2.0 mm with a blow-up ratio of 2.2:1 to 2.8:1 increases transverse tensile strength, while a frost line height below 4 die diameters limits crystallite growth and improves optical clarity. Haze is measured under ASTM D1003-21 or ISO 14782:1999, and gloss is measured under ASTM D2457-21. Butene-LLDPE grades generally produce haze values below 12% at 25 µm when the die lips are clean and the air ring is balanced, but surface scratches from secondary slitting and bag-making can raise haze beyond customer limits even when the wound roll was initially acceptable. After corona treatment to 38 mN/m to 42 mN/m surface energy, the film is printed and laminated to BOPP or metallized PET; the finished laminate is tested for seal strength under ASTM F88/F88M-21 and for retained adhesive performance after 48 h of cure. In such structures, layer reverse-printing can expose the FP33 web to residual solvent; converters must ensure that retained solvent levels remain below the concentration specified in the film converter’s process specification and that the final article complies with FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011.

    The seal initiation behaviour of FP33 in lamination film is influenced by superficial dust and additive exudation. Silica-free antiblock levels above 2,000 ppm can reduce coefficient of friction but may also increase haze and reduce seal strength of thin-gauge webs. Slip additives should be matched to the downstream packaging line speed; excessive erucamide bloom can create plate-out on the seal jaws and reduce the available sealing window by up to 10 °C. Converters running FP33 at thicknesses below 20 µm must give particular attention to bubble stability because the melt strength of a 1.0 g/10 min butene-LLDPE is generally lower than that of a fractional-melt LDPE. Die gaps below 1.5 mm are not recommended for this grade on high-output lines because the apparent shear stress at the die lip can exceed the critical value for sharkskin, producing surface roughness that reduces gloss and interferes with lamination bond strength. When sharkskin is observed, the first corrective action is not a melt temperature increase but an increase in die gap or a reduction in line speed, followed by evaluation of the die-lip exit velocity distribution.

    Film Oscillation, Nip Collapse, and Layer Distribution in Stretch Hood Converting

    During stretch hood conversion of FP33 as a core layer between EVA or metallocene polyethylene skins, film thickness typically ranges from 80 µm to 140 µm, with a blow-up ratio of 2.8:1 to 3.2:1 and a die gap of 2.5 mm to 3.0 mm. The core layer supplies melt strength and bubble stability, while the skins carry cling, slip, or antistatic additives. Layer distribution is adjusted through die gap and air ring temperature profiling; microtome cross-sections should show core-layer variation no greater than ±5% of nominal, because greater eccentricity creates asymmetric stretch force in the final hood. On lines with oscillating die or rotating haul-off, edge beading is controlled by nip collapse geometry and internal bubble cooling. A bowed air ring lip or uneven air ring temperature produces thickened bands at the lay-flat edges, which appear as gauge deviations outside ±10% of nominal across the web. Such edge thickening leads to telescoped rolls and to irregular containment force when the hood is applied by automated pallet wrapping equipment. FP33 in the core is normally run between 190 °C and 210 °C; if EVA skins are present, the overall melt temperature must remain below 220 °C to avoid acetic acid generation from the EVA phase. Film performance is tested under ASTM D5748-23 for puncture, ISO 527-3:2018 for tensile properties, and ASTM D1922-23 for tear resistance.

    Because stretch hood film is held under continuous tension after application, stress relaxation of butene-LLDPE can reduce containment force after 24 h of pallet storage. Converters measure retained containment force with a stretch-wrapper force transducer at fixed elongation percentages and at defined outdoor or warehouse temperatures. Published stress-relaxation data for FP33 specifically is limited; therefore the converter must validate the final hood dimensions on actual pallet configurations rather than relying on resin density and melt index alone. Cold-climate application of stretch hood film below -10 °C may increase the force required to open and unwrap the hood, particularly if surface slip additives have not migrated to the film skin. End users must be cautioned that polyethylene film does not provide a barrier to water vapour or oxygen suitable for long-term corrosion protection; for metal coils or machinery, the hood film is normally supplemented with vapour corrosion inhibitor emitter packs rather than relying on the polymer film as a barrier. The use of recycled trim in stretch hood film is possible below 10 wt%, but reclaimed material containing EVA skin fragments or tackified surface layers can form gel specks that reduce dart impact and create weak points at the folded edge.

    For can liners and industrial refuse sacks filled with sharp scrap, glass cullet, or metal turnings, FP33 is processed at 40 µm to 80 µm on single-layer lines with a die gap of 2.0 mm to 2.5 mm, a blow-up ratio of 2.0:1 to 2.4:1, and a melt temperature of 180 °C to 200 °C. Puncture and tear are tested under ASTM D1709-24 and ASTM D1922-23. Recycled trim levels above 10 wt% reduce transverse-direction tear and introduce gel contamination; melt filtration through 80 to 100 mesh screens is mandatory. The final liner is frequently evaluated for pinhole count under a stationary light source after stretching over a rigid frame to simulate filling stress.

    Which Regulatory Documents Govern Olefin Film Compliance for FP33?

    Food-contact and industrial packaging specifications for FP33 must be reviewed against the following compliance matrix. The table is not a substitute for lot-specific certification from the resin manufacturer; final converters are responsible for migration testing on the finished article under actual time, temperature, and food simulant conditions.

    Regulatory or normative referenceScopeVerification practice
    FDA 21 CFR 177.1520US olefin polymers for food contact, including extractives and compositional limitations.Resin supplier FDA status letter; end-use condition check for fatty, aqueous, or acidic foods.
    Regulation (EU) No 10/2011 as amendedEU plastic materials and articles intended to contact food.Overall migration by food simulants; specific migration for additives from final structure.
    REACH 1907/2006Registration, evaluation, authorisation of substances in EU industrial use.Safety data sheet review; SVHC content below 0.1 wt% per article.
    Directive 94/62/EC and amendmentsPackaging and packaging waste, including sum of heavy metals.Heavy-metal concentration not exceeding 100 ppm by weight in packaging components.
    ASTM D3985-17Oxygen transmission rate through plastic films for packaging applications.Thickness-normalised OTR measurement for any modified-atmosphere package.
    Free Quote

    Competitive Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem FP33 is a linear low-density polyethylene (LLDPE) butene copolymer designed for blown film extrusion. The resin is sold as a pelletized ethylene/1-butene copolymer with a nominal density of 0.918 g/cm³ when tested under ASTM D792 or ISO 1183-1, and a nominal melt mass-flow rate of 1.0 g/10 min at 190 °C/2.16 kg when tested under ASTM D1238 or ISO 1133-1. The 1-butene comonomer introduces short-chain branching along the ethylene backbone; this distinguishes FP33 from hexene- and octene-based LLDPE resins and influences melt rheology, film mechanical properties, and seal response. Typical uses include general-purpose packaging film, industrial liners, carrier bags, and protective over-wrap, produced on monolayer or coextruded blown film lines. The grade is processed on single-screw extruders with L/D 24:1 to 30:1 and with LLDPE-specific barrier screws; melt temperature should remain below 250 °C to avoid oxidative gel formation. The values reported in product literature are nominal lot averages and are not production specifications; the certificate of analysis for a delivered lot should be reviewed for density and melt-flow compliance.

    Table 1. Nominal resin properties for Braskem FP33
    PropertyTest methodNominal value
    Melt mass-flow rateASTM D1238 / ISO 1133-1, 190 °C/2.16 kg1.0 g/10 min
    DensityASTM D792 / ISO 1183-10.918 g/cm³
    Comonomer type13C NMR or FTIR compositional analysis1-butene

    The resin is normally packaged in 25 kg bags or bulk containers. Storage below 50 °C and protection from ultraviolet exposure are recommended to preserve pellet integrity and avoid additive degradation. Pellets that have been allowed to block due to high storage temperature should be loosened before feeding; mechanical crushing of fused pellets should be avoided because particle size distribution changes can distort gravimetric feed rates.

    What blown film processing window is associated with FP33?

    The melt temperature measured at the die is typically maintained between 190 °C and 230 °C for standard blown film extrusion. Die temperatures above 240 °C increase the risk of gel formation and oxidised inclusions, while die temperatures below 180 °C may cause bubble instability and surface melt fracture. Die gap settings of 1.5 mm to 2.5 mm and blow-up ratios of 2.0:1 to 3.0:1 are common on conventional monolayer lines. On 45 mm to 65 mm single-screw extruders, a barrier screw with a Maddock or pineapple mixing section improves melt homogeneity at screw speeds above 60 rpm. Output above the cooling capacity of the air ring can cause bubble flapping and gauge variation; the frost line is typically set 6 to 10 die diameters downstream of the die for this density class. LLDPE has lower melt strength than LDPE, so a stabilised bubble guide or internal bubble cooling is used on high-output lines. For drawdown to 20 µm or lower, a higher-stalk bubble configuration or blending with LDPE may be required. Published data for the specific response of FP33 on high-output rotating die lines is limited, and start-up trials should establish the stable operating envelope for a given die diameter and air-ring geometry.

    Drying is not normally required for FP33 because polyethylene is not hygroscopic. If condensed moisture is present on cold pellets after outdoor storage, the pellets should be brought to 20 °C to 25 °C before entering the extruder feed throat to prevent steam pitting and bubble defects in the film. Barrel temperature profiles for LLDPE butene extrusion often start at 140 °C to 160 °C in the feed zone, rise to 180 °C in the compression zone, and reach 200 °C to 220 °C at the die. The actual profile must be adjusted for screw speed, screen pack, and die diameter. A melt pump between the extruder and die reduces output variation and helps maintain melt temperature below 230 °C at high screw speeds. If the melt temperature approaches 240 °C, the screw should be cooled or the back pressure reduced; operation above 250 °C accelerates oxidative degradation and increases gel specks in the film.

    On a 250 mm die with a 1.8 mm die gap, a melt temperature of 200 °C to 210 °C is often used for 25 µm to 50 µm film, with a blow-up ratio of 2.5:1. Increasing the blow-up ratio above 3.0:1 improves transverse direction tear under ASTM D1922 but may reduce bubble stability if the air ring lacks dual-lip flow control. Internal bubble cooling is preferable on lines exceeding 150 kg/h to keep the frost line below 4 die diameters; without it, gauge control may degrade when the frost line exceeds 8 die diameters. Purging with a high-viscosity HDPE or commercial purging compound is required after processing colour concentrates or high-melt-index resins to prevent black specks and gels in subsequent film.

    In coextruded structures, FP33 is commonly used in core or sealant layers. The outer skin layer may be a higher-alpha-olefin LLDPE or an LDPE-rich blend for heat seal and optical performance. Layer thickness control below 10 µm per layer requires gravimetric feeding and melt pumps; unmatched viscosity across layers can cause interfacial instability. Viscosity differences between FP33 and a high-MI LDPE skin resin should be evaluated using melt-flow data under ASTM D1238, but a single-point melt-flow comparison does not capture the full shear-rate response. For LLDPE-rich structures, the die adaptor and spiral mandrel should be designed for low shear heating; excessively high shear at the spiral section can create flow lines that appear as thin-gauge bands in the film.

    Film mechanical property evaluation in a 25 µm monolayer blown film provides a useful reference point. When tested under ASTM D882 at 500 mm/min, LLDPE butene film in this density and melt-index class typically shows tensile yield strength in the machine direction of 10 MPa to 12 MPa and elongation at break above 600%. Dart impact resistance measured under ASTM D1709 Method A falls in the range of 80 g to 120 g for many commercial butene LLDPE resins, but the value for FP33 is influenced by frost line height, blow-up ratio, and additive loading. Elmendorf tear strength under ASTM D1922 frequently shows an anisotropic profile, with transverse direction tear values in the range of 300 gf to 500 gf and machine direction tear values below 200 gf. Optical haze measured under ASTM D1003 is commonly 8% to 15% for unpigmented 25 µm butene LLDPE film. These values are class-level ranges, not guaranteed FP33 specifications; the manufacturer’s certificate of analysis should be consulted for lot-specific data.

    For applications requiring seal performance, heat-seal initiation and hot-tack should be measured under ASTM F88 and ASTM F1921. Butene LLDPE resins typically develop seal strength at temperatures 5 °C to 10 °C higher than lower-density plastomer grades, but the exact seal initiation temperature is a function of density, additive bloom, and contact time. Seal-bar temperature profiles should be verified on the actual film substrate, because slip additive migration can depress seal strength if the coefficient of friction is below 0.15.

    Molecular architecture and property differences against hexene- and octene-based LLDPE resins

    The primary structural variable in FP33 is the use of 1-butene as the alpha-olefin comonomer. At equivalent melt index and density, butene-based LLDPE grades generally develop a lower tie-chain concentration in the amorphous regions than hexene- or octene-based copolymers, because the shorter branch length is less effective in bridging lamellae under load. This produces lower dart impact and Elmendorf tear values when compared under ASTM D1709 and ASTM D1922. The differential is most evident at gauge below 30 µm, where octene LLDPE films often retain impact resistance more effectively than butene resins. Conversely, the shorter branch length alters seal initiation and optical response; seal strength is measured under ASTM F88, and butene LLDPE generally shows comparable or slightly lower hot-tack performance than hexene or octene grades at the same seal temperature. In coextruded films, FP33 may be placed in a core layer where tensile demands are lower, while a higher alpha-olefin grade is used in the outer layers for puncture and tear performance. The choice between FP33 and a hexene LLDPE should be based on film toughness, available die cooling capacity, and cost per kg of packaged product.

    Table 2. Qualitative performance ranking by comonomer class at equivalent melt index and density
    Performance attributeTest methodButene LLDPE (FP33 class)Hexene LLDPEOctene LLDPE
    Dart impactASTM D1709 Method Alowerintermediatehigher
    Elmendorf tearASTM D1922lowerintermediatehigher
    Puncture resistanceASTM D5748lowerintermediatehigher

    Property differences between comonomer types are most visible in dart impact and tear propagation because these tests involve high local strain rates. In tensile testing under ASTM D882, the yield stress difference between butene and hexene LLDPE at equivalent density is often small, whereas the energy-to-break difference is larger. Therefore, replacing FP33 with a hexene or octene grade in a film can produce only a modest change in stiffness but a measurable change in impact and tear toughness. Product selection should use data generated on the same film line at the same gauge, since air-ring efficiency and frost line height interact with comonomer type.

    When FP33 is blended with LDPE or combined with slip and antiblock masterbatch

    Adding LDPE at 10 wt% to 30 wt% to FP33 blown film blends is a standard method to improve bubble stability and reduce melt fracture on high-output lines. The blend increases melt strength but lowers dart impact and Elmendorf tear values; the reduction is measurable under ASTM D1709 and ASTM D1922. A 20 wt% LDPE addition can shift the dart impact of a 25 µm film by 10% to 30% lower than the neat butene-LLDPE value, although the exact change depends on the LDPE melt index and frost line height. For reduced surface friction, slip agents such as erucamide are used at 500 ppm to 1500 ppm, with antiblock silica at 1000 ppm to 3000 ppm; coefficient of friction is measured under ASTM D1894 or ISO 8295. Slip migration in LLDPE is slower than in LDPE, so the film should be conditioned at 23 °C and 50% relative humidity for 24 h to 48 h before friction testing. A known failure mode in roll form is blocking when slip additive concentration is below 500 ppm or when storage temperature exceeds 40 °C; blocking force can be assessed by ASTM D3354. The critical thermal limitation is oxidative degradation at melt temperatures above 250 °C, which generates by-products that can interfere with heat-seal strength under ASTM F88.

    Food-contact status for FP33 depends on the specific additive package and conversion conditions. The base ethylene/1-butene copolymer is of a type covered as an olefin polymer under 21 CFR 177.1520(c), with extraction and end-use limitations defined in the regulation. For European Union applications, compliance may be assessed under Regulation (EU) No 10/2011, including an overall migration limit of 10 mg/dm² and specific migration limits for additives. REACH registration and applicable national packaging regulations require confirmation from the supplier for the delivered lot. No direct food-contact suitability claim should be made without reviewing the manufacturer’s food-contact declaration for the specific grade and lot.

    RoHS Directive 2011/65/EU limits lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE at 0.1 wt% per homogeneous material; polyolefins produced without metallic pigments or contaminated filler normally satisfy these limits. Conflict minerals or REACH Candidate List substances require supply-chain confirmation. For industrial packaging, the resin may be classified under standard resin identification code 4 according to ASTM D7611 for LDPE/LLDPE materials. Product-specific certifications for food contact, Kosher, and Halal are available from Braskem for qualified grades, but these are lot-specific and must be requested before commercial use.

    Top