| HS Code | 714379 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) Copolymer |
| Comonomer | Butene-1 |
| Density | 0.924 g/cm³ |
| Melt Index | 0.9 g/10 min at 190°C/2.16 kg |
| Melting Point | 123 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700 % |
| 1 Secant Modulus | 260 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 11 % |
| Gloss At 45 | 65 |
| Coefficient Of Friction | 0.2 |
| Processing Temperature | 190–210 °C |
As an accredited Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem FM31D LLDPE blown film extrusion polyethylene copolymer supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for industrial shipping. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Braskem FM31D LLDPE blown film extrusion polyethylene copolymer: palletized bags, dry, securely stowed for transport. |
| Shipping | Braskem FM31D LLDPE copolymer resin is shipped as non-hazardous solid pellets in 25 kg bags or bulk octabins/pallets. Packaging is moisture-resistant and labeled with lot and safety info. Transport in clean, dry vehicles at ambient temperature; avoid direct sunlight, heat, and contamination. No special dangerous goods classification applies. |
| Storage | Store Braskem FM31D LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original containers sealed and off the floor to prevent moisture and contamination. Avoid strong oxidizing agents. Use first-in, first-out inventory. Maintain ambient temperatures, typically below 50°C, and avoid prolonged UV exposure. Do not store near food or drinking water. |
| Shelf Life | Recommended shelf life: 24 months from production date when stored in original packaging, dry, below 50°C, away from direct sunlight. |
In heavy-duty sack and liner extrusion, Braskem FM31D—a linear low-density polyethylene copolymer with nominal density 0.918 g/cm³ per ASTM D792-20 and melt flow rate 1.0 g/10 min per ASTM D1238-20—is blended with high-pressure low-density polyethylene at addition levels of 70–85 wt% FM31D and 15–30 wt% LDPE. A slip/antiblock masterbatch is added at 1–4 wt%, and a polymer processing aid concentrate is introduced at 0.5–1.5 wt% to suppress melt fracture on air-cooled blown film lines. The downstream process is a single-screw extruder with a barrier screw design, L/D ratio 30:1–36:1, die diameter 200–400 mm, die gap 1.8–2.5 mm, blow-up ratio 2.0:1–3.0:1, melt temperature 190–230°C, and frost line height held within 4–6 die diameters. On production lines converted from high-pressure LDPE, bubble sway and edge flutter are observed when the frost line is pushed above 6 die diameters or when the melt temperature exceeds 230°C at the die head; the instability is attributable to limited melt strength of linear polyethylene and requires lower specific output than comparable LDPE campaigns. Resin temperature above 240°C is not recommended because oxidative gel formation increases and may produce film defects at the die lips. Compliance for non-food heavy-duty sacks and FIBC liners is assessed against ASTM D1709-16a for dart drop, ASTM D1922-15 for Elmendorf tear, ASTM D882-18 for tensile properties, ISO 21898:2004 for FIBC non-dangerous goods packaging, and the registration and downstream communication obligations of EU REACH. Terminal product types include FIBC internal liners, heavy-duty shipping sacks for polymer resin, granular fertilizer, petrochemical additive bags, and construction material sacks.
Frozen vegetable, seafood, and ice cream packaging operations introduce FM31D as the primary blown film resin at 60–80 wt%, with high-pressure low-density polyethylene at 10–25 wt%, a metallocene plastomer at 5–15 wt% to depress low-temperature brittle point, and a slip/antiblock concentrate at 1–3 wt%. The extruded web is a three-layer coextruded blown film structure, with die gap 1.5–2.0 mm, blow-up ratio 1.8:1–2.5:1, melt temperature 175–210°C, and corona-treating set to a target wetting tension of 38–42 dyn/cm prior to lamination or surface print. The die gap is narrower than in sack film to maintain gauge uniformity in low-thickness webs of 40–80 μm, and the low-temperature impact response is monitored by ASTM D1790 or ASTM D1709 with specimens conditioned at −18°C to −25°C. Compliance for frozen food contact uses FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011 Annex I with overall migration testing per EN 1186-1, and food contact GMP under 2023/2006/EC. Published data for this specific FM31D frozen food configuration is limited; therefore, migration testing is executed on the finished laminate rather than extrapolated from resin TDS values. Terminal product types include frozen vegetable pouches, frozen seafood bags, ice cream overwrap, and barrier laminate sealant webs used in vertical form-fill-seal lines.
The selection of a three-layer coextruded cover structure begins with additive partitioning and surface bloom behavior, not short-term tensile strength. In this application, FM31D is melt-compounded at 72–88 wt% with a UV-stabilizer masterbatch at 8–18 wt%, an anti-fog/anti-dust concentrate at 1–3 wt%, and an IR-blocking thermal additive system at 2–5 wt% where night-time heat retention is specified. The downstream production process is three-layer coextruded blown film with die gap 1.8–2.4 mm, blow-up ratio 2.5:1–4.0:1, melt temperature 190–230°C, and separation of the UV-stabilizer-rich outer layer from the anti-fog-rich inner layer to prevent interlayer additive migration and surface bloom defects. Industrial line observation indicates that UV masterbatch let-down below 8 wt% at the specified carrier concentration produces uneven surface distribution in the outer layer, with localized haze bands and premature film cracking after 12–18 months of continuous exposure; this is a processing limitation rather than a resin limitation. Compliance is evaluated under EN 13206 for agricultural covering films, ISO 4892-2 accelerated weathering, ASTM D1003 for haze, ASTM D624 for tear resistance, and ISO 527-3 for tensile properties of films. Terminal product types include multi-season greenhouse covers, low-tunnel covers, silage bunker covers, and nursery overwintering films.
E-commerce mailer and carrier bag film produced with post-consumer recyclate relies on virgin LLDPE dilution to restore impact and tear strength after the recycled melt fraction introduces gel particles, residual unsaturation, and variable melt flow. In this configuration, FM31D is added at 50–75 wt%, post-consumer recycled LDPE/LLDPE at 20–40 wt%, a processing aid masterbatch at 1–3 wt%, and an antioxidant concentrate at 0.5–1.5 wt%. The extruder requires a grooved-feed or barrier screw with length-to-diameter 30:1–36:1, a screen changer fitted with 80–120 μm mesh packs, a vacuum vent configured to reduce residual moisture below 0.1 wt%, and die gap 1.8–2.8 mm because the recycled melt fraction lowers bubble stability. Blow-up ratio is held at 2.0:1–3.0:1, melt temperature at 185–225°C, and line speed is adjusted to prevent draw resonance at the lower melt strength of recyclate-containing blends. Compliance for the finished mailer includes EU Packaging and Packaging Waste Directive 94/62/EC with aggregate heavy metals not exceeding 100 mg/kg for lead, cadmium, mercury, and hexavalent chromium, EU REACH registration and SVHC disclosure, and ISO 14021 for recycled content claims if verified through controlled blending batch records. Terminal product types include e-commerce shipping mailers, parcel bags, industrial donation sacks, and retail carry-out bags with post-consumer recycled content targets.
Operationally, pallet unitization with stretch hood film requires a tubular film that survives downward stretching over palletized freight without puncturing at sharp corners, and FM31D is used in this application as the dominant layer resin at 65–80 wt%, with high-pressure LDPE at 20–35 wt% and a processing aid concentrate at 0.5–1.5 wt%; no cling additive is incorporated because the holding force is generated by elastic recovery rather than tack adhesion. The film is produced on three-layer coextruded blown film lines with die gap 1.6–2.4 mm, blow-up ratio 2.5:1–4.0:1, melt temperature 190–225°C, and film thickness 60–150 μm, followed by gusseting, layflat winding, and perforation on the converting line. Excessive blow-up ratio above 4.0:1 or melt temperature above 225°C leads to bubble instability and inconsistent TD stretch distribution during hood application, a production-scale failure mode reported on hood lines running at high output. Compliance is verified by ASTM D882 for tensile elongation at break, ASTM D1922 for Elmendorf tear, ASTM D1709 for dart impact, and REACH communication obligations; the product is not intended for direct food contact unless the structure includes a separately compliant food-contact layer. Terminal product types include stretch hood film for palletized freight, building material transit wraps, white goods protective covers, and industrial furniture stretch covers.
For thin-gauge produce, bakery, and garment bag films produced from FM31D, the formulation space is deliberately narrow because the resin is operated at 85–100 wt%, with slip/antiblock concentrate at 0.5–2.5 wt% and processing aid at 0.3–1.0 wt%, and all additive concentrates must be selected from food-contact-compliant masterbatch systems under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. The process uses a monolayer or two-layer blown film line with die gap 1.2–2.0 mm, blow-up ratio 1.5:1–2.5:1, melt temperature 170–200°C, and a reduced frost line height to control haze via rapid quenching. Unlike heavy-duty sack or hood film, the operating window is narrower at the lower end because the thin web is sensitive to melt fracture and gauge bands when the die gap is below 1.2 mm or when the processing aid let-down is below 0.3 wt%. Compliance testing for the finished film uses ASTM D1003 for luminous transmittance and haze, ASTM D1894 for coefficient of friction, ASTM D2457 for gloss, and ASTM D882 for tensile properties, with food-contact migration testing per EN 1186-1 where applicable. Terminal product types include fresh produce bags, bakery overwrap, dry goods bags, and garment bags used in retail and distribution. Published data for this specific FM31D direct-food overwrap configuration is limited, so the resin supplier's food-contact statement should be confirmed for each converter-specific formulation.
Competitive Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem FM31D is a butene-comonomer linear low-density polyethylene copolymer supplied for blown film extrusion. The grade is pelletized and intended for general-purpose film applications in which balanced toughness, processability, and density are required. Its nominal melt index is 1.0 g/10 min when determined in accordance with ASTM D1238 at 190 °C/2.16 kg, and its nominal density is 0.918 g/cm³ when determined in accordance with ASTM D1505. The combination places the material in a range commonly selected for industrial liners, shipping sacks, protective packaging, and agricultural or construction films. The grade is not a metallocene-catalyzed high-clarity resin, nor is it formulated as a high-melt-strength LDPE substitute; its position is defined by moderate sealing performance, good puncture resistance, and predictable processing on conventional blown film lines.
The butene comonomer introduces ethyl branches along the polyethylene backbone. Compared with hexene and octene comonomers, butene produces a more economic short-chain-branch structure but generally yields lower tie-molecule effectiveness at equivalent density and melt index. The density of 0.918 g/cm³ reduces crystalline fraction and increases ductility relative to high-density polyethylene, while the melt index of 1.0 g/10 min retains sufficient viscosity for bubble formation and film gauge control. Because FM31D is produced with a conventional Ziegler-Natta catalyst system, its composition distribution is broader than that of a single-site metallocene resin. The broader distribution widens the melting and sealing range and lowers optical uniformity but can improve extrusion stability on older blown film lines that lack the high die-pressure capability often required for metallocene grades. Melt index ratio, defined as the ratio of high-load melt index at 21.6 kg to standard melt index at 2.16 kg, is frequently used as a processability indicator; published data for this specific FM31D configuration is limited, but Ziegler-Natta LLDPE film grades in this melt-index class typically exhibit sufficient shear thinning for stable blown film extrusion.
Replacing LDPE with FM31D on an existing monolayer line normally requires adjustment of die gap, cooling-air balance, and melt-temperature profile. High-pressure LDPE derives melt strength from long-chain branching; FM31D is a linear resin with short-chain branches only. The loss of long-chain branching reduces melt tension and increases the sensitivity of bubble stability to air-ring configuration. A die gap of 1.8–2.5 mm is commonly used for LLDPE, compared with 0.8–1.2 mm for LDPE, to reduce die-lip shear stress and delay sharkskin melt fracture. On grooved-feed extruders with L/D ratios from 24:1 to 30:1, breaker-plate and screen-pack differential pressure should be monitored because linear resins can generate higher melt pressure through narrow die gaps. If the differential approaches the limit specified by the extruder manufacturer, a wider screen-pack open area or a higher die temperature is required before output can be increased.
Barrel zone setpoints are commonly maintained between 190 °C and 220 °C, while adapter and die temperatures are held between 205 °C and 225 °C to reduce melt fracture at high output. Blow-up ratio from 2.0:1 to 3.0:1 balances machine-direction and transverse-direction properties. Lower blow-up ratios tend to favor machine-direction tear strength due to molecular orientation, while higher blow-up ratios improve transverse-direction tear. Frost-line height is not an independent setpoint; it is controlled through cooling-air mass flow, bubble diameter, and melt temperature. On commercial monolayer lines equipped with dual-lip air rings and internal bubble cooling, stable operation is usually obtained for film thicknesses from 25 µm to 150 µm. Converters running below 25 µm often observe vertical bubble oscillation unless the lower air-ring lip is raised and die temperature is increased.
Extrusion lines with high-shear barrier screws and tight clearances may exhibit a rise in melt temperature as screw speed increases, particularly when the die gap is set below 1.8 mm. Viscous dissipation in the metering section can shift the resin beyond the intended 190–220 °C range and into the 230–240 °C band without a corresponding change in barrel setpoint. The resulting film may show surface haze and micro-gel formation at the die lips. On some commercial lines using a 60 mm grooved-feed extruder and a 300 mm die, reducing screw speed by 10–15 rpm and increasing die gap returns melt temperature to the acceptable range. Published data for this specific configuration is limited, but the behavior is consistent with viscous heating in linear LLDPE melts.
| Parameter | Reference range or condition | Unit or note |
|---|---|---|
| Melt temperature | 180–220 °C | Barrel and die |
| Die temperature | 205–225 °C | To limit sharkskin |
| Die gap | 1.8–2.5 mm | Monolayer die |
| Blow-up ratio | 2.0:1–3.0:1 | Balanced orientation |
| Film thickness | 25–150 µm | Typical stable window |
| Predrying | Not required if dry; 60 °C for 2 h if surface moisture | Hopper dryer |
Optical properties of FM31D film are moderate because the Ziegler-Natta composition distribution and butene branching produce more surface and bulk scatter than metallocene grades. Haze measured under ASTM D1003 and gloss measured under ASTM D2457 are affected by frost-line height, cooling rate, and die-gap setting. Rapid quenching through a low frost line produces smaller lamellar structures and generally lower haze, but the improvement is limited by the resin’s broad composition distribution. For industrial liners and shipping sacks, haze values above 10 % are commonly acceptable; exact values must be established on the production line because laboratory cast film is not representative of blown film morphology.
Mechanical properties of FM31D film must be validated on the converting line because measured tensile, tear, and dart impact values depend on blow-up ratio, die gap, frost-line height, and film gauge. Comparative data for butene LLDPE resins of 0.918 g/cm³ density show that down-gauge films generally exhibit elongation at break above 700 % under ISO 527-3 and higher dart impact than LDPE of equivalent density under ASTM D1709. Puncture resistance is particularly relevant for industrial liners and shipping sacks; instruments using ISO 7765-2 or ASTM D5748 show that linear LLDPE films resist puncture better than high-pressure LDPE at equivalent gauge, but published data for this specific FM31D configuration is limited and should be generated on the target line.
The sealing behavior of FM31D film is governed by density, comonomer type, and molecular composition distribution. Seal initiation temperature can be established under ASTM F2029 by measuring the minimum jaw temperature at which a seal strength of 1.0 N/25 mm is first obtained. Butene LLDPE films of 0.918 g/cm³ density usually seal within a temperature range of 95–110 °C, but the FM31D-specific value must be determined on the actual film sample and not inferred from resin density alone. Hot-tack behavior measured under ASTM F1921 is narrower than that of LDPE because linear chains solidify over a narrower temperature interval. On vertical form-fill-seal machines, a narrow hot-tack window becomes a throughput constraint at elevated package speeds; seal-bar temperature mapping is required to avoid bottom-seal opening during product loading.
For film below 50 µm, dwell times of 0.3–0.5 s are typical on industrial packaging lines, while thicker films require longer dwell or higher bar temperature. Seal strength should be measured under ASTM F88 after conditioning at 23 °C and 50 % relative humidity for 24 h. Hot-tack force is particularly important when the product drops into the bag before the seal has fully crystallized; hot-tack failure appears as seal separation along the bottom seam, especially when seal-bar temperature is set just above the initiation threshold rather than in the middle of the available window. Knurled seal bars often perform better than polished flat bars with LLDPE at high speed because they mechanically displace molten polymer into contact and increase the effective sealing area at low dwell time. Published data for this specific configuration is limited outside Braskem technical service reports.
FM31D can be reprocessed as in-house scrap, but repeated heat history raises the probability of gel formation and oxidative discoloration. Regrind addition up to 20 % in monolayer structures is usually processable without major shifts in melt pressure, provided the scrap is clean, dry, and free of slip or anti-block contamination from other film sources. When regrind content exceeds 30 %, melt pressure and melt temperature should be monitored because degraded linear chains can produce crosslinked gel particles that appear as optical defects and weak spots. The melt temperature should not exceed 240 °C; interruptions longer than 15 min at this temperature increase the risk of yellowing and surface roughness, especially when the scrap has been stored under humid conditions.
Polyethylene is not hygroscopic, and FM31D does not require routine pre-drying when stored indoors. If sacks or octabins are stored outdoors, surface moisture can produce steam inclusions in the film; a hopper dryer at 60 °C for 2 h removes surface water without altering the stabilization system. Melt-contact surfaces should be stainless steel rather than copper or copper-based alloys because copper at elevated temperature accelerates oxidative degradation of polyolefins. The exact antioxidant and additive package is lot-specific and should be confirmed against the certificate of analysis. Processors adding slip or anti-block masterbatch at the hopper should verify concentrate compatibility before large-scale use because some amine-based processing aids can interact with phenolic stabilizers and cause discoloration.
On three-layer coextrusion lines, FM31D is typically placed in the core or in a skin layer where toughness and melt stability are required. It can be combined with LDPE skins to improve melt strength and sealability; the blend ratio depends on die geometry and final film specifications. Because FM31D is a butene-based resin, its use in high-performance sealant layers is limited by a higher seal-initiation temperature relative to metallocene plastomers. Published data for this specific configuration is limited outside Braskem technical service documents.
Industrial liners and shipping sacks produced from FM31D commonly use film thicknesses from 80 µm to 150 µm because the design requirement is resistance to puncture by sharp edges and tearing at gusset corners. A blow-up ratio near 2.2:1 to 2.5:1 is a common converter starting point for balanced machine-direction and transverse-direction toughness. For agricultural cover film and light industrial sheeting, blending FM31D with LDPE or recycled polyethylene is used to modify bubble stability and reduce gauge variation; the specific blend ratio must be established by trial on the target line because published data for this specific configuration is limited.
For food-contact applications, base LLDPE copolymers of this type are generally classifiable under 21 CFR 177.1520(c) when the final article satisfies extractive and migration limits. Converters placing FM31D-based articles on the European market should obtain the supplier’s regulatory certificate for EU 10/2011 and REACH compliance. As supplied without additional masterbatches, the grade does not contain heavy-metal-based pigments or fillers; any colorant or processing aid added downstream transfers compliance responsibility to the converter.
When comparing FM31D to other Braskem film grades, the primary differences are comonomer type and density-melt-index position. High-density blown film grades offer higher modulus and lower permeability at the expense of dart impact; metallocene LLDPE grades offer better optical clarity, higher dart impact, and lower seal initiation temperature at the expense of narrower processing latitude and often higher melt pressure. FM31D occupies a general-purpose position in which converter familiarity, material cost, and balanced mechanical properties are more important than maximum optical or seal performance.