| HS Code | 720152 |
| Density | 0.921 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.1 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 103 °C |
| Tensile Strength At Yield | 10.5 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 650 % |
| Flexural Modulus | 260 MPa |
| Dart Drop Impact | 300 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12 % |
| Gloss 60 | 70 |
| Coefficient Of Friction | 0.20 |
As an accredited Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer comes in 25 kg polyethylene bags for safe storage and handling. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer, palletized bags in dry container, securely stowed. |
| Shipping | Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer ships as non-hazardous polyethylene pellets in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. Use clean, dry transport; avoid heat, moisture, and contamination. Standard commercial packaging; no special DOT/ADR hazard classification required. |
| Storage | Store Braskem Flexus® 9211 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers or bags closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid prolonged stacking or extreme temperatures. Follow the manufacturer’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Shelf life: 24 months from production date when stored unopened in original packaging, dry, ambient conditions, away from direct sunlight. |
In heavy-duty FIBC liner and bulk-sack coextrusion, Braskem Flexus® 9211 LLDPE blow film extrusion polyethylene copolymer is introduced at 70–80 wt% in skin and core layers, with LDPE at 20–30 wt% and a slip/antiblock masterbatch at 1.0–2.0 wt% to control blocking during roll storage. The butene comonomer distribution of Flexus 9211, with a nominal melt flow rate of 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg and density of 0.918 g/cm³ under ASTM D792, provides dart impact retention in 100 µm liners with specified minimum ASTM D1709-16A Method A values of 250–600 g depending on fill mass and drop height. Compliance for FIBC liners is assessed under ISO 21898:2004, and sack drop performance is audited using ISO 7965-1:1984 with simulated fill loads of 25–50 kg; weld seam strength is tested to ISO 13953:2001. Processing on a three-layer blown film line with die diameter 250–450 mm, die gap 1.8–2.4 mm, blow-up ratio 2.2:1–2.8:1, and frost line height 500–700 mm from the die face stabilizes the bubble; a barrier screw with L/D 30:1 and barrel profile from 180 °C at the feed throat to 220 °C at the die is used, with die lip temperature variation maintained within ± 2 °C to avoid gauge bands. On high-output lines, melt temperatures above 240 °C increase gel formation and reduce dart impact; conversely, reducing Flexus 9211 below 70 wt% lowers tear propagation resistance below 300 gf under ASTM D1922-15 in the machine direction. Granulate stored in outdoor silos at relative humidity above 60% should be conveyed through hoppers maintained above 40 °C to avoid surface moisture transport into the feed throat. Terminal products include FIBC liners for hygroscopic resin shipment, fertilizer sacks, mineral and salt bags, and PE liners for corrugated octabins.
Addition ratios for silage bale wrap and greenhouse cover film are separated by cling and UV stabilization demands. In silage wrap, Flexus 9211 is limited to 55–70 wt% when coextruded with EVA at 15–25 wt%, tackifier masterbatch at 5–10 wt%, and UV stabilizer masterbatch at 3–6 wt%; exceeding 70 wt% lowers cling and decreases machine-direction elongation retention after 500 h of ASTM G154-16 UV-A 340 exposure at 0.76 W/m² and 340 nm below the 50% threshold required by EN 14932:2018. Greenhouse cover film, in contrast, uses 60–80 wt% Flexus 9211 with LDPE at 15–30 wt% and a hindered amine light stabilizer masterbatch at 5–10 wt%; film manufacturers validate weathering under EN 13206:2017 and report tensile strength retention under ISO 527-3 after xenon-arc aging. Extrusion on a three-layer blown film line with die gap 1.6–2.4 mm, blow-up ratio 2.5:1–3.0:1, and frost line height 700–900 mm is used because the EVA phase softens the bubble and increases blocking; cooling air at 10–18 °C and a polymer processing aid at 0.5–1.0 wt% reduce die lip deposit. Melt temperature at the die is restrained to 200–215 °C to avoid EVA decomposition and acetic acid corrosion on downstream collapsing frames; output per die circumference is typically 1.2–2.0 kg/h/mm. Terminal products include round bale silage wrap, greenhouse tunnel covers, temporary grain storage covers, and ensilage stretch film.
Because frozen-food form-fill-seal lines require seal initiation below 105 °C and hot-tack strength above 2.0 N/25 mm at 115 °C seal bar temperature, Braskem Flexus 9211 is blended into sealing layers at 30–50 wt%, with metallocene LLDPE at 40–60 wt% and anti-fog masterbatch at 2–4 wt%. The combination lowers apparent melt viscosity and stabilizes seal transfer through high-speed jaw cycles measured under ASTM F1921-18; seal strength after 0.5 s dwell is verified using ASTM F88/F88M-21. Food-contact compliance is governed by FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with overall migration not exceeding 10 mg/dm² in final structures validated for fatty and aqueous simulants; converter responsibility includes confirmation that slip and anti-fog additives meet positive lists. Production on a three-layer blown film line with die gap 1.2–1.8 mm, blow-up ratio 2.0:1–2.5:1, and die temperature 200–215 °C maintains low gel counts, with optical surface inspection rejecting gels above 200 µm; internal bubble cooling and layflat width control within ± 5 mm prevent registration drift during pouch conversion. Terminal products include frozen vegetable pillow pouches, frozen seafood lidding film, ice-pack film, and frozen bakery overwrap.
| Downstream application | Industry compliance standard | Test method or equipment | Numeric acceptance criterion |
|---|---|---|---|
| Heavy-duty FIBC liners and bulk sacks | ISO 21898:2004, ISO 7965-1:1984 | ISO 13953:2001 | Minimum dart drop 250–600 g at 100 µm; seam weld tested by sack type |
| Agricultural silage wrap and greenhouse film | EN 14932:2018, EN 13206:2017 | ASTM G154-16, ISO 527-3 | MD elongation retention above 50% after 500 h UV-A 340 |
| Frozen-food flexible packaging | FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 | ASTM F1921-18, ASTM F88/F88M-21 | Overall migration ≤ 10 mg/dm²; hot tack 2.0 N/25 mm at 115 °C |
| Surface protection and vapour retarder film | ASTM E1745-17 | ASTM E96/E96M-16, ASTM D4833-07 | Water vapour permeance ≤ 0.1 perms; puncture 150–300 N/mm at 200 µm |
| Collation shrink film | ASTM D2732-14 | Shrink tunnel at 135 °C | MD free shrink 15–25%; TD free shrink 20–35% |
| Liquid bag-in-box liners | FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011, REACH (EC) No 1907/2006 Article 33 | ASTM F392/F392M-21 | 500–1,000 Gelbo flex cycles at –20 °C |
| Stretch hood pallet unitisation | ISO 527-3, ASTM D5748-95(2019) | Automated stretch hood machine | Protrusion puncture 25–45 N at 80 µm; machine stretch 50–70% |
Film structures for temporary surface protection and below-slab vapour retarders are compounded with Flexus 9211 at 60–75 wt%, LDPE at 20–35 wt%, and a colour/UV masterbatch at 3–5 wt%. The puncture resistance of a 200 µm film is specified through ASTM D4833-07 with minimum index puncture values of 150–300 N/mm, while water vapour permeance under ASTM E96/E96M-16 is specified at ≤ 0.1 perms for vapour retarder applications conforming to ASTM E1745-17 Class A, B, or C. Processing at high gauge requires die gap 2.0–2.6 mm, blow-up ratio 1.8:1–2.2:1, and frost line height 300–500 mm to suppress excessive transverse orientation that would increase shrinkage on concrete surfaces; melt temperature is held at 215–230 °C, and output per die circumference is 1.5–2.5 kg/h/mm. Production records from surface-protection film lines show that reducing Flexus 9211 below 55 wt% produces edge tear during tape cutting and roll slitting, while increasing LDPE above 35 wt% reduces dart impact below job-site requirements. Terminal products include adhesive-backed temporary floor protection film, below-slab vapour retarders, masonry surface protection, and OEM appliance film.
During high-speed collation shrink packaging of beverage multipacks, Flexus 9211 is incorporated into the core layer at 25–40 wt%, with LDPE at 50–65 wt% and EVA at 10–15 wt% in skin layers. The film must achieve free shrink values of 15–25% in machine direction and 20–35% in transverse direction at 135 °C under ASTM D2732-14, with shrink force sufficient to hold 6–24 can multipacks without distortion; published data for this specific Flexus 9211 configuration is limited, so laboratory confirmation on the target shrink tunnel is required. Extrusion is performed on a single-bubble blown line with die gap 0.8–1.2 mm, blow-up ratio 3.0:1–4.0:1, and frost line 300–600 mm; the bubble is collapsed under low winding tension to preserve shrink curvature. Terminal products include printed shrink bundling film for beverage cans, bottled water multipacks, and canned food tray overwrap.
Liquid bag-in-box liner coextrusion uses Flexus 9211 at 60–80 wt% with LDPE at 20–30 wt% and anti-block masterbatch at 1–2 wt%; in three-layer structures, the core layer may contain 10–20 wt% metallocene LLDPE to raise flex-crack resistance. The specification for flex-crack durability is evaluated under ASTM F392/F392M-21 with 500–1,000 Gelbo flex cycles at –20 °C, and pinhole formation is counted after 200 cycles. Food-contact structures are controlled under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; industrial liquid liners outside food contact are assessed for chemical compatibility according to the liquid manufacturer’s immersion protocol. Under REACH Regulation (EC) No 1907/2006, Article 33 communication obligations apply when candidate list substances exceed 0.1 wt% w/w in the final article. Processing on a three-layer blown film line with die gap 1.5–2.0 mm, blow-up ratio 2.0:1–2.5:1, and die temperature 200–215 °C reduces pinhole density; melt temperature above 230 °C is avoided because it creates low-molecular-weight fractions that extract into acidic liquids. Terminal products include bag-in-box liners for wine, edible oil, liquid egg, and industrial adhesive intermediates.
In stretch hood pallet unitisation, Flexus 9211 is formulated at 70–85 wt% with metallocene LLDPE at 10–20 wt% and polyisobutylene tackifier masterbatch at 2–4 wt%. The film is stretched at 50–70% elongation on automated stretch hood machines; machine-direction tensile properties are measured under ISO 527-3, and protrusion puncture resistance is evaluated under ASTM D5748-95(2019) with a minimum protrusion puncture value of 25–45 N for 80 µm film. Processing uses a monolayer or two-layer blown line with die gap 2.0–3.0 mm, blow-up ratio 2.5:1–4.0:1, and frost line height 600–1,000 mm from the die face to develop axial orientation. Field failure on high-speed hood machines occurs as vertical tear propagation from film edge nicks; maintaining Flexus 9211 above 70 wt% and frost line above 600 mm reduces edge tear, while lowering melt temperature below 200 °C increases gels that initiate tear. Terminal products include stretch hood film for pallet loads of cement bags, glass containers, and appliance cartons.
Competitive Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer is a linear low density polyethylene resin formulated for blown film extrusion. The product is classified as a butene-1 copolymer and carries a nominal melt flow rate of 1.0 g/10 min when measured in accordance with ASTM D1238 or ISO 1133-1:2022 at 190 °C under a 2.16 kg load. The nominal density is 0.921 g/cm³ when determined in accordance with ASTM D1505 or ISO 1183-1. These two values position the product in the LLDPE range for thin-gauge film, where converters require a balance between extensibility, bubble stability, impact resistance, and drawdown. The base resin is supplied as pellets and is normally formulated with an antioxidant and process stabilizer package; slip, antiblock, and ultraviolet stabilizers are not included as standard and must be introduced by the converter through masterbatch addition. The product is typically processed into films between approximately 10 µm and 120 µm for industrial liners, heavy-duty shipping sacks, carrier bags, freezer film, agricultural films, and form-fill-seal packaging. The distinction between this resin and high-pressure LDPE at similar density is mainly molecular architecture: the butene-1 copolymer backbone is predominantly linear with short-chain branching, whereas high-pressure LDPE contains long-chain branching that alters melt rheology, optical behavior, and mechanical response.
The melt flow rate of 1.0 g/10 min is a specification intended to reduce the risk of melt fracture at commercial film shear rates while retaining sufficient molecular weight to maintain dart impact and tear resistance. The density of 0.921 g/cm³ separates the product from medium-density film grades near 0.926 g/cm³ to 0.940 g/cm³, which exhibit higher stiffness but generally lower dart impact and tear at equivalent thickness. Lot-specific values for melt index and density may vary within Braskem specification ranges, and the certificate of analysis should be reviewed before final process setup. Published technical datasheet values for Flexus 9211 should be used for detailed film property comparisons because blown film mechanical performance is influenced by die gap, blow-up ratio, frost line height, melt temperature, and gauge control, not merely by resin density and melt flow rate.
The molecular architecture of Braskem Flexus 9211 produces a shear-viscosity response that differs from high-pressure LDPE. High-pressure LDPE contains long-chain branches that increase low-shear viscosity, enhance shear thinning, and stabilize the bubble at high draw ratios, but long-chain branching also reduces tensile strength and tear propagation resistance at a given density. Flexus 9211, as a butene-1 LLDPE, has a predominantly linear backbone and short-chain branches at comonomer positions. This configuration generally contributes to higher tensile strength, higher dart impact, and higher puncture resistance relative to high-pressure LDPE at equivalent thickness. The resin also typically demonstrates improved resistance to environmental stress cracking, which is relevant for agricultural films and industrial liners exposed to surfactants or soil chemicals. However, the linear backbone provides lower melt strength than high-pressure LDPE, so bubble stability and gauge uniformity can become limiting if the process is not adjusted.
Compared with metallocene-catalyzed LLDPE grades at equivalent density and melt index, Flexus 9211 is characterized by a broader molecular weight distribution and a more heterogeneous comonomer distribution. This generally provides higher low-shear viscosity and greater melt strength, which can improve bubble stability on conventional low-pressure die systems. Metallocene LLDPE grades often exhibit superior optical properties and lower seal initiation because of a narrower comonomer distribution, but their narrower molecular weight distribution can increase pressure and torque sensitivity during direct substitution. In contrast, high-pressure LDPE is frequently added to Flexus 9211 at controlled levels to improve bubble stability and optical clarity, but the addition reduces dart impact and machine-direction tear. Material selection therefore cannot be reduced to a single density or melt index comparison; the branching architecture and molecular weight distribution must be considered against the film property targets measured under ASTM D882, ASTM D1709, and ASTM D1922.
On a monolayer blown film line equipped with a grooved-feed extruder having an L/D ratio between 25:1 and 30:1, Flexus 9211 is normally processed at melt temperatures from 180 °C to 220 °C. The die gap is commonly set between 1.5 mm and 2.5 mm for thin-gauge film, with wider gaps generally preferred when melt pressure and melt fracture become limiting. A blow-up ratio of 2.0:1 to 3.0:1 and a frost line height of 2 to 4 die diameters are used to control bubble geometry and orientation. At the same melt temperature, Flexus 9211 can generate higher extruder torque and die pressure than high-pressure LDPE at equivalent output because of its linear molecular architecture. Operators should avoid abrupt reductions in die temperature because LLDPE solidification across the frost line is sharper than high-pressure LDPE, and uneven frost line movement can produce gauge variation. External or internal bubble cooling, stable air ring settings, and consistent melt temperature are critical for maintaining thickness uniformity in films below 25 µm.
At high shear rates, LLDPE can exhibit sharkskin melt fracture at the die lip. In production, fluoropolymer-based polymer processing aids are commonly used at concentrations from 200 ppm to 800 ppm to delay melt fracture and reduce die deposit. The exact addition level should be determined by measuring melt pressure and film surface roughness on the target line. Published data for this specific configuration is limited, so converter trials are required to establish the minimum effective processing aid concentration. Purging with a low-density polyethylene or a commercial LLDPE-compatible purging compound is recommended when transitioning from high-clarity LDPE; residual LDPE may temporarily reduce haze but generally does not harm film strength. The lower melt strength of LLDPE relative to LDPE may require a reduction in drawdown speed or a slight increase in blow-up ratio to maintain bubble stability.
Mechanical film properties are evaluated after conditioning at 23 °C ± 2 °C and 50% ± 5% RH according to standard practice. Tensile strength, elongation at break, and modulus are measured under ASTM D882 or ISO 527-3; dart drop impact is measured under ASTM D1709; Elmendorf tear is measured under ASTM D1922; haze and luminous transmittance are measured under ASTM D1003; specular gloss is measured under ASTM D2457; and coefficient of friction is measured under ASTM D1894. Braskem technical data for Flexus 9211 should be consulted for typical values, but the resin class is generally positioned to deliver high dart impact and balanced machine-direction and transverse-direction tear relative to the density. A film produced from a 0.921 g/cm³ butene-1 LLDPE typically shows lower tensile modulus than a film from a 0.926 g/cm³ LLDPE, while the lower density favors higher dart impact and improved low-temperature flexibility. In contrast, high-pressure LDPE at a similar density usually exhibits lower tensile strength and puncture resistance, better optical properties, and easier bubble handling.
The relationship between die gap and tear balance is particularly important for this resin class. Narrow die gaps increase shear rates and can improve optical properties, but they may elevate die pressure and reduce the melt residence time needed to fully relax orientation in the machine direction. Wider die gaps tend to shift tear resistance into a more balanced configuration but may reduce bubble stability if melt strength is insufficient. Similarly, increasing the blow-up ratio generally increases transverse-direction orientation and transverse-direction tear, while decreasing machine-direction tear. A blow-up ratio between 2.0:1 and 3.0:1 is commonly used to obtain acceptable mechanical balance in heavy-duty bag films. These effects must be quantified on the specific film line because the final gauge profile, frost line heat transfer, and bubble cooling rate influence the crystalline orientation and subsequent mechanical properties measured under ASTM D882 and ASTM D1922.
In heavy-duty bag and industrial liner applications, the product is typically converted at film thicknesses from 50 µm to 120 µm, where puncture resistance and tear propagation under load are more critical than optical clarity. The density of 0.921 g/cm³ provides a lower crystalline fraction than a 0.926 g/cm³ film resin, reducing stiffness in cold environments and improving low-temperature flexibility. For agricultural films and silage covers, resistance to environmental stress cracking and long-term retention of mechanical properties when compounded with carbon black or hindered amine light stabilizer masterbatches are selection factors; the base resin is not UV-stabilized and must be modified for outdoor service. In frozen food packaging, low-temperature dart impact and seal integrity at refrigerated storage temperatures are evaluated before replacing LDPE-rich blends with Flexus 9211. Industrial liners intended for liquids or fine powders may require evaluation of creep resistance under load, which is influenced by density, film thickness, and winding tension.
When replacing high-pressure LDPE in a formulation, converters often begin by substituting 20% to 30% of the LDPE with Flexus 9211 and then increase the LLDPE fraction based on dart impact and tear results. The lower long-chain branching of Flexus 9211 reduces melt strength, so bubble instability may appear at high LLDPE content unless die gap and blow-up ratio are adjusted. Compared with a metallocene-catalyzed LLDPE with the same melt index, Flexus 9211 often provides greater melt strength and easier operation on conventional lines, but film clarity may be inferior. Compared with a higher-density LLDPE at 0.926 g/cm³, Flexus 9211 typically yields lower tensile modulus and higher dart impact. These differences are not qualitative defects; they define the application space in which Flexus 9211 is technically appropriate.
In form-fill-seal and lamination applications, heat-seal strength and hot-tack performance are evaluated according to ASTM F88 and ASTM F1921. Because Flexus 9211 has a linear backbone and a density of 0.921 g/cm³, its seal initiation temperature is typically higher than that of high-pressure LDPE but lower than that of medium-density LLDPE. Seal strength in the plateau region is generally higher than that of high-pressure LDPE at equivalent film thickness, which permits downgauging of the sealant layer. However, the optimum sealing bar temperature depends on the thermal conductivity of the film structure, dwell time, and jaw pressure; a temperature range of 110 °C to 140 °C is often used as a starting point but must be validated on the specific packaging line. Hot tack is particularly important in vertical form-fill-seal operations, where the molten seal must support product weight immediately after sealing; butene-based LLDPE generally shows adequate hot tack but may not match metallocene-based sealants in very fast cycling at low seal temperatures.
Stiffness-sensitive applications such as stand-up pouches, freezer bags, or heavy fill spouts may require blending with high-density polyethylene or a higher-density LLDPE. Addition of high-density polyethylene increases modulus and heat resistance but reduces dart impact and tear. Blending Flexus 9211 with high-pressure LDPE improves optics and bubble stability but reduces tensile yield and increases seal initiation. The correct blend ratio is determined by testing film properties according to ASTM D882, ASTM D1709, and ASTM D1922, rather than by nominal resin properties alone. For coextruded structures, Flexus 9211 may serve as a core or sealant layer in combination with high-pressure LDPE skins for surface properties, or with a higher-density LLDPE for stiffness and downgauging. The selection of layer distribution should consider melt flow matching across the die gap; mismatched viscosities can lead to interfacial instability and gauge variations in the finished web.
For food-contact applications, polyethylene grades such as Flexus 9211 are typically evaluated under FDA 21 CFR 177.1520, which lists olefin polymers and associated specifications. The resin should be used only after confirmation that the specific monograph conditions, including the food type and temperature, are met. The product may also be assessed under EU Regulation No 10/2011 for plastic materials intended to come into contact with food, with compliance demonstrated through migration testing as required by the final packaging structure. Under REACH Regulation (EC) No 1907/2006, the substance is registered and no intentional SVHC addition is expected above 0.1% w/w per article. Electrical and electronic equipment packaging is not within the scope of RoHS, but if a RoHS declaration is requested, Directive 2011/65/EU restrictions on lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE apply.
| Regulation / standard | Designation | Typical assessment parameter |
|---|---|---|
| FDA food contact | 21 CFR 177.1520 | Olefin polymer specification; density and extractables limits depending on use condition |
| EU plastics regulation | EU Regulation No 10/2011 | Overall migration and specific migration limits; positive list entries for monomers and additives |
| REACH | Regulation (EC) No 1907/2006 | Registration dossier; SVHC content not above 0.1% w/w |
| RoHS | Directive 2011/65/EU | Lead, mercury, cadmium, hexavalent chromium, PBB, PBDE thresholds |
The resin is not supplied with slip or antiblock additives, so blocking may occur if film is wound at high tension or stored at elevated temperature. Pre-drying is not normally required when the material is stored under clean, dry conditions with relative humidity below 60%. If storage humidity exceeds 60% RH, surface moisture can contribute to bubble instability and surface defects; pre-drying in a hopper dryer at 60 °C to 80 °C for 2 h to 4 h may be required. Thermal degradation may occur if melt temperature exceeds 260 °C, with odor, gel formation, and discoloration as indicators. Direct contact with strong oxidizing agents or strong mineral acids is not recommended for continuous service because polyethylene is not resistant to all aggressive chemical environments. For high-clarity shrink film, Flexus 9211 is not the preferred candidate when optical performance is the dominant requirement; high-pressure LDPE or metallocene LLDPE typically yields lower haze and higher gloss.