| HS Code | 421131 |
| Density | 0.921 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 98 °C |
| Tensile Strength At Yield Md | 10.5 MPa |
| Tensile Strength At Yield Td | 10.5 MPa |
| Tensile Strength At Break Md | 38 MPa |
| Tensile Strength At Break Td | 32 MPa |
| Elongation At Break Md | 500 % |
| Elongation At Break Td | 700 % |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Md | 250 g |
| Elmendorf Tear Td | 350 g |
| Haze | 7 % |
| Gloss 45 | 75 |
| Seal Initiation Temperature | 100 °C |
| Coefficient Of Friction | 0.15 |
As an accredited Braskem Flexus® 9210 LLDPE Blown Film Extrusion factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem Flexus® 9210 LLDPE blown film extrusion resin: typically packaged in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg). |
| Container Loading (20′ FCL) | 20′ FCL loading for Braskem Flexus® 9210 LLDPE Blown Film Extrusion: palletized 25 kg bags, floor-loaded, moisture-protected, secured for export. |
| Shipping | Braskem Flexus® 9210 LLDPE Blown Film Extrusion resin is supplied as solid pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. It is non-hazardous for transport. Store in a cool, dry, sealed area away from sunlight, heat, and ignition sources. Follow local regulations. |
| Storage | Store Braskem Flexus® 9210 LLDPE Blown Film Extrusion resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep sealed in original packaging on pallets, off the floor. Avoid contamination by oils, chemicals, or strong odors. Use first-in, first-out rotation. Maintain moderate ambient temperatures and protect from UV exposure. |
| Shelf Life | Braskem Flexus® 9210 LLDPE Blown Film Extrusion typically has 12 months shelf life when stored unopened, dry, at moderate temperatures. |
Flexus 9210 is a blown-film extrusion LLDPE with a nominal density of 0.921 g/cm³ and a melt flow rate near 1.0 g/10 min determined under ISO 1133-1:2022 at 190 °C/2.16 kg. In heavy-duty sack manufacture for fertilizer, polymer chip, and construction aggregate, the grade is converted at thicknesses between 80 µm and 200 µm, where high dart impact and low-temperature tear resistance determine field performance. On high-stalk lines, the bubble is operated at a blow-up ratio of 2.5:1–3.2:1 with a die gap of 2.0–2.5 mm and a frost line height of 8–10 die diameters; this geometry increases machine-direction tear propagation resistance without sacrificing dart drop resistance measured under ASTM D1709-15. Barrel temperatures are typically profiled from 170 °C to 205 °C, with melt temperature at the die between 205 °C and 220 °C. Since the resin has higher shear viscosity than LDPE, extruder drive loads on 30:1 L/D grooved-feed units can be 10–18% higher, and melt pressure before the screen changer should be monitored to avoid exceeding the breaker-plate rating.
When sacks are filled at rates above 600 bags/h, coefficient of friction and heat seal strength become mandatory secondary parameters. A typical formulation is 80–90 wt% Flexus 9210 with 10–20 wt% LDPE film resin to lower gauge variation at high output, plus 0.3–0.8 wt% slip/antiblock masterbatch if the sack enters vertical form-fill-seal equipment. For outdoor chemical sacks, 2–4 wt% carbon black masterbatch with a UV-stabilized carrier is used; the film must retain impact strength after UV exposure when tested by ISO 527-3 and ISO 6383-2. The main failure mode observed on sack lines is bubble instability at the die lip when die gap is reduced below 2.0 mm, leading to gauge bands that become side-seal weak points. Pre-drying is not required for the LLDPE itself, but if granulate is stored at relative humidity above 80%, surface condensation can cause film defects; hopper heating at 60 °C for 2 h is a common preventive measure. Published data for this specific grade under dangerous-goods sack certification drop tests is limited; converter validation should be conducted on filled sacks rather than on film specimens.
Agricultural silage and bale-wrap film is converted at 25–70 µm thickness, where oxygen transmission and puncture failure at folded silo corners create a process-property conflict. The film requires enough extensional stress at the frost line to orient the LLDPE chains in both directions, but over-orientation increases oxygen transmission through microvoiding; converters therefore hold blow-up ratio between 2.0:1 and 2.8:1, with a die gap of 1.8–2.3 mm. Because the film must cling to itself on round bales, a cling agent such as polyisobutylene or an EMA blend at 2–6 wt% is commonly added; this additive reduces the surface energy of the film and lowers blocking between layers during storage. At -20 °C, the silage film must still withstand puncture from corn stalks and frozen stems; retained puncture resistance is evaluated using ASTM D5748-19, while oxygen transmission rate is measured by ASTM D3985-05 at 23 °C/0% RH.
The compliance position of an agricultural silage film is defined by EN 13207-1:2001, which sets requirements for mechanical properties, weathering, and oxygen permeability. Because EN 13207-1:2001 does not replace the converter's internal silo-bag test, field evaluations on commercial baling machines with a target stretch of 50–70% are required to detect neck-in and clamp tears. UV stabilization for 12–24 month outdoor exposure requires a HALS package at 0.3–0.6 wt% plus a benzotriazole UV absorber at 0.1–0.3 wt%; under-loaded film will lose dart impact after 400 h of accelerated weathering and can split during bale ejection. On a 70 mm single-screw extruder with 28:1 L/D, the practical output range for this application is commonly 90–140 kg/h depending on frost line cooling; above this range, sharkskin may appear unless 200–500 ppm fluoropolymer processing aid is added. The main incompatibility is with high levels of inorganic antiblock: loadings above 2 wt% silica will raise oxygen permeability and create stress concentrators at the silo corner.
In blown stretch-film production, cling force after migration of a low-molecular-weight tackifier is the controlling property, and the level must be measured after 24 h at 23 °C/50% RH rather than immediately after winding. Flexus 9210 is processed at 15–35 µm gauge with a blow-up ratio of 2.5:1–3.5:1 and a die gap of 2.0–2.5 mm; the high blow-up ratio increases transverse stretch but reduces ultimate machine-direction elongation, so pallet load stability is specified as a combination of cling strength, puncture resistance, and stretch force at 200% elongation. A blown stretch grade typically requires 0.5–2.0 wt% tackifier masterbatch, often polyisobutylene in a compatible LLDPE carrier, while slip additive is limited to 0.2–0.5 wt% because slip erosion reduces cling after 7 days of warehouse storage. Compliance testing for blown stretch wrap includes ASTM D5458-95 for cling, ASTM D5748-19 for puncture resistance, and ASTM D882-18 for tensile elongation; pre-stretch equipment on the pallet wrapping station is set at 60–90% for low-speed and 150–250% for high-speed rotary arms.
Compared with cast film produced on chill-roll lines, blown stretch film has higher puncture resistance but lower machine-direction tear propagation; this is not a defect but a performance boundary. Published data for Flexus 9210 under cast and blown monoextrusion is limited; converter trials on a 65 mm grooved-feed blown-film extruder with 28:1 L/D have shown that output rates above 120 kg/h require a fluoropolymer processing aid at 200–500 ppm to suppress sharkskin at the die lip. The operational boundary is additive bloom: if tackifier loading exceeds 2.0 wt%, cling increases initially but the film blocks on the reel after storage above 40 °C. The winding tension must also be reduced as film gauge decreases below 20 µm because stretched film wound at high tension can lose cling through surface flattening.
Frozen food packaging films place hot tack above ultimate seal strength because vertical form-fill-seal lines transfer product while the seal is still partially molten. Flexus 9210 can serve as the sealant web in coextrusions at 30–70 µm total thickness when blended with 10–20 wt% LDPE or plastomer; the blend lowers seal initiation temperature and widens the hot tack window. The sealant layer is extruded at melt temperatures of 195–215 °C, with a die gap of 1.8–2.2 mm and a blow-up ratio of 2.2:1–2.8:1, because stable neck geometry at the frost line controls gauge variation that would otherwise shift the seal initiation point. Hot tack is measured under ASTM F1921-20 and seal strength under ASTM F88-21 after a dwell time of 0.5 s and seal pressure of 0.4 MPa; general butene-LLDPE seal initiation falls between 95 °C and 115 °C, but published data specific to Flexus 9210 under production-scale sealing conditions is limited.
For direct food contact, the sealant layer must comply with FDA 21 CFR 177.1520 and EU 10/2011, including overall migration below 10 mg/dm² for the intended food simulant; specific migration of slip additives is controlled through additive masterbatch selection. At frozen storage conditions of -20 °C to -40 °C, flex-crack resistance is assessed using the Gelbo test method ASTM F392-07 with 10 cycles and pinhole count as the failure criterion. The main boundary condition is moisture condensation: if film is taken from a cold warehouse into a humid packaging hall above 80% RH, surface moisture can destabilize the bubble during extrusion and create gels that increase seal failures; pre-drying is not required for the LLDPE itself, but granulate storage should stay below 60% RH to avoid surface condensation in the hopper. In addition, screw speed should be kept below the point where melt temperature exceeds 220 °C, because oxidative degradation shifts the seal initiation temperature upward and narrows the hot tack window.
For stand-up pouch sealant webs, the useful processing window is defined by corona treatment retention through the lamination nip and not by the film's tensile properties alone. Flexus 9210 is extruded at 20–40 µm as a monolayer or coextruded sealant film, then corona treated in-line to a surface energy of 38–42 mN/m measured by ASTM D2578-17 with formamide/ethylene glycol monoethyl ether test fluids. The bubble is held at a blow-up ratio of 2.0:1–2.5:1 and a die gap of 1.8–2.2 mm; excessive oxidation from corona dosage above 4.0 kW on a 1.2 m web can create low-molecular-weight oxidized species that reduce solventless polyurethane lamination bond strength measured by ASTM F904-16 after 48 h cure at 25 °C. In a typical PET/adhesive/LLDPE structure, the sealant layer is the interface that controls seal-through-contamination performance for liquid detergents and dry foods; the film must be sealed through dust without losing hermetic seal integrity.
Regulatory compliance for food-contact lamination is governed by EC 1935/2004 for the finished article and EU 10/2011 for migration limits; for the US market, FDA 21 CFR 177.1520 applies to the polyethylene sealant web, and any added slip/antiblock masterbatch must have its own food-contact status. REACH compliance requires confirmation that no SVHC above 0.1 wt% is present in the film or its masterbatch. The main operational boundary is additive bloom: excessive erucamide slip in the sealant web can migrate to the adhesive interface and lower bond strength after 72 h; hence the slip level is typically capped at 800–1500 ppm for lamination grades, while antiblock at 2000–4000 ppm may be needed to prevent blocking on the wound reel. Interchangeable use in high-speed horizontal form-fill-seal lines requires seal strength above 10 N/15 mm when tested by ASTM F88-21; below this value, pouch failures occur at the gusset fold during hot filling.
Below 100 µm, vapour barrier film is rejected on construction sites by puncture and tear during backfill; thus, underslab vapour retarders are converted from Flexus 9210 at 100–250 µm thickness, where the formulation may include 2–4 wt% carbon black masterbatch for UV resistance during a limited outdoor exposure before concrete pour. The process uses a die gap of 2.5–3.0 mm and a blow-up ratio of 2.0:1–2.5:1, with melt temperature held at 200–215 °C to avoid excessive bubble instability at high gauge. Water vapour permeance is measured by ASTM E96/E96M-20 at 23 °C/50% RH, and the material is likely to meet a maximum permeance of 0.1 perm when the thickness exceeds 150 µm; however, published permeance data for this specific grade is limited, and the value must be confirmed per project specification.
The installed film must satisfy ASTM E1745-11 for flexible water vapor retarders used in contact with soil or granular fill, including tensile strength, puncture resistance, and permeance after wetting. Internal bubble cooling is often used above 200 µm; it improves output but may introduce haze that does not affect the functional performance of the vapour retarder. As a boundary condition, surface rusting on steel decks or alkaline concrete contact does not degrade polyethylene film but can cause slip in the field; therefore, the film is supplied with a textured surface or a friction-enhancing additive to maintain walkability. The principal incompatibility is with long-term UV exposure: unstabilized or under-stabilized Flexus 9210 film will embrittle after 30–60 days outdoors, so construction schedules that leave the vapour retarder exposed for longer periods require a separate UV-stabilized masterbatch or an immediate concrete cover. Tensile properties are reported according to ISO 527-3 and ASTM D882-18, and puncture is characterized by ASTM D5748-19.
Competitive Braskem Flexus® 9210 LLDPE Blown Film Extrusion prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Flexus® 9210 is a linear low-density polyethylene resin formulated for blown film extrusion. The product’s nominal density is 0.921 g/cm³ when tested under ASTM D1505, and its nominal melt flow rate is 1.0 g/10 min when tested under ASTM D1238 at 190 °C with a 2.16 kg load. The material is supplied as a butene-based LLDPE, a structural assignment that places it between conventional low-density polyethylene and higher-alpha-olefin linear low-density grades in melt relaxation and solid-state orientation behavior. Density and melt flow rate are the primary product specification values; additive and stabilizer concentrations are proprietary and should be confirmed with the current supplier datasheet. Primary conversion occurs on single-screw blown film lines with 25:1 to 30:1 L/D extruders, typically producing monolayer and coextruded films in the 25 µm to 125 µm thickness range. Film properties should be interpreted as gauge-dependent values; standardized film preparation and conditioning are required before comparing supplier literature to plant results. The grade is used in heavy-duty sacks, industrial liners, agricultural film, and bag-in-box structures. The 0.921 g/cm³ density reduces flexural modulus relative to high-density polyethylene, which can improve tear and puncture resistance as measured by ASTM D1709 and ASTM D1922 but lowers tensile stiffness as measured by ASTM D882. Those trade-offs are examined in the following sections.
Bubble stability in Flexus 9210 conversion is governed by melt temperature, die gap, blow-up ratio, frost line height, and air ring configuration. On production lines using 80 mm single-screw extruders with 30:1 L/D and low-work barrier screws, typical melt set points range from 190 °C to 220 °C. Below 185 °C, unmelted pellets and elevated melt viscosity produce bubble nonuniformity; above 230 °C, oxidative chain scission can reduce melt strength and cause bubble sag. The die gap is normally set between 1.8 mm and 2.5 mm. An undersized die gap raises shear stress and can initiate melt fracture at elevated output, while an oversized gap reduces molecular orientation and may lower film tensile properties under ASTM D882.
Blow-up ratios are typically maintained between 2.0:1 and 3.0:1. Blow-up ratios above 3.5:1 reduce bubble process latitude and increase transverse-direction gauge variation. Frost line height is generally managed at 4 to 8 die diameters; frost line positions greater than 10 die diameters raise machine-direction orientation and may reduce transverse-direction Elmendorf tear as measured under ASTM D1922. The grade’s melt flow rate of 1.0 g/10 min provides moderate shear viscosity, and bubble pressure is generally lower than for high-molecular-weight HDPE. Internal bubble cooling is usually unnecessary below 60 µm but may be used above 100 µm to improve output. Published rheograms for this specific grade are limited; commercial butene-copolymer LLDPE resins with comparable melt index typically show a power-law index from 0.55 to 0.65 at 190 °C. Operators should not transfer process settings from a metallocene LLDPE without rebalancing the air ring because melt strength and shear-thinning profiles differ measurably.
Thermal transitions also set process limits. LLDPE of 0.921 g/cm³ density typically exhibits a differential scanning calorimetry melting peak between 120 °C and 124 °C, although additive nucleation and cooling rate can shift the measured value. The extruder feed zone should remain below 80 °C to avoid premature pellet sticking and feed-throat bridging; zones after the compression section are normally profiled from 160 °C to 220 °C. Screen pack pressure and melt temperature should be monitored during long runs because degradation of slip or anti-block additives can raise die lip deposits and create gauge bands. Production lines with oscillating haul-off and reverse-wind film towers reduce gauge band repeat periods that originate from die lip inhomogeneity.
Film property testing for Flexus 9210 uses standard polyolefin film preparation and conditioning. Tensile properties are reported under ASTM D882 after conditioning at 23 °C ± 2 °C and 50% ± 5% relative humidity. Dart impact is tested under ASTM D1709 Method A with a 38.1 mm hemispherical dart; Elmendorf tear is tested under ASTM D1922. Optical haze is tested under ASTM D1003, and gloss is tested at 45° under ASTM D2457. Because film properties shift with gauge, blow-up ratio, and frost line height, single-point literature values are not product release limits. The density of 0.921 g/cm³ places the grade in the lower-modulus region of LLDPE film resins; stiffness is lower than a 0.940 g/cm³ grade and higher than a 0.910 g/cm³ plastomer.
| Property | Test method | Unit | Nominal value or basis |
|---|---|---|---|
| Density | ASTM D1505 | g/cm³ | 0.921 |
| Melt flow rate | ASTM D1238 | g/10 min | 1.0 at 190 °C/2.16 kg |
| Dart impact | ASTM D1709 Method A | g | Gauge-dependent; consult current datasheet |
| Elmendorf tear | ASTM D1922 | gf | Orientation-dependent |
| Tensile strength at break | ASTM D882 | MPa | Film thickness and BUR dependent |
| Haze | ASTM D1003 | % | Gauge-dependent |
| Gloss 45° | ASTM D2457 | — | Gauge-dependent |
For heavy-duty sack downgauging, dart impact under ASTM D1709 is often the controlling metric. A film at 100 µm may be downgauged to 90 µm only after production trials demonstrate equivalent or acceptable dart impact and tear retention on the intended line. The difference between machine-direction and transverse-direction tear strength reflects orientation balance; higher blow-up ratios typically reduce the MD/TD tensile differential measured under ASTM D882 but can increase haze measured under ASTM D1003. The final product specification should therefore be based on a statistically valid set of production samples, not on a single datasheet value.
Haze and gloss are strongly affected by die line roughness and frost line position. A high frost line can reduce surface quenching and increase crystallinity at the outer surface, raising haze under ASTM D1003. The same film construction tested at 1.8 mm and 2.5 mm die gaps can produce different optical values even at equal blow-up ratio because shear history changes surface morphology. This is why ASTM D1003 and ASTM D2457 values from laboratory cast film cannot be extrapolated to production blown film.
Substitution of a 0.918 g/cm³ butene LLDPE with Flexus 9210 increases density by 0.003 g/cm³, which can raise secant modulus by a measurable but small amount under ASTM D882. The change may reduce low-temperature puncture resistance slightly because the higher-density crystalline fraction can increase stiffness and lower ductility at subzero temperatures. However, the grade’s melt flow rate of 1.0 g/10 min supports lower extruder head pressure than a 0.75 g/10 min heavy-duty film resin and can improve output on fixed-speed lines. Processors comparing Flexus 9210 with a lower-MI resin often record motor load and melt temperature on 90 mm extruders with 30:1 L/D. At a fixed screw speed and die set, the 1.0 g/10 min melt flow rate is expected to reduce head pressure relative to a 0.75 g/10 min grade, but the magnitude depends on screw design and should not be extrapolated without a trial. Published data for this specific configuration is limited.
Compared with metallocene-based LLDPE, Flexus 9210 generally exhibits a broader molecular weight distribution and lower puncture resistance in thin-gauge film. Metallocene grades often provide higher dart impact under ASTM D1709 and improved optical clarity at the same density, but they may require higher extruder torque and more aggressive air ring adjustment due to lower melt strength. Flexus 9210 is therefore selected when drawdown and bubble stability are more important than maximum optical clarity. It is not intended for high-clarity applications; butene-copolymer films typically show haze above 10% under ASTM D1003, and if the specification requires haze below 8%, a metallocene or higher-alpha-olefin LLDPE should be evaluated. Relative to high-density film grades, the 0.921 g/cm³ density provides higher Elmendorf tear and dart impact but lower yield strength and tensile modulus.
In heavy-duty sack structures, the grade can be used as a core layer or in monolayer sacks where tape or woven fabric is not needed. Coextruded structures with an HDPE outer layer can add stiffness while the Flexus 9210 layer contributes tear resistance. The replacement of a lower-MI LLDPE with Flexus 9210 may alter bubble diameter because melt viscosity is lower; operators should reset the die adapter temperature and lower the nip speed slightly to maintain the same web tension. In multilayer lines, the grade’s rheology should be matched with the skin layer polymer to avoid interfacial instability, especially when coextruding with nylon or EVOH barrier layers; maleated tie layers are required for adhesive bonding to polar layers.
Food-contact suitability of Flexus 9210 must be confirmed by a current supplier compliance letter. The olefin base polymer may fall under FDA 21 CFR 177.1520, but the final film is subject to end-use extraction and migration limits under 21 CFR 176.170 and 21 CFR 177.1520. The exact conditions of use—food type, temperature, contact time, and film layer position—determine whether the film meets U.S. regulatory requirements. For EU applications, Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food applies, and specific migration limits for the additive package must be verified using the appropriate food simulants. Industrial films placed on the EU market are evaluated under REACH Regulation (EC) No 1907/2006; as a polymer article, REACH registration generally does not apply to the polymer itself, but substances of very high concern in the additive package must be below threshold concentrations. RoHS Directive 2011/65/EU restrictions apply only if the film is incorporated into electrical and electronic equipment; general packaging and agricultural film are outside its primary scope.
| Requirement | Reference | Verification basis |
|---|---|---|
| U.S. food-contact olefin polymer | FDA 21 CFR 177.1520 | Supplier compliance letter |
| U.S. food-contact article | 21 CFR 176.170 | End-use migration testing |
| EU food-contact plastic | Regulation (EU) No 10/2011 | Specific migration testing |
| EU chemical regulation | Regulation (EC) No 1907/2006 | Supplier declaration; SVHC check |
| RoHS hazardous substances | Directive 2011/65/EU | Supplier declaration if applicable |
Because polymer additives, including slip and anti-block agents, can affect regulatory status, processors should not rely on the base-resin classification alone. A change in color concentrate, processing aid, or regrind source must be re-evaluated under the same migration framework. For industrial non-food applications, a supplier REACH and RoHS declaration is normally sufficient, but converters should retain documentation in accordance with their quality management system. If the film is sold into food service, non-intentionally added substances from processing aids and printing inks must also be considered under EU good manufacturing practice for food-contact materials.
Resin handling should control surface moisture uptake. Although polyolefins do not require predrying at relative humidity below 60%, condensation from cold pellets entering a warm silo can introduce surface moisture, producing splay and bubble defects. Incoming lots should be checked for melt flow rate and density against the certificate of analysis to monitor batch-to-batch variance. Storage is recommended as first-in-first-out in a dry silo at ambient temperature. Avoid extended direct sunlight exposure to reduce oxidation of the stabilizer package. Blends with post-consumer recycled LLDPE must be validated at the target addition level because recycled melt flow variability and contamination can destabilize the bubble. At recycled content above 20%, dart impact and Elmendorf tear should be retested under ASTM D1709 and ASTM D1922, and the coefficient of friction should be checked under ASTM D1894 if slip-agent bloom is disturbed. Avoid masterbatch carriers based on incompatible polymers that can form gel particles and reduce film quality. If the film will contact aggressive surfactants or solvents, environmental stress crack resistance should be tested under ASTM D1693 using the relevant environment. Shrinkage and oxidative stability can be evaluated by ASTM D2732 and ASTM D5510 when the application requires thermal aging data. No post-annealing is required after extrusion, and the film can be converted immediately after cooling.
During production, recurring bubble marks can originate from blocked air-ring lips, while die lines are commonly traced to oxidized resin stagnation at the die lip or to filler agglomeration. Gauge bands with a period equal to the haul-off circumference indicate eccentric nip roll pressure rather than melt fracture. Such mechanical signatures should be separated from resin-related defects before adjusting the polymer grade. If a masterbatch or recycled blend is introduced, the film should be screened at startup for gel counts under internal optical inspection because gel formation is not captured by standard melt flow testing.