Braskem Flexus 7200 Lldpe Cast Film Extrusion

Braskem Flexus® 7200 LLDPE Cast Film Extrusion

    • Product Name: Braskem Flexus® 7200 LLDPE Cast Film Extrusion
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 303137
    Polymer Type Linear Low-Density Polyethylene (LLDPE)
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 3.5 g/10 min
    Melting Temperature 122 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 800 %
    Flexural Modulus 220 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 4 %
    Gloss 45 80 %
    Coefficient Of Friction 0.20

    As an accredited Braskem Flexus® 7200 LLDPE Cast Film Extrusion factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Flexus® 7200 LLDPE Cast Film Extrusion comes in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg total).
    Container Loading (20′ FCL) 20′ FCL container loaded with Braskem Flexus® 7200 LLDPE, palletized and secured for cast film extrusion, ensuring safe, efficient transport.
    Shipping Braskem Flexus® 7200 LLDPE Cast Film Extrusion is shipped as non-hazardous, free-flowing pellets. Typical packaging includes 25 kg polyethylene bags, 500–1000 kg octabins, or bulk trucks/railcars. No special transport classification; follow local regulations. Store sealed in a cool, dry, well-ventilated area, away from sunlight, heat, and contamination.
    Storage Store Braskem Flexus® 7200 LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and strong odors. Keep original packaging sealed, clean, and undamaged on pallets. Avoid contact with chemicals, dust, or water. Stack safely to prevent deformation. Rotate stock using FIFO. Follow supplier guidelines for safe storage.
    Shelf Life Shelf life: 24 months from production date when stored unopened in original packaging, cool, dry, away from direct sunlight.
    Application of Braskem Flexus® 7200 LLDPE Cast Film Extrusion

    Published grade-specific data for Braskem Flexus 7200 are limited beyond nominal cast-extrusion design intent; the ranges below are drawn from C6/C8 LLDPE cast film production practice and are presented as boundary conditions rather than product guarantees.

    Pallet unitization on high-speed cast film lines is first constrained by the melt curtain geometry formed at a die gap of 0.8–1.2 mm and the subsequent draw ratio before contact with a chilled, polished roll. The web is typically quenched at 15–22°C to suppress crystallinity gradients that raise haze under ASTM D1003 above 2.0–3.5% for a 15–23 µm machine film. On a three-layer A/B/C structure with a 2.5 m coat-hanger die and a 60:1 draw ratio, neck-in reduces usable width by 7–15% unless an air knife or vacuum box maintains pinning. The central core layer is often blended with recycled edge trim and post-industrial reclaim at 10–20 wt%; inclusion beyond that threshold is associated with gel-induced dart impact failures under ASTM D1709 dropping below 150 g for a 20 µm film. Cling layers containing 1.5–2.0 wt% polyisobutylene or EVA-based tackifier produce machine-direction cling values above 120 g under ASTM D5458, but when tackifier loading exceeds 2.5 wt%, roll blocking in storage can appear at core temperatures above 38°C. The operating melt temperature for this conversion stage is held within 240–270°C; below 235°C, die-lip buildup from oxidized gel increases, and above 275°C, oxidative chain scission widens molecular weight distribution and reduces elongation at break measured under ASTM D882 to less than 350% in machine direction. Pre-stretch at 200–250% on power roller sets is controlled by film stiffness; a 23 µm film with a modulus below 250 MPa under ISO 527-3 can show transverse wrinkles when cast edges are uneven. Production-grade failure modes include telescoping rolls when transverse gauge variation exceeds ±1.5%, and pitch striping caused by unstable pump pressure oscillations above ±2 bar at the feedblock.

    How Do Sealant Webs in Form-Fill-Seal Lamination Retain Hot Tack Under High-Output Conditions?

    Cast sealant webs for horizontal and vertical form-fill-seal packages are judged first by hot-tack strength and seal initiation temperature, because vertical pouches are filled within 40–80 ms after sealing on rotary equipment. A 25–40 µm cast LLDPE layer applied in a PET/aluminum/LLDPE or BOPP/LLDPE lamination is typically sealed at 105–125°C with a dwell of 0.3–1.0 s; hot-tack values above 4 N/25 mm at 110°C under ASTM F1921 are required to prevent creep before the seal solidifies. The low crystallinity of cast LLDPE and rapid quench on a chill roll support a broader plateau seal curve than blown LDPE, but the seal curve is sensitive to surface additives. Slip levels above 800 ppm erucamide and antiblock concentrations above 1,500 ppm migrate to the seal interface and can reduce seal strength under ASTM F88/F88M by 10–25% when the film is stored longer than 21 days. Therefore, converter-grade variants use low-slip skin formulations and maintain a core layer with a standard additive package. Regulatory compliance is anchored to FDA 21 CFR 177.1520(c)3.1a for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² under EN 1186 test conditions; specific migration limits are procedure-defined and additive-specific. Amine-based additives and certain silanes are avoided because they can generate organoleptic taint at seal-bar temperatures above 150°C or during microwave reheating. Processing on a cast line uses a 30:1 L/D barrier screw and a gear pump to hold die pressure at 120–180 bar; polymer melt temperature is limited to 230–255°C to minimize low-molecular-weight oxidation products that contribute to odor. Chill roll surface finish is specified as Ra < 0.1 µm for low haze and consistent coefficient of friction under ASTM D1894; a matte surface can be used for bag-in-box applications where seal bar slip is prioritized. Wrinkle-related seal failures at gusset corners are reduced when transverse gauge variation is held below ±0.8% using an NDC infrared scanning gauge.

    Compliance or mechanical parameterTest method / designationConverter target for 25–40 µm cast sealant web
    Olefin polymer food contactFDA 21 CFR 177.1520(c)3.1aComplies as polyolefin, no plasticizer
    Overall migrationEU 10/2011 / EN 1186<10 mg/dm²
    Hot tackASTM F1921≥4 N/25 mm at 110°C
    Seal strengthASTM F88/F88M≥800 g/25 mm at 120°C, 0.5 s dwell
    Kinetic COFASTM D18940.20–0.45 on metal platen
    Haze for clear gradesASTM D1003<4.0% for 30 µm film

    Cast Surface Protection Webs for Coil and Sheet Lamination

    Surface protection film for stainless steel, aluminum composite panels, and coated coil is cast at 30–80 µm in a two-layer or three-layer construction with a low-gel LLDPE core and a pressure-sensitive adhesive skin. The primary defect mechanism is gel transfer: oxidized gel particles above 150 µm create protrusions that transfer to Class A sheet surfaces under contact pressure. The cast film process mitigates this by running a fine-mesh screen pack of 120–200 mesh and by keeping melt temperature below 255°C; gel counts are evaluated inline by optical cameras or by manual inspection against chart standards. The film is wound with interleaf paper or differential slip to prevent blocking because the adhesive layer is tacky at ambient temperature. Mechanical requirements include elongation at break above 400% under ASTM D882, because the film must follow bending radii during coil slitting and stamping without lifting; low elongation grades crack and leave residue. Peel adhesion is formulated between 0.02–0.5 N/25 mm for low-tack applications and up to 2.0 N/25 mm for high-tack UV-resistant masking; testing follows ASTM D3330 or FINAT Test Method 1. The base film must have a haze below 2.0% under ASTM D1003 and a gloss above 90 GU at 60° under ASTM D2457 if optical inspection of the protected surface is required. Chill roll temperature is maintained at 18–24°C; lower temperatures can increase thermal stress and later shrinkage under ambient storage above 40°C, measured as dimensional stability under ASTM D1204. Shrinkage of the protection film during outdoor exposure or coil storage should remain below 1.5% in machine direction and 0.8% in transverse direction. Static decay below 0.5 s at 15% relative humidity under MIL-PRF-81705D is necessary for films used near electronic or dust-sensitive fabrication; antistatic additives are added only to the adhesive or skin layer to avoid reducing core clarity. Processing failures on production lines include die-lip build-up from adhesive concentrated at the edges, and slack edges when the cast line is stopped; automated edge trim removal and a vacuum box are required for stable winding at speeds above 300 m/min.

    Filled cast webs entering hygiene backsheet lamination impose a thermal stabilizer and filler dispersion boundary that is not present in clear cast film. A breathable film formulation based on LLDPE carrier resin is compounded with calcium carbonate at 45–60 wt% and processed through a twin-screw compounder, then extruded on a cast line with a 0.5–0.8 mm die gap. The film is microporous after machine-direction stretching at draw ratios of 2.5:1–3.5:1; water vapor transmission rate for a 18–25 µm film ranges from 1,200–2,500 g/m²/24 h under ASTM E96/E96M wet cup conditions, depending on filler content and calender orientation. The processing window for stretching is narrow: if web temperature at the orientation unit falls below 55°C, film tears; above 75°C, pores collapse and WVTR drops below 800 g/m²/24 h. Stabilizer packages must withstand this thermal history, so a primary antioxidant plus a secondary phosphite are used at combined loadings of 1,000–2,000 ppm; overstabilization beyond 2,500 ppm can cause die-lip deposits that become visible as specks on the nonwoven lamination line. The cast web is adhesive-laminated to a spunbond polypropylene nonwoven with a 1.5–3.0 g/m² hot-melt pattern; bond strength above 0.5 N/25 mm under ASTM D1876 is required to survive high-speed converting and end-use abrasion. Elongation at break is specified above 300% MD and 350% CD under ISO 527-3; low levels of gel and good filler dispersion are critical because a 100 µm filler agglomerate becomes a pinhole in a stretched 20 µm film. Grade-specific published data for this exact resin in filled breathable systems are limited; feasibility must be validated on a pilot cast line with a high-shear mixing screw before commercial conversion.

    When Puncture Resistance in Forage Wrapping Must Track Silage Bale Storage Cycles

    Silage bale wrapping is not a conventional pallet wrap extension; it demands high retention of puncture resistance after repeated rewinding, UV exposure, and contact with chopped forage stems. Cast film of 20–28 µm thickness is stretched at 50–70% on a bale wrapper, but the film must withstand puncture energies above 20 J/mm under ASTM D5748 when tested against a standard probe. The film requires a UV stabilizer system sufficient for 12-month outdoor storage, often evaluated by cumulative UV irradiation of 150–250 kLy with retained elongation under ASTM D882 of at least 50% of original value. The tack layer must maintain cling after dust and dew exposure; therefore, cling levels are often specified above 150 g under ASTM D5458 and are achieved with a PIB concentration between 1.0–2.0 wt% in the skin layer. A higher PIB concentration above 2.5 wt% creates a property cliff-edge: initial cling rises, but the coefficient of friction becomes humidity-dependent and film transport on wrapper rollers may become erratic. For silage wrap, color masterbatches using white or green pigments at 4–8 wt% are common to reduce solar heat gain and reflect UV; these masterbatches must have a melt index within ±15% of the base resin to avoid dispersion-related pinholes. The film is typically produced on a three-layer cast line with core layer containing reclaim at 15–25 wt%; higher reclaim fractions can reduce dart impact below 160 g for a 25 µm film under ASTM D1709. Wrapping failures in the field include birdmouth tears at bale corners where cast film has cross-direction tear resistance below 15 N/mm under ASTM D1922, and oxygen ingress due to pinholes from stem puncture. A film with insufficient tack will unwrap in high winds; roll storage above 30°C before wrapping can cause blocking that prevents unwinding on a bale wrapper. Therefore, cast film for silage is wound with differential center tension and stored below 28°C.

    Running High-Speed Form-Fill-Seal Liners Without Seal-Point Failure

    Form-fill-seal sacks and industrial liners made from cast LLDPE typically use a 40–80 µm web in a monolayer or two-layer structure. The web is converted on FFS equipment that reaches 80–120 packages/min; this requires consistent coefficient of friction under ASTM D1894 between 0.20–0.35 on steel and good seal-through-contamination resistance. The cast film process provides gauge uniformity within ±1.0% and low orientation, which reduces differential shrinkage at seal corners compared with blown film. Dart impact values under ASTM D1709 for a 60 µm film typically fall above 300 g, but this depends on resin density and film gauge. Manufacturing limitations include die-lip build-up at high backpressure and the requirement not to exceed 260°C melt temperature to avoid oxidation gels. General-purpose liner conversion is well established, so the application boundary is controlled by gauge uniformity and additive package rather than complex rheological thresholds.

    Free Quote

    Competitive Braskem Flexus® 7200 LLDPE Cast Film Extrusion prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem Flexus® 7200 is a butene-comonomer linear low-density polyethylene supplied as a cast-film extrusion grade. The nominal melt flow rate is 2.0 g/10 min determined at 190°C/2.16 kg under ISO 1133-1:2022, and the nominal density is 0.918 g/cm³ under ISO 1183-1:2019. The pellet formulation includes a processing stabiliser package and a slip/antiblock additive system. The material is positioned for thin-gauge cast wrapping film, lamination webs, and overwrap structures in which the converter specifies draw-down, gauge uniformity, and coefficient of friction rather than bubble stability. Because the 2.0 g/10 min melt flow rate is higher than that of typical blown-film LLDPE, the resin reduces head pressure on slot-die lines while retaining sufficient melt extensibility for draw-down to 10–30 µm gauge values at industrial line speeds. Some supplier technical documentation classifies the grade as a high-draw cast-film resin with a density in the lower LLDPE range, which lowers quenched-web modulus relative to higher-density LLDPE.

    Film-level tensile, dart-impact, and tear-resistance values for Flexus 7200 are gauge-dependent and must be taken from the supplier batch certificate and verified on the target line. Published data for the exact cast-film configuration across all line speeds is limited; no single value is representative across a 10–80 µm gauge range. The table below therefore records only the grade-identification values normally available in the technical data sheet and supplier safety documentation.

    PropertyNominal value or descriptionReference method
    Melt flow rate2.0 g/10 minISO 1133-1:2022, 190°C/2.16 kg
    Density0.918 g/cm³ISO 1183-1:2019
    Comonomer typeButene-based LLDPESupplier grade disclosure
    Additive packageAntioxidant, slip, antiblockSupplier formulation; concentration not public
    Physical formPelletsVisual/line audit

    What physical parameters separate Flexus 7200 from blown-film LLDPE on a cast line?

    Three polymer-structure variables govern the difference. The 2.0 g/10 min melt flow rate lowers shear viscosity relative to blown-film grades commonly supplied at 0.5–1.0 g/10 min. On cast lines that do not require a stable tube, the higher flow permits a narrower die gap and lower adapter pressure at equivalent screw speed. The absence of long-chain branching in the LLDPE backbone reduces extensional hardening, so the melt web is drawn over a short 15–25 mm air gap and quenched before significant sag occurs. The 0.918 g/cm³ density reduces modulus build-up after chill-roll solidification; cast webs of higher-density LLDPE often develop greater necking force and edge split at the pinning edge when the draw ratio exceeds 50:1. The broader molecular weight distribution also distinguishes the grade from metallocene-catalysed cast-film resins: higher chain-length heterogeneity reduces screw torque but can produce a wider melting range and different surface roughness after orientation. On a blown-film line, this resin would show lower bubble stability than a grade with long-chain branching or a high-molecular-weight tail; conversion into blown film therefore requires blending with LDPE or a melt-strength enhancer.

    On a cast-film line configured with a single-screw extruder having an L/D ratio of 30:1 to 36:1 and a barrier feed section, the typical melt temperature is 240–260°C measured at the adapter. Die-body zones are usually held 5–15°C above the adapter set point to compensate for heat loss across the slot die. The die gap is set at 0.8–1.2 mm, and the air gap is maintained at 15–25 mm. Chill-roll temperature is normally 18–25°C; lower roll temperatures can increase quench rate but also increase condensation risk under high relative humidity. The vacuum box or air knife should be regulated to pin the extrudate before edge-necking narrows the web by more than 2–5% of die width. At line speeds above 450 m/min, the vacuum blower must be trimmed upward because the air boundary layer follows the film into the nip and reduces contact between the web and the chill roll. Insufficient contact transfers latent crystallization heat unevenly and produces optical haze bands parallel to machine direction. The screw temperature profile is not the sole control point: die-lip temperature, frost-line length, and chill-roll surface temperature interact. A drop of 2°C in chill-roll surface temperature may shift the quench rate enough to alter the size of spherulitic structures and reduce clarity; an increase of 2°C may produce blocking because the film enters the winder with a higher surface temperature and insufficient crystallized skin.

    Edge trim and post-industrial reclaim handling on Flexus 7200 cast-film runs are line-specific but boundary conditions remain. Because the resin is a non-hydroscopic polyolefin, it does not require drying after normal storage; however, pellets stored in unheated warehouses at relative humidity above 75% can carry surface moisture into the feed throat and produce micro-voids when the melt exits the die at 240°C or above. Regrind addition is typically limited to 15–25 wt% depending on gel-level specification and film end-use; higher levels can introduce oxidized material from edge trim that has experienced multiple heat cycles. The granulator screen size should be maintained at 4–6 mm to prevent feed segregation. On high-speed lines, a crammer feeder or grooved-barrel throat can be used when the bulk density of the regrind reduces feed stability; otherwise screw-speed fluctuation may produce gauge bands that repeat at a period equal to the feed-screw rotation.

    When slip and antiblock loadings fall below 1,500 ppm in thin-gauge webs

    The surface additive package in cast-film LLDPE is not cosmetic. Erucamide or oleamide slip agents migrate to the film surface over 24–72 h after extrusion; if the total slip loading is below the supplier-designated threshold, the kinetic coefficient of friction measured under ASTM D1894 can remain above 0.40, which is often unacceptable for high-speed pre-stretch machines. Conversely, elevated slip concentrations can create a transfer film on the chill roll and lower differential wetting tension after corona treatment. Corona treatment targets a surface tension of 38–44 mN/m measured under ASTM D2578; excessive slip bloom can reduce the treated surface energy within 24 h. Synthetic silica antiblock particles with typical particle sizes of 2–6 µm create micro-roughness, but excessive loadings above the supplier limit raise internal haze because the refractive index mismatch between the polymer matrix and the particle creates light scattering. Blocking force can be measured on film-to-film specimens under ASTM D3354 at 23°C and 50% RH; a value above the target upper limit for the winding hardness indicates that the antiblock level is insufficient for the reel diameter in use. On a production cast-film line, the first external sign of additive imbalance is unwind tack at the stretch wrapper; the second is deposition on corona treater electrodes and downstream reducing roller. Published data for the exact additive concentration in Flexus 7200 is limited, but the grade is formulated with slip and antiblock function intended for thin-gauge machine wrap. Batch-to-batch coefficient of friction should be verified on the cast web after 72 h of ageing at 23°C before reel conversion. Converters running below 15 µm should also monitor blocking during warehouse storage at temperatures above 30°C, because additive migration and film softening are accelerated by heat.

    Against metallocene-catalysed cast-film LLDPE of comparable density, Flexus 7200 typically requires lower extrusion pressure because its broader molecular weight distribution suppresses shear viscosity at the die lip. However, the broader distribution can reduce the maximum machine-direction tear after orientation and produce a less uniform comonomer distribution, which affects optical haze after quenching. The comparative table below summarises the main resin-class differences that converters should review before substituting one grade for another.

    ParameterFlexus 7200 cast-film positioningButene LLDPE blown-film gradeMetallocene LLDPE cast-film gradeLDPE cast-film grade
    Nominal melt flow rate2.0 g/10 min0.5–1.0 g/10 min0.5–2.0 g/10 min2.0–4.0 g/10 min
    Nominal density0.918 g/cm³0.918–0.922 g/cm³0.916–0.920 g/cm³0.920–0.925 g/cm³
    Chain architectureZiegler-Natta LLDPE, broad molecular weight distributionZiegler-Natta LLDPE with higher molecular weight tailMetallocene, narrow distribution, uniform comonomerFree-radical long-chain branched
    Cast-film process responseLow head pressure at thin gaugeLower gauge uniformity in cast configurationHigher torque but higher punctureLower haze but lower puncture
    Typical film testing standardISO 527-3, ASTM D1709AISO 527-3ISO 527-3, ASTM D5748ASTM D1003, ASTM D2457

    Regulatory boundaries that govern olefin food-contact use

    Compliance of the finished article is not established by the resin grade alone. For food-contact applications in the United States, the base polyethylene may be covered under 21 CFR 177.1520(c) 3.2a when the converter establishes that the finished film meets any applicable overall and specific migration limits. In the European Union, olefin polymers used in food-contact films are evaluated under Regulation (EU) No 10/2011 as amended by Regulation (EU) 2020/1245, with migration testing conducted according to the EN 1186 series methods and food simulant selection fixed in the regulation. REACH registration under Regulation (EC) No 1907/2006 and restriction compliance under Annex XVII are separate obligations applied to the resin supplier and the downstream user depending on the formulation. RoHS verification for electrical and electronic packaging is assessed against Directive 2011/65/EU as amended by (EU) 2015/863, with restricted substances such as lead, cadmium, mercury, and hexavalent chromium each held to 0.1 wt% or 1000 ppm at the homogeneous material level, except cadmium at 0.01 wt% or 100 ppm. Converters must request the supplier’s food-contact statement and verify lot-level heavy-metal certificates before use in regulated packaging.

    In five-layer cast stretch-film structures, resins in this density and melt-flow class are frequently assigned to the core layers, where surface tack and cling are not the primary requirement. The outer cling layer typically contains an ethylene-vinyl acetate or metallocene resin with a tackifier, while the opposite skin may contain controlled slip and antiblock. Flexus 7200 is not intended for blown-film dies, blow moulding, or rotational moulding. Unmodified LLDPE of this type also lacks adhesion to polar barrier resins such as PA or EVOH in cast barrier structures; when such structures are produced, an adhesive tie layer must be included. The grade is not recommended for applications requiring long-term outdoor UV exposure unless a carbon black or hindered amine stabilizer package is introduced by the converter, because the standard stabilization package is designed for indoor conversion, storage, and distribution. Converters handling high levels of post-industrial trim should limit regrind addition to the level correlated with acceptable gel count on the target film specification; increasing regrind without gel monitoring can shift the film’s optical quality from the certified range.

    The upper processing boundary is set by the thermal-oxidative degradation kinetics of the stabilizer package rather than by the polymer melting point. Residence times above 15 min at melt temperatures above 270°C can initiate gel formation and a shift in the film’s yellowness index measured under ASTM E313; this is observed as fish-eye defects on the chill roll. During start-up, the screw should be purged with the resin itself rather than with a lower-density purge compound that can remain in the die lips. Shutdown at below 160°C is required before stopping the screw to avoid stagnant material in the adapter and feedback. These limits are generic for butene LLDPE cast-film grades; the Flexus 7200 batch certificate should be consulted for the supplier’s specific thermal stability index.

    Top