| HS Code | 840749 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) Copolymer |
| Comonomer | Butene-1 |
| Density | 0.921 g/cm³ |
| Melt Index 190 C 2 16 Kg | 3.3 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 96 °C |
| Tensile Strength At Yield | 9 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 150 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 3% |
| Gloss 45 | 90 |
| Coefficient Of Friction | 0.2 |
| Blocking | 30 g |
| Form | Pellets |
| Recommended Process | Cast Film Extrusion |
As an accredited Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg polyethylene-lined bags, palletized at 1,000 kg per pallet; optional 1,000 kg bulk bags available. |
| Container Loading (20′ FCL) | 20′ FCL loading: Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer in 25 kg bags, palletized, shrink-wrapped, secured for export. |
| Shipping | Braskem FL31 LLDPE cast film extrusion polyethylene copolymer ships as non-hazardous, dust-free pellets in 25 kg bags or bulk octabins, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Store cool, dry, away from direct sunlight and ignition sources. No UN hazard class required. |
| Storage | Store Braskem FL31 LLDPE in original, sealed bags or containers in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, flames, and strong oxidizers. Protect from moisture, dust, and contamination; avoid prolonged UV exposure. Stack pallets securely to prevent damage. Maintain ambient storage conditions and follow the supplier’s SDS and local regulations. |
| Shelf Life | Typically 24 months from production when stored unopened in original packaging, dry, cool, away from direct sunlight and contamination. |
On high-speed pre-stretch pallet-wrapping lines operating at 250–300 m/min with 100–200% pre-stretch, Braskem FL31 is processed as the primary core resin in a three-layer cast coextrusion. The material is dosed at 70–85 wt% in the core layer, with mLLDPE at 15–25 wt% to raise ASTM D5748-95 protrusion puncture resistance, while the outer skins carry a polyisobutylene cling concentrate at 0.8–2.0 wt% and a silica-based antiblock at 0.5–1.5 wt%; layer distribution is set at 10/80/10 for 17–23 µm machine-grade film. Under ASTM D5458-95 peel cling, removable cling force typically shifts from 0.8 N/cm to 1.4 N/cm as the cling concentrate moves from 1.0 wt% to 2.0 wt%. The downstream cast line uses a 35:1 L/D barrier screw, 0.7 mm die gap, 90–120 mm air gap, and a chrome chill roll held at 18–24°C; edge trim is recycled at 10–20%. Above 20% edge trim, screw torque fluctuation and gel formation in the melt curtain increase. The material is also tested in accordance with ISO 527-3:2018 tensile and ISO 7765-1:1988 free-falling dart. Terminal grades include machine-grade palletization rolls, coreless pre-stretched rolls, and hand-wrap tubes.
The use of Braskem FL31 as a heat-seal web in adhesive lamination with 12 µm polyester or 20 µm biaxially oriented polypropylene places the cast layer in direct food-contact position. Compliance under FDA 21 CFR 177.1520(c) applies to the olefin polymer; for export to the EU, Regulation (EU) No 10/2011 requires overall migration below 10 mg/dm² under the assigned food simulant. In a cast coextrusion formulation, FL31 is run at 60–75 wt%, LDPE at 20–30 wt% to widen the processing window and suppress draw resonance, and an erucamide slip concentrate at 0.5–1.5 wt% to bring kinetic coefficient of friction to 0.10–0.20 when measured under ISO 8295:1995. The downstream process uses a 0.5–0.8 mm die gap, melt temperature 230–260°C, and an air knife at 4–6 bar pinning the web to a polished 15–25°C chill roll; corona treatment is set to 38–42 mN/m before lamination. Solventless adhesive coating at 1.5–3.0 g/m² or extrusion lamination with LDPE at 8–10 g/m² is used downstream. Pre-drying is not required below 60% relative humidity; in humid transfer conditions above 60% RH, a 60°C hopper dryer for 1 h prevents surface moisture defects. Terminal types include sealant webs for snack laminates, frozen food pouches, condiment sachets, and lidding films.
On bale-wrapping lines programmed for 32–36 wraps per bale and 50% pre-stretch, the cast web is converted from 22–25 µm three-layer silage film produced with Braskem FL31 at 75–85 wt% in the core. The outer layers contain LDPE at 10–20 wt%, a combined HALS/UV masterbatch at 4–6 wt%, and pigment masterbatch at 2–5 wt%; this loading is balanced because UV masterbatch above 6 wt% reduces ASTM D5748-95 puncture resistance and increases chill roll fouling. Compliance is anchored to EN 13207:2018 for thermoplastic stretch films used for ensiling, with tensile and tear properties verified under ISO 527-3:2018. The cast process runs through a 2200 mm die, a gear pump, 0.8 mm die gap, 120–160 mm air gap, and a matte-finish chill roll held at 18–22°C to create differential cling; edge trim at 8–12% is reintroduced to the core. Film is post-slit to 750 mm rolls and wrapped under high tension on bale wrappers. Terminal formats include white, black, and green bale wrap for grass haylage, maize silage, and whole-crop ensiling.
Conversion from blown-line to cast coextrusion for breathable or non-breathable backsheet webs places Braskem FL31 at 70–85 wt% of the film layer, with LDPE at 10–20 wt% to improve chill roll release, and titanium dioxide masterbatch at 5–10 wt% to achieve opacity for nonwoven lamination. A fluoropolymer processing aid at 0.2–0.5 wt% is added only when melt fracture appears above 260°C. Compliance records typically include Regulation (EC) No 1907/2006 REACH SVHC screening, OEKO-TEX Standard 100 product class I, and ISO 10993-5:2009 cytotoxicity when the converter is qualifying the finished absorbent article; published data for this specific configuration is limited at the raw-resin level, and end-use validation remains on the finished device. The cast process uses a 4.5 m die, 80–150 mm air gap, silicon rubber nip chill roll at 15–20°C, and a melt temperature window of 235–260°C. Corona treatment is set to 39–41 mN/m for adhesive lamination to spunbond polypropylene; above 42 mN/m, surface oxidation can weaken adhesive bond strength after 90 days. Terminal products are cast backsheet webs for infant diaper lamination, adult incontinence backsheet, and feminine hygiene outer layers.
For temporary surface protection, a 40–60 µm cast masking web is produced with Braskem FL31 at 80–90 wt% as the backing film, mLLDPE at 5–15 wt% for tear propagation control, an anti-static concentrate at 0.5–1.5 wt% to prevent dust attraction on flat glass, and UV stabilizer at 0.5–1.0 wt% when outdoor exposure exceeds 30 days. The web is tested under ASTM D882-18 tensile and ASTM D3330/D3330M-04(2018) peel adhesion to stainless steel, with typical film-to-substrate adhesion kept below 0.5 N/cm to avoid adhesive transfer after 90 days of weathering. The cast backing film is extruded through a 0.8 mm die gap, 150–180 mm air gap, and a matt steel chill roll at 20–25°C; one side is corona treated to 38–42 mN/m and then coated with water-based acrylic pressure-sensitive adhesive at 3–5 g/m² dry coat weight. Anchorage below 38 mN/m leads to adhesive pick-off during high-speed unwind. Terminal types include temporary masking for stainless steel sheet, anodized aluminium extrusions, PMMA sheet, and flat glass handling.
At 25–35 µm gauge and 180–250 m/min overwrap line speed, Braskem FL31 is processed in mono-layer cast film with 80–95 wt% FL31, 5–15 wt% LDPE to reduce neck-in, and a slip/antiblock masterbatch at 1.0–2.0 wt%. Haze measured under ISO 14782:1999 is held below 6% using a polished chill roll with roughness below 0.3 µm Ra at 20–25°C; coefficient of friction under ISO 8295:1995 is maintained at 0.20–0.35 to avoid tray jams in overwrap machines. The film is corona treated to 38–40 mN/m before printing, but pot-life of the treated surface is 30–60 days; after that the roll must be retreated or rejected. Compliance includes FDA 21 CFR 177.1520(c) for indirect food contact in paper packaging, and Regulation (EU) No 10/2011 when the wrapped product is stored adjacent to food. Terminal types include clear overwrap for paper reams, tissue bundles, napkin sleeves, and sanitary protection bundles.
Competitive Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem FL31 is a linear low-density polyethylene copolymer supplied for cast film extrusion. The resin is produced with a butene comonomer and is characterized by a nominal melt flow rate of 3.0 g/10 min measured at 190 °C/2.16 kg under ASTM D1238/ISO 1133-1 and a nominal density of 0.918 g/cm³ under ASTM D792/ISO 1183-1. These values place the material in the medium melt-flow, low-density segment of the polyethylene range used for thin chilled-roll webs from approximately 15 µm to 50 µm. The butene short-chain branching distribution reduces crystallinity relative to ethylene homopolymers and provides a balance of low-temperature seal response, optical clarity, and tear propagation resistance. The grade is supplied in pellet form and is specified for cast film lines rather than blown film lines; its melt flow and additive system are not optimized for long-duration bubble stability at high blow-up ratios.
FL31 should be plasticated in a single-stage barrier screw extruder with an L/D ratio of 24:1 to 32:1 and a compression ratio of 3:1 to 4:1. A Maddock or dispersive mixing section is recommended to homogenize the broad molecular weight distribution and reduce unmelted-particle defects. Barrel temperatures are typically profiled from 180 °C at the feed throat to 240–260 °C at the adapter and die. The melt temperature entering the flat die is maintained between 240 °C and 260 °C; below 215 °C, high viscosity raises head pressure and promotes sharkskin melt fracture, while above 280 °C, oxidative gel formation increases, particularly in stagnant areas of the coat-hanger manifold. A stable positive pressure of 100–250 bar at the die inlet is typical on production-scale cast lines.
Draw resonance in butene LLDPE cast film is controlled by the interaction among die gap, air gap, and draw ratio. The absence of long-chain branching reduces extensional strain hardening; periodic gauge bands may appear when the draw ratio exceeds approximately 30:1 in combination with an air gap above 25 mm. On a 1,200 mm wide three-layer coextrusion line running a 20 µm web at 120 m/min, a die gap of 0.5 mm and an air gap of 20 mm provide stable gauge uniformity when the melt temperature is held at 250 °C and the chill-roll temperature is held at 20 °C ± 2 °C. If edge neck-in exceeds 35 mm per edge, gauge bands and edge-trim losses increase; operators typically adjust vacuum-box position or reduce die gap before changing line speed.
| Parameter | Typical range | Unit |
|---|---|---|
| Barrel temperature profile | 180–250 | °C |
| Adapter and die temperature | 240–260 | °C |
| Melt temperature | 240–260 | °C |
| Die gap | 0.5–1.0 | mm |
| Air gap | 15–25 | mm |
| Chill-roll temperature | 18–30 | °C |
| Draw ratio | 20:1–40:1 | — |
| Die inlet pressure | 100–250 | bar |
Physical property data for FL31 are generated on cast film prepared under controlled conditions. The following published typical values are used for comparative selection; actual values depend on gauge, cooling rate, and coextrusion structure, and the current supplier datasheet remains the controlling document. Dart drop impact, F50, of a 25 µm monolayer film is in the range of 90–110 g under ASTM D1709A. Elmendorf tear values are typically 250–400 gf in the machine direction and 400–550 gf in the transverse direction under ASTM D1922. Tensile yield strength is 10–12 MPa in both directions under ASTM D882, with elongation at break in excess of 600%. Haze is typically below 3.0% and 45° gloss above 75 GU under ASTM D1003 and ASTM D2457, respectively. These optical values are sensitive to chill-roll temperature and air-knife control; laboratory cast-film data should not be transferred directly to production results without line validation.
| Property | Test method | Unit | Nominal or typical value |
|---|---|---|---|
| Melt mass-flow rate | ASTM D1238/ISO 1133-1 | g/10 min | 3.0 |
| Density | ASTM D792/ISO 1183-1 | g/cm³ | 0.918 |
| Tensile yield strength, MD/TD | ASTM D882 | MPa | 10–12 |
| Elongation at break, MD/TD | ASTM D882 | % | >600 |
| Elmendorf tear, MD | ASTM D1922 | gf | 250–400 |
| Elmendorf tear, TD | ASTM D1922 | gf | 400–550 |
| Dart drop impact, F50 | ASTM D1709A | g | 90–110 |
| Haze | ASTM D1003 | % | <3.0 |
| Gloss at 45° | ASTM D2457 | GU | >75 |
The optical response of FL31 depends on the rate at which the melt is cooled through the crystalline solidification range. A chill-roll temperature of 18–25 °C typically produces haze below 3% and 45° gloss above 75 GU; raising the chill-roll surface temperature to 40 °C can increase haze by 1–3 percentage points because slower solidification permits larger spherulitic light-scattering structures. The chill-roll boundary layer must be removed by an air knife or electrostatic pinning; entrapped air between the polymer melt and the chill roll creates a matte surface and can reduce gloss from 80 GU to below 60 GU. For lamination or printing, surface treatment should target 38–42 mN/m wetting tension; corona output must be adjusted for line speed and film thickness. In coextruded cast stretch film, FL31 can serve as a core layer where optical values are less critical than draw stability and stretch recovery.
FL31 differs from autoclave or tubular LDPE in molecular architecture. LDPE carries long-chain branching and typically shows higher melt strength, lower neck-in, and lower draw-down capability. FL31 has a linear backbone with short-chain butene branches; this improves dart impact, Elmendorf tear, and stress-crack resistance relative to LDPE of comparable density, but it reduces melt strength. Compared with metallocene-catalyzed LLDPE, FL31 has a broader molecular weight distribution and lower extensional strain hardening. Metallocene grades typically outperform FL31 in dart impact and puncture energy but generate higher extruder head pressure and are more sensitive to die-lip buildup. In cast stretch-film structures requiring a dart impact above 140 g F50 under ASTM D1709A at 20 µm, a metallocene or hexene-rich copolymer should be considered; FL31 is positioned for standard machine wrap and overwrap where stable draw and lower raw material cost are controlling. Against hexene- or octene-based Ziegler-Natta LLDPE, FL31 shows lower tear and dart impact because butene comonomer creates a shorter tie-chain population at equivalent density; however, FL31 often processes with lower melt pressure and broader gauge-control latitude. Published direct comparative data for the exact grade are limited, particularly at gauges below 15 µm.
Seal initiation temperature is a function of density, comonomer type, and thermal history. For a 25 µm cast film at 0.918 g/cm³, seal initiation is commonly observed in the range of 95–105 °C when tested under ASTM F1921 with a dwell time of 0.5 s and sealing pressure of 0.5 N/mm². This is typically 10–15 K lower than an LDPE of equivalent density, allowing higher sealing throughput on vertical form-fill-seal equipment. The hot-tack window is narrower than that of a metallocene grade; packaging lines running high coefficient-of-friction films may require jaw-release timing adjustment. If a converter requires sealing below 85 °C, FL31 is not the appropriate resin; a lower-density metallocene or ionomer-containing structure should be evaluated. Seal response also shifts with coextrusion skin layers and with migration of slip additives; final seal performance must be measured on the finished structure, not on resin pellets.
Polyethylene copolymer grades such as FL31 may be suitable for food-contact applications when the finished film meets the conditions of use specified in 21 CFR 177.1520(c) 3.1a or 3.2a. Under EU Regulation (EU) No 10/2011, compliance requires that the final film meets an overall migration limit of 10 mg/dm² under the applicable food simulant and migration test condition, typically OM2 or OM3 for room-temperature or refrigerated contact. REACH registration for the polyethylene monomer and polymer is managed by the supplier; RoHS substance restrictions are not typically relevant to the base polymer but may apply to the finished electrical or electronic packaging article. No statement of conformity to drug or medical packaging standards is implied by cast film processability; converters must validate FDA or EU approval on the final structure because coextruded layers, adhesives, and additives can change migration behavior. The typical antistat and slip additives present in commercially available film grades are disclosed in the supplier safety and regulatory documentation; their addition levels may influence organoleptic performance in sensitive food applications.