Braskem Fg31d Lldpe Blown Film Extrusion Polyethylene Copolymer

Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 564796
    Polymer Type Linear Low Density Polyethylene (LLDPE) Copolymer
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Flow Index 190 C 2 16 Kg 0.90 g/10 min
    Melting Temperature 121 °C
    Vicat Softening Temperature 96 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800%
    Dart Drop Impact 110 g
    Elmendorf Tear Strength Md 220 g
    Elmendorf Tear Strength Td 330 g
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction > 0.5
    Slip Additive No
    Antiblock Additive No
    Processing Method Blown Film Extrusion
    Typical Film Thickness 25-100 µm
    Physical Form Pellets
    Color Natural

    As an accredited Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem FG31D LLDPE blown film extrusion copolymer is supplied in 25 kg polyethylene-lined paper bags, palletized, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL container loading Braskem FG31D LLDPE blown film extrusion polyethylene copolymer; packaged goods, palletized, dry, secure, compliant, and transport-ready.
    Shipping Braskem FG31D LLDPE copolymer is shipped as solid, non-hazardous pellets in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk lined trucks/railcars. Keep packaging closed and dry, away from moisture, heat, sunlight, and contaminants. Store in a cool, ventilated area and handle per the safety data sheet and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Use clean pallets; avoid stacking damage. Maintain ambient temperatures, protect from UV and odors. Follow local regulations and manufacturer’s SDS. Use first-in, first-out stock rotation. Keep away from ignition sources.
    Shelf Life Typically 12 months from manufacture if stored unopened in original packaging, cool, dry, away from direct sunlight and moisture.
    Application of Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer

    On a 2.0 m blown film line configured with a 75 mm grooved-feed extruder at 30:1 L/D and a 250 mm spiral mandrel die with a 2.0 mm die gap, Braskem FG31D is processed into heavy-duty industrial liners and bulk shipping sacks at thicknesses from 100 µm to 250 µm. The resin is supplied with a nominal density of 0.918 g/cm³ and a melt flow rate of 1.0 g/10 min measured at 190 °C under 2.16 kg in accordance with ASTM D1238. The butene-copolymer linear low-density polyethylene has a narrower molecular weight distribution than high-pressure LDPE, which creates a more abrupt onset of sharkskin melt fracture when extruder output pushes die-lip shear stress beyond the critical level. Die gaps below 1.8 mm are generally unsuitable for thick-gauge FG31D because the reduced die land length increases shear rate at the lip and produces visible surface roughness on the inner bubble surface. Melt temperature is held between 190 °C and 220 °C; below 190 °C, screw torque and melt pressure rise, while above 220 °C, the bubble becomes difficult to stabilize at high blow-up ratios because the zero-shear viscosity drops. Production-scale instability appears as edge weave and sagging between the collapsing frame hips. Blow-up ratio is set between 2.0:1 and 2.8:1, with the lower end favoring MD tear and the upper end improving TD impact. Frost line height is adjusted between 700 mm and 1,100 mm from the die face. Raising the frost line increases MD orientation and machine-direction tensile modulus, but reduces dart impact retention under ASTM D1709 Method A. The necked bubble geometry produced by a high frost line also improves bubble stability, which is necessary when the film is used in unsupported liners for FIBCs and drum liners that must withstand two-person handling. The critical qualification matrix for these structures is defined by the test methods shown in Table 1.

    Qualification propertyTest methodRelevant unit
    Puncture resistanceASTM D5748N
    Elmendorf tearASTM D1922g
    Dart impactASTM D1709g
    Tensile propertiesASTM D882MPa
    Secant modulusISO 527-3MPa

    Why does frost line height govern dart impact retention in agricultural covers?

    Agricultural film converters blend FG31D with 10–20 wt% high-pressure LDPE and a UV stabilizer masterbatch let down at 2–4 wt% to produce silage clamp films and greenhouse side-sheets at 150–200 µm. The LDPE fraction modifies bubble stability, but the higher melt strength contribution does not compensate for orientation losses if the frost line is raised beyond the point where the spherulitic structure is quenched. Accelerated weathering is evaluated under ISO 4892-2 using UVA-340 lamps at 0.76 W/m² irradiance and a black panel temperature of 60 °C; film exposed without adequate hindered amine light stabilizer loses elongation at break rapidly, and field failure occurs as wind-induced flex cracking at fold creases. The addition of HALS at 0.15–0.35 wt% active content is typical for multiseason performance in temperate climates, although regions with solar loads above 120 kLy/yr may require a higher stabilizer package or coextruded surface layers. The frost line in the agricultural process window is set at 2–3 die diameters for high TD tear; raising it to 8–10 die diameters increases MD tensile modulus but reduces dart impact retention measured by ASTM D1709. The failure mode in silage clamps is multi-axial puncture followed by tear propagation; therefore TD Elmendorf tear is used as the primary field failure predictor. In LLDPE blown film, TD tear is typically two to three times MD tear, with the exact ratio depending on blow-up ratio and frost line height. Gauge uniformity across the layflat is controlled with a capacitive profile sensor to within ±5 % of nominal thickness. Sections below −5 % are prone to propagation tearing when the film is stretched over silage pile edges.

    When frozen food converters replace cast LDPE sealant webs with FG31D blown film in a three-layer structure, re-qualification of seal-bar pressure and dwell time is required because the broader melting distribution retains more residual heat at the seal interface. The frozen food film is typically blown at 40–80 µm total thickness with a layer ratio of 20/60/20 and a BUR of 2.2:1; the inner sealant layer is FG31D-rich, while the core may contain metallocene or C4-LLDPE to raise hot-tack. Seal initiation is evaluated on flat jaw laboratory sealers in accordance with ASTM F88. The plateau for butene LLDPE emerges between 100 °C and 130 °C, with a hot-tack window measured under ASTM F1921 that narrows when the film is run above 80 m/min on vertical form-fill-seal equipment. Low-temperature impact resistance after conditioning at −18 °C is the critical property; dart impact under ASTM D1709 Method A shows that FG31D retains a greater proportion of ambient-temperature impact strength than cast LDPE at the same gauge, which is the reason converters select it for ice cream pouches and frozen vegetable bags. However, frost line fluctuations during production alter this low-temperature performance because quench rate affects crystal size distribution. The objective of the converter is to keep frost line height within ±10 % of the set point; deviations produce localized crystal size differences that create high-stress points along crease lines. Food-contact compliance for the resin is established under 21 CFR 177.1520 for olefin polymers and under EU 10/2011 with overall migration limits of 10 mg/dm². Specific migration of primary aromatic amines is not applicable because the resin does not contain aromatic diisocyanate residues; however, each finished structure must be verified by the converter using a migration testing program tailored to the final food type and storage duration. The compliance matrix is summarized in Table 2.

    Regulation / standardScopeEnd-of-use verification
    21 CFR 177.1520Olefin polymers for food contactExtraction testing per FDA methods
    EU 10/2011Plastic materials and articlesOverall migration 10 mg/dm²
    REACH Annex XVIIRestricted substancesSupply chain statement
    RoHS Directive 2011/65/EUHeavy metalsXRF screening per IEC 62321

    Coextruded hygiene overwrap and tissue bundling film structures

    Tissue bundling operations running at 120 packs/min require a blown film with low coefficient of friction and stable gauge that can withstand the sudden acceleration of the wicket packer. In a five-layer line, FG31D is used in the core or surface layer at 25–45 % of the structure, with LDPE or plastomer skin layers selected to adjust hot tack and seal through residual tissue dust. The film is produced at 25–35 µm, with a BUR of 2.5:1 and a die gap of 1.6–2.0 mm; the narrower die gap is acceptable because the lower film gauge does not generate the same lip shear stress as heavy-duty liners. Slip and antiblock additives are incorporated at 500–1,000 ppm to achieve a kinetic coefficient of friction below 0.25 when measured by ASTM D1894. Higher antiblock levels can increase haze and reduce heat-seal strength; therefore the formulation is adjusted against optical measurements using ASTM D1003. The main processing failure observed on automatic bundlers is film flutter caused by thickness variation above ±5 %; this can be corrected by rotating the die and air ring more frequently when processing FG31D at high output. Weld integrity at the overwrap tail is evaluated with ASTM F88 after sealing at 115–130 °C; welds that fail at the interface before film yield indicate contamination from paper dust or an excessive slip additive concentration.

    Extrusion lamination sealant webs operate in the plateau region between seal initiation and hot-tack failure.

    Adhesive lamination lines use FG31D blown film as the sealant web for PET/foil/PE and OPP/PE laminates. The film is blown at 30–50 µm and then adhesively laminated; corona treatment is applied upstream of the lamination nip to raise surface energy to 38–42 dyn/cm as measured by dyne solutions conforming to ASTM D2578. If surface energy falls below 38 dyn/cm, the adhesive wets unevenly and laminate bonds fail during subsequent pouch forming. The sealant web’s heat-seal performance is determined by ASTM F2029 for hot-tack and ASTM F88 for seal strength; converters target a seal bar temperature window that avoids seal-through of the laminated foil while achieving hermetic seals on high-speed pouching machines. Because FG31D has a melt flow rate of 1.0 g/10 min, the web contributes enough melt strength to prevent burn-through at high seal-bar temperatures. Package integrity is verified by ASTM F2338 vacuum decay; laminate structures that show channel leaks along the seal edge commonly have a surface energy defect or a gauge depression from collapsing frame misalignment. The processing conflict in extrusion lamination is that high line tension can stretch the FG31D web prior to nip lamination, causing MD neck-in and reducing finished laminate width. Tension control is therefore maintained within ±3 % of setpoint to prevent permanent elongation of the sealant web. Published data for this specific configuration is limited, and pouch converters are required to qualify final seal strengths against their own fillet and closure geometry.

    In collation shrink overpackaging for canned goods and bottled water, FG31D is processed in a three-layer high-stalk bubble configuration where the outer layers provide sealing and slip properties while the core layer carries the mechanical load. The film is produced at 50–80 µm with a BUR of 2.0:1 to 2.5:1; melt temperature is held at 190–210 °C. Shrink values are evaluated by ASTM D2732 at 150 °C; the actual TD and MD shrink percentages depend heavily on the blend ratio with LDPE and on the high-stalk frost line height, and published data for this specific configuration is limited. The key processing conflict is that higher stalk height increases MD shrink but reduces bubble stability; the operator must balance the effect against the requirement for sufficient shrink force to hold cans on a corrugated tray during distribution. Shrink force is measured on a strain gauge sample holder after immersion in an oil bath; the resulting force must exceed 0.5 N/15 mm to secure the pack, although this limit will vary with pack geometry and gauge. The main field failure is TD splitting at the tray bottom, which arises when the film is over-shrunk or when gauge variation along the collapsing frame exceeds ±6 %. The corrective action is to reduce frost line height and operate at the lower end of the BUR range, sacrificing some MD shrink while retaining TD tear strength.

    Free Quote

    Competitive Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem FG31D is a linear low density polyethylene copolymer intended for blown film extrusion. The grade is polymerized with a butene comonomer and is supplied as free-flowing pellets for monolayer and coextruded film structures. Its nominal melt flow rate is 1.0 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg applied mass, and its nominal solid density is 0.918 g/cm³ under ASTM D1505. These values place FG31D in the medium-molecular-weight butene LLDPE category used for industrial liners, heavy-duty shipping sacks, frozen food packaging, agricultural film, and coextruded carrier bags. The resin is differentiated from high-pressure LDPE by a linear backbone with short-chain branching, and from hexene or metallocene LLDPE by shorter branch length and a different balance of impact, tear, and seal performance.

    Material Identity, Regulatory Anchors, and Limiting Specifications

    The molecular architecture of FG31D is dominated by a linear ethylene backbone with short-chain branches introduced by 1-butene. During film cooling, these branches limit lamellar thickness and reduce density to 0.918 g/cm³; the crystallinity fraction calculated from two-phase density models is approximately 47% using a crystal density of 1.000 g/cm³ and an amorphous density of 0.855 g/cm³. The melt flow rate of 1.0 g/10 min reflects a molecular weight distribution that balances extrusion amperage, backpressure, and film toughness. Because the resin is not hygroscopic, pre-drying is normally unnecessary under closed-bag storage at relative humidity below 60%. Condensation on pellets should be removed by warm-air drying at 80 °C for 2 h before processing.

    For food-contact applications, the manufacturer’s product stewardship bulletin should be consulted for the specific condition of use under 21 CFR 177.1520; olefin polymers of this class are generally recognized for direct food contact when the finished article meets extractive limits and end-use restrictions. Compliance with EU No 10/2011 and REACH EC 1907/2006 must be verified from the current supplier declaration and not inferred from resin type alone. Thermal analysis of similar butene LLDPE grades typically shows a peak melting endotherm between 120 °C and 124 °C under ASTM D3418; FG31D-specific values may vary with thermal history and additive package.

    What Distinguishes a Butene LLDPE from High-Pressure LDPE and Hexene Copolymers?

    High-pressure LDPE contains both short-chain and long-chain branches produced under radical polymerization, which confer high melt tension, pronounced strain hardening, and stable large-diameter bubbles at high blow-up ratios. FG31D, as a butene LLDPE, has a narrower molecular weight distribution and lacks significant long-chain branching; its melt strength is lower, so bubble stability is more sensitive to die gap, air ring performance, blow-up ratio, and frost line position. Compared with hexene LLDPE at equivalent density and melt flow rate, butene comonomer creates shorter branches that are less efficient at generating interlamellar tie molecules. The practical result is lower dart impact under ASTM D1709, lower Elmendorf tear under ASTM D1922, and less balanced MD/TD tear orientation than hexene LLDPE. FG31D nevertheless provides a cost-performance position in non-demanding film structures where lower seal initiation than LDPE and moderate toughness are sufficient.

    Qualitative differentiation of film resin families
    Film propertyHigh-pressure LDPEButene LLDPEHexene LLDPEMetallocene LLDPE
    Dart impact at 25 µmLowerHigher than LDPEHigher than buteneHighest
    MD/TD tear balanceTD-dominantTD-dominant with lower MDMore balancedMore balanced
    Melt strengthHigherModerateModerateLower
    OpticsHigh glossModerate hazeModerateHighest
    Seal initiation temperatureHigherLower than LDPELower than buteneLowest

    On production-scale blown film lines with 60 mm to 90 mm barrier-screw extruders and 30:1 L/D ratios, similar 0.918 g/cm³, 1.0 g/10 min butene LLDPE grades are typically processed at melt temperatures of 190 °C to 220 °C. A common starting point is a die gap of 2.0 mm, blow-up ratio of 2.5:1, and frost line height between 6 and 10 die diameters. These conditions do not constitute a universal recipe for FG31D because die diameter, air ring design, tower height, and ambient conditions shift the stable operating window. Published data for FG31D-specific output on a 60 mm grooved-feed extruder with a 200 mm die and 2.0 mm gap is limited; operators should establish a stable bubble by incremental adjustment of the air ring and internal bubble pressure while monitoring gauge variation across the web.

    For high-output lines exceeding 100 kg/h on 90 mm extruders, internal bubble cooling is often required to remove heat from the interior of the bubble and to increase output without raising melt temperature. FG31D should be processed with the melt temperature kept below 240 °C; prolonged hold-up above 250 °C can produce oxidative gels and odor. In feed zones, screw cooling should be set to prevent premature pellet melting and bridging. Discharge pressures above 400 bar should be investigated for screen pack fouling or excessive screw wear.

    When Die Gap, Blow-Up Ratio, and Frost Line Height Are Not Controlled Independently

    The relationship between die gap and blow-up ratio determines molecular orientation in the molten web before solidification. A thin die gap combined with high blow-up ratio increases transverse orientation, which raises transverse-direction tear under ASTM D1922 but can depress machine-direction tear. A thick die gap with low blow-up ratio preserves machine-direction orientation but reduces bubble geometry and gauge uniformity. For FG31D, which is already biased toward transverse-direction tear resistance, high blow-up ratios above 3.0:1 may produce a wide difference between MD and TD tear, leading to premature failure in bag handles or printed areas. Frost line height controls the time available for molecular relaxation: a low frost line increases quench rate, smaller crystallite size, and haze, while a high frost line increases crystallinity and can raise film stiffness but reduce dart impact. Therefore, frost line should be adjusted with melt temperature and output to keep bubble neck stable and avoid bubble breathing.

    On-line thickness measurement using a capacitance or beta gauge traversing the bubble is necessary to quantify gauge bands. For similar butene LLDPE, gauge variation of ±5% or lower across the layflat is achievable on well-maintained dies; values exceeding ±10% indicate die bolt misalignment, uneven air ring cooling, or melt temperature maldistribution. In coextruded structures, layer-to-layer viscosity mismatch can distort the bubble and create local thickness nonuniformity. FG31D’s 1.0 g/10 min melt flow rate is close to many LDPE and HDPE skin resins, but layer ratio changes may require adjustment of die temperature zones.

    Downstream Conversion and End-Use Requirements

    For heavy-duty shipping sacks and industrial liners, the primary acceptance criteria are dart impact under ASTM D1709-16A and Elmendorf tear under ASTM D1922. In frozen food packaging, seal strength is measured under ASTM F88/F88M-21 and hot-tack under ASTM F1921. Low-temperature seal initiation of butene LLDPE is typically lower than high-pressure LDPE but higher than metallocene plastomers; this places FG31D in intermediate seal performance. Agricultural film applications require puncture resistance measured by probe puncture testing under ASTM D5748 and UV stabilization tailored to the exposure period. The resin itself does not contain carbon black or UV stabilizers unless specified in a compounded variant; converters must add masterbatch or purchase a pre-compounded grade if long-term outdoor exposure is required.

    In coextruded structures, FG31D may be used as a sealant layer or core layer. Its density and melt flow rate allow pairing with HDPE skins for stiffness or LDPE skins for optics. The seal layer thickness can be adjusted to achieve a target seal initiation temperature. Blending with high-viscosity LDPE improves melt strength but dilutes dart impact; blending with HDPE raises modulus but reduces tear resistance. The grade should not be blended with polypropylene or incompatible ionomers without compatibility testing. Avoid direct contact with copper-based stabilizer packages if long-term oxidative stability is required.

    Is the Regulatory Basis Sufficient for High-Temperature Food Contact?

    Food-contact suitability depends on the finished article, not on the resin pellet. Olefin polymers of this class may be used in contact with food under 21 CFR 177.1520(c) when the polymer is produced with permitted catalysts and additives, and when the finished article meets extractive specifications for the intended food type and temperature. A resin compliance statement for an unfilled, unmodified FG31D article does not eliminate the need for migration testing if the food-contact condition exceeds the limitations of the regulation. High-temperature food contact above 100 °C may require specific migration testing under EU No 10/2011 or total migration testing under FDA 21 CFR 177.1520(c)(2) depending on jurisdiction. The grade should not be used in boiling-water or retort applications without verification because seal integrity and additive migration change with thermal history.

    Regulatory and test anchors relevant to FG31D film end uses
    Standard or regulationDesignationRelevance
    FDA food contact21 CFR 177.1520Olefin polymer compliance for food-contact articles
    EU food contactEU No 10/2011Overall migration and specific migration limits
    Melt flow rateASTM D1238Material identity and consistency
    DensityASTM D1505Solid-state structure and crystallinity proxy
    Dart impactASTM D1709Film impact toughness
    Elmendorf tearASTM D1922MD/TD tear resistance
    Tensile propertiesASTM D882Film tensile strength and elongation
    Seal strengthASTM F88Heat seal strength of flexible film

    In a high-speed carrier-bag line using a 75 mm grooved-feed extruder, a 250 mm die with 2.2 mm gap, and a 2.8:1 blow-up ratio, butene LLDPE of this class is typically run at melt temperatures near 205 °C to 215 °C. The bubble is quenched by a dual-lip air ring with lower-lip flow adjusted to maintain venturi control and upper-lip flow adjusted to cool the expanding bubble. Winder tension must be controlled to avoid flatness defects; excessive winding tension can stretch the film and reduce apparent dart impact under ASTM D1709. For printed films, corona treatment should maintain a surface energy of 38 mN/m to 42 mN/m as measured by ASTM D2578; lower values reduce ink adhesion, while higher values can cause backside adhesion and blocking. Published data for FG31D-specific performance on that exact line configuration is limited, but the operating envelope is typical for medium-molecular-weight butene LLDPE.

    Top