| HS Code | 715822 |
| Product Name | Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) Copolymer |
| Comonomer | Butene-1 |
| Form | Pellets |
| Color | Natural |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield Md | 10 MPa |
| Tensile Strength At Yield Td | 9 MPa |
| Tensile Strength At Break Md | 30 MPa |
| Tensile Strength At Break Td | 25 MPa |
| Elongation At Break Md | 500% |
| Elongation At Break Td | 700% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 450 g |
| Haze | 12% |
| Gloss 45 | 55% |
| Coefficient Of Friction | 0.20 |
| Processing Temperature | 180-220 °C |
As an accredited Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem FG31 LLDPE copolymer packaged in 25 kg polyethylene bags, palletized and stretch-wrapped, 1,000 kg per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer, palletized bags, sealed, securely stowed for ocean freight. |
| Shipping | Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer is shipped as solid resin pellets in 25 kg PE bags or bulk containers, palletized and stretch-wrapped. Transport in clean, dry, covered vehicles. Store cool, dry, away from heat, sunlight, and ignition sources. Not regulated as dangerous goods. |
| Storage | Store Braskem FG31 LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging closed and pallets stable to prevent moisture, contamination, and spillage. Avoid prolonged UV exposure and excessive stacking pressure. Maintain ambient temperatures; use good housekeeping because pellets can create slippery floors. |
| Shelf Life | Braskem FG31 has a shelf life of 24 months when stored in original unopened packaging, dry, away from sunlight, at moderate temperatures. |
On rotary stretch-wrap lines converting 23 µm machine film at pre-stretch ratios of 200–270%, Braskem FG31 is specified as the core layer in a three-layer A/B/C coextrusion where the outer skins carry cling and puncture response. The resin is supplied with a nominal density of 0.918 g/cm³ under ASTM D1505 and a melt index of 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg. These values place the core melt in the high-viscosity region needed for bubble stability at thin gauges. Single-screw extruders from 45 mm to 75 mm with 24:1–30:1 L/D barrier screws and die diameters between 200 mm and 350 mm operate at melt temperatures of 195–215 °C. Die gap is held at 1.0–1.5 mm; blow-up ratio is maintained between 2.5:1 and 3.0:1. Frost line height is positioned 600–900 mm above the die face. The outer layers are typically metallocene-catalyzed ethylene-hexene copolymers or EVA compounded with polyisobutylene tackifier at 0.5–1.5 wt%. In this configuration, FG31 contributes load-holding stiffness to the 12–25 µm film while the skins control cling and unwind noise. At output rates above 350 kg/h, the process window narrows. If the frost line is too low, transverse direction tear increases. If the frost line is too high, haze rises and pre-stretch recovery declines. Operators adjust dual-lip air ring chiller temperature to 7–12 °C and maintain die land pressure drop below 180 bar to avoid melt fracture. Stretch-film performance is validated according to ASTM D5458 for cling, ASTM D882 for tensile elongation, and ASTM D5748 for puncture resistance. In pallet wrapping, the film must survive 250–300% power pre-stretch at 35–45 wraps/min. Film produced with FG31 in the core generally achieves this when total gauge is not below 20 µm and core layer fraction is controlled at 60–75 wt%. On high-speed rotary arms, edge fold-over and core telescoping are controlled by winding taper tension between 2–6 N per 500 mm width.
Agricultural film converters running 3-layer blown lines with 70–90 mm extruders and 250–400 mm dies produce silage wrap at 25–75 µm total film thickness. FG31 is usually placed in the core at 45–55 wt%, while the outer layers combine LLDPE or metallocene plastomer with carbon black masterbatch at 3–6 wt% and UV stabilizer masterbatch at 2–4 wt%. The processing conflict is the relationship between blow-up ratio and dart impact retention. Blow-up ratio is set between 2.2:1 and 2.8:1 to balance machine-direction and transverse-direction tear propagation. Frost line height is maintained at 8–12 times the die diameter for stable neck geometry. If the frost line is raised beyond 1,100 mm, bubble oscillation increases and film enters the collapsing frame with uncontrolled thickness asymmetry. If the frost line is lowered below 700 mm, film shows higher tensile strength but also excessive transverse-direction shrinkage and poor layflat. Terminal products include round bale wrap, silage bag tubes, and bunker silo cover sheets. For bale wrap, puncture resistance is tested per EN 14932 or ASTM D5748. Tensile properties follow ISO 527-3. In silage cover applications with 150–200 µm thickness, the film must survive contact with silage effluent and ammonia vapor without pinholes. Converters often coextrude a black inner layer containing 2.5–3.0 wt% carbon black for UV blocking and a white outer layer to reflect solar load. The FG31 core supplies melt strength during high-output conversion at 300–500 kg/h. Post-consumer recyclate should be limited to 15–25 wt% because higher levels can reduce sub-zero dart impact below reusable film thresholds. At ambient relative humidity above 70%, batches containing hygroscopic fillers or rework require hopper drying at 60–70 °C for 2–3 hours to prevent melt-phase hydrolysis of silane-based coupling agents present in some UV masterbatch carriers. Film friction is reduced with slip masterbatch at 500–1,200 ppm erucamide to allow bale wrapping at 20–40 rpm without surface blocking.
Below −25 °C storage temperatures, vertical form-fill-seal packaging of IQF vegetables, frozen fish fillets, and meat portions requires a blown film that retains seal strength and puncture resistance after frozen distribution. In this application, FG31 is dry-blended or compounded with a plastomer at 15–25 wt% and processed into 40–85 µm monolayer or 3-layer film on lines with 45–65 mm extruders. Melt temperature is limited to 180–205 °C because higher heat history increases gel formation and degrades seal initiation consistency. Seal jaws on vertical FFS machines are set between 115 °C and 145 °C, with dwell times of 40–80 ms. FG31 provides the stiffness necessary for high-speed bag forming at 80–110 pouches/min; the plastomer lowers seal initiation temperature by approximately 8–12 °C relative to a 100% FG31 film. Film produced with this structure is tested for seal strength according to ASTM F88/F88M, dart impact per ASTM D1709 Method A, and low-temperature brittleness via ASTM D1790 or ISO 8570. Converters serving the EU market target overall migration below 10 mg/dm² under EU 10/2011; US food-contact compliance relies on FDA 21 CFR 177.1520 olefin polymer requirements. Terminal packaging includes pillow pouches for frozen corn, bottom-gusset bags for seafood, and resealable zipper packs. A processing limitation occurs on vertical FFS mandrels with high film tension: FG31-rich film exhibits higher coefficient of friction than EVA-rich sealant. Slip agent masterbatch is therefore added at 1,000–2,000 ppm erucamide and 500–800 ppm silica to maintain kinetic coefficient of friction below 0.30 when measured per ISO 8295. Excess slip reduces zipper seal integrity and can transfer to seal jaws, so loading must be validated across the full reel width and at 38–42 °C seal jaw surface temperature.
Coextruded heavy-duty films in 100–250 µm thickness are manufactured for flexible intermediate bulk container liners, construction debris sacks, and chemical drum liners. The converter incorporates 30–40 wt% post-industrial in-house reclaim with FG31 as the dilution resin in the core layer. Because reclaim lowers melt viscosity and introduces gels, the extruder configuration shifts from a smooth-bore extruder to a grooved-feed section with 25:1–33:1 L/D and a continuous melt filter using 80–120 mesh screen packs. Barrel temperatures are profiled from 160 °C at the feed throat to 210 °C at the die adapter. Die gap widens to 2.0–3.0 mm to limit melt fracture at throughputs of 400–600 kg/h. Blow-up ratio remains low at 2.0:1–2.5:1 to maximize transverse-direction tear resistance. Frost line height is set at 5–8 times the die diameter. FG31-rich skins, typically 25–30 wt% of total film mass, provide dart impact and surface quality. The recyclate core controls cost and raises modulus. Heavy-duty film is tested for tensile yield and break per ISO 527-3, Elmendorf tear per ASTM D1922, and puncture resistance per ASTM D5748. For chemical drum liners, stress-crack resistance is evaluated according to ASTM D1693, with notched specimens in 10% Igepal CO-630 at 50 °C. The most significant process conflict is an extruder pressure ceiling. Recycled fractions above 40 wt% typically lower melt pressure but increase screen pack change frequency due to gel buildup. A 120-bar head-pressure limit is maintained by adjusting screen pack mesh and reclaim pellet size. Published data for FG31 specifically in high-reclaim chemical drum liner structures is limited; converters validate incoming reclaim melt flow rate per ASTM D1238 at 190 °C/2.16 kg and ash content per ASTM D5630 before line start-up. Drum liner drop testing at −18 °C is performed on filled containers to confirm dart impact retention after reclaim addition.
Adhesive lamination converters running blown film sealant webs at 20–35 µm use FG31 as the inner heat-seal layer in duplex and triplex structures for frozen fruit pouches, salted snack packs, and pet food bags. The blown film line is configured with a 50–75 mm extruder, 1.2–1.8 mm die gap, 2.5:1–3.0:1 blow-up ratio, and a frost line positioned 5–7 times the die diameter. Melt temperature is held between 190 °C and 205 °C. Corona treatment is applied in-line at 1.5–2.5 kW to achieve surface energy of 38–42 dynes/cm, measured using ASTM D2578 dyne solutions. The treated film is laminated to oriented polyester or biaxially oriented polypropylene with solventless polyurethane adhesives at 1.5–2.5 g/m². Seal strength of the laminate is measured per ASTM F88/F88M; the sealant film must maintain consistent seal initiation above 110 °C and survive flex-crack testing per ASTM F392. For food-contact laminates, the EU declaration of compliance follows EU 10/2011 Annex I and II; US compliance follows FDA 21 CFR 177.1520. Terminal packaging includes stand-up pouches with bottom gussets and zipper closures for nuts and snack mixes. A processing boundary occurs with solventless lamination. Unaged films may retain residual slip additives that alter adhesive wetting. Film is therefore released to lamination only after 24–48 hours of post-treatment aging at 20–25 °C and 40–50% RH. If treated film is stored beyond 90 days, surface energy decay below 36 dynes/cm can occur, causing delamination in high-stress pouch corners. For higher-speed flexographic printing, antistatic masterbatch is added at 3–5 wt% to reduce ink dry-back variability on the outer web.
In vapor barrier and temporary containment film production, FG31 is used in 150–300 µm multilayer films for below-slab vapor retarders and hazardous material enclosure. The process uses a 90–120 mm grooved-feed extruder, 2.5–3.5 mm die gap, and 1.8:1–2.2:1 blow-up ratio to limit orientation-induced shrinkage. Films are tested per ASTM E1745 for water vapor permeance with Class A limits below 0.1 Perm. Tensile properties follow ASTM D882. Puncture resistance follows ASTM D1709 and ASTM D5748. FG31 is blended with 10–20 wt% LDPE and 5–15 wt% calcium carbonate masterbatch to improve stiffness and reduce tear sensitivity during staple attachment to framing. The main process conflict is bubble instability at large blow-up ratio with high filler loading. Operators hold frost line below 4 times the die diameter and use internal bubble cooling to maintain gauge uniformity across 1,200–1,800 mm wide layflat. Terminal products include 3-meter-wide under-slab vapor retarders, temporary enclosure films for lead paint abatement, and dust containment barriers. Because wide-web gauge variation above ±5% creates folded edge memory, die bolt adjustment and air ring velocity must be logged per reel. Published data for FG31 in ASTM E1745 vapor retarder structures is limited; converters determine water vapor permeance at 38 °C and 90% RH on finished film rather than on resin correlates. At 10 °C installation temperature, the film must retain tensile elongation above 300% to survive framing movement and foot traffic before slab placement.
| Downstream application | Standard or regulation | Parameter or requirement |
|---|---|---|
| Stretch wrap for pallet unitization | ASTM D5458 | Cling between film layers |
| Stretch wrap for pallet unitization | ASTM D5748 | Puncture resistance |
| Agricultural silage film | EN 14932 | Bale wrap film performance |
| Frozen food packaging | EU 10/2011 | Overall migration below 10 mg/dm² |
| Frozen food packaging | FDA 21 CFR 177.1520 | Olefin polymer food-contact conformance |
| Lamination sealant web | ASTM F88/F88M | Seal strength |
| Lamination sealant web | ASTM D2578 | Wetting tension |
| Protective film backing | ASTM D3330 | Peel adhesion |
Surface-protection films in 30–60 µm thickness are produced as multilayer structures where one skin is a low-tack pressure-sensitive adhesive layer and the opposite skin is an FG31-based backing. The backing layer is typically 50–65 wt% FG31, 15–25 wt% LDPE for bubble stability, and 5–10 wt% of a conductive compound to address static discharge during peeling. Blown film process conditions include 1.5–2.0 mm die gap, 1.8:1–2.4:1 blow-up ratio, and melt temperatures of 180–200 °C to minimize odor and volatile release. Static decay is measured at 12% RH and 23 °C per FTMS 101C 4046 or MIL-PRF-81705D. A decay from 5,000 V to 500 V in under 2.0 seconds is required for clean removal from automotive painted panels. The backing film is tested for elongation at break per ASTM D882 and Elmendorf tear per ASTM D1922. The adhesive layer usually contains 20–35 wt% EVA or ethylene-octene plastomer to produce peel adhesion between 0.05 N/25 mm and 1.5 N/25 mm when tested per ASTM D3330. Terminal applications include masking films for coil-coated metal, ABS appliance panels, and automotive body parts during assembly. A technically limiting factor is high unwind static on fast peeling lines above 100 m/min. FG31 backings without conductive additive can generate surface charges above 15 kV. The conductive compound must be dispersed without raising haze above 25%, requiring a twin-screw compounding pass at 190–210 °C before film extrusion. Published data for conductive FG31-based protection film is limited; converters verify surface resistivity per ASTM D257 and adjust conductive masterbatch loading in 2 wt% increments. Blocking is controlled with low-migration antiblock masterbatch at 800–1,500 ppm loaded in the backing layer only, preventing transfer to the pressure-sensitive adhesive skin during roll storage at 30–40 °C.
Competitive Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer is a linear low-density polyethylene resin classified as an ethylene/α-olefin copolymer for blown film extrusion. The grade is specified in monolayer and coextruded film structures in which downgauging, tear resistance, and predictable bubble stability are controlling process parameters. Regional Braskem technical literature places the nominal density at 0.919 g/cm³ and the nominal melt flow rate at 1.0 g/10 min, with typical acceptance ranges of 0.917–0.920 g/cm³ when determined according to ISO 1183-1:2019 or ASTM D1505, and 0.9–1.1 g/10 min when determined according to ISO 1133-1:2022 or ASTM D1238-20 at 190 °C/2.16 kg. The exact comonomer identity is not disclosed in every regional datasheet beyond the ethylene/α-olefin copolymer designation; therefore, comparative statements involving comonomer length should be verified against the supplier’s certificate of analysis rather than inferred solely from the grade number.
| Assessment area | Standard designation | Typical condition |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 190 °C / 2.16 kg |
| Density | ISO 1183-1:2019 | 23 °C immersion liquid |
| Film tensile properties | ISO 527-3 / ASTM D882-18 | 50 µm blown film |
| Dart drop impact | ISO 7765-1:2004 / ASTM D1709-16a | F50 normalized gauge |
| Elmendorf tear | ASTM D1922 / ISO 6383-2 | MD/TD normalized gauge |
| Seal strength | ASTM F88/F88M-21 | Finished package seal area |
| US food contact | FDA 21 CFR 177.1520 | Finished article |
| EU food contact | EU Regulation 10/2011 | Overall migration testing |
Unlike high-pressure LDPE, FG31 has a predominantly linear backbone with short-chain branches introduced by the comonomer. This molecular architecture produces a narrow melting range, lower melt strength, and higher extensional viscosity under large strain. It also supports higher tensile elongation in the solid state. The grade is not identical to HDPE, which has a density above 0.947 g/cm³ and a higher crystalline fraction. Those structural distinctions control the processing window, additive response, and final film failure mode. Film property comparisons should normalise thickness to 50 µm because dart impact, tear, and tensile values scale with gauge. A datasheet value obtained at 25 µm is not directly comparable to a value obtained at 100 µm; the user must recalculate using the relevant standard’s thickness dependence or request film samples produced at the target gauge. Published data for FG31-specific configurations is limited unless the converter generates its own pilot-line data on the exact die, air ring, and cooling configuration.
On commercial blown film lines, FG31 class resin is run with wider die gaps than high-pressure LDPE. Die gaps are commonly set at 1.6–2.5 mm, whereas LDPE lines may operate at 0.7–1.0 mm. The wider gap reduces wall shear stress at the die lip and delays the onset of sharkskin melt fracture. For linear polyethylene, sharkskin typically appears when the wall shear stress reaches 0.1–0.3 MPa; FG31-specific critical shear stress is not published, so the lower limit should be established by trial runs that measure film surface roughness and haze to ASTM D1003-13 or ISO 14782.
Melt temperature targets are normally 190–230 °C in the adapter and die zones. Operation below 190 °C may increase head pressure and reduce output; operation above 230 °C increases oxidative degradation, die-lip build-up, and gel streaks. The bubble is typically run at a blow-up ratio of 2.0:1 to 3.0:1 and a frost-line height of 4–8 die diameters. Internal bubble cooling is recommended when output exceeds approximately 150 kg/h on dies larger than 200 mm; below that rate, external air-ring cooling is usually sufficient if the die gap is correctly set.
Extruder hardware for LLDPE should use a barrier-type or mixing screw with an L/D ratio of 24:1 to 30:1. Screws designed primarily for HDPE may generate excessive shear heating, while shallow LDPE metering sections may reduce output at constant screw speed. On 45–75 mm extruders, converters often observe an output penalty of 5–15% relative to LDPE at fixed screw speed because the LLDPE melt exhibits higher low-shear viscosity. The actual penalty depends on metering depth, compression ratio, and barrel temperature profile. On a 65 mm grooved-feed blown film line, a start-up sequence that heats the barrel to 180 °C and then steps to 210 °C reduces initial motor overload; direct start-up at full production speed can produce pressure spikes above 50 MPa and bubble instability.
Bubble stability can be improved by blending 10–30 wt% of high-pressure LDPE, but this reduces dart impact and tear strength. The trade-off must be evaluated under ASTM D1709-16a and ASTM D1922. If melt fracture persists with a clean die and correct gap, a fluoroelastomer-based polymer processing aid at 200–800 ppm can lower apparent wall shear stress and condition the die after 30–60 min. Rheological response is more Newtonian than LDPE; bubble diameter response to air-ring changes can lag by 2–5 s, so automatic gauge control loops should use longer integral time settings than typical LDPE profiles.
Differences from low-density and high-density resins become measurable when film properties are normalized to 50 µm and tested under ISO 527-3 or ASTM D882-18. The linear backbone of LLDPE provides higher tensile strength at break and elongation than high-pressure LDPE at comparable density because short-chain branches permit tie-molecule entanglement without the globular long-chain branching that restricts strain hardening. High-density polyethylene at densities above 0.947 g/cm³ has higher secant modulus and yield stress but lower dart impact and lower machine-direction Elmendorf tear; FG31 class resin occupies the intermediate density range where low-temperature impact is balanced against stiffness. Relative to octene-based LLDPE of the same nominal density and MFR, butene-based grades typically show lower dart impact and tear strength in class-typical data collected under ASTM D1709-16a and ASTM D1922; the quantitative offset for FG31 must be obtained from the current datasheet because comonomer length and distribution are grade-specific. For converters using existing LDPE tooling, FG31 generally requires die-gap widening but allows downgauging without a proportional loss in load-bearing capacity when validated by burst-strength and drop-test acceptance criteria. In coextruded structures, FG31 is typically placed in the core or seal layer to improve toughness and seal integrity, while HDPE or LDPE skins provide stiffness and film surface optics.
Replacement of LDPE by FG31 in heavy-duty sacks with basis weights of 100–160 g/m² alters the seal initiation temperature. LLDPE seal layers typically initiate sealing at 5–15 °C higher than LDPE-rich layers; the exact shift depends on comonomer content, film thickness, and dwell time. Converters should re-verify the seal curve using ASTM F88/F88M-21 and ASTM F2029-16 before changing film structures, because converting machine profiles optimised for LDPE can produce weak seals or excessive film thinning at the jaw edge.
Mechanical performance in sacks is dominated by dart drop impact and tear resistance. LLDPE film generally exhibits higher dart impact than LDPE of equal thickness; field data on heavy-duty sacks show that gauge reduction of 10–20% is often possible when drop-test acceptance is based on the final filled sack rather than on resin datasheet comparisons. The gauge reduction limit must be established by filled-bag drop tests, such as those described in ISO 7965-2 or end-user specifications, because laboratory dart impact alone does not predict seam and closure failure.
Freezer film and agricultural film are additional reported applications. In freezer film, the resin is specified for service at temperatures down to −20 °C or lower; low-temperature brittleness is lower than for LDPE because the linear backbone retains more segmental mobility at sub-zero temperatures. Agricultural films require UV-stabiliser masterbatch loading; typical addition levels are 2–5 wt% depending on exposure and geographic UV index. The exact grade-specific compatibility with high-loading carbon black or mineral masterbatch should be confirmed by pilot trials. Published data for this specific configuration is limited when combination masterbatch packages exceed 8 wt% total addition. Unless the grade is specifically supplied with slip and antiblock additives, the film may have higher coefficient of friction; converters should add slip/antiblock masterbatch and measure static and kinetic coefficient of friction according to ISO 8295 or ASTM D1894.
Die-lip build-up becomes the primary defect source when melt temperatures exceed 230 °C for extended campaigns. Oxidised material accumulates at the die lip and intermittently detaches into the film as gel streaks. A melt filtration screen pack of 20/40/60 mesh is used to remove crosslinked gels and degraded particles; pressure rise above 10–15% over the clean-screen baseline indicates screen blocking. The maximum allowable head pressure should be taken from the extruder manual; many blown film dies have pressure transducers rated to 70 MPa, but continuous operation near that limit reduces screw life and increases energy input.
Purging after shutdown should be performed with a fractional-melt LDPE or a commercial LLDPE purge compound. Polypropylene or PET residues are incompatible and must be avoided because immiscible domains produce fish-eye defects and localised weak spots. Moisture uptake of polyethylene is below 0.01 wt%, so pre-drying is not normally required; however, condensation on cold pellets after outdoor storage should be avoided by allowing 24 h of temperature equilibration when dew-point control is poor. Long-term storage above 40 °C or in direct sunlight accelerates consumption of phenolic antioxidants and can shift melt flow rate during extended warehouse residence.
Food-contact status for FG31 should be confirmed through the regional regulatory statement. Olefin polymer compliance in the United States is typically evaluated under FDA 21 CFR 177.1520; in the European Union, finished packaging must satisfy overall migration and specific migration limits under EU Regulation 10/2011. The neat resin datasheet does not replace end-use migration testing because processing aids, masterbatches, and coextruded layers alter the final film composition.