Braskem Fc31d Lldpe Blown Film Extrusion Polyethylene Copolymer

Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 357358
    Productname Braskem FC31D
    Manufacturer Braskem
    Grade FC31D
    Polymertype Linear Low Density Polyethylene (LLDPE) Copolymer
    Process Blown Film Extrusion
    Comonomer 1-Butene
    Form Pellets
    Color Natural
    Density 0.921 g/cm3
    Meltflowrate 1.0 g/10 min at 190C/2.16 kg
    Meltingpoint 122 C
    Vicatsofteningpoint 100 C
    Tensilestrengthatbreakmd 33 MPa
    Tensilestrengthatbreaktd 30 MPa
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Dartdropimpact 100 g
    Elmendorftearmd 200 g
    Elmendorfteartd 300 g
    Haze 14%
    Gloss45 70
    Coefficientoffriction 0.2

    As an accredited Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem FC31D LLDPE copolymer is typically packaged in 25 kg moisture-resistant polyethylene bags, 55 bags per pallet, stretch-wrapped.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Braskem FC31D LLDPE blown film extrusion polyethylene copolymer, palletized 25 kg bags, shrink-wrapped in dry container.
    Shipping Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer ships as non-hazardous solid pellets in 25 kg bags or 1000 kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, protected from moisture, heat, sunlight, and contamination. No dangerous-goods labeling required; store indoors under standard industrial hygiene.
    Storage Store Braskem FC31D LLDPE in original, closed containers/packages in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, sparks, flames, and strong oxidizers. Protect from moisture, dust, and contamination. Avoid excessive stacking or pressure that may deform pellets. Maintain good housekeeping; use first-in, first-out stock rotation. Consult SDS for specific temperature and handling limits.
    Shelf Life Shelf life is typically 2 years from manufacture when stored in original packaging, cool, dry, and away from direct sunlight.
    Application of Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer

    On high-throughput tubular film lines producing heavy-duty shipping sacks and industrial liners, Braskem FC31D is processed as the primary sealable core resin or as a 15–25 wt% let-down component in blends with high-pressure LDPE. The base resin has a density of 0.918 g/cm³ by ASTM D1505 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg by ASTM D1238. Annular dies for this segment use a die gap of 1.8–2.4 mm. The blow-up ratio is held between 2.0:1 and 2.8:1. Adapter melt temperature is limited to 190–220 °C.

    The controlling process conflict in heavy-duty sack production is frost-line height selection. A frost-line height of 6–8 die diameters increases quench rate and improves bubble stability on grooved-feed extruders with 24:1–30:1 L/D. It also preserves transverse-direction orientation but can reduce machine-direction tear resistance. A frost-line height of 10–12 die diameters lowers orientation and improves machine-direction tear but increases bubble flutter on wide-gusseted films above 600 mm flat width. Dual-lip air rings with internal bubble cooling are specified when lay-flat width exceeds 800 mm. Dart impact is measured by ASTM D1709 Method A. Elmendorf tear is measured by ASTM D1922. Film thickness ranges from 80 µm to 180 µm. Gusseted tubes are converted on bottom-seal or side-gusset bag machines. Finished articles include FIBC liners, fertilizer sacks, resin pellet sacks, and construction aggregate bags. Published data for this specific configuration is limited; converters generally validate dart impact and tear on a 350 mm pilot die before full-width production.

    What Melt Processing Limits Govern Silage and Greenhouse Film Production with FC31D?

    In silage and greenhouse cover film, the lower melt temperature is set by melt pressure at the die lip. FC31D is extruded at adapter temperatures of 195–210 °C. Bubble stability is maintained at a blow-up ratio of 2.2:1–2.6:1. The frost-line height is positioned at 8–10 die diameters to balance optics and retained tear strength. Die gap is 1.8–2.2 mm. Silage films are generally three-layer structures. The outer layers contain carbon black masterbatch or titanium dioxide concentrates. The centre layer receives hindered amine light stabilisers at 0.2–0.6 wt% and slip/antiblock concentrates at 0.1–0.3 wt%. A LLDPE-carrier masterbatch rather than an LDPE carrier reduces viscosity mismatch in the screw mixing zone. The terminal products include bale wrap at 150–200 µm, silage trench covers at 100–150 µm, and greenhouse side or roof films at 150–200 µm. Weathering performance is evaluated by ASTM G155 or EN 13206 depending on the end-use specification. Acidic silage leachate resistance is not governed by the base polyolefin but by the stabiliser package; converter validation is required for ammonia-rich environments. Published data for this specific configuration is limited.

    Placed in the sealant layer of three-layer or five-layer coextruded barrier films, FC31D provides the low seal-initiation temperature required on vertical form-fill-seal machines. Seal initiation is observed in the range of 95–110 °C for LLDPE blown film grades of this density and melt-index class. Hot-tack strength is measured by ASTM F1921. Seal strength after cooling is measured by ASTM F88. Frozen-food formats use 40–90 µm gauge. Dry-goods pouches commonly use 50–70 µm. Melt temperature in coextrusion is set between 205 °C and 225 °C. Die gap is 1.5–2.0 mm. Blow-up ratio is 2.0:1–2.5:1.

    Food-contact compliance is determined by the full formulation, not by the base resin alone. The olefin polymer is evaluated under 21 CFR 177.1520(c). European converters validate overall and specific migration against EU 10/2011 as amended. Migration testing is conducted by EN 1186-1 and EN 13130-1. Low-temperature toughness for frozen-food packs is assessed by dart impact on ASTM D1709 with films conditioned at -18 °C for 24 h. The conditioning is outside the standard ambient procedure but is common converter practice. Published data for this specific configuration is limited; end-use validation is required because coextrusion quench rates alter sealant-layer crystallinity and additive distribution.

    Pallet Containment Film Blends and Cling Layer Structuring

    On a three-layer blown film line dedicated to stretch hood film, FC31D is used in the core and machine-direction load-bearing layers. Film gauge is between 80 µm and 120 µm. A blow-up ratio of 2.0:1–2.4:1 is set to preserve machine-direction elongation. Die gap is held at 2.0–2.4 mm to avoid melt fracture at high output. Melt temperature is maintained between 190 °C and 220 °C. Stretch hood film requires a balance of stiffness, tear resistance, and puncture resistance. The slip additive system controls cling and release. Erucamide slip at 500–1500 ppm is used for pallet containment films. Coefficient of friction is measured by ISO 8295 or ASTM D1894. Puncture resistance is measured by ASTM D5748. The terminal products are pallet hoods, agricultural wrap, and top sheets. Slip levels above 1500 ppm can produce surface bloom that reduces sealability in folded hood corners. Die-lip deposit formation occurs when low melt temperature is combined with high slip additive concentration. A fluoropolymer processing aid at 400–1000 ppm is used to delay deposit formation. Published industrial data for this specific grade in pallet containment is limited; converters validate on 400 mm dies with three-layer heads.

    Comparative processing window for six downstream conversion regimes
    ApplicationDie gapBlow-up ratioMelt temperaturePrimary test method
    Heavy-duty sacks1.8–2.4 mm2.0:1–2.8:1190–220 °CASTM D1709
    Silage/cover1.8–2.2 mm2.2:1–2.6:1195–210 °CASTM D1922
    Food sealant layer1.5–2.0 mm2.0:1–2.5:1205–225 °CASTM F88
    Pallet hood2.0–2.4 mm2.0:1–2.4:1190–220 °CASTM D5748
    Lamination film1.5–2.0 mm2.0:1–2.6:1195–215 °CASTM D1876
    Protective masking1.2–1.8 mm2.0:1–2.5:1190–215 °CASTM D3330

    When FC31D Is Specified as the Sealable Core Layer in Laminated Bulk Packaging

    Operators specifying FC31D in laminated PP woven bulk bags generally use a blown film of 20–40 µm bonded to the woven substrate. The film is corona-treated inline to 38–42 mN/m. Wetting tension is measured with ISO 8296. Bond strength after lamination is evaluated by ASTM D1876 or by the converting line peel test. The sealant layer forms the inner surface of the bag. Sealing is performed on heat impulse or hot-bar closing systems at 140–180 °C. The low melt viscosity of FC31D relative to LDPE reduces channeling in the seal area but increases the risk of web stretching on adhesive laminators. Tension control is set below 0.2 N/mm per film width for 30 µm gauge. The finished articles include dry bulk FIBC liners, mineral export bags, and chemical cargo sacks. Data for chemical permeation with specific cargoes is limited; converters test with the relevant cargo or simulant according to the transport specification.

    Die Lip Deposits Are Managed by PPA and Reverse Barrel Profiles

    Masking films for stainless steel sheet, PVC profiles, and automotive transit require low gel counts and low visual defect levels. FC31D is run with a fluoropolymer processing aid at 400–1200 ppm to delay die lip deposit formation. The die gap is narrowed to 1.2–1.8 mm for film gauges of 30–60 µm. Blow-up ratio is set at 2.0:1–2.5:1. Melt temperature is held between 190 °C and 215 °C. The low upper limit is selected to reduce gel formation. The penalty is reduced die lip purge interval. A lower melt temperature increases shear stress at the die lip and accelerates deposit formation with some slip and antiblock packages. Barrel temperature profiles are set with a reverse profile: 180 °C in the feed section and 205 °C at the metering section. The raw film is corona-treated to 40–44 mN/m for adhesive coating. Peel adhesion of the finished protective film is measured by ASTM D3330 or FINAT FTM 1. The base resin does not contribute tack; adhesion derives from the coextruded or coated adhesive layer. Incompatibility with solvent-borne adhesives should be tested because low-molecular-weight fractions may migrate and alter peel adhesion over time. Published data for this specific configuration is limited; converters usually approve batches by gel count on a 250 mm blown film pilot line and by 1000 kg extrusion scale-up.

    Free Quote

    Competitive Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem FC31D is a linear low-density polyethylene copolymer supplied specifically for blown film extrusion. The grade is classified under ISO 1872-1 as an ethylene copolymer with a nominal density of 0.918 g/cm³ measured by ASTM D1505 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg measured by ASTM D1238. The polymer architecture is linear rather than long-chain branched, and the short-chain branching distribution is controlled by comonomer incorporation. Producer literature commonly associates FC-series resins with 1-butene as the comonomer, which differentiates the grade from hexene- or octene-based LLDPE materials. The resin contains an antioxidant and processing stabilizer package, but no intentionally added slip or antiblock agents; surface additives must be introduced via masterbatch during extrusion.

    Dense industrial bags, freezer films, agricultural stretch films, and collation shrink overwrap are typical conversion routes for FC31D. On monolayer blown film lines with die diameter between 200 mm and 400 mm, the resin is processed at melt temperatures of 190–230 °C and die gaps of 1.5–2.5 mm. Bubble cooling with dual-lip air rings is recommended when film thickness falls below 25 µm to control gauge variation. The resin feeds uniformly on grooved-feed extruders with barrier screws having length-to-diameter ratios of 24:1 to 30:1; shorter screws without mixing sections tend to produce temperature inhomogeneity and visible gel formation. A blow-up ratio between 2.0:1 and 2.5:1 is conventional for balancing machine-direction and transverse-direction tear properties, while frost line height is held at 6–10 times the die diameter to stabilize the bubble before crystallization completes.

    How Do Melt Fracture and Oxidation Limits Influence Output?

    LLDPE resins of this melt index typically exhibit sharkskin melt fracture at wall shear stresses above approximately 0.14 MPa. For 100% FC31D extrusion, die gap should not be reduced below 1.5 mm unless a fluoropolymer processing aid is included at 200–800 ppm; the processing aid also suppresses die-lip build-up and reduces back pressure. Melt temperatures above 240 °C accelerate thermo-oxidative degradation, producing gels, specks, and color bodies in the film. Temperatures below 180 °C raise melt pressure and reduce output stability. The adapter temperature is optimally maintained at 190–230 °C, with the die lip held 5–10 °C lower to improve bubble stability. Extended hold-up times above 230 °C are incompatible with the stabilizer package and should be avoided during line stoppages.

    Against metallocene-catalyzed LLDPE grades of equivalent density and melt index, FC31D exhibits a broader molecular weight distribution and a less uniform comonomer distribution. This produces lower extrusion pressure and improved bubble stability on conventional blown film equipment, but published comparative studies indicate lower dart impact and higher haze than hexene- or octene-based mLLDPE at matched gauge. In coextruded structures, FC31D is typically placed in core or outer layers where processability and moisture resistance dominate, while mLLDPE is reserved for sealant or abuse layers requiring higher toughness. Compared with LDPE film grades of 0.919–0.924 g/cm³ density, FC31D provides higher dart drop impact and puncture resistance at the same gauge, but lower melt strength and higher motor load. Blends with LDPE at 10–20 wt% are conventionally used on older lines to improve bubble stability; this blend reduces dart impact and Elmendorf tear compared with 100% LLDPE and shifts haze upward.

    Mechanical Property Profile Under ASTM D882 and D1709 Loading

    PropertyTypical ValueTest Method
    Density0.918 g/cm³ASTM D1505
    Melt flow rate1.0 g/10 minASTM D1238
    Tensile strength at break, MD38 MPaASTM D882
    Tensile strength at break, TD32 MPaASTM D882
    Elongation at break, MD750%ASTM D882
    Elongation at break, TD950%ASTM D882
    Dart drop impact, F50120 gASTM D1709-A
    Elmendorf tear strength, MD400 gfASTM D1922
    Elmendorf tear strength, TD500 gfASTM D1922
    Haze13%ASTM D1003
    Gloss at 60°70ASTM D2457

    These values are representative of producer technical literature and are not lot-specific specification limits. Tensile elongation exceeding 700% indicates high chain extension capacity but does not constitute a design allowable. The dart drop median failure energy of 120 g by ASTM D1709-A should be verified on the finished film at the target storage temperature because impact resistance decreases as temperature approaches the glass transition of the amorphous fraction.

    Regulatory Conformance and Food-Contact Boundary Conditions

    FC31D is designed for compliance with olefin polymer food-contact requirements. Compliance depends on final article composition, migration testing, and the specific conditions of use. The following conformance matrix identifies the principal standards applied.

    Standard or RegulationScopeCondition
    FDA 21 CFR 177.1520Olefin polymers for direct food contactSubject to end-use migration limits
    EU Regulation (EU) No 10/2011Plastic materials for food contactOverall migration limit 10 mg/dm²
    REACH (EC) No 1907/2006Registration of monomer and additive substancesRegistered for EU market access
    RoHS Directive 2011/65/EURestriction of hazardous substancesNo intentionally added restricted substances

    For non-food applications requiring low-temperature flexibility, film produced from FC31D remains ductile below -30 °C; however, the upper continuous service temperature for unstressed film is limited to 60–70 °C because of thermal softening. Pre-drying is normally unnecessary when storage humidity remains below 60% RH. Wet resin should be dried at 80 °C for 2 h in a desiccant dryer to prevent surface bubbling and screw slippage. The grade should not be combined with copper-based stabilizers or amine-based additives unless compatibility is confirmed by thermal stability testing. During shutdown, the extruder should be purged with a lower-viscosity LDPE or a commercial purging compound to reduce residual gel formation at the die lip.