Borealis Stamylex™ 1046F LLDPE

    • Product Name: Borealis Stamylex™ 1046F LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 460517
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Butene
    Density 0.920 g/cm³
    Meltflowrate 190c 2 16kg 1.0 g/10 min
    Meltingtemperature 122 °C
    Vicatsofteningtemperature 95 °C
    Tensilemodulus Md Td 220 MPa / 240 MPa
    Tensilestrengthatbreak Md Td 30 MPa / 25 MPa
    Elongationatbreak Md Td 500 % / 700 %
    Dartdropimpact 100 g
    Elmendorftearstrength Md Td 100 g / 200 g
    Haze 12 %
    Gloss 20deg 60 %

    As an accredited Borealis Stamylex™ 1046F LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Borealis Stamylex™ 1046F LLDPE typically comes in 25 kg polyethylene bags on pallets for safe industrial handling and storage.
    Container Loading (20′ FCL) Borealis Stamylex™ 1046F LLDPE loaded in 20′ FCL: 25 kg PE bags on pallets, shrink-wrapped and secured for safe transport.
    Shipping Borealis Stamylex™ 1046F LLDPE ships as non-hazardous polyethylene pellets, typically in 25 kg polyethylene bags on pallets, stretch-wrapped, or in bulk octabins/trucks. It is not regulated for transport. Store dry, away from heat and sunlight; use standard freight and industrial handling. No special transport classification or labels are required.
    Storage Store Borealis Stamylex™ 1046F LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep material in original, labeled packaging, palletized and off the floor. Prevent moisture, dust, and contamination. Avoid prolonged UV exposure and elevated temperatures. Use first-in, first-out stock rotation. Maintain good housekeeping and follow local regulations.
    Shelf Life Shelf life is typically two years when stored unopened in original packaging, dry, below 50°C, away from direct sunlight.
    Application of Borealis Stamylex™ 1046F LLDPE

    Borealis Stamylex™ 1046F is a linear low-density polyethylene film grade with a nominal density of 919 kg/m³ per ISO 1183-1 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. In frozen IQF vegetable packaging, the grade is run in an A/B/A three-layer blown film structure where the core layer contains 60–70 wt% Stamylex 1046F and 30–40 wt% LDPE with an MFR of 0.25–0.5 g/10 min to increase melt integrity; each skin layer is blended at 50 wt% Stamylex 1046F with 50 wt% LDPE of density 0.921–0.924 g/cm³. The ratio is not increased beyond 70 wt% in the core because bubble breathing on 250 mm dies becomes measurable at higher concentrations. Compliance for this direct food contact structure requires EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² according to EN 1186-1:2002, as well as olefin polymer clearance under FDA 21 CFR 177.1520(c) with extractable limits aligned to 21 CFR 176.170(c). Pellet drying is not required at ambient relative humidity below 60%; if silo condensation is observed, a desiccant hopper set at 60 °C for 2 h with a dew point of -20 °C removes surface moisture without thermal degradation.

    Conversion is performed on a three-layer coextrusion line with a die diameter of 250–300 mm, die gap 1.8–2.4 mm, blow-up ratio 2.0–2.8, and frost-line height 600–900 mm; melt temperatures are held between 215 °C and 230 °C to avoid resin oxidation while maintaining adequate film optics. Internal bubble cooling with exhaust dew point below 5 °C stabilizes the bubble at output rates of 25–35 kg/h. A blow-up ratio of 2.0–2.4 yields balanced dart impact and machine-direction tear resistance; exceeding 2.8 BUR on this grade without additional LDPE reduces bubble stability on conventional air-ring systems. The finished product is a gusseted freezer bag or pillow pouch for portioned frozen vegetables, with surface treatment maintained at 38–42 dyne/cm before flexographic or rotogravure printing.

    What Limits Bubble Stability When 1046F Is Blended with LDPE on a 350 mm Die for Heavy-Duty Shipping Sacks?

    Heavy-duty shipping sack film based on Borealis Stamylex™ 1046F is formulated at 70–85 wt% 1046F with 15–30 wt% LDPE of melt index 0.2–0.4 g/10 min. The inclusion of LDPE below 15 wt% is insufficient to suppress high-frequency bubble oscillation on a 350 mm annular die, while LDPE above 30 wt% lowers tear propagation resistance to an extent that sack integrity tests according to ASTM D1922-15a fall below the 120 g acceptance threshold on 120 µm film. The production line is a mono-layer blown film extruder with a 350 mm die, 2.2–2.6 mm die gap, internal bubble cooling, and a dual-lip air ring; lay-flat width is set between 700 mm and 1,100 mm by adjusting blow-up ratio from 3.0 to 3.8. Melt temperature is kept at 215–240 °C, and the frost line is raised to 1,000–1,400 mm to shift molecular orientation toward the transverse direction, reducing pipe-splitting on FFS lines. Melt temperature above 245 °C is avoided because gel formation in the film increases and die lip deposit rates accelerate under continuous production.

    Regulatory compliance for non-food industrial sacks rests on Regulation (EC) No 1907/2006 and Directive 94/62/EC packaging material recovery provisions; mechanical qualification uses ASTM D1709-16a dart impact, ASTM D882-18 tensile, and ISO 527-3 elongational break. Film thickness is set at 120–180 µm depending on fill weight, with 150 µm specified for 25 kg resin sacks. The terminal product is a gusseted form-fill-seal sack for polymer granules, fertilizers, or industrial additives, with valve closure or open mouth dependent on downstream FFS clamp configuration.

    In greenhouse cover converting, Stamylex 1046F is let down into a monolayer blown film formulation at 80–90 wt% with ethylene-vinyl acetate copolymer of 12–18% VA content at 10–20 wt% to raise light transmission and low-temperature flexibility; a hindered amine light stabilizer masterbatch is added at 5–7 wt%, and a silica antiblock masterbatch is added at 3–5 wt%. The governing specification is EN 13206:2017 for thermoplastic greenhouse coverings, with tensile retention after artificial weathering tested under ISO 4892-2 and ISO 527-3, and haze under ASTM D1003-21. UV masterbatch below 5 wt% is not recommended for multi-season covers intended for latitudes above 45°; converter-validated photosynthetically active radiation transmission above 85% at 160 µm thickness is used as an internal quality gate before commercial shipment.

    Processing is completed on a blown film line with a 400 mm die, die gap 2.0–2.5 mm, blow-up ratio 1.8–2.2, melt temperature 220–240 °C, and lay-flat widths up to 3,000 mm for greenhouse arch covers. Because EVA increases oxygen permeability and can lower tear propagation in LLDPE/EVA blends, pressurised air flow is tuned to maintain a constant stalk height of 1,200–1,500 mm; sudden changes in cooling air temperature below 10 °C produce gauge bands that are rejected under ISO 4591 thickness mapping. The terminal product is a multi-season greenhouse cover, silage clamp cover, or bale wrap; when used as silage wrap the formulation is modified with carbon black or UV barrier masterbatch to reduce oxygen ingress below 0.1 m³/m²/day/atm as a control point for anaerobic fermentation systems.

    Lamination Sealant Layers in Complex Flexible Packaging Structures

    A sealant web based on Borealis Stamylex™ 1046F is prepared at 85–95 wt% 1046F with 5–15 wt% LDPE or polyolefin plastomer to depress seal initiation temperature to 85–105 °C for low-distortion sealing against oriented PET or aluminium foil. The web is produced on a three-layer blown film coextrusion line with die diameter 250 mm, die gap 1.6–2.0 mm, blow-up ratio 2.0–2.4, melt temperature 215–230 °C, and final film thickness 40–80 µm. The resulting sealant film is adhesive-laminated to reverse-printed PET at 12 µm or aluminium foil at 7–9 µm using a solventless polyurethane adhesive at 1.8–2.2 g/m² coat weight. Food contact clearance for the sealant web requires FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 with test conditions assigned by food simulant type: 10 days at 40 °C for aqueous foods, 10 days at 60 °C for alcoholic foods up to 20% alcohol, and 10 days at 20 °C for dry foods.

    Seal strength is verified on the laminate using ASTM F88/F88M-21, with minimum seal strength of 18 N/15 mm at 120 °C seal jaw setting. The compliance matrix below applies to converters supplying the EU and United States food packaging sectors; the absence of a listed verification does not remove responsibility for converter-specific migration screening under the finished laminate configuration.

    RequirementStandard or regulationVerification target
    Overall migration in aqueous simulantsEU Regulation (EU) No 10/2011, EN 1186-1:2002≤ 10 mg/dm²
    Olefin polymer clearanceFDA 21 CFR 177.1520(c)Extractables per 21 CFR 176.170(c)
    Good manufacturing practiceFDA 21 CFR 174.5, Regulation (EC) No 2023/2006Traceability and hygiene controls
    REACH SVHC screeningRegulation (EC) No 1907/2006Candidate list check and declaration

    The terminal product is a stand-up pouch, three-side seal sachet, or lidding sealant layer for dried food, frozen food, or liquid condiments. The sealant web is not recommended for retort steam sterilization above 121 °C because seal integrity decline is observed on accelerated ageing under ASTM F1980-21 in high-acid packaged media.

    Because Stamylex 1046F retains high elongational viscosity at low melt temperatures, stretch hood film manufacturers run the grade at 70–85 wt% with 15–30 wt% VLDPE or polyolefin plastomer of density 0.900–0.910 g/cm³ in a three-layer coextruded blown stretch line to achieve machine-direction permanent set below 40% after 200% elongation. The resin combination is processed on a 450 mm die with 2.0–2.4 mm die gap, blow-up ratio 3.5–4.0, melt temperature 215–235 °C, and film thickness 80–130 µm. The line is configured with high-gloss cooling at 12–15 °C to reduce ambient blocking of the cling-free outer layers; when temperature drops below 5 °C, the drawn film becomes prone to transverse thickness variation beyond ±8% on 3,000 mm lay-flat.

    Mechanical qualification follows ASTM D5459-16a for machine-direction elastic recovery and permanent set, ASTM D882-18 for tensile, and ISO 527-3 for elongation at break. For pallet unitization the film is fabricated into gusseted stretch hoods with a lay-flat width of 1,600–2,400 mm and is applied by stretch-hood machines at clamp speeds up to 1.2 m/s; the grade is not intended for high-speed cast stretch wrapping below 15 µm gauge due to its melt flow index and melt elasticity. The terminal product is a heavy-duty stretch hood for building material pallets, bagged cement, or garden products.

    When a Converter Runs 1046F in High-Clarity Collation Shrink Film Below 200 °C Melt Temperature

    In collation shrink film for beverage cans and rigid food containers, Borealis Stamylex™ 1046F is compounded in a 50–70 wt% blend with 30–50 wt% LDPE of density 0.921–0.924 g/cm³ to control the shrink window and reduce free shrink onset below 120 °C. The film is converted on a double-bubble line rather than a single-bubble line because the second bubble orientation fixes both machine-direction and transverse-direction shrink at 4.0:1 and 4.5:1 ratios respectively; the first bubble melt temperature is maintained at 190–220 °C, while the second orientation bubble is heated to 115–130 °C with external air pressure trimmed to prevent gauge bands below 8% deviation. Die diameter is 200–250 mm, die gap 1.4–1.8 mm, and final film thickness is 35–60 µm. Lower melt temperature below 190 °C causes unmolten particle formation in the first bubble, while exceeding 220 °C narrows the shrink window and increases blocking on the second bubble collapsing frame.

    Compliance for collation shrink in retail distribution is based on Directive 94/62/EC and Regulation (EU) No 10/2011 if the film contacts packaged food; shrink tension and shrink percentages are quantified under ISO 14616:2019 and ASTM D2732-20. Published data for the specific combination of 1046F in a 200 mm double-bubble line is limited, so converter-specific shrink-curve development is required before commercial qualification. The terminal product is a clear or printed collation shrink wrap for canned beverages, bottled water, or multipack rigid containers.

    Free Quote

    Competitive Borealis Stamylex™ 1046F LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Borealis Stamylex™ 1046F LLDPE is a solution-polymerised linear low density polyethylene resin intended for monolayer and coextruded blown film. Manufacturer-published nominal values include a density of 0.918 g/cm³ determined according to ISO 1183-1 and a melt flow rate of 1.0 g/10 min at 190 °C under a 2.16 kg load determined according to ISO 1133-1. The polymer is an ethylene-octene-1 copolymer, so the short-chain branching length is longer than that of butene-1-based LLDPE grades at similar density. Film produced at 40 µm gauge is therefore evaluated for dart drop by ISO 7765-1, Elmendorf tear by ISO 6383-2, and tensile properties by ISO 527-3. Thermal analysis by ISO 11357-3 places the peak melting temperature near 122 °C for this density class, while the Vicat softening temperature is typically close to 96 °C under ISO 306/A50.

    The “F” film designation indicates a formulated additive package that typically includes slip and silica-based antiblock. Additive concentration is not fixed by the base resin specification and must be confirmed against the current technical datasheet because it controls film-to-film blocking, coefficient of friction measured by ISO 8295, and haze measured by ISO 14782. Conversion routes include grocery sacks, heavy-duty shipping sacks, laminating films for flexible packaging, and agricultural films where a hindered amine light stabiliser package is added separately for service life.

    The solution polymerisation route for Stamylex™ 1046F produces an LLDPE with a narrower short-chain branching distribution than many gas-phase butene-1 grades. This morphological feature reduces the population of very high-density, rapidly crystallising chains that contribute to haze and low impact in thin blown film. The density of 0.918 g/cm³ corresponds to a crystalline fraction in the region of 38–42% when calculated from differential scanning calorimetry using 290 J/g as the reference heat of fusion for fully crystalline polyethylene. These derived values are not direct resin specifications; they vary with comonomer content and cooling rate. At the specified melt flow rate, the shear viscosity at 190 °C and 100 s⁻¹ is typical of film-grade LLDPE in the 300–700 Pa·s range, but published capillary or rotational rheometry data for this specific configuration is limited and line-specific capillary data should be generated before a screw or die retrofit.

    Why does the processing window narrow below 190°C on high-output blown-film lines?

    On production-scale blown-film lines, the extruder barrel profile is normally set from 40–50 °C at the water-cooled feed throat to 190–210 °C in the compression and metering zones, with adapter and die setpoints of 200–215 °C. Screws with an L/D ratio of 25:1 to 30:1 and a compression ratio of 3.0–3.5:1 are suitable; a Maddock mixer or equivalent dispersive section improves temperature homogeneity. At melt temperatures below 190 °C, shear stress in the die lip region increases sufficiently to induce visible melt fracture on conventional single-lip air rings, especially at die gaps below 1.6 mm. Above 225–230 °C, gel and odour generation accelerate when residence time exceeds 20 min, and the bubble becomes more sensitive to cooling-air instability.

    A typical die gap of 1.8–2.2 mm is used. The blow-up ratio is maintained at 2.2:1 to 3.0:1, and the frost line is positioned between 3 and 7 die diameters. On a representative three-layer line with 50 mm/60 mm/50 mm screw diameters and a 350 mm die, output rates can be raised until the bubble begins to breathe; the first corrective action is to increase internal bubble cooling pressure and raise the frost line rather than increase melt temperature. If the frost line is held below 2 die diameters, film blocking and gauge variation along the bubble circumference both increase. When Stamylex™ 1046F is processed on cast-film lines, the die temperature is usually set between 220 °C and 240 °C, and the chill roll is held at 15–25 °C. An air gap of 8–12 cm is used to maintain draw resonance margins, while draw-down ratios above 20:1 require edge-pinning or vacuum-box adjustment to limit neck-in.

    Moisture-related processing defects are uncommon at warehouse relative humidity below 60%. If surface condensation has occurred, predrying in a desiccant or hot-air hopper dryer at 60 °C for 2 h reduces pinpoint pinholes and surface splay. The resin should not be processed with barrel temperatures above 240 °C if the line is expected to stop for more than 15 min; purge with a lower-viscosity polyethylene and seal the hopper to limit oxidation.

    When compared with a gas-phase butene-1 LLDPE of the same 0.918 g/cm³ density and 1.0 g/10 min melt flow, the octene-1 solution-polymerised structure generally lowers the fraction of high-density, highly crystalline chains. This difference lowers haze and raises dart drop impact and machine-direction tear resistance at equivalent gauge, as measured by ISO 14782, ISO 7765-1, and ISO 6383-2. The longer comonomer also modifies seal initiation behaviour: the onset of acceptable seal strength is generally shifted toward lower temperatures relative to a butene-1 grade, but the exact seal bar temperature must be established on the target form-fill-seal line under ASTM F1921 or a similar pressure- and dwell-controlled method.

    Differences against metallocene LLDPE are more nuanced. Metallocene grades with equivalent density and melt flow can show higher dart impact and better haze performance, but their shear thinning is often less pronounced and extruder backpressure may rise. Stamylex™ 1046F is therefore preferred when existing single-screw extruders lack high-pressure die capability. When bubble stability is insufficient, blending with 10–20 wt% high-pressure LDPE of melt flow 0.25–0.5 g/10 min improves melt strength without requiring a full screw change. The grade is not intended for injection moulding: its 1.0 g/10 min melt flow is too low for thin-wall filling, and the molecular architecture is optimised for film orientation rather than shear-dominated mould filling. For injection moulding or high-speed extrusion coating, higher-MFR grades should be selected.

    Performance parameterStamylex 1046F relative to butene-1 LLDPE at equivalent density and MFRRelevant test method
    Dart drop impact at 40 µmHigher relative ranking; absolute value is line-dependentISO 7765-1
    Elmendorf tear, machine directionHigher relative rankingISO 6383-2
    HazeLower relative rankingISO 14782
    Seal initiation temperatureGenerally lower than butene-1 equivalent; exact value must be measured on lineASTM F1921
    Bubble stabilityLower than high-pressure LDPE; blow-up ratio control is more criticalProcess parameter; no single standard

    Heavy-duty sack producers running 70–120 µm film typically monitor dart drop according to ISO 7765-1 and tensile energy to break according to ISO 527-3. The octene-1 grade is selected when the filled sack must survive multi-drop protocols under ISTA 3A or equivalent distribution tests. The resin does not contain antistat as supplied; dust attraction in agricultural or construction sacks may require a separate antistat masterbatch in the 1–3 wt% range, which must then be retested for food compliance if the package contacts food. For frozen food films at 50 µm, low-temperature impact behaviour is evaluated by dart drop after conditioning at −18 °C for 24 h. The grade is not intended for autoclave retort films because the crystalline melting point is below retort temperatures of 121–134 °C; polypropylene or higher-density polyethylene layers are required in sterilizable structures.

    When food-contact film converting requires low extractables and predictable seal performance

    Stamylex™ 1046F is used in food-contact monolayer and multilayer films where the converter must demonstrate compliance with US FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Under EU legislation, the overall migration limit is 10 mg/dm² or 60 mg/kg according to Annex I, Article 12, using simulants selected under Annex III. The polymer itself, when drawn into film without unidentified post-polymerisation additives, is regarded as an olefin polymer for which compliance documentation is available from Borealis. Finished-article testing remains the responsibility of the converter because migration is governed by layer position, film thickness, sealing layer, and package surface-to-mass ratio.

    Seal initiation temperature must be determined on the target line. A pressure-controlled heat sealer with a 0.5 s dwell time and 1.0 N/mm² jaw pressure is appropriate for comparison, but the result is not directly transferable to a packaging machine with different jaw profile and thermal inertia. A typical measured seal initiation range for this density class falls between 95 °C and 105 °C, but the exact value depends on film gauge, layer sequence, and cooling rate from the blown-film line.

    Regulatory and standards matrix for Stamylex 1046F as supplied

    RequirementStandard or regulationStatus and converter action
    Food-contact olefin polymerUS FDA 21 CFR 177.1520(c)Resin conforms in accordance with manufacturer designation; finished article must be tested.
    Plastic materials in food contactEU Regulation (EU) No 10/2011, Annex I and Article 12Overall migration limit 10 mg/dm² or 60 mg/kg; simulants per Annex III.
    Density test methodISO 1183-1Used for density specification of 0.918 g/cm³.
    Melt flow rate test methodISO 1133-1Used for MFR specification at 190 °C/2.16 kg.
    SVHC communicationREACH Regulation (EC) No 1907/2006, Article 33Converter must verify with supplier for SVHC above 0.1% w/w.

    The table is not a complete legal opinion. It identifies the principal standards used in resin specification and food-contact compliance. For a specific film structure, the converter must validate migration, organoleptic properties, and vacuum or gas-flush packaging performance.

    Storage at ≤40 °C in a dry, ventilated warehouse is required to preserve additive distribution and prevent surface oxidation. The resin should not be stored in direct sunlight because the supplied formulation does not contain a UV stabiliser for long-term exposure; outdoor films require additional HALS and UV absorber addition, typically in the 0.1–0.5 wt% range, depending on exposure and film thickness. The grade is not recommended for continuous service above 70 °C because creep resistance and additive migration accelerate at elevated temperature.

    Processors should avoid contamination with acetal or PVC resins, which can release acidic decomposition products and cause brown specks and odour in polyolefins. Halogenated solvents and strong oxidising agents must not be used for purging or cleaning because they can attack the polymer and create surface defects. If dust or fines accumulate, the lines should be cleaned before starting a food-contact run because fines can increase gel-like visual defects in thin film. Published data for specific configurations is limited; therefore, converter-scale trials under actual die geometry, gauge, and line speed are required before final specifications are fixed.