| HS Code | 223236 |
| Density | 0.926 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Modulus | 250 MPa |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 600 % |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 10 % |
| Gloss | 70 % |
As an accredited Borealis Stamylex™ 1026F LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Borealis Stamylex 1026F LLDPE is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped; 1000 kg bulk bags available. |
| Container Loading (20′ FCL) | Borealis Stamylex™ 1026F LLDPE loaded in 20′ FCL containers as 25 kg bags on pallets, approximately 20–25 tonnes per container. |
| Shipping | Borealis Stamylex™ 1026F LLDPE ships as non-hazardous polymer pellets, typically in 25 kg PE bags on stretch-wrapped pallets or 1000 kg octabins/bulk bags. Transport clean, dry, and sealed. Store away from sunlight, heat, and ignition sources; follow local rules and the supplier’s SDS. Handle with care to prevent package damage. |
| Storage | Store Borealis Stamylex™ 1026F LLDPE indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed in original packaging to prevent moisture, dust, and contamination. Avoid strong oxidizers. Use first-in, first-out stock rotation and protect from prolonged UV exposure and excessive stacking pressure. |
| Shelf Life | Store in original packaging in a cool, dry, well-ventilated place away from direct sunlight; typical shelf life is 24 months. |
On a three-layer cast film line converting Borealis Stamylex™ 1026F, a 1-octene linear low-density polyethylene with nominal density 0.919 g/cm³ per ISO 1183-1 and melt mass-flow rate 2.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022, the core layer is metered at 55–75 wt% of the total layer mass. The outer skin layers receive a blend of 15–25 wt% LDPE, 5–10 wt% metallocene LLDPE, and 1–3 wt% polyisobutylene tackifier masterbatch; edge trim is closed-loop recirculated at up to 15 wt% after grinding and odour-neutralisation. Melt temperature at the die lip is held between 240°C and 260°C, the primary chrome-plated chill roll with surface roughness Rz 0.05–0.10 µm operates at 20–30°C, and the secondary roll at 15–25°C; this two-stage quench stabilises low-gel web formation at line speeds of 350–600 m/min. The dominant failure mode recorded on lines of this type is transverse thickness oscillation when the edge trim fraction exceeds 15 wt%, which disturbs die-lip pressure balance and produces stretch-force outliers in pre-stretch units. Compliance for industrial pallet wrap is limited to Regulation (EC) No 1907/2006 REACH Article 33 and EN ISO 9001 process control; this application is not a direct food-contact structure. Terminal products include machine stretch film rolls of 17–25 µm, hand stretch film of 12–20 µm, and pre-stretched formats with elongation at break measured according to ASTM D882-18.
| Layer | Stamylex 1026F addition | Co-resin split | Additive split | Primary function |
|---|---|---|---|---|
| Core | 55–75 wt% | 20–30 wt% LDPE, 0–10 wt% mLLDPE | 0–3 wt% colour/UV masterbatch | Puncture resistance and retention force |
| Skin | 20–40 wt% | 25–40 wt% LDPE, 20–30 wt% mLLDPE | 1–3 wt% PIB tackifier, 0.5–1.5 wt% antiblock | Cling and unwind noise control |
Bale wrap produced from 1026F blends is typically converted on a mono-layer or three-layer blown film line with a 250 mm die, die gap 1.8–2.4 mm, twin-lip air ring lip angle 15–20°, and blow-up ratio 2.8–3.5. The 1026F fraction is set at 70–85 wt% across the core and outer plies; the remainder comprises 10–20 wt% higher-clarity metallocene LLDPE and 5–8 wt% carbon black-UV stabiliser masterbatch with a polyethylene carrier. Pre-drying of the masterbatch at 70–80°C for 4–6 h is required when ambient RH exceeds 60%, because surface moisture in carbon black creates microvoids and pinhole defects during bubble expansion. Frost-line height is maintained at 2.5–4.0 die diameters to balance dart impact and tear propagation resistance; a lower frost-line position improves dart impact but reduces Elmendorf tear resistance measured according to ASTM D1922-23. Oxygen transmission retention over a 400-day weathering interval is a film-level property governed by carbon black dispersion and film thickness; resin-grade data alone is insufficient for declaring bale wrap service life. The relevant compliance standard is EN 13207:2018, which sets black silage film classification for mechanical durability and oxygen transmission retention; REACH Article 33 applies to the UV stabiliser package. Terminal finished products include 750 mm × 25 µm and 1,000 mm × 30 µm bale wrap rolls for round and square balers.
Where seal initiation temperature must remain below 95°C as measured by ASTM F1921-18 in monolayer or coextruded pouches for frozen vegetables, 1026F is blended at 75–90 wt% with 10–20 wt% high-pressure LDPE to improve bubble stability, plus 2,000–3,500 ppm antiblock and 500–1,500 ppm slip additives. The formulation is processed on a blown film line with a 200–300 mm die, 2.2–3.0 blow-up ratio, and 35:1–45:1 L/D barrier screw; screw geometry is critical because at slip loadings above 1,500 ppm the film enters the nip with reduced friction and exhibits winding wander unless the collapsing frame angle is reduced by 5–10° from standard. Food-contact compliance is anchored to FDA 21 CFR 177.1520(c) 3.1a/3.2a and Regulation (EU) No 10/2011 Annex I, Table 2 overall migration limits of 10 mg/dm²; migration kinetics for the slip additive package must be verified per EN 1186-14 if the pouch fat content exceeds 20 wt%. Terminal product types include frozen vegetable pouches, rice pouches, and dry-mix pillow packs in the 40–70 µm sealant web range.
| Compliance checkpoint | Standard/method | Limit / value |
|---|---|---|
| U.S. food-contact olefin polymer | FDA 21 CFR 177.1520(c) 3.1a/3.2a | Compliant as polyolefin |
| EU overall migration | Regulation (EU) No 10/2011 Annex I, Table 2 | 10 mg/dm² |
| Fatty food simulant migration | EN 1186-14 | As specified for final lamination |
| Density verification | ISO 1183-1 | 0.919 g/cm³ nominal |
| Melt mass-flow rate | ISO 1133-1:2022 | 2.0 g/10 min at 190°C/2.16 kg |
On a 300 mm annular die with a 1.8 mm die gap and 40/80/40 mesh screen pack, 120–180 µm gusseted heavy-duty sacks are produced from a blend of 70–85 wt% 1026F, 10–20 wt% high-pressure LDPE, and 5–10 wt% reprocessed clean edge trim. Increasing the 1026F fraction above 85 wt% raises dart impact retention but simultaneously increases melt pressure at the screen pack by 12–18% and triggers bubble instability at the frost line; below 70 wt%, dart impact measured according to ASTM D1709-22 Method A falls below the accepted threshold for 25 kg petrochemical sack service. The process uses a grooved feed extruder with 30:1 L/D and barrier mixing section to handle the stiffer LLDPE viscosity at 220–240°C; the bubble is collapsed through lower nip haul-off at 8–15 m/min and side gussets are formed before winding. Compliance for transport packaging of dangerous goods requires ISO 7965-1:2004 drop tests after filling and conditioning; the resin alone does not provide a certified sack, but it must support the certified sack structure. Terminal product types include 25 kg petrochemical sacks, mineral filler sacks, and form-fill-seal sacks for synthetic resin powders.
Collation shrink lines operating at 300–450 m/min on 40–60 µm film require a blend in which 1026F is used at 85–92 wt%, with 5–10 wt% LDPE and 2–5 wt% slip-antiblock masterbatch. The shrink response is measured in hot air at 120–150°C using ASTM D2732-20 unrestrained linear thermal shrinkage; typical transverse shrinkage values for this film class are 8–15% and machine-direction shrinkage 5–12%. Published shrinkage data for this exact 1026F-containing blend are limited; tunnel dwell validation is required on the target shrink tunnel with a length of 3–5 m and air velocity 12–18 m/s. 1026F contributes high hot tack because the octene-1 side chains depress the seal initiation point while maintaining the seal plateau above 140°C, measured according to ASTM F1921-18. The main process conflict is that excessive LDPE above 10 wt% increases shrinkage but reduces hot tack and widens the seal temperature window, causing droop in tall multipack bundles when the hot air tunnel temperature fluctuates by more than ±5°C. Compliance is governed by ISO 14616:2004 for shrinkage stress and by REACH for the additive package; direct food-contact status applies only if the film forms the primary package. Terminal products include bottle multipacks, canned goods collation sleeves, and shrink-bundled cartons.
Across blown-film lamination lines with a 350 mm die and polyurethane nip rolls, 1026F is processed as a 40–80 µm sealant web in two-ply and three-ply structures for dry food and non-food laminates. The sealant layer is formulated with 75–85 wt% 1026F, 10–15 wt% LDPE, and 3–7 wt% antiblock masterbatch; where heat-seal peel strength above 4 N/15 mm is required, measured according to ASTM F88/F88M-21, the film enters a post-extrusion lamination nip with a solventless polyurethane adhesive at 1.2–2.0 g/m² dry coating weight. Registration at the laminator unwind is maintained by controlling film surface slip to a coefficient of friction of 0.25–0.45 measured according to ASTM D1894-24; corona treatment of the film surface prior to coating is held at 42–46 dyn/cm to prevent adhesive dewetting. Deviation above the coefficient-of-friction range causes web tracking errors in the adhesive station, while values below 0.25 create blocking at the winder. Industry compliance for food laminates is governed by FDA 21 CFR 177.1520(c) 3.1a/3.2a for the LLDPE layer and Regulation (EU) No 10/2011 Annex I, Table 2 for the complete structure; adhesive and ink layers require separate compliance under 21 CFR 175.105 and Regulation (EU) No 10/2011. Terminal finished products include snack food laminates, cheese overwrap, and retort-shy dry powder sachets.
Competitive Borealis Stamylex™ 1026F LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Borealis Stamylex™ 1026F is a linear low density polyethylene (LLDPE) film-extrusion resin produced via a solution polymerisation route and supplied as pellets. The nominal density is 918 kg/m³ measured according to ISO 1183-1:2019, and the melt flow rate is 2.0 g/10 min at 190 °C under 2.16 kg load in ISO 1133-1:2022. The resin is copolymerised with 1-octene, so the polyethylene backbone carries short-chain branches of six carbon atoms. This differentiates the material from 1-butene-copolymerised LLDPE grades, which carry two-carbon branches, and from high-pressure low-density polyethylene, which contains long-chain branching. The F designation identifies a film-grade additive system rather than a rotomoulding or injection-moulding compound. In cast-film operations, Stamylex™ 1026F is specified where down-gauging, puncture resistance, and stable draw behaviour are required.
The short-chain branch length is not a minor variable; it affects the probability of tie-molecule formation between adjacent lamellae after quench. In 1-octene LLDPE, the longer branch length increases the number of tie molecules at equal density and melt flow rate, producing measurable differences in dart impact and tear propagation. Because the grade is produced in solution polymerisation, gel formation and residual catalyst behaviour differ from gas-phase or slurry LLDPE. Published datasheet values for optical defects and gel counts are lot-dependent, and converters routinely verify them on incoming material before film runs. The resin is not recommended as a direct substitute for high-pressure LDPE in blown-film applications without bubble-stability adjustment, because its linear backbone produces lower melt strength.
On production-scale cast-film lines, the resin is processed through single-screw extruders with 25:1 to 33:1 L/D ratios, typically with barrier screws and screen packs of 100/120/40 mesh configuration. Die-zone melt temperature is maintained between 240 °C and 280 °C. Below 220 °C, surface melt fracture and gauge variation become more probable at commercial output rates; above 280 °C, thermo-oxidative degradation accelerates, and low-molecular-weight fractions can build up on die lips during prolonged runs. A die gap of 0.6 mm to 1.0 mm and chill-roll set points of 15 °C to 30 °C are common. On wide-web lines, a chill-roll temperature gradient greater than ±1.5 °C has been associated with uneven quench and variable optical haze.
The melt flow rate of 2.0 g/10 min permits cast film thicknesses down to 12 µm; thicknesses below 10 µm generally require a higher-melt-index grade or tighter die-gap control. Published capillary rheometry data for this exact grade are limited. Melt flow rate testing under ISO 1133-1:2022 does not describe the shear-thinning behaviour at die shear rates of 100 s⁻¹ to 1,000 s⁻¹, so pre-run rheometer verification is used. Pre-drying is not required when pellet moisture is below 0.05% by weight. If surface condensation occurs at relative humidity above 60%, drying at 60 °C for 2 h is specified to suppress pinholes and surface streaks. Processors should avoid uncontrolled dry blending with amine-based antistatic or antifog additives without extended ageing validation; such systems can alter slip-agent bloom and increase haze.
For coextruded cast film, the resin is used in core or sealant layers with LDPE or metallocene LLDPE skins. On cast stretch-film lines, pre-stretch ratios of 200% to 300% are typical for octene-LLDPE-based formulations, but final values depend on cling-agent concentration, film gauge, and line speed. When blown film is attempted, blending with 10–20 wt% high-pressure LDPE is generally required to stabilise the bubble. Production-scale failure modes observed in cast film operations include edge-trim breaks at high line speeds, die-lip build-up after 8–12 h of continuous running, and gauge bands linked to die-bolt adjustment or chill-roll vibration. The grade’s melt flow rate reduces some viscosity-related gauge variation, but it does not eliminate mechanical alignment issues. Melt filtration is typically monitored by pressure drop; a rise above 60 bar across the screen pack indicates gel accumulation or screen blinding requiring change-out.
The specific advantage of Stamylex™ 1026F over conventional butene-based LLDPE arises from the length of the short-chain branch. 1-Octene inserts a hexyl branch; 1-butene inserts an ethyl branch. At equivalent density and melt flow rate, the longer branch is more effective at creating tie molecules between crystalline lamellae after quench. Generic cast-film datasets for octene-based LLDPE show dart impact improvements of 30% to 60% relative to butene-based LLDPE at 25 µm thickness under ASTM D1709-15a, but published grade-specific values for Stamylex™ 1026F remain limited. The same molecular mechanism influences puncture energy under ASTM D5748 and machine-direction Elmendorf tear under ISO 6383-2, although absolute values depend on quench rate, layer structure, and film thickness.
Compared with metallocene-catalysed LLDPE, the product may exhibit broader molecular weight distribution if conventional Ziegler-Natta catalysis is used for the Stamylex family, as reported in public trade literature. The broader distribution improves extrusion processibility and melt-pressure stability but can reduce ultimate clarity and gloss at equal film thickness. Compared with high-pressure LDPE, the linear backbone lowers melt strength, which is why cast-film processing is preferred and blown-film structures usually require an LDPE blend. Within the Stamylex film range, lower-melt-flow grades are more commonly directed to blown film, while 1026F is positioned for cast film output. In five-layer cast film structures, placing the resin in the core at 30–40% of total thickness can improve toughness while maintaining surface optics; however, the optimum layer distribution is line-specific and is normally confirmed by pilot trials.
Regulatory status for food contact is confirmed through the manufacturer’s compliance declaration. The grade conforms to EU Regulation (EU) No 10/2011 when processed under the conditions specified in the compliance statement, and to FDA 21 CFR 177.1520 for olefin polymers. It is covered by REACH Regulation (EC) No 1907/2006; according to the supplier safety data sheet, no substance of very high concern is present above 0.1% w/w. If the final article is electrical or electronic equipment, RoHS Directive 2011/65/EU applies only when the LLDPE is not cross-linked or compounded with restricted substances. The table below summarises the principal specification and compliance designations.
| Standard or regulation | Scope | Relevance to Stamylex™ 1026F |
|---|---|---|
| ISO 1183-1:2019 | Density of non-cellular plastics | Nominal 918 kg/m³ |
| ISO 1133-1:2022 | Determination of melt flow rate | 2.0 g/10 min at 190 °C/2.16 kg |
| ASTM D1709-15a | Dart drop impact of film | Comparative differentiation vs butene-LLDPE |
| ASTM D5748 | Puncture resistance of stretch wrap film | Low-temperature toughness evaluation |
| EU Regulation (EU) No 10/2011 | Food contact plastics | Manufacturer compliance declaration |
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | End-use dependent |
In vertical form-fill-seal and lamination structures, Stamylex™ 1026F is used in sealant layers where seal initiation temperature and seal strength across a high-speed jaw cycle are limiting parameters. The density of 918 kg/m³ is lower than higher-density LLDPE grades in the 0.923–0.926 kg/m³ range, which generally lowers seal initiation temperature and widens the sealing window. Packaging-line trials using heat-seal testers constructed to ASTM F2029-16 have reported a seal initiation shift of 2–5 °C relative to higher-density LLDPE, although published grade-specific seal curves remain limited. The shift is small in absolute terms but can be operationally significant on high-speed lines with short dwell times.
In frozen food packaging, puncture resistance at -20 °C is evaluated under ASTM D5748; the low density and tie-molecule population reduce brittle fracture relative to fractional-MFR LDPE or higher-density LLDPE. The resin is not recommended for steam sterilisation above 121 °C, continuous hot-fill above 80 °C, or direct contact with strong oxidising agents, because softening and thermo-oxidative degradation compromise mechanical integrity. Injection-moulding and blow-moulding configurations are outside the intended use; published data for those processes are limited. The grade should be stored in dry, clean conditions and protected from prolonged UV exposure to avoid surface oxidation.