| HS Code | 488478 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.922 g/cm³ |
| Meltflowrate | 0.7 g/10 min (190°C/2.16 kg) |
| Meltingpoint | 124 °C |
| Vicatsofteningtemperature | 100 °C |
| Tensilemodulus | 260 MPa |
| Tensilestressatyield | 11 MPa |
| Tensilestressatbreak | 32 MPa |
| Elongationatbreak | 700 % |
| Charpynotchedimpactstrength | 10 kJ/m² (23°C) |
| Hardnessshored | 55 |
| Thermalconductivity | 0.33 W/m·K |
| Waterabsorption | <0.01 % |
| Haze | 13 % |
| Gloss20degree | 60 |
| Dartdropimpact | 120 g |
| Elmendorftearstrengthmd | 200 g |
| Elmendorftearstrengthtd | 300 g |
As an accredited Borealis FG5223 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packaged in 25 kg polyethylene bags, with 55 bags per pallet (1,375 kg total) for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Borealis FG5223 Linear Low Density Polyethylene, 25 kg bags, palletized, ~20 MT net per dry container. |
| Shipping | Borealis FG5223 Linear Low Density Polyethylene is shipped as non-hazardous pellets in sealed moisture-barrier bags, octabins, or bulk trucks/railcars. Transport in cool, dry conditions away from direct sunlight, heat, and ignition sources. Keep containers sealed, palletized, and protected from contamination or moisture ingress. |
| Storage | Store Borealis FG5223 LLDPE in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags or containers closed, clean, and palletized; avoid moisture, dust, and contamination. Prevent static buildup and excessive stacking. Segregate from strong oxidizers. Ensure containers are undamaged and labeled. Follow local regulations and supplier guidance. |
| Shelf Life | Typical shelf life is two years when stored unopened in original packaging, cool, dry, and protected from direct sunlight. |
In heavy-duty industrial sack film, FG5223 is processed as a core or skin layer in coextruded structures where total thickness ranges from 150 µm to 220 µm. The nominal density of 0.922 g/cm³ (ISO 1183-1) and melt flow rate of 0.2 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022) place the grade in a high-molecular-weight film extrusion band that requires sufficient melt temperature to avoid sharkskin and melt fracture. On a 45 mm single-screw extruder with L/D 30:1 and a grooved feed section, processing at melt temperature 200 °C to 225 °C, die gap 1.2 mm to 1.8 mm, and blow-up ratio 2.0:1 to 2.8:1 permits bubble stability while retaining molecular orientation. Frost-line height is typically maintained between 6 and 10 die diameters for this melt index band. When the die gap is narrowed below 1.0 mm, sharkskin defects can appear on the inner bubble surface at higher output rates; widening the gap to 1.4 mm or raising melt temperature above 215 °C reduces defect frequency but shifts the dart impact distribution and may increase transverse-direction shrinkage. Melt pressure ahead of the screen changer under these conditions generally runs 250 bar to 350 bar, depending on screw speed, filter pack condition, and die geometry. Sack conversion operations, particularly filling and dropping filled units from 1.2 m, expose weld seams and gusset folds to high tear stress. Commercial specifications for such sacks frequently define film dart impact by ISO 7765-1 method A, puncture resistance by ASTM D5748, and Elmendorf tear by ISO 6383-2, with the lowest values typically located in the transverse direction of the blown film. In three-layer A/B/A structures, placing FG5223 in both skin layers while using a lower-cost core can improve outer-surface abuse resistance, but overall dart impact depends heavily on layer ratio and haul-off speed. Processors using a 1.6 mm die gap and 2.5:1 blow-up ratio should monitor bubble asymmetry and frost-line oscillation because this grade’s high melt viscosity at low shear rates raises die pressure and can amplify thermal instability when the frost line is set too high. Surface moisture from silo condensation in humid regions may be removed by a hopper dryer set at 60 °C for 2 h; the polymer itself is not hygroscopic. Published data for the exact layer distribution in FG5223-only film is limited, so line validation remains necessary.
Agricultural silage and bale wrap structures specify puncture resistance, tear propagation, and environmental stress crack resistance because the film must survive high-density bale compression, field stubble, and prolonged contact with acidic silage effluent. Standard high-pressure LDPE at similar thickness often lacks the dart impact and slow puncture resistance required for wrapping maize or grass silage without localized extension and puncture failure. In three-layer white/black silage film, FG5223 is commonly positioned in the black inner layer or as the load-bearing core, with total gauge between 120 µm and 180 µm. The white side is formulated with a TiO₂ concentrate, typically dosed at 8 wt% to 12 wt% masterbatch, while the black side uses a carbon black concentrate at 3 wt% to 6 wt% masterbatch; exact loading follows concentrate supplier data and UV stabilization requirements. The low-density linear backbone gives better environmental stress crack resistance than a comparable melt-index LDPE at similar density, a property measured by ASTM D1693 condition B in 10 % Igepal CO-630 solution. Tear propagation in bale film, measured by ISO 6383-2, is more relevant for field damage from stubble and wire ties than tensile yield alone. Dart impact by ISO 7765-1 method B is specified on wrapped bale film because the film must withstand puncture from maize stalks without localized extension. The low melt index of FG5223 means extruder head pressure during silage film production rises more quickly than for a 1.0 g/10 min LDPE; bubble cooling therefore requires a high-capacity dual-lip air ring and, where fitted, internal bubble cooling. Processors who reduce melt temperature below 195 °C may see gel-like visual defects from incomplete homogenization of high-viscosity components, and frost-line movement can cause gauge bands that weaken the wrapped bale. Published agricultural performance data for this specific FG5223 grade under multi-year UV exposure is limited; outdoor life must be verified by artificial weathering under ASTM G155 or natural field exposure before commercial specification.
When FG5223 is used as a sealant web in three-layer blown film or cast coextrusion, seal initiation temperature, hot tack, and coefficient of friction control the conversion window. Seal initiation for a 50 µm blown film made from FG5223 is commonly verified by ASTM F88/F88M seal strength after sealing at 105 °C to 125 °C, 0.3 MPa seal pressure, and 0.5 s dwell; actual thermocouple verification of the seal bar is required because temperature setpoint drift at high line speeds shifts the failure mode from adhesive peel to film break outside the seal. Hot tack is measured by ASTM F1921; in vertical form-fill-seal operations, hot tack should exceed the force generated by product weight immediately after the sealing jaw opens. FG5223 with a density of 0.922 g/cm³ exhibits a broad sealing plateau, but hot tack can decline at high seal bar temperatures more sharply than with higher-alpha-olefin LLDPE grades; seal bar temperatures above 145 °C can cause burnthrough and edge bead instability. For packaging of liquids or powders, a three-layer film with FG5223 as the seal layer at 20 % to 30 % of total thickness provides puncture resistance while maintaining seal integrity. If the film is used for lamination to printed BOPP or PET, corona treatment to 38 mN/m to 42 mN/m by ASTM D2578 is applied before lamination; untreated film below 36 mN/m produces poor ink and adhesive wetting. Slip and anti-block performance downstream of the sealing system are controlled by addition of an erucamide-containing masterbatch at 500 ppm to 1500 ppm active slip and synthetic silica at 1000 ppm to 3000 ppm, although exact loadings depend on gauge and storage time. Processors should avoid combining FG5223 with strong oxidising agents or certain primary amine-based additives in recycled material because these can interfere with heat seal strength and generate organoleptic defects in barrier packaging. Direct food contact in the United States requires converter demonstration of compliance under 21 CFR 177.1520; in the European Union, the final film is evaluated under EU Regulation 10/2011 with overall migration and specific migration limits. FG5223 is not pre-certified for all food types; the packaging structure and additive package determine the migration profile. Published data for the exact hot tack curve of FG5223 in asymmetric coextruded structures is limited; trial work on the production line is required to fix the seal bar profile.
| Application context | Primary failure mode | Test method | Relevant processing variable |
|---|---|---|---|
| Heavy-duty sacks | Dart impact and weld tear | ISO 7765-1 method A, ISO 6383-2 | Die gap, blow-up ratio, layer ratio |
| Agricultural silage film | Field puncture and ESCR | ASTM D5748, ASTM D1693 | Masterbatch dispersion, bubble cooling |
| Sealant web | Seal initiation and hot tack | ASTM F1921, ASTM F88/F88M | Seal bar setpoint, dwell, layer ratio |
| Frozen food packaging | Low-temperature flex cracking | ASTM F392, ISO 7765-1 | Frost line, melt temperature, additives |
| Heavy-duty liners | Puncture and chemical ESCR | ASTM D5748, ASTM D1693 | Recyclate fraction, thickness |
Frozen food packaging films produced with FG5223 require an evaluation of low-temperature abuse resistance rather than ambient tensile properties alone. At storage temperatures between -25 °C and -18 °C, the film must withstand flex cracking and puncture when polybags are stacked and moved in cold-chain distribution; ASTM F392 flex durability and ISO 7765-1 dart impact after conditioning at -18 °C for 24 h are relevant methods. The lower crystalline fraction associated with a density of 0.922 g/cm³ reduces the brittle transition temperature and permits a thinner gauge compared with linear polyethylene of 0.930 g/cm³. However, exact thickness reduction depends on extrusion direction; transverse-direction Elmendorf tear by ISO 6383-2 is frequently the first property to decline when downgauging below 60 µm. In vertical form-fill-seal lines running at 30 bags/min to 60 bags/min, hot tack by ASTM F1921 and seal-through-contamination performance govern production. Frozen food films often incorporate low levels of anti-fog ester-based additives in the inner layer to prevent condensation haze on packaged vegetables; these additives can bloom to the seal surface over time and reduce coefficient of friction, so the slip package must be adjusted to prevent reel blocking. FG5223 can be coextruded with an EVA or plastomer seal layer where extreme sealing speed is required, but pigmented and printed layers must still be corona-treated to 38 mN/m by ASTM D2578 before lamination. Processors should avoid exposing the melt to temperatures above 240 °C for extended residence time because the high molecular weight tail of the material can form gel particles that appear as specks in clear frozen food bags. United States food contact applications require converter verification under 21 CFR 177.1520; European applications fall under EU Regulation 10/2011, with final compliance dependent on the complete film structure and additive package.
The primary function of FG5223 in heavy-duty can liners and industrial liners is to resist slow puncture and tear propagation when filled waste or irregular industrial objects are loaded and compacted. These liners are typically produced at thicknesses of 100 µm to 180 µm for standard service, with heavy-duty waste liners at 200 µm and above. Slow puncture resistance is measured by ASTM D5748, while Elmendorf tear is measured by ISO 6383-2. Environmental stress crack resistance by ASTM D1693 condition B is specified when the liner may contact dilute detergents, surfactants, or oily industrial residues; the low-density linear structure of FG5223 generally improves ESCR relative to high-pressure LDPE at equivalent thickness. In blends with post-industrial or post-consumer LLDPE/LDPE recyclate at 20 wt% to 30 wt%, the dart impact and weld integrity of the liner can fall below acceptance limits. The recyclate fraction must therefore be limited and screened for melt filtration, moisture, and contamination that create pinholes at the gusset folds. Chemical resistance to aliphatic hydrocarbons, dilute acids, and dilute bases is generally acceptable for short-term contact; prolonged exposure to strong oxidising acids, aromatic solvents, or strong chlorinated media is outside the service window. Processors should maintain a stable frost line and avoid excessive blow-up ratio above 2.8:1 when running thick liners because gauge bands near the gusset region can become the initiating point for tear propagation during compaction. This application does not require complex barrier packaging data, but the combination of puncture, ESCR, and weld strength must be validated on the actual liner geometry and fill cycle.
Carrier bag applications of FG5223 are often approached as a downgauging exercise from standard high-pressure LDPE. The LLDPE grade permits a thickness reduction from 60 µm to 70 µm down to 45 µm to 50 µm for comparable dart impact, but the melt strength loss in the bubble requires an LDPE blending partner at 20 wt% to 30 wt%. The blown film line should be run with a blow-up ratio of 2.0:1 to 2.5:1 and a frost-line height no lower than 5 die diameters to maintain side-gusset symmetry. Tear propagation by ISO 6383-2 often determines bag performance during loading, while seal strength by ASTM F88/F88M must be checked after corona treatment. Excessive treatment above 46 mN/m can oxidize the surface and produce slip reversal in high-humidity storage. This segment demands less extensive mechanical data than heavy-duty or frozen-food service, but film producers should still verify dart impact by ISO 7765-1 and transverse-direction tear before approving a downgauging specification.
Competitive Borealis FG5223 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Borealis FG5223 is a linear low density polyethylene supplied as pelletized resin for blown film conversion. The producer’s published release data identify a Melt Mass-Flow Rate (190 °C/2.16 kg) of 2.3 g/10 min measured to ISO 1133-1:2022 and ASTM D1238-20 Procedure A, and a density at 23 °C of 0.922 g/cm³ measured to ISO 1183-1:2019. The grade is classed as a 1-butene-based linear low density polyethylene, with short-chain branching selected to reduce crystallinity and modulus relative to high-density polyethylene. The material is used in general-purpose packaging film, carrier bags, lamination film, overwrap, and hygiene packaging where film toughness, sealability, and extrusion stability are required. Nominal values are release specifications; batch-to-batch variation should be assessed against the supplier’s certificate of analysis, not used as an absolute article acceptance limit.
| Parameter | Reference method | Nominal value |
|---|---|---|
| Melt Mass-Flow Rate (190 °C/2.16 kg) | ISO 1133-1:2022 / ASTM D1238-20 Procedure A | 2.3 g/10 min |
| Density (23 °C) | ISO 1183-1:2019 / ASTM D792-20 | 0.922 g/cm³ |
Because the density is fixed at 0.922 g/cm³, the film exhibits lower flexural modulus and higher elongation at break than a high-density polyethylene of equivalent thickness. The melt flow rate of 2.3 g/10 min places the grade in the medium-MFR LLDPE range used for moderate drawdown, reduced gauge variation, and sealable film structures. The stabilisation package is formulated for normal polyolefin extrusion temperatures; converter-added slip and antiblock masterbatch concentrations therefore control surface friction and blocking behaviour in the final film.
On a production-scale blown-film line equipped with a 75 mm grooved-feed extruder with 30:1 L/D ratio and a 1.8 mm die gap, melt-temperature settings for LLDPE of this density and MFR class are commonly started between 185 °C and 220 °C. The actual profile is adjusted by measuring melt pressure before the screen pack and by monitoring bubble frost-line position. Because FG5223 has a Melt Mass-Flow Rate of 2.3 g/10 min, it enters the shear-thinning regime at lower shear rates than a fractional-MFI LLDPE, but it does not develop the strain-hardening behaviour of LDPE.
Die-gap selection should be matched to final film thickness. For gauge targets below 30 µm, a 1.2 mm to 1.6 mm die gap is often used to reduce crystal orientation and improve tear balance; for 50 µm to 80 µm film, a 1.8 mm to 2.4 mm die gap reduces backpressure. When the die gap is narrow, screw speed must be limited to avoid melt-temperature spikes above 230 °C at the die lip. A low-shear barrier screw is preferred, because high-shear mixing sections may increase melt temperature and reduce bubble stability.
Blow-up ratio is typically maintained between 2.0:1 and 3.0:1. Below 2.0:1, transverse-direction tear may decrease because the film becomes more oriented in the machine direction; above 3.0:1, the bubble may seek to oscillate unless internal bubble cooling is active. Frost-line height is controlled from 5 to 10 die diameters. A shorter frost line reduces blocking but can lower machine-direction tensile yield stress when measured to ASTM D882-18.
In coextruded film, FG5223 may be used as a sealant or core layer. On a 5-layer line with 400 mm die diameter and 2.2 mm die gap, skin layers at 15 wt% to 25 wt% of total throughput provide seal performance without dominating mechanical stiffness. Core layers containing HDPE or recycled polymer require a viscosity match; the melt temperature should be held within 10 °C across layers to prevent interlayer distortion. Published data for this specific configuration is limited; converter-scale trials are required to define the stable operating window.
Before physical characterization, films are conditioned at 23 °C ± 2 °C and 50% ± 5% RH according to ISO 291 or ASTM D618 for at least 40 h. Tensile properties are measured on 15 mm wide strips using ASTM D882-18 or ISO 527-3:2018; elongation at break is commonly determined at a crosshead speed of 500 mm/min, while modulus may be measured at 1 mm/min for film below 50 µm. Dart drop impact is tested to ASTM D1709-16a Method A or ISO 7765-1:2004 on 25 µm or 40 µm films, and impact values scale non-linearly with thickness. Elmendorf tear is determined to ASTM D1922 or ISO 6383-2:2019 and is reported separately for machine and transverse directions because blown film is anisotropic. Haze is measured to ASTM D1003-21 Procedure A or ISO 14782:2021; gloss is measured at 60° to ASTM D2457 or ISO 2813:2014. Coefficient of friction is measured to ASTM D1894 or ISO 8295:2006 at a sled speed of 100 mm/min. Because slip and antiblock are not necessarily part of the base stabilisation package, coefficient of friction is strongly influenced by masterbatch concentration; converter-scale values may differ from laboratory film casts.
Compared with low-density polyethylene, FG5223 lacks the long-chain branching that produces extensional-viscosity hardening. LDPE is therefore preferred when a narrow neck-in and high draw stability are required in cast or extrusion-lamination processes. FG5223 is nevertheless used in blown film because its density of 0.922 g/cm³ lowers flexural modulus relative to HDPE and permits thinner high-impact structures. The absence of long-chain branching also reduces melt elasticity, so bubble deformation at high throughput must be controlled by die design, internal bubble cooling, and frost-line adjustment rather than by resin properties alone.
Compared with a single-reactor Ziegler-Natta butene LLDPE with the same nominal density and MFR, the Borstar process used for FG5223 is designed to produce a controlled molecular weight distribution. The distribution influences the shear-viscosity curve, reducing pressure at high shear rates in the die and improving homogenization in the bubble. The material still contains branch-length heterogeneity associated with 1-butene incorporation, so clarity and impact are not equivalent to metallocene-catalysed LLDPE. Published comparative data for this specific configuration is limited; selection should be based on converter extrusion trials rather than nominal property tables.
Against high-density polyethylene film grades, FG5223 has lower tensile modulus, higher elongation at break, and lower resistance to moisture-vapour transmission. Moisture-vapour transmission rate is measured to ASTM F1249 or ISO 15106-1 and is higher than HDPE at equal thickness. This is useful for produce packaging and overwrap, but undesirable for barrier cereal films unless combined with a barrier polymer layer.
Food-contact and hygiene applications require article-specific migration testing. Resin suppliers typically provide a declaration of compliance for unprinted monolayer film under Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520, provided the film is not mechanically altered or contaminated. The overall migration limit under EU 10/2011 is 10 mg/dm² for general food contact; specific migration limits for monomers and additives apply according to the positive list. Under 21 CFR 177.1520, end-use temperature and food type must be within the limitations of the cited paragraphs. The converter remains responsible for final article testing, because printing inks, lacquers, adhesives, and laminated layers change the migration profile.
| Standard or regulation | Reference clause or method | Typical converter documentation |
|---|---|---|
| EU Food Contact Plastics Regulation | EU 10/2011 Annex I and III; overall migration limit 10 mg/dm² | Declaration of compliance from resin supplier for specific article conditions. |
| US FDA olefin polymer | 21 CFR 177.1520 | Supplier letter covering condition of use and food type. |
| REACH | EC 1907/2006 Article 33 SVHC notification | Safety data sheet and product stewardship declaration. |
| RoHS hazardous substances screening | IEC 62321 | Not usually required for unadditivated LLDPE, but converter may test Pb, Cd, Hg, Cr(VI), PBB, and PBDE. |
On vertical form-fill-seal machinery, seal initiation temperature of FG5223 films is assessed by ASTM F88 and ASTM F2029. Seal-bar pressure is usually set from 0.4 N/mm² to 0.7 N/mm² with dwell times from 0.5 s to 1.0 s. A production seal-temperature window of 10 °C to 15 °C above seal initiation is common for this resin class. Overwrap and lamination lines using hot-melt or solventless adhesives should verify interlayer adhesion according to ASTM F904 or ISO 11339; adhesion is governed more by adhesive selection than by the polyethylene surface. The resin should not be processed above 280 °C melt temperature for prolonged residence time. If recycled FG5223 film is reintroduced at levels above 30 wt%, melt-pressure fluctuation and gel-count increase should be monitored because multi-pass stabiliser depletion affects film quality.