Borealis Borstar Le8706 Natural Bimodal Lldpe Jacketing Compound For Energy And Communication Cables

Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables

    • Product Name: Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 926542
    Density 923 kg/m³
    Melt Flow Rate 190 C 2 16 Kg 0.6 g/10 min
    Tensile Strength At Break 25 MPa
    Elongation At Break >600%
    Flexural Modulus 800 MPa
    Vicat Softening Temperature 105°C
    Hardness Shore D 50
    Environmental Stress Crack Resistance Escr >1000 h
    Volume Resistivity >1E14 ohm·m
    Dielectric Constant 1 Mhz 2.3
    Dissipation Factor 1 Mhz 0.0002
    Water Absorption <0.01%
    Processing Temperature 190-230°C
    Uv Stabilization Yes

    As an accredited Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied as natural pellets in 25 kg polyethylene bags, 40 bags per 1000 kg pallet, or 1000 kg octabins.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags of Borealis Borstar LE8706 Natural Bimodal LLDPE Jacketing Compound, securely stowed for ocean transport.
    Shipping Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables is shipped as natural pellets in 25 kg polyethylene bags on stretch-wrapped pallets. It is transported in dry trucks or containers under ambient conditions, classified non-hazardous, and kept dry, clean, and protected from sunlight and excessive heat.
    Storage Store Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original packaging sealed and palletized off the ground to prevent contamination and moisture pickup. Avoid prolonged UV exposure and temperatures above 50°C. Use FIFO stock rotation; condition before processing if stored cold.
    Shelf Life The product's shelf life is typically 24 months from production date when stored dry below 30°C, protected from direct sunlight.
    Application of Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables

    The sheathing line for XLPE-insulated medium-voltage distribution cable to IEC 60502-2:2014 is configured as a 90 mm single-screw extruder with 30:1 L/D ratio and 2.8:1 compression ratio, fitted with a melt pump and pressure die. Borstar LE8706 Natural is metered as 100 parts by mass of the outer sheath compound. When direct-burial UV and mechanical requirements under HD 620 S2 Part 10C are enforced, a carbon black masterbatch is added at 2.5±0.3 parts by mass to achieve a carbon black content of 2.0–2.5% by mass and dispersion rating no greater than 2 under IEC 60811-505:2012. Melt temperature at the die is held at 205±5°C with barrel zones from feed to head at 175°C, 185°C, 195°C, 205°C, and 210°C. Melt pressure is maintained between 180 bar and 240 bar, and screw speed is clamped at 35–60 min⁻¹ to avoid shear heating above 215°C, above which the bimodal high-molar-mass fraction can generate gel particles observed as surface pimples on the sheath. Cooling is staged in three troughs at 20±2°C, 35±2°C, and 45±2°C over a total cooling length of 24 m, supporting line speeds of 15–40 m/min. Sheath thickness is maintained at 2.0–3.4 mm for 12/20 (24) kV three-core constructions, and the jacket layer constitutes approximately 8–14% of total cable mass. The finished product is XLPE-insulated medium-voltage distribution cable for buried or ducted urban networks, rated from 6/10 (12) kV through 18/30 (36) kV depending conductor size.

    Compliance parameterStandard referenceTest condition
    Tensile strength and elongation before ageingIEC 60811-501:201825 mm gauge length, 250 mm/min
    Thermal ageing of sheathIEC 60811-401:2012100°C, 168 h
    Carbon black contentIEC 60811-505:2012Muffle furnace oxidation
    Sheath shrinkageIEC 60811-507:2012100°C, 1 h
    Low-temperature brittlenessASTM D746−76°C

    What Processing Window Prevents Post-Extrusion Shrinkage in Fibre Optic Loose-Tube Cables?

    Fibre optic loose-tube cable sheathing imposes residual stress constraints that are not present in copper conductor cable jackets because a 0.9–1.5 mm jacket with axial shrinkage above 1% produces microbending attenuation in 12–288 fibre counts and breaches the 0.5% maximum permitted by IEC 60794-1-2:2017 for outdoor duct cables. The formulation is run at 100 parts by mass Borstar LE8706 Natural with 3–5 parts by mass of a PE-based colour masterbatch; no processing aid is introduced, and the melt flow rate of 0.7 g/10 min under ISO 1133-1:2022 is retained unless recycled PE regrind is added, which is limited to 10 parts by mass because higher addition dilutes the bimodal tie-molecule population and reduces environmental stress crack resistance in contact with cable filler gels. The extrusion process uses a 65 mm 24:1 L/D single-screw extruder with barrier mixer and a pressure die sized 7.5 mm above the cable core diameter; barrel temperatures are set at 160/170/180/185/190°C, die temperature at 195°C, and melt temperature is held at 190–200°C, below the 210°C upper limit published in the manufacturer’s processing guideline. After the crosshead, the cable enters a water trough segmented at 15°C, 28°C, and 40°C; pay-off and take-up tension is maintained at 12±4 N on aramid strength members to prevent core displacement but not high enough to indent the jacket at line speeds of 30–60 m/min. The terminal product is an outdoor loose-tube or central-tube fibre optic cable for FTTx backbone and distribution networks, compliant with ITU-T G.652.D fibre parameters and IEC 60794-3-10:2014 for duct installation, but not compliant with NFPA 262 plenum requirements because the compound is not flame retardant.

    When Coaxial Drop Cable Abrasion Resistance Is Measured at −20°C, Which Compound Variables Dominate?

    Coaxial drop cable outer jackets respond to cold abrasion through crystalline lamellae thickness distribution and the high-molar-mass fraction of the bimodal molecular weight distribution, not merely Shore D hardness. Borstar LE8706 Natural is introduced at 100 parts by mass; outdoor drop cable jackets add a UV-stabilized carbon black masterbatch at 2.5±0.3 parts by mass to meet weathering resistance under IEC 61196-1:2021 and EN 50117-1:2018, while indoor-outdoor variants use 4–6 parts by mass non-black pigment masterbatch. The jacket is extruded on a 45–50 mm 24:1 L/D single-screw line directly over the aluminium foil or braid shield at melt temperature 180–195°C, screw speed 50–90 min⁻¹, and line speed 60–120 m/min. The die gap is set at 1.8 times the final jacket thickness of 0.8–1.2 mm to permit draw-down without melt fracture, while the shear rate in the die land is kept below 800 s⁻¹ to avoid reducing low-temperature impact strength in cold-climate drop installations. The terminal product is RG-6 and RG-11 coaxial drop cable for HFC, direct-to-home satellite, and cable television systems; the jacket layer typically constitutes 22–28% of cable mass, and the finished cable must pass the jacket cold-bend test at −20°C without visible cracking.

    Industrial instrumentation and control cable sheathing in onshore process plants is specified against resistance to oils, wet trenches, and sunlight where vertical-tray flame propagation is not mandated. Borstar LE8706 Natural is processed at 100 parts by mass with carbon black masterbatch at 2.5±0.5 parts by mass or colour masterbatch at 4–6 parts by mass; the natural resin contains stabilizers sufficient for extrusion but not for long-term outdoor exposure unless carbon black is added. The compliance framework is ANSI/ICEA S-73-532/NEMA WC 57 for control cables with thermoplastic PE jackets, while IEC 60092-350:2020 for shipboard cable materials applies only if project-specific fire performance requirements are waived or replaced, because the compound is not flame retardant and will not meet IEC 60332-3-22 vertical tray flame propagation. On production floors, the jacket is applied using a 60 mm 25:1 L/D single-screw extruder with a crosshead die over screened pairs, foil shields, and binder tapes; melt temperature is 190–205°C, die pressure 140–180 bar, screw speed 30–50 min⁻¹, and line speed 15–35 m/min for cable diameters of 8–18 mm. The process requires low die swell and a draw ratio below 2.0:1, otherwise the jacket indents the underlying polyester binder tape and reduces insulation resistance under wet conditions. The terminal product is 300/500 V or 0.6/1 kV instrumentation and control cable for outdoor open-air installations, chemical plant trays, and buried ducts where thermoplastic sheathing is permitted in non-hazardous or adequately protected routes.

    Low-Voltage Overhead Bundled Cable Sheathing in Rural Energy Distribution

    The use of a bimodal LLDPE jacket in low-voltage ABC lines is governed by long-term UV ageing, tracking resistance under pollution, and peel adhesion to the phase insulator. In this application, the compound is used at 100 parts by mass, and 2.5±0.5 parts by mass of carbon black masterbatch is added to achieve the UV protection level required by HD 626 S2:2018; the carbon black primary particle size is specified below 25 nm without agglomerates larger than 60 μm, because larger agglomerates initiate surface tracking across the sheath under wet polluted conditions. Production is carried out on rotating capstan lines with a 75 mm 25:1 L/D single-screw extruder, pressure extrusion die, and a cooling trough divided into 4 m stages at 20°C, 30°C, 45°C, and 50°C; melt temperature is 200±5°C, and line speed is restricted to 25–50 m/min to limit sheath eccentricity below 5% over the assembled phase conductors. Sheath thickness is set at 1.4–2.0 mm for 0.6/1 kV bundled configurations of 2–5 conductors, with the jacket representing 8–12% of total cable mass. The terminal product is a self-supporting low-voltage overhead bundled cable for rural distribution networks, designed for span lengths of 30–80 m without a separate messenger wire, and tested in accordance with HD 626 S2 and national variants such as NF C33-209 for French installations.

    Free Quote

    Competitive Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables is a natural-colour, bimodal linear low-density polyethylene supplied in pellet form for extrusion of outer sheaths. The polymer is produced in a dual-reactor Borstar process, generating a bimodal molecular weight distribution in which a high-molecular-weight fraction contributes slow crack growth resistance and low-temperature impact strength, while a lower-molecular-weight fraction maintains shear thinning and melt-phase homogeneity. The density is 0.923 g/cm³ when measured under ISO 1183-1, and the melt flow rate is 0.7 g/10 min at 190 °C/2.16 kg under ISO 1133-1. The product is designed for cable jacketing rather than primary insulation; its mechanical properties are therefore assessed by tensile and elongation methods such as ISO 527-2 and IEC 60811-501, while electrical insulation properties are not the primary design criterion.

    A Bimodal Molecular Architecture Engineered for Extrusion Jacketing

    The molecular design is distinguished from unimodal LLDPE by a controlled placement of short-chain branches on high-molecular-weight chains. This architecture increases tie-molecule concentration in the amorphous phase; the increase is measurable as higher environmental stress crack resistance under ASTM D1693-15 condition B. Typical resin properties are summarised in Table 1. The Shore D hardness of approximately 55 under ISO 868 and flexural modulus of approximately 350 MPa under ISO 178 place the compound between low-density polyethylene and medium/high-density polyethylene jacketing grades in stiffness. The tensile stress at break of approximately 25 MPa and elongation at break above 800% under ISO 527-2 allow the jacket to undergo bending and tensile strain during installation without splitting.

    PropertyTest MethodUnitTypical Value
    DensityISO 1183-1g/cm³0.923
    Melt flow rateISO 1133-1, 190 °C/2.16 kgg/10 min0.7
    Tensile stress at breakISO 527-2, 50 mm/minMPa25
    Elongation at breakISO 527-2%>800
    Flexural modulusISO 178MPa350
    Shore D hardnessISO 868—55
    Low-temperature brittlenessASTM D746°C<-76
    Environmental stress crack resistance, F50ASTM D1693-15, condition B, 10% Igepalh>1000

    The values shown are typical production data and are not specification minima or maxima. Site-specific batch records from pelletising extrusion lines indicate that density and melt flow rate remain stable within the supplier’s published control limits; however, incoming resin should be validated against the melt flow rate and density methods listed above before extrusion. At the molecular level, the Borstar dual-reactor process permits incorporation of longer chains with a higher comonomer content than is possible in conventional single-reactor Ziegler-Natta LLDPE. The resulting crystallinity distribution is broader; the high-density crystallites provide strength, while the low-crystallinity interfacial regions provide ductility. This morphology can be probed by differential scanning calorimetry under ISO 11357-3, where the melting endotherm typically shows a peak near 124 °C.

    What processing boundaries govern thin-wall cable jacket extrusion?

    For thin-wall jackets below 0.5 mm, the limiting variables are melt temperature, die shear rate, and haul-off tension. The compound is processable on single-screw cable jacketing extruders with grooved-feed sections and L/D ratios of 24:1 to 30:1; barrier screws with mixing sections are recommended to homogenise the melt and disperse high-molecular-weight fractions. Capillary rheometry under ISO 11443 shows a pronounced shear-thinning response at shear rates above 100 s⁻¹, which permits higher line speed at a given melt pressure than a unimodal grade of the same melt flow rate. Barrel temperature settings should be adjusted to produce a melt temperature between 205 °C and 225 °C; lower melt temperatures increase melt viscosity and can produce sharkskin on the jacket surface, while sustained exposure above 250 °C may consume the antioxidant package and reduce oxidative stability. Published data for this specific configuration is limited; therefore, each line should establish a melt-temperature profile by thermocouple measurement in the adapter and die.

    Polyethylene is not hygroscopic; therefore, pre-drying is normally unnecessary if pellets are stored indoors and free of surface condensation. When material has been exposed to humid air or condensation, hopper drying at 60 °C to 80 °C for 2 h to 4 h can be applied. Water-cooled trough temperature and haul-off tension must be controlled because residual stress in the jacket is released during shrinkage testing under IEC 60811-503; excessive melt drawdown can produce anisotropic shrinkage and reduce stress crack resistance. The die diameter and draw-down ratio should be selected so that the final jacket thickness is achieved without drawing the melt below its natural die swell; this preserves the high-molecular-weight orientation and prevents slit-edge tearing during cable bending. Drawdown ratios above 3:1 may produce frozen-in strain that later manifests as longitudinal shrinkage after installation.

    Environmental stress crack resistance is evaluated under ASTM D1693-15 condition B in 10% Igepal CO-630 at 50 °C; the bimodal molecular weight distribution delays craze formation and crack propagation, with typical F50 values exceeding 1000 h. For installations in cold climates, the low-temperature brittleness measured under ASTM D746 is below -76 °C. The combination of high elongation at break above 800% and low-temperature ductility reduces the incidence of jacket fracture during low-temperature coiling and cold impact events. Slow crack growth resistance in polyethylene jackets is particularly relevant at stress concentrators such as connector discontinuities, cable ties, and crushing points; the high-molecular-weight fraction increases the number of tie molecules that bridge adjacent lamellae and resist fibril breakage.

    When Natural Resin Replaces Carbon-Black-Filled Jacketing Grades

    The natural form of LE8706 does not contain carbon black and therefore does not provide the UV screening required for long-term outdoor exposure. Outdoor jackets must be processed with a carbon black masterbatch to a final carbon black content of 2.0% to 2.5%, determined by ISO 6964 or ASTM D1603. The carbon black grade and dispersion quality influence weathering performance, and accelerated weathering tests should follow ISO 4892-2 or ASTM G154. Without carbon black, photo-oxidative chain scission under ultraviolet exposure leads to surface crazing, embrittlement, and loss of elongation. The absence of carbon black in the base resin, however, allows reproducible addition of colour masterbatches for indoor communication cables and prevents carbon black carryover into light-coloured jackets.

    Users should verify oxidation induction time after masterbatch addition; the base resin stabilisation package is intended to maintain processability during extrusion, but acidic or metal-containing pigments can deactivate hindered phenolic antioxidants. Avoid blending with unsaturated ester-containing fillers or oils that can migrate to the jacket surface and reduce printability. The product should be stored in a dry area below 40 °C and protected from direct sunlight; if stored in conditions above 60% relative humidity, condensation drying may be required before extrusion.

    Compared with a conventional unimodal LLDPE jacketing compound of similar density and melt flow rate, the bimodal molecular weight distribution of LE8706 provides higher environmental stress crack resistance, often exceeding 1000 h under ASTM D1693-15 condition B, whereas published data for conventional unimodal LLDPE grades in the same test commonly show F50 values below 200 h. The difference is explained by the higher tie-molecule probability in the bimodal high-molecular-weight population. Against a medium-density or high-density polyethylene jacket with density near 0.945 g/cm³, LE8706 has a lower flexural modulus of approximately 350 MPa, reducing the force required for bending the cable around mandrels. Against an LDPE jacketing compound, LE8706 has higher tensile stress at break and improved low-temperature durability, although LDPE may remain more flexible at room temperature. These differences are measurable by the methods listed in Table 1.

    Energy and Communication Cable Jacket Constructions Using LE8706

    In energy cable constructions, the compound is used as an outer sheath over XLPE or ethylene-propylene rubber-insulated cores, where jacket tensile strength and elongation are specified by IEC 60811-501. The density of 0.923 g/cm³ is suitable for low- and medium-voltage cable jackets that require a balance of mechanical protection and installation flexibility. In telecommunication cables, the product is extruded over aluminium/polyethylene moisture barriers; the high stress crack resistance reduces the likelihood of environmental stress cracking at connector strain reliefs. For fibre optic cable outer sheaths, carbon black masterbatch is mandatory for buried or aerial installations, and the dispersion of carbon black in the natural base resin should be assessed by ASTM D5596 or by pressure-impulse testing to detect carbon black agglomerates.

    Jacket thickness can range from 0.3 mm for indoor fibre optic drop cables to several millimetres for heavy-duty energy cable sheaths, with the final thickness controlled by the relevant cable product standard. On production-scale lines, the main processing defects are surface melt fracture at high shear rates, centre-line void formation from excessive draw-down, and carbon black dispersion defects after masterbatch addition. These failure modes are mitigated by adjusting die land length, reducing melt draw-down ratio, and maintaining melt temperature within the range described above. Communication cables installed in ducts may be exposed to pulling lubricants; because lubricants can act as environmental stress cracking agents, chemical compatibility should be evaluated under ASTM D543 for specific site fluids. Published data for this specific configuration is limited; therefore, validation on the target cable line is required.

    Top