Borealis Borstar Fb4250t Lldpe For Blown Film

Borealis Borstar® FB4250T LLDPE for Blown Film

    • Product Name: Borealis Borstar® FB4250T LLDPE for Blown Film
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 598982
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Hexene
    Density 0.942 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.4 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 20 g/10 min
    Melting Temperature 131 °C
    Vicat Softening Temperature 114 °C
    Tensile Modulus 800 MPa
    Tensile Stress At Yield 18 MPa
    Tensile Strain At Yield 10 %
    Tensile Stress At Break 35 MPa
    Tensile Strain At Break 600 %
    Flexural Modulus 800 MPa
    Hardness Shore D 60
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 15 %
    Gloss 60 %
    Coefficient Of Friction 0.20
    Blocking 50 g

    As an accredited Borealis Borstar® FB4250T LLDPE for Blown Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Borealis Borstar® FB4250T LLDPE for Blown Film comes in 25 kg polyethylene bags, 55 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags, approx. 22 MT Borealis Borstar® FB4250T LLDPE for Blown Film, shrink-wrapped and secured.
    Shipping Borealis Borstar® FB4250T LLDPE for Blown Film is typically shipped as non-hazardous polymer pellets in 25 kg polyethylene bags on pallets, octabins, or bulk trucks/containers. Keep dry, protected from sunlight, heat, and contamination. Standard road, rail, or sea freight is used. It should be stored in a cool, dry warehouse.
    Storage Store Borealis Borstar® FB4250T LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed to prevent moisture, dust, and contamination. Do not stack excessively or expose to prolonged UV; use clean, dry handling equipment. Maintain good housekeeping and follow local regulations and supplier recommendations.
    Shelf Life Typically 24 months from production when stored unopened in original packaging, dry, below 50°C, and protected from direct sunlight.
    Application of Borealis Borstar® FB4250T LLDPE for Blown Film
    Borealis Borstar® FB4250T is specified in blown film converting where a bimodal linear low-density polyethylene must combine a melt flow rate of 0.4 g/10 min (190 °C, 2.16 kg, ISO 1133-1:2022) with a density of 0.923 g/cm³ (ISO 1183-1:2019). The route scope below is limited to established blown film downstream sectors; it excludes injection moulding, blow moulding, and extrusion coating. Each application section records the regulatory premise, the blend ratio window, the production equipment, and the terminal article type.
    Application routeEU/international referenceUS referenceRelevant test method
    FFS heavy-duty sacksEU Regulation (EU) 10/2011; ADR 6.1.5.2.4FDA 21 CFR 177.1520(c); US DOT 49 CFR Part 178ISO 527-3:2018; ASTM D1709-16a
    Frozen-food lamination sealant webEU Regulation (EU) 10/2011 Annex IIFDA 21 CFR 177.1520(c)ASTM F88/F88M-21
    Agricultural greenhouse/silage coversEN 13206:2017; REACH Regulation (EC) 1907/2006No direct food-contact referenceEN ISO 4892-2:2013; ISO 527-3:2018
    Collation shrink filmREACH Regulation (EC) 1907/2006; EU Regulation (EU) 10/2011 where food-contactApplication-dependentISO 14616:1997
    UN 13H3 sacksADR 6.1.5.2.4; REACH Regulation (EC) 1907/2006US DOT 49 CFR Part 178ASTM D5748-19; ASTM D1922-15(2020)
    Heavy-duty container linersREACH Regulation (EC) 1907/2006; EU Regulation (EU) 10/2011 where food ingredientFDA 21 CFR 177.1520(c)ASTM D1709-16a; ISO 527-3:2018

    What Limits Bubble Stability When FB4250T Is Processed on High-Stalk Form-Fill-Seal Film Towers?

    High-stalk blown film lines with grooved-feed extruders and screw L/D ratios of 30:1 to 37:1 are the primary conversion route for form-fill-seal heavy-duty sacks. The resin is normally processed at a melt temperature of 190 °C to 215 °C, with a die gap of 1.0 mm to 1.4 mm and a blow-up ratio between 3.0:1 and 4.0:1. Bubble stability becomes the limiting factor when the frost-line height exceeds 8 die diameters or when the extrusion rate is pushed above 350 kg/h on a 300 mm die; below these limits, the grade maintains a stable neck and avoids melt fracture. In a neat 100 wt% FB4250T formulation, the film typically achieves machine-direction tensile values above 35 MPa when tested at 500 mm/min according to ISO 527-3:2018, and dart impact values above 150 g using ASTM D1709-16a method A. Where converters require additional melt strength for lightweighting from 80 µm to 60 µm, a blend of 80 wt% FB4250T with 20 wt% high-pressure LDPE with a melt flow rate below 1.0 g/10 min is substituted; this blend reduces film modulus but raises the bubble's axial stability. Regulatory compliance for food-contact dry goods is based on EU Regulation (EU) 10/2011 Annex I and FDA 21 CFR 177.1520(c), with overall migration testing conducted according to EN 1186-1:2002; for non-food chemical precursors, transportation requirements are set by UN 13H3 where applicable. The downstream finished articles include FFS sacks for cement, granular fertilizer, petrochemical masterbatch, and industrial salts.In lamination converting, the sealant web is produced on three-layer blown film lines where FB4250T forms the inner sealing layer at a thickness of 20 µm to 30 µm within a 45 µm to 70 µm total web. The formulation blends 60 wt% FB4250T with 30 wt% metallocene-catalysed hexene LLDPE and 10 wt% LDPE to widen the heat-seal plateau; a higher FB4250T fraction above 70 wt% reduces hot-tack strength when the web is subjected to dwell times below 0.3 s on rotary pouch equipment. Production conditions include a melt temperature of 185 °C to 200 °C, a die gap of 0.8 mm to 1.2 mm, and a blow-up ratio of 2.0:1 to 2.8:1 to limit transverse orientation. Heat-seal strength is measured on a 25 mm wide specimen in accordance with ASTM F88/F88M-21; converters commonly require seal initiation below 105 °C at a jaw pressure of 0.3 MPa to qualify the web for cold-chain pouches. The downstream converting step uses solventless polyurethane adhesive lamination onto biaxially oriented polyester or polyethylene terephthalate, followed by slitting to 400 mm to 1,200 mm reels. EU food-contact compliance for this structure is evaluated under EU Regulation (EU) 10/2011 Annex II, and US compliance under FDA 21 CFR 177.1520(c). Terminal finished products are primarily frozen seafood and vegetable pouches, lidding film for modified-atmosphere trays, and industrial ingredient pouches.

    Dosing HALS and UVA Masterbatches into FB4250T for Wide-Span Greenhouse and Silage Cover Films

    Addition of the stabiliser masterbatch is performed by gravimetric dosing at the extruder feed throat to maintain a final formulation of 88 wt% FB4250T, 6 wt% LDPE, and 6 wt% additive masterbatch, of which the hindered amine light stabiliser component is 0.3 wt% to 0.5 wt% and the UV absorber component is 0.2 wt% to 0.4 wt%. The film is produced on a monolayer blown film line with internal bubble cooling, a 300 mm die, a die gap of 1.2 mm to 1.6 mm, and a blow-up ratio between 3.0:1 and 4.0:1 to balance machine-direction and transverse-direction tensile strength. Thickness ranges from 120 µm to 200 µm for greenhouse covers and from 60 µm to 120 µm for silage sheets, with frost-line height set higher than for food films to stabilise the large-diameter bubble. Accelerated weathering is assessed according to EN ISO 4892-2:2013 cycle A1, with tensile elongation at break measured according to ISO 527-3:2018; agricultural films are required to retain at least 70% of initial elongation after 6,000 hours of artificial weathering in many EU purchase specifications. The relevant product standard is EN 13206:2017, which covers thermoplastic films for use in agriculture and horticulture; where the film is used as a silage cover inside farms, no direct food-contact migration testing is required, but the masterbatch must comply with the environmental provisions of REACH Regulation (EC) 1907/2006. Terminal finished articles include greenhouse outer covers, silage clamp covers, and temporary crop storage liners.Where shrink force must remain below 2.0 N/cm on collation shrink lines for beverage multipacks, FB4250T is converted as part of a multilayer blown structure rather than as a neat monolayer. The formulation for the structural layer is 70 wt% FB4250T and 30 wt% high-pressure LDPE, while the outer skins are built from metallocene-catalysed hexene LLDPE to raise free-shrink above 50% at 120 °C. Blown film production uses a die gap of 0.8 mm to 1.0 mm, a blow-up ratio of 3.5:1 to 4.5:1, and a low melt temperature of 180 °C to 195 °C to preserve molecular orientation; the bubble is then collapsed and annealed through a series of temperature-controlled rollers before edge trim. Compression shrink force is measured on a 100 mm × 100 mm specimen after 30 s in an oil bath at 120 °C, with the test performed in accordance with ISO 14616:1997. Compliance for collation shrink films is generally limited to REACH Regulation (EC) 1907/2006 and, for direct food-contact bundled packs, EU Regulation (EU) 10/2011 when the film contacts unwrapped food surfaces. Terminal product forms are collation shrink hoods for mineral water bottles, soft drink multipacks, and logistics shrink films for corrugated tray consolidation.

    When a UN 13H3 Dangerous Goods Sack Requires Both Puncture Resistance and Low Creep

    Blending 15 wt% to 20 wt% of a high-density polyethylene with FB4250T raises the plane-strain creep resistance of a hazardous-goods sack without removing the essential tubular bubble stability during conversion. The production route is a high-output three-layer blown film line in which the core layer comprises 80 wt% FB4250T and 20 wt% HDPE, while the outer layers are composed of neat FB4250T to maintain sealing integrity. Extrusion occurs through a 250 mm to 400 mm die with a die gap of 1.0 mm to 1.3 mm, a blow-up ratio of 3.0:1 to 3.6:1, and a melt temperature of 190 °C to 210 °C. The finished converter tests puncture resistance according to ASTM D5748-19 and Elmendorf tear according to ASTM D1922-15(2020); a 100 µm sack film generally requires a machine-direction tear value above 8 N and a puncture resistance above 50 N to pass the UN drop and stacking protocols specified in ADR 6.1.5.2.4 for 13H3. Because these sacks carry pigments, carbon black masterbatch, or low-toxicity chemical powders, food-contact regulatory approval is not required, but the final article must satisfy REACH Regulation (EC) 1907/2006 and, for export to North America, US DOT 49 CFR Part 178 packaging specifications. Terminal finished products are UN 13H3 valve sacks and open-mouth sacks for organic pigments, carbon black, flame retardants, and construction chemicals.

    Heavy-Duty Container Liners in 250–400 µm Basis Weight with Low Gel Count and High Dart Impact

    Extruder screw geometry on high-output three-layer lines is set with barrier screws and mixing sections to deliver a melt temperature of 195 °C to 215 °C, a 300 mm to 500 mm die, a die gap of 1.2 mm to 1.5 mm, and a blow-up ratio of 2.2:1 to 3.0:1; this route is used for container liners that must withstand filling with bulk powders or liquids. The formulation is 90 wt% FB4250T and 10 wt% LDPE, with no calcium carbonate or regrind above 5 wt% because gel counts in the liner wall are directly correlated with leak-site formation on filling stations. Dart impact resistance for a 300 µm liner is measured according to ASTM D1709-16a method B, with acceptance typically above 400 g; tensile modulus is measured according to ISO 527-3:2018, and the expected modulus in the machine direction is above 230 MPa. Regulatory documentation for non-food bulk chemical packaging includes REACH Regulation (EC) 1907/2006 and, for materials exported as food ingredient liners, FDA 21 CFR 177.1520(c) or EU Regulation (EU) 10/2011. The downstream terminal product types include FIBC liners, drum liners, intermediate bulk container liners, and flexible tank liners for liquid polyol and latex intermediates.
    Free Quote

    Competitive Borealis Borstar® FB4250T LLDPE for Blown Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Borealis Borstar® FB4250T is a linear low-density polyethylene resin specified for blown film extrusion. The grade is produced by the Borstar bimodal polymerisation process, in which controlled dual-reactor conditions generate a polymer with a bimodal molecular weight distribution rather than the monomodal distribution typical of conventional gas-phase C4-LLDPE. Nominal density is 0.925 g/cm³ when determined in accordance with ISO 1183-1, and nominal melt flow rate is 0.75 g/10 min when determined at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022. The resin is supplied without intentionally added slip or antiblock additives; post-reactor additive incorporation is left to the converter so that coefficient of friction and blocking behaviour can be tailored for packaging, lamination, or industrial film operations. The molecular-weight split in FB4250T differentiates it from unimodal C4-LLDPE grades by allowing higher melt strength at lower head pressure, which is a processing consequence of a low-molecular-weight fraction that reduces shear viscosity and a high-molecular-weight fraction that stabilises the bubble.

    Bubble Stability and Shear-Thinning Response in Bimodal LLDPE

    During blown film extrusion, the polymer melt experiences shear flow through the annular die and extensional deformation in the bubble formation zone. In a unimodal C4-LLDPE, the same molecular population must satisfy both demands; raising molecular weight improves bubble stability but increases melt pressure at the die. In FB4250T, the low-molecular-weight tail depresses shear viscosity under die-lip shear rates, while the high-molecular-weight tail contributes to extensional viscosity at the lower strain rates experienced in the bubble. Capillary rheometry conducted per ISO 11443 shows a pronounced shear-thinning response relative to a unimodal C4-LLDPE of equivalent density and MFR. Melt strength measured with a Rheotens apparatus per ISO 16790 can be used to monitor lot-to-lot consistency, although published data for this specific configuration is limited. The practical effect is that the bubble remains stable across wider variations in blow-up ratio and frost line height than would be possible with a monomodal resin of the same nominal density.

    Processing lines with die diameters between 50 mm and 250 mm and die gaps from 1.0 mm to 2.0 mm are commonly used for this density and MFR class. Low die gaps increase shear stress and may amplify melt fracture; gaps above 2.0 mm reduce orientation and may lower tear properties. The die gap selected for FB4250T is therefore a function of film gauge, blow-up ratio, and desired tear balance rather than a fixed resin property.

    Because the grade is designed for high-speed monolayer and coextruded film operations, equipment temperature profiles are set to minimise gel formation while maintaining gauge uniformity. Extruders with L/D ratios of 30:1 to 33:1 and barrier screws are typically used. Barrel set points from feed to adapter in the range of 170–210 °C are standard; adapter and die temperatures are held at 190–220 °C. Melt temperature measured at the die should not exceed 240 °C for prolonged periods, because higher temperatures accelerate thermo-oxidative degradation and increase surface oxidation. Back pressure is maintained with a screen pack of 60/80/100 mesh; higher back pressure improves dispersion but reduces throughput. Specific energy consumption on single-screw extruders is typically 0.22–0.28 kWh/kg for this density and MFR class, although the value for any specific line is machine-dependent.

    Blow-up ratio is maintained between 2.0:1 and 3.0:1; a BUR above 3.0:1 can overstretch the high-molecular-weight fraction and produce gel-like surface defects, while a BUR below 1.8:1 can yield excessive machine-direction tear imbalance. Frost line height is set between 5 and 8 times the die diameter. Cooling air volume is adjusted to avoid frost line oscillation greater than ±10 mm, because oscillation at the frost line is directly transmitted to film thickness variation.

    When FB4250T Is Coextruded with LDPE Skins or HDPE Stiffness Layers

    In three-layer blown film structures, FB4250T is often placed in the core layer to contribute puncture resistance and tear strength while skin layers control sealing, slip, or stiffness. Layer ratio depends on end-use gauge: for heavy-duty packaging, a 20/60/20 distribution is common; for thin films, 30/40/30 or inverse structures are used. Coextrusion with LDPE skins lowers seal initiation temperature and improves optical clarity, but the LDPE fraction should not exceed 30 wt% of the total structure if dart impact retention is critical. HDPE skins increase modulus but reduce Elmendorf tear and dart impact; a 5–15 wt% HDPE addition is typically used when stiffness is required without excessive toughness loss.

    Interlayer melt viscosity mismatch is a cause of interfacial instability. Viscosity curves obtained at the shear rate expected at the die lip, typically 10–100 s⁻¹ in annular dies, should be matched within 20–30% at the processing temperature. If the skin and core melt temperatures differ by more than 20 °C, viscosity mismatch may cause wave instability. For FB4250T, melt temperature should be set within ±10 °C of the adjacent LDPE or HDPE melt to minimise interfacial distortion.

    Film-Gauge Property Acquisition and Lot Acceptance Testing

    Film properties are measured on 40 µm monolayer blown film produced under controlled conditions because gauge and orientation history influence all mechanical values. Tensile properties are determined in accordance with ISO 527-3 as machine-direction or transverse-direction specimens cut from tubular film. Dart impact resistance is determined by ISO 7765-1 using the staircase method, while Elmendorf tear resistance is measured under ASTM D1922 or ISO 6383-2. Coefficient of friction is measured under ASTM D1894 or ISO 8295; blocking is measured under ISO 11501 or ASTM D3354. Haze and clarity are determined with ASTM D1003 or ISO 14782. Because FB4250T is supplied without slip or antiblock, friction-related values are not intrinsic resin properties but a function of the additive masterbatch and aging time after extrusion.

    Resin lot acceptance typically includes determination of melt flow rate and density only; conversion-related properties require film extrusion because the pellet form does not carry the orientation or thermal history of the final film. When the film is intended for food contact, the converter must confirm that the finished article complies with the overall migration limit of 10 mg/dm² specified in Regulation (EC) No 10/2011 and with the olefin polymer provisions of FDA 21 CFR 177.1520(c). The base resin is formulated to support these clearances, but compliance of the final article is a function of the complete formulation and processing conditions.

    Compared with metallocene-catalysed LLDPE, FB4250T exhibits lower optical clarity and lower dart impact at equal density but superior bubble stability and lower extruder head pressure. The higher melt strength allows downgauging in applications where film stiffness is maintained by orientation rather than polymer density. For high-clarity packaging, metallocene LLDPE remains the preferred resin; for industrial liners and agricultural films where process robustness and tear propagation resistance dominate, FB4250T is typically specified. The choice between FB4250T and a hexene C6-LLDPE depends on puncture resistance and tear balance: C6-LLDPE often provides greater dart impact at equivalent density, but FB4250T can be processed on narrower die gaps without melt fracture.

    Storage of FB4250T follows standard polyolefin handling. The pellets are supplied in moisture-protected packaging and are not hygroscopic under normal warehousing; pre-drying is generally unnecessary below 60% relative humidity. If surface condensation has occurred, drying at 70–80 °C for 2–4 h using a desiccant dryer is sufficient. The grade should not be processed with halogenated flame-retardant additives at concentrations above those permitted by the relevant electrical or electronic equipment directive, because halogenated species may generate corrosion in the blown film die. Hindered amine light stabilisers are compatible, but acidic additives should be evaluated for catalysed oxidation at melt temperatures above 230 °C.

    What Operational Boundaries Govern Slip and Antiblock Masterbatch Additions?

    Because FB4250T contains no post-reactor slip or antiblock, additive masterbatch dosing is controlled at the throat or through a side feeder. Slip additives such as erucamide are typically added at 300–1000 ppm active content, with higher levels reducing coefficient of friction but increasing surface bloom and potential sealing interference. Antiblock agents, usually synthetic silica or talc, are dosed at 500–3000 ppm; higher levels reduce blocking but increase haze and may reduce dart impact. The concentration must be verified by the converter because additive distribution in blown film depends on screw geometry, melt temperature, and die shear history. When the film is used for printing, migration of slip additives can reduce surface energy below 36 mN/m, and corona treatment may be required to restore ink adhesion.

    The following compliance matrix summarises the principal regulatory and test standards applicable to FB4250T blown film applications.

    Regulatory or standard referenceScope relevant to FB4250T blown film
    ISO 1183-1Density determination by immersion method for polyolefin pellets
    ISO 1133-1:2022Melt mass-flow rate determination at 190 °C and 2.16 kg
    ISO 11443Shear viscosity determination by capillary rheometry
    ISO 16790Melt strength and extensional viscosity measurement for process control
    ISO 527-3Tensile property determination on polyethylene film
    ISO 7765-1 / ASTM D1709Dart impact resistance by free-falling dart method
    ASTM D1922 / ISO 6383-2Elmendorf tear resistance of blown film
    ASTM D1894 / ISO 8295Coefficient of friction of film surfaces
    ASTM D1003 / ISO 14782Haze and luminous transmittance of film specimens
    FDA 21 CFR 177.1520(c)Olefin polymers for food contact; converter must verify end-use conditions
    Regulation (EC) No 10/2011Plastic materials and articles intended to contact food; overall migration limit 10 mg/dm²
    REACH (EC) No 1907/2006Substance registration and SVHC declaration obligations
    RoHS Directive 2011/65/EURestricted substance content limits where applicable to electrical or electronic film components

    High-stalk blown film extrusion, used for heavy-duty sacks and industrial liners, imposes greater extensional strain on the melt because the bubble is drawn over a longer distance at a lower melt temperature. Unimodal C4-LLDPE frequently exhibits lower strain hardening and can tear under these conditions. FB4250T, through its bimodal distribution, provides greater process tolerance; plant trials have shown that the frost line can be raised without losing bubble stability. However, high-stalk operation requires careful control of external cooling because the longer stalk increases melt relaxation time and may lead to gauge variability if air ring baffles are not balanced. In such configurations, the die gap is usually set at the upper end of the LLDPE range, between 1.6 mm and 2.0 mm, to reduce shear stress and preserve the high-molecular-weight fraction for extensional strength.

    Top