| HS Code | 960316 |
| Density | 0.923 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Modulus | 260 MPa |
| Tensile Stress At Break | 30 MPa |
| Tensile Strain At Break | 600% |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 5 N |
| Elmendorf Tear Strength Td | 15 N |
| Haze | 10% |
| Gloss | 80 |
| Seal Initiation Temperature | 105 °C |
As an accredited Borealis Borstar® FB4230 LLDPE for Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Borealis Borstar® FB4230 LLDPE for Film is supplied in 25 kg polyethylene bags, suitable for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL: Borealis Borstar® FB4230 LLDPE for Film in 25 kg bags, 55 bags/pallet, 16 pallets, 22 MT net. |
| Shipping | Borealis Borstar® FB4230 LLDPE for Film is shipped as non-hazardous polymer pellets in 25 kg bags or octabins on pallets. Transport in clean, dry trucks or containers. Avoid moisture, contamination, direct sunlight, and excessive heat. Store in original packaging at ambient temperature; no special dangerous-goods documentation required. |
| Storage | Store Borealis Borstar® FB4230 LLDPE for Film in original, sealed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, and ignition sources. Keep away from strong odors, dust, and contaminants. Stack pallets securely without excessive load. Do not store outdoors. Maintain ambient temperature, good housekeeping, and first-in, first-out rotation to preserve quality. |
| Shelf Life | Borealis Borstar® FB4230 LLDPE for Film: 2-year shelf life if stored dry, below 50°C, in original packaging, away from sunlight. |
Borealis Borstar® FB4230 is a linear low-density polyethylene film resin produced by the Borstar bimodal process. The nominal density is 0.923 g/cm³ and the nominal melt flow rate is 0.4 g/10 min at 190°C under 2.16 kg, measured to ISO 1183-2:2019 and ISO 1133-1:2022. The low melt flow rate and moderate density place FB4230 in the high-molecular-weight film-grade LLDPE envelope, which changes bubble cooling, die pressure, and seal response in downstream lines compared with conventional C4-LLDPE. The scenarios below are separated by process boundary rather than by market label, and each identifies compliance anchors, addition levels, downstream production route, and terminal product types.
| Application scenario | Primary compliance anchors | Typical FB4230 addition range | Terminal product class |
|---|---|---|---|
| Heavy-duty sack and liner | ISO 527-3:2018; ASTM D1709-16a; ASTM D1922-15a; EU 94/62/EC | 75–85 wt% | 80–200 µm sacks and liners |
| Surface protection film | RoHS 2011/65/EU Annex II; REACH 1907/2006 | 60–85 wt% | 30–80 µm masking films |
| Agricultural silage and greenhouse film | EN 13206:2017; EN 14932:2006 | 40–60 wt% | 20–200 µm agricultural films |
| Form-fill-seal laminate web | FDA 21 CFR 177.1520(c); EU 10/2011 | 55–80 wt% | 20–60 µm sealant webs |
| Stretch hood film | REACH 1907/2006 | 50–70 wt% | 80–120 µm pallet hoods |
On three-layer and five-layer blown-film lines producing heavy-duty industrial sacks, FB4230 is run as the core layer at 75–85 wt%; LDPE with an MFR of 0.25–0.7 g/10 min is added at 10–20 wt% to stabilise the bubble, and a processing-aid masterbatch is introduced at 0.02–0.05 wt% only if die-lip build-up or melt fracture becomes visible. The downstream process is defined by grooved-feed extruders with screw diameters of 75–120 mm and L/D ratios of 30:1–33:1, annular die diameters of 350–600 mm, die gaps of 2.0–2.5 mm, blow-up ratios of 2.2:1–2.8:1, and melt temperatures of 195–220°C. Internal bubble cooling is used on lines where total film gauge must remain within ±5%; without IBC, long-term gauge variation in 100 µm sacks increases because the low-MFR resin retains heat longer in the frost-line zone. Output on such lines ranges from 450 kg/h to 650 kg/h, but the rates are constrained by cooling capacity rather than torque. The critical processing boundary is frost-line height: with an MFR of 0.4 g/10 min, the frost line is normally held at 6–8 die diameters; a movement of even ±10 mm can alter MD/TD tear balance and reduce dart impact on high-output lines. Screen-changer pressure behaviour is another operational indicator. On a 90 mm grooved-feed extruder with an 800 µm filter pack, pressure at the breaker plate is typically maintained below 400 bar; when regrind content exceeds 15 wt%, pressure drift of 20–40 bar over a 7-day run has been observed, and the resulting shear-heating shift changes melt temperature at the die lip. Mechanical acceptance is anchored to ISO 527-3:2018 for tensile yield and elongation, ASTM D1709-16a Method A for dart impact, and ASTM D1922-15a for Elmendorf tear; the packaging itself must satisfy heavy-metal and source-reduction provisions under EU Packaging and Packaging Waste Directive 94/62/EC and REACH 1907/2006. Terminal products include 80–200 µm heavy-duty sacks for polymer resin, carbon black masterbatch, precipitated silica, construction chemicals, salts, and mineral fillers, as well as heavy-duty drum liners and inner liners for flexible intermediate bulk containers.
In coextruded temporary protective films for anodised aluminium profiles, polycarbonate glazing, stainless steel sheet, and PVC window sections, FB4230 is placed in the structural core at 60–85 wt%; the skins are compounded from EVA or POE resins at 15–40 wt% to lower heat-seal initiation and supply controlled cling without a pressure-sensitive adhesive masterbatch. The production route is three-layer cast-film extrusion with slot die widths of 450–1,200 mm, die gap 0.8–1.5 mm, chill-roll temperature 18–28°C, and line speed 80–180 m/min; cooling capacity generally limits throughput because the skin layers are more sensitive to chill-roll contact and sticky web transfer. Peel force is determined by the converter against the specific substrate and surface roughness rather than by a single universal standard; where an internal specification is required, the film is evaluated by tensile properties under ISO 527-3:2018 and puncture resistance under ASTM D5748-23 or equivalent substrate-specific methods. Compliance for electrical and electronic applications is driven by RoHS Directive 2011/65/EU Annex II, while REACH 1907/2006 screening applies to all commercial shipments; phthalate and organotin restrictions are mandatory when the film is used on coated metal or glass in enclosed spaces. Terminal products include 30–80 µm protective masking for aluminium composite panel cladding, temporary surface-protection film for stainless steel sheet during bending and laser cutting, and protective film for rigid glazing sheets during transport and installation.
For three-layer agricultural film programmes that alternate silage-wrap and greenhouse-cover formats on the same die, FB4230 is used as the structural core at 40–60 wt% of total formulation; the outer skins carry the functional additive load. UV-stabiliser masterbatch is added at 4–8 wt% to the exposed layer, anti-fog masterbatch at 1–3 wt% where condensation control is specified, and titanium-dioxide white masterbatch at 6–12 wt% for high-reflectance greenhouse cover and basal silage wrap. The manufacturing route is blown-film coextrusion with die gap 1.8–2.4 mm, blow-up ratio 2.2:1–2.6:1, melt temperature 210–230°C, and total thickness 20–30 µm for silage bale wrap or 150–200 µm for multi-season greenhouse cover. A process boundary emerges on lines that switch from silage to greenhouse formats without purging the white masterbatch thoroughly; carrier-polymer residues from the white masterbatch can produce gel-like specks in transparent greenhouse film, and the die gap should be opened by 0.2–0.4 mm during the transition to compensate for the higher additive loading. Compliance is anchored to EN 13206:2017 for agricultural covering films and EN 14932:2006 for stretch silage wrapping film; where the film contacts animal feed, the converter applies Regulation (EC) No 183/2005 feed-hygiene controls and REACH 1907/2006. Published data for FB4230 as a high-tack silage cling layer is limited; the cling skin is normally a different LLDPE or EVA grade. Terminal products include silage bale wrap, high-reflectance greenhouse cover, low-tunnel film, and side-film for multi-bay polytunnels.
Cast-film laminating lines producing sealant webs for BOPP/BOPET/aluminium foil laminates use FB4230 at 55–80 wt% in the sealant layer, diluted with EVA containing 12–18% vinyl acetate or with LDPE at 20–45 wt% to reduce seal initiation and improve hot tack. The cast line is specified with a slot die 1,200–1,600 mm wide, sealant-layer thickness 20–60 µm, matte chill-roll finish Ra 0.4–1.0 µm, and line speed 100–200 m/min. Hot-tack and seal-strength behaviour is measured under ASTM F1921-12 and ASTM F88/F88M-21; seal initiation for a 40 µm cast sealant web is typically checked from 100–115°C, but the actual heat-seal window shifts when the web is laminated to aluminium foil or BOPET because the upper laminate layer changes heat transfer into the sealant. The critical processing risk is substitution without re-setting the sealing equipment. If a converter changes from a conventional C4-LLDPE sealant grade to FB4230 at 50–80 wt% and leaves seal jaw pressure, dwell, and anvil temperature unchanged, leaker formation in vertical form-fill-seal packaging shifts to corner gussets and is detected only by water-bath or dye-penetration testing because the higher-molecular-weight resin requires longer chain diffusion at the seal interface. Barrier and migration compliance for food use is anchored to FDA 21 CFR 177.1520(c), EU Regulation No 10/2011 Annex I with an overall migration limit of 10 mg/dm², and EC Regulation 2023/2006 for good manufacturing practice; where the laminate is used for dairy or high-fat products, the converter must perform migration testing with the final printed and adhesively laminated structure, not the cast web alone. Terminal products include dry-mix pouches, frozen-food flow-wrap, coffee valve bags, lidding films for dairy multipacks, and pillow pouches for powdered drinks.
In five-layer stretch-hood lines, FB4230 is assigned to the central load-bearing layer at 50–70 wt% of total gauge; the two skin layers carry cling and slip packages while the tie layers are selected for layer-to-layer adhesion. Total film thickness is 80–120 µm, and the film is produced by blown-film or cast-film coextrusion followed by transverse welding into hoods. On a 1,200 mm annular die, throughput is usually limited by blocking and creasing on the collapsing frame rather than by extruder torque. Compliance is driven by REACH 1907/2006 and destination-market packaging regulations; there is no single EU harmonised product standard for stretch-hood film, so load retention is generally verified by instrumented stretch-hood testing on the purchaser’s pallet geometry. Published data for FB4230 in sustained high-stretch hood applications is limited; the selected gauge should be validated on the target hooder under 10–15% nominal pre-stretch rather than extrapolated from pallet-wrap film. Terminal products include stretch hoods for palletised household appliances, bagged cement, insulation rolls, and building panels.
Competitive Borealis Borstar® FB4230 LLDPE for Film prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Borealis Borstar FB4230 is a linear low-density polyethylene (LLDPE) designed for blown-film extrusion. The grade is produced through the Borstar bimodal polymerisation process, in which a high-molecular-weight copolymer fraction contributes to melt strength and bubble stability and a lower-molecular-weight fraction contributes to shear thinning and extruder processability. The product is supplied as natural pellets with a stabiliser package; external slip and antiblock additives are not incorporated in the base grade. Borstar FB4230 is differentiated from conventional Ziegler-Natta butene-copolymer LLDPE by its 1-octene comonomer, its nominal density of 923 kg/m³, and its low melt mass-flow rate of 0.4 g/10 min at 190 °C/2.16 kg. The density places it at the upper end of the linear low-density range, giving films higher tensile modulus and creep resistance than a 918–920 kg/m³ butene-LLDPE while retaining tear and impact energy absorption. Table 1 summarises typical physical properties from the manufacturer’s published datasheet; these values are not specification limits and vary with lot and laboratory conditions.
| Property | Typical value | Test method |
|---|---|---|
| Nominal density | 923 kg/m³ | ISO 1183-1 |
| Melt mass-flow rate (190 °C/2.16 kg) | 0.4 g/10 min | ISO 1133-1 |
| Melting temperature (DSC peak) | 124 °C | ISO 11357-3 |
| Vicat softening temperature A50 (10 N) | 100 °C | ISO 306 |
| Comonomer type | 1-octene | — |
The low melt flow rate is not a general-purpose injection-moulding indicator; for blown film it is a deliberate molecular design feature. At equivalent film gauge, the higher molecular weight and bimodal distribution shift the failure mode under dart drop impact from brittle puncture to ductile energy absorption. The property difference is not linear with density and is evaluated using ISO 7765-1 method A. The resin is homogeneous in pellet geometry; silo handling and gravimetric feeder calibration should follow the bulk density stated in the supplier’s certificate of analysis, not a generic LDPE value.
FB4230 cannot be substituted directly into every monolayer line designed for 1.0 g/10 min butene-copolymer LLDPE without process adjustments. The lower ISO 1133-1 melt flow rate indicates higher average molecular weight and higher shear viscosity at the die lip. On a single-screw extruder with a 25:1 L/D smooth-bore barrel and a conventional low-shear screw, melt pressure at the die can exceed 350 bar when screw speed is raised above 60 rpm; this pressure approaches the mechanical limit of older annular die heads and can produce melt fracture or bubble instability. The supplier’s processing guidance specifies barrel-temperature set points of 190–210 °C in the feed zone, 210–230 °C in the compression zone, and 200–220 °C at the die, while melt temperature at the die lip should remain below 240 °C to avoid oxidative degradation. A die gap of 1.2–1.8 mm and a blow-up ratio of 2.0–3.0 are typically used for 25–50 µm film. Grooved-feed extruders with 30:1 L/D or longer reduce pressure fluctuation; barrier screws with Maddock mixing sections improve thermal homogeneity. At these conditions, the high-molecular-weight fraction of FB4230 stabilises the bubble, allowing frost-line heights of 2–6 die diameters and reducing bubble sag under high air-ring cooling. The specific energy input is typically 20–35% higher than that of a 1.0 g/10 min C4-LLDPE at the same screw speed, and the difference widens if die temperature is reduced from 220 °C to 200 °C.
In tandem lamination lines, Borstar FB4230 is used as a sealant layer or a low-melt-index build layer in PET/aluminium/PE and oriented-PP/PE laminates. The low MFR contributes to draw-down stability when the melt is delivered into a chill-roll nip, which is relevant at coating weights below 25 g/m². Cylinder and adapter temperatures are normally set at 200–230 °C; the polymer melt is oxidised in the air gap to improve adhesion to aluminium foil. In-line corona treatment or ozone treatment is applied to raise surface energy; laminate converters typically specify a wetting tension above 38 mN/m in accordance with ISO 8296. For frozen-food packaging, the grade is selected because the ductile-to-brittle transition temperature, measured by low-temperature impact tests derived from ISO 7765-1, remains below -20 °C; this prevents brittle failure at freezer-storage temperatures. Published data for this specific configuration are limited, and end-use validation is required because adhesion depends on foil corona treatment level, line speed, and melt temperature.
The bimodal molecular weight distribution is observable in rotational-rheology data. The crossover frequency at which storage modulus equals loss modulus is lower than that of unimodal C4-LLDPE, indicating a longer relaxation time. The practical consequence is higher melt elasticity and die swell. On annular dies with die gaps below 1.0 mm, die swell can alter the final film thickness distribution and reduce bubble stability at high draw-down ratios. Gel analysis by internal film inspection is generally lower than conventional Ziegler-Natta LLDPE because the Borstar polymerisation process controls the reaction exotherm; however, no polymer is gel-free. Therefore, optical film applications requiring 100% defect-free surface are outside the working envelope. The high-molecular-weight tail also raises the oxidation induction time for a given stabiliser package, but long residence times above 240 °C can still produce oxidised gel particles. These particles appear as fisheyes in 20 µm film and are detectable by an internal light box or camera inspection system.
In heavy-duty sack film at target thicknesses of 50–80 µm, FB4230 is used to down-gauge from conventional C4-LLDPE constructions of 70–90 µm while maintaining dart drop impact and Elmendorf tear resistance. Converter comparative trials run on three-layer coextrusion lines with 250 mm annular dies and dual-lip air rings have demonstrated that a 40 µm film from FB4230 can achieve ISO 7765-1 method A dart drop values and ISO 6383-2 tear values comparable to 60 µm C4-LLDPE films, but the exact ratio depends on die gap, blow-up ratio, frost-line height, and outer-layer HDPE content. The 923 kg/m³ density gives the film a higher tensile modulus than lower-density C4-LLDPE; tensile force at break is measured according to ISO 527-3 in both machine and transverse directions. Agricultural silage films and greenhouse cladding exploit the higher puncture resistance; EN 14477 puncture tests are used to quantify slow-puncture behaviour. The material is not suitable for display-grade shrink film or high-clarity applications because haze measured according to ISO 14782 typically exceeds 5%; for film structures where a haze value below 5% is required, metallocene LLDPE or LDPE is preferred.
Laboratory film evaluation of FB4230 requires control of extrusion conditions because the tear balance and dart drop are influenced by crystalline orientation. Film samples should be produced on a laboratory blown-film line with constant die gap, blow-up ratio, frost-line height, and haul-off speed; otherwise, comparative results are not reproducible. The orientation balance is quantified by measuring tensile properties in the machine and transverse directions under ISO 527-3; the ratio of transverse tear to machine tear under ISO 6383-2 is used as a gauge of anisotropy. If the frost-line height is too low, the bubble is quenched rapidly and machine-direction orientation increases, reducing transverse tear. If the frost-line height is too high, blocking and bubble instability occur. These interactions are especially relevant in down-gauging because a film that passes dart drop at 60 µm may fail at 30 µm if the transverse orientation is not preserved.
The replacement changes the extrusion and sealing envelope. Because FB4230 has a melt flow rate of 0.4 g/10 min compared with 1.0 g/10 min for common C4-LLDPE, screw speed must be reduced or barrel temperature increased by 10–20 °C to maintain the same melt pressure. The melt is more pseudoplastic; therefore, the drop in viscosity at high shear is greater than expected from the lower MFR alone. In a three-layer A/B/A structure with HDPE skins and FB4230 core, the higher melt strength permits a longer frost-line height without bubble instability. Sealing performance differs from metallocene LLDPE. Seal initiation temperature, measured by ASTM F88/F88M, is typically 5–15 °C higher than that of a hexene- or octene-metallocene LLDPE of similar density, which means dwell time or seal-bar temperature must be increased on vertical form-fill-seal machines to achieve the same hot-tack strength. Hot-tack behaviour is measured according to ASTM F1921. The increase in seal-bar setpoint is determined on production machines with dwell times of 0.3–0.8 s; no universal correction exists.
Compared with high-density PE film grades of density 945–955 kg/m³, FB4230 provides lower tensile modulus and lower temperature resistance. This lower modulus improves conformability in lamination and reduces crinkle noise; the trade-off is lower top-load resistance in stand-up pouches. Compared with LDPE of density 920–922 kg/m³, FB4230 has higher dart drop impact and puncture resistance but lower optical clarity. It is not a drop-in for LDPE cling or shrink film. Blending with 10–30 wt% LDPE is common to adjust haze and bubble stability, but the blend is not a simple viscosity average because the high-molecular-weight fraction of FB4230 can dominate bubble tension at low frost-line heights. Layer adhesion in coextrusions with HDPE skins is generally stable when adjacent layer melt temperatures are held within 10 °C at the die entry; larger mismatches can produce interfacial instability in the bubble.
Regulatory status is use-specific. The base resin is classified as an olefin polymer under FDA 21 CFR 177.1520 and is assessed under Regulation (EU) No 10/2011 as amended. The overall migration limit of 10 mg/dm² of food-contact surface applies to the finished article; this value is not a resin property but a fabricated-film property that depends on thickness, additive masterbatch, and conversion aids. Table 2 summarises the compliance assessment matrix.
| Framework | Status | Test or criterion |
|---|---|---|
| EU food contact | Assess under final article | Regulation (EU) No 10/2011; overall migration limit 10 mg/dm² |
| US food contact | Olefin polymer baseline | 21 CFR 177.1520 |
| REACH SVHC | Declaration required | Regulation (EC) No 1907/2006; 0.1% w/w |
| RoHS | Not applicable to packaging | Directive 2011/65/EU Annex III exemptions if relevant |
FB4230 is not formulated for high-speed extrusion at melt temperatures below 200 °C. The absence of slip and antiblock in the base resin requires the addition of masterbatch for film-surface friction control; erucamide-based slip systems require 24–72 h at 23 °C for migration to the surface before coefficient of friction stabilises. Measurement of static and dynamic coefficient of friction is performed per ISO 8295. The grade should not be exposed to acidic or amine-based additives that can deactivate the hindered amine stabiliser package; such interactions can result in colour-body formation or loss of oxidative stability. The product is intended for blown-film extrusion and is not recommended for injection moulding or rotomoulding, because the low melt flow rate would produce excessive melt-pressure loss and poor mould filling. The film property profile is not optimised for high-clarity shrink or display applications; those applications require metallocene LLDPE or LDPE with haze values below 5% under ISO 14782.