| HS Code | 734939 |
| Product Name | Borealis Borstar® FB2310 LLDPE for Film |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Manufacturing Technology | Borstar |
| Comonomer | 1-Butene |
| Density | 0.923 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature A50 | 106 °C |
| Tensile Modulus | 500 MPa |
| Tensile Stress At Yield | 13 MPa |
| Tensile Stress At Break | 30 MPa |
| Tensile Strain At Break | 600 % |
| Shore D Hardness | 55 |
| Film Tensile Stress At Break Md | 45 MPa |
| Film Tensile Stress At Break Td | 40 MPa |
| Film Tensile Strain At Break Md | 500 % |
| Film Tensile Strain At Break Td | 700 % |
| Dart Drop Impact | 250 g |
| Haze | 10 % |
| Gloss 20 | 80 |
| Coefficient Of Friction | 0.2 |
| Seal Initiation Temperature | 110 °C |
As an accredited Borealis Borstar® FB2310 LLDPE for Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Borealis Borstar® FB2310 LLDPE for Film is supplied in 25 kg polyethylene bags, 55 per pallet (1,375 kg), stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loads ~25 MT Borealis Borstar FB2310 LLDPE film resin, typically 25 kg bags, palletized or floor-loaded per shipping requirements. |
| Shipping | Borealis Borstar® FB2310 LLDPE for Film is transported as non-hazardous polymer pellets. Typical packaging includes 25 kg PE bags on pallets, 1,000 kg octabins, or bulk silo trucks. Keep dry, cool, and protected from UV and contamination. No dangerous goods classification or special transport documentation required. |
| Storage | Store Borealis Borstar® FB2310 LLDPE for Film in a cool, dry, well-ventilated warehouse. Keep in original, closed packaging to protect from moisture, dust, and contamination. Avoid direct sunlight, heat, and ignition sources; maintain temperatures below 50°C where possible. Stack pallets securely, rotate stock, and keep away from incompatible materials. Follow local regulations and the safety data sheet. |
| Shelf Life | Borealis Borstar® FB2310 LLDPE for Film has a 24-month shelf life when stored dry, cool, and protected from direct sunlight. |
Industrial sack lines processing Borstar® FB2310 in monolayer FIBC liner film are typically specified with grooved-feed extruders at 30:1 L/D, dual-lip air rings, and internal bubble cooling; the grade has a butene-based bimodal molecular weight distribution, a density of 0.923 g/cm³, and an MFR of 0.75 g/10 min under ISO 1133-1:2022. Compliance for non-hazardous bulk bag liner webs references ISO 21898:2004, while dangerous-goods FIBC constructions are assessed under Chapter 6.5 of the UN Model Regulations; tear strength is screened with ISO 6383-2 and dart impact with ASTM D1709-22. The formulation addition ratio of FB2310 is set at 70–100 wt% in monolayer load-bearing films, with 0.5–2.5 wt% fluoropolymer processing aid and 2–4 wt% of carbon black or white masterbatch; in coextruded heavy-duty sacks the FB2310 core layer is held at 40–60 wt% between LDPE skins. Downstream production uses die gaps of 1.8–2.5 mm, melt temperatures of 195–215°C, blow-up ratios of 2.0–3.0, and frost line heights of 600–900 mm; bubble instability and surface roughness appear when the die gap is reduced below 1.8 mm at high output, which raises the risk of melt fracture and blocks stable internal bubble cooling. Inline gusset boards and bottom-seal units then convert the film into sewn or heat-sealed open-mouth sacks. Converted outputs include FIBC inner liners, heavy-duty shipping sacks for 25 kg and 50 kg dry bulk loads, construction rubble bags, and palletised dust covers.
Low-tunnel and greenhouse cover converting in Mediterranean and Alpine horticulture frequently positions Borstar® FB2310 in the middle layer of a three-layer blown film at 15–30 wt%, with EVA or metallocene LLDPE outer layers and a UV-stabilised LDPE skin. The compliance framework for this end use is anchored to EN 13206:2017, which defines durability, optical transmission, and dimensional stability for agricultural thermoplastic films; photodegradation resistance is verified through EN ISO 4892-2 and ASTM G154 accelerated weathering, and tensile retention after irradiation is measured according to ISO 527-3. The addition ratio of FB2310 is deliberately maintained below 30 wt% because higher fractions increase secant modulus at the expense of low-temperature fold endurance, a critical parameter when films are repeatedly deployed over hoops and arches. Downstream production uses IBC-equipped blown film lines with die gap 2.0–2.4 mm, blow-up ratio 2.8–3.5, melt temperature 190–205°C, and thickness 150–220 µm; anti-condensation additives are dosed at 1–2 wt% to maintain PAR transmission above 85%. Published data on the specific UV retention synergy between FB2310 and hindered amine stabiliser packages is limited, and the 15–30 wt% range reflects commercial agricultural film trials rather than a single datasheet value. Finished product types include greenhouse covers with 24–36 month service life, low tunnel films, silage pit underlay sheets, and temporary fumigation covers for horticultural soil treatment.
Collation shrink lines substituting Borstar® FB2310 for mLLDPE at 20–40 wt% in the outer layers observe a narrowing seal initiation window when the addition ratio exceeds 40 wt%; the bimodal MWD suppresses premature orientation lock-up during bubble stretching but also raises seal initiation temperature by up to 8°C on rotary sealing jaws. The applicable compliance control is not a single product standard but a combination of ISO 14616:2004 for shrink tension and contraction stress, ASTM D2732-20 for unrestrained linear thermal shrinkage at 120–135°C, and ASTM F1921-18 for seal strength after jaw sealing. Production occurs on high-stalk blown film lines with blow-up ratio 3.5–5.0, die gap 1.6–2.0 mm, melt temperature 185–200°C, and post-bubble annealing rolls; the orientated film is then slit and perforated before shrink bundling. Terminal product formats include shrink bundles for beverage cans and bottles, collation film for cartoning lines, and printed shrink labels with controlled MD free shrink below 10% per ASTM D2732-20.
Where thin-gauge refuse sack lines switch from LDPE-rich to LLDPE-dominant formulations, Borstar® FB2310 is added at 30–50 wt% with post-consumer recyclate at 20–40 wt% and a linear masterbatch at 1–2 wt%, puncture resistance is tested under EN 14477:2004, the film is blown on high-stalk lines with BUR 3.0–4.0 and die gap 0.8–1.2 mm, and the output is converted into 18–40 µm refuse sacks, bin liners, and carrier bags.
| Segment | Reference standard | Critical test |
|---|---|---|
| Heavy-duty FIBC liner | ISO 21898:2004; UN Chapter 6.5 | ISO 6383-2 tear |
| Agricultural cover | EN 13206:2017 | EN ISO 4892-2 weathering |
| Collation shrink | ISO 14616:2004; ASTM D2732-20 | shrink force |
| Refuse sacks | EN 14477:2004 | puncture |
| Food pouches | EU 10/2011; FDA 21 CFR 177.1520 | OML 10 mg/dm² |
Food-contact pouch structures using Borstar® FB2310 as a 20–35 wt% sealant-layer component in coextruded or extrusion-laminated webs are qualified under Commission Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm² under Article 12 and food simulant mapping according to Annex III; for U.S.-bound materials, FDA 21 CFR 177.1520 applies to olefin polymers under Conditions of Use C through G, subject to hot-fill or retort limits. The addition ratio of FB2310 in the heat-seal layer is limited to 20–35 wt% because higher loadings reduce hot-tack force and extend seal initiation time, measured via ASTM F1921-18 and ISO 527-3 after sealing. Downstream production includes blown film or cast film lamination, corona treatment to a minimum surface energy of 38 dyn/cm, lamination with metallised PET or aluminium foil using solventless polyurethane adhesives, and reel-to-reel slitting. Converted end products include retort and hot-fill pouches, frozen food bags, dry mix sachets, and bakery film overwraps with seal integrity retained under powdered-fill contamination.
Cast film lines producing temporary surface protection for pre-painted metal, powder-coated aluminium profiles, and glass panels commonly run Borstar® FB2310 at 50–80 wt% as the backing substrate, with LDPE at 10–30 wt% and anti-block/slip masterbatch at 1–3 wt%. Industry compliance for adhesive peel behaviour on stainless steel or coated steel is evaluated under ASTM D3330/D3330M-20 Method A and ISO 29862:2010; tensile elongation and yield are recorded according to ISO 527-3. The downstream process uses cast film extrusion with die gap 0.4–0.8 mm, chill roll temperature 18–22°C, corona treatment to 40–42 dyn/cm, and subsequent coating with solvent-free UV acrylate adhesives before slitting to 25–1500 mm widths. Slit reels are supplied as temporary protection film for stainless steel sheet, powder-coated aluminium window profiles, glass panels, and pre-painted metal sheets; the film should retain room-temperature unwind peel below 2.0 N/25 mm to avoid adhesive transfer after outdoor ageing.
Competitive Borealis Borstar® FB2310 LLDPE for Film prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Borealis Borstar® FB2310 is a bimodal linear low-density polyethylene supplied as a blown-film extrusion resin. The material is produced in the Borstar cascade process, in which a loop reactor and a gas-phase reactor are operated in series to build a controlled bimodal molecular weight distribution. That reactor sequence separates a low-molecular-weight fraction, which lowers high-shear viscosity in the die, from a high-molecular-weight fraction, which increases melt strength and bubble stability. The base resin is specified by a melt mass-flow rate of 0.7 g/10 min at 190 °C and 2.16 kg load according to ISO 1133-1:2022, and a density of 923 kg/m³ according to ISO 1183-1:2019. These values place the grade in the medium-flow, medium-density LLDPE class used for heavy-duty sacks, industrial liners, lamination sealant webs, and agricultural film structures. The product is not a high-clarity resin; its design priority is the processing-property balance required for thicker, tougher film rather than optical transparency. Additive packages vary by region and should be confirmed against the supplier’s certificate of analysis, because slip, antiblock, and processing stabilizer levels are not fixed across all sales specifications. The lot-specific certificate of analysis remains the controlling document, not generic datasheet values.
Table 1. Base-resin values from supplier technical data.
| Property | Method | Typical value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 0.7 g/10 min |
| Density | ISO 1183-1:2019 | 923 kg/m³ |
These values are typical, not specification limits. For film property data, the supplier’s data sheet should be read together with the specific extrusion conditions used to generate the test specimens.
On a blown-film die, the bimodal molecular weight distribution is observed as a non-linear shear-thinning response. The low-molecular-weight mode contributes to flow in the die land, lowering pressure drop relative to a unimodal LLDPE of the same 0.7 g/10 min melt index. The high-molecular-weight mode contributes extensional viscosity after the melt leaves the die, which stabilizes the bubble against flutter. On L/D 30:1 barrier screws, this can appear as reduced specific energy input and lower melt-pressure variability at constant throughput. Spiral mandrel dies with die gaps between 1.2 mm and 1.6 mm, blow-up ratios from 2.5:1 to 3.5:1, and melt temperatures from 200 °C to 220 °C are commonly used. The onset of sharkskin is often delayed relative to conventional C4-LLDPE of the same density at die shear rates above approximately 500 s−1, but this response is a function of die metallurgy, land length, and temperature and is not a guaranteed product property.
On a production-scale monolayer line using a 65 mm single-screw extruder with L/D 30:1, a Maddock mixing section, and a 300 mm spiral mandrel die with dual-lip air ring, the barrel zones are frequently set between 180 °C and 210 °C and the die zones at 210–215 °C. The melt temperature should remain below 240 °C during long runs. Above this threshold, oxidative gel formation becomes increasingly visible as surface specks, and gel specks can initiate local stress concentrations in the film. The resin is not hygroscopic like polyamide or PET, but cold pellet surfaces can condense water when transferred into a warm production hall. If the pellet surface temperature is below the dew point, liquid water enters the feed throat and can produce steam-induced voids in the extrudate. A hopper residence time below 30 min and pellet surface temperature above the dew point are usually sufficient; pre-drying is not normally required at ambient relative humidity below 60%.
For heavy-duty sack applications, the critical failure modes are dart impact, tear propagation, and slow puncture. The relationship between process conditions and these properties is nonlinear. Increasing the blow-up ratio from 2.0:1 to 3.0:1 raises transverse tensile strength while lowering machine-direction tensile strength; a blow-up ratio between 2.5:1 and 3.0:1 is often selected to balance tear resistance. Frost-line height defines the point at which crystallization quenches; a higher frost-line height allows longer relaxation before crystallization, which can increase dart impact but reduce machine-direction modulus. These trade-offs should be evaluated using tensile testing to ISO 527-3, Elmendorf tear to ASTM D1922, dart impact to ASTM D1709A, and puncture resistance to ASTM D5748. The resin itself does not remove these trade-offs; the bimodal molecular weight distribution widens the range of conditions at which the bubble remains stable while the converter moves toward a given property target.
Downgauging shifts the film failure criterion from tensile yield toward tear and impact because the web has less material available to redistribute stress. The bimodal high-molecular-weight fraction is useful in this regime because it increases orientation strength, but the low-molecular-weight fraction is equally important because narrower die gaps used for thin film raise die shear stress and can trigger melt fracture. If output is maintained by increasing melt temperature instead of reducing die gap, dart impact measured by ASTM D1709A can decline because excessive thermal relaxation reduces orientation. If frost-line height is lowered too far, transverse tear strength measured by ISO 6383-2 deteriorates because the film is quenched before the transverse-oriented chain segments can relax. Published data for this specific configuration is limited, so a converter comparing FB2310 with alternative LLDPE grades should hold die gap, blow-up ratio, frost-line height, output, and gauge profile constant. Typical heavy-duty sack film thicknesses are 60–120 µm, but the grade can be drawn below 40 µm on lines with adequate bubble stabilization and internal bubble cooling.
In comparison with a conventional unimodal Ziegler-Natta C4-LLDPE at the same 923 kg/m³ density and 0.7 g/10 min melt index, the Borstar resin typically produces lower die pressure at equivalent screw speed and maintains a wider bubble-stability window. Against a metallocene-catalysed hexene LLDPE, the broader molecular weight distribution and Ziegler-Natta catalyst chemistry usually reduce melt-fracture sensitivity but sacrifice some clarity and organoleptic properties. The product is therefore selected when film toughness and process stability are the primary demands, while a metallocene hexene grade is preferred for high-clarity frozen-food packaging or low-extractable structures. The difference is not universally favorable; it is a shift along the processing-property envelope. Comparative trials should include dart impact ASTM D1709A, Elmendorf tear ASTM D1922, tensile properties ISO 527-3, and haze ASTM D1003 on specimens produced under identical line conditions.
Extrusion equipment constraints determine whether the resin’s bimodal melt strength becomes an advantage. On a smooth-bore extruder, a compression ratio between 2.5:1 and 3.0:1 is common for LLDPE; a grooved feed section increases throughput but can raise melt temperature if the barrel cooling is insufficient. The breaker-plate pressure should be monitored continuously. If the pressure exceeds the extruder manufacturer’s maximum, the first response is to reduce screw speed or raise rear-barrel temperature, not to lower die temperature, because die temperature reduction can increase shear stress and accelerate melt fracture. Screen packs of 20/40/60 mesh are typical; fine 100-mesh screens can create pressure surges on high-output lines and are usually avoided unless forced by product purity requirements. Bubble cooling configuration also affects throughput: at bubble diameters above approximately 300 mm, a dual-lip air ring or internal bubble cooling is required to maintain frost-line stability at high output.
For food-contact use, the base polymer is generally assessed under FDA 21 CFR 177.1520 for olefin polymers. In the European Union, the final film must comply with EU Regulation 10/2011 on plastic materials intended to come into contact with food, and the converter must verify that the specific additive package and any masterbatch meet the applicable specific migration limits. REACH registration is the supplier’s obligation, but the downstream user is responsible for documenting the final article. The base resin does not contain long-term UV stabilizers; outdoor service requires a UV masterbatch. Boiling-water sterilization should be avoided because the film softens near the Vicat temperature range of the density class. Slip and antiblock additives, if introduced, migrate to the film surface and may lower seal strength or increase haze. Seal strength should therefore be tested after the final formulation is selected, using ASTM F88 for seal strength and ASTM F1921 for hot-tack.
On high-speed form-fill-seal equipment, the seal initiation temperature for 923 kg/m³ LLDPE webs is typically observed between 95 °C and 110 °C at laboratory dwell times near 0.5 s. The bimodal high-molecular-weight fraction can raise seal strength after initiation while slightly narrowing the hot-tack window relative to a metallocene LLDPE. This behavior is line-dependent because jaw temperature, dwell time, and cooling air dominate the thermal cycle. Converters should map seal bar temperature, dwell time, and cooling air against film thickness on the target form-fill-seal machine before locking packaging speeds.
Recycled material blended at high levels can introduce unknown stabilizer or acid-scavenger chemistries that alter the additive balance. The grade should not be combined with additive packages containing unverified metal stearates or strongly basic scavengers without compatibility testing, because these may shift the acid-scavenger balance and alter surface slip or seal. The film’s coefficient of friction should be measured after aging according to ISO 8295; a freshly produced film may not yet have reached equilibrium surface slip. For heavy-duty sacks, the final film should be tested for dart impact and tear after the addition of recycled content, because recycled content shifts the property envelope and a simple dilution rule does not always hold.