Birch Plastics Lldpe Virgin Lldpe 2 Melt Index Film

Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film

    • Product Name: Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 873764
    Melt Index 2.0 g/10 min
    Density 0.918 g/cm³
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 600%
    Flexural Modulus 250 MPa
    Vicat Softening Point 100°C
    Shore D Hardness 55
    Dart Drop Impact 150 g
    Elmendorf Tear Strength 300 g
    Haze 10%
    Gloss 80%
    Coefficient Of Friction 0.2
    Seal Initiation Temperature 110°C

    As an accredited Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film is packaged in 25 kg multi-wall bags or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Birch Plastics virgin LLDPE film, 2 melt index, braced for shipment.
    Shipping Birch Plastics Virgin LLDPE (2 Melt Index, Film) ships as non-hazardous polymer resin, typically in 25 kg PE bags or bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers at ambient temperature, avoiding moisture, UV, and contamination. Not regulated for transport.
    Storage For Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film: Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid strong oxidizers. Stack pallets securely, maintain labels, and use first-in, first-out inventory. No special ventilation is required under normal conditions.
    Shelf Life Typically 12 months when stored sealed in original packaging, cool, dry, away from direct sunlight, heat, moisture, and ignition sources.
    Application of Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film

    Film extrusion plants running high-burst-strength liners for bulk chemical and mineral packaging select a 2.0 g/10 min virgin LLDPE for its balance between melt strength and drawdown across a 2.0:1–2.5:1 blow-up ratio. On a 450 mm three-layer blown-film die with 2.4 mm die gap, melt temperature at the adapter is maintained at 215–225 °C, and screw back-pressure is held at 250–320 bar. Slip-antiblock masterbatch is metered at 1.2–1.8 wt%, and a fluoropolymer processing aid is added at 500–800 ppm to prevent die-lip buildup during 72-hour continuous runs. Industry compliance for non-food industrial liners is governed by REACH and RoHS; where the liner is converted as an inner ply for food-contact bulk packaging, FDA 21 CFR 177.1520(c) 3.2a applies. Downstream converting uses bottom-seal and side-gusset forming on rotary heat-seal equipment with dwell times of 1.2–1.8 s at 135–155 °C. Terminal product types include FIBC inner liners, drum liners, steel coil covers, pallet shrouds, and construction films.

    When a 2.0 g/10 min LLDPE is processed on a three-layer cast-film line with a 0.6–0.8 mm slot gap and a chill roll maintained at 22–26 °C, the melt index permits stable drawdown at line speeds between 300 m/min and 350 m/min. In the outer layers, a polyisobutylene-based tackifier masterbatch is metered at 1.0–2.5 wt%, and a silica antiblock concentrate is added at 0.3–0.8 wt%; the core layer remains 100% virgin resin to preserve elongation and tear resistance. Friction and cling are controlled to 0.25–0.45 µ static and 0.20–0.35 µ dynamic per ASTM D1894, while elongation at break is measured according to ASTM D882. REACH and RoHS govern industrial pallet-wrap applications; for food-contact stretch overwrap on fresh-cut produce trays, FDA 21 CFR 177.1520(c) 3.1a and EU Regulation No 10/2011 are applied, with overall migration limited to 10 mg/dm². Downstream equipment includes edge-pinning systems, vacuum boxes, and oscillating haul-off to flatten gauge bands before conversion into 12–30 µm hand pallet wrap, machine wrap, pre-stretched rolls, and bundling film.

    What Changes When a 2.0 g/10 min LLDPE Replaces EVA in Silage Wrap?

    Replacement of EVA with a 2.0 g/10 min LLDPE in silage bale wrap shifts the film’s elongation behavior from high-tack cohesive failure to controlled plastic deformation, requiring adjustment of prestretch depth from 55% to 65–75% to avoid neck-in and edge tear. The formulation is compounded with a hindered amine light stabilizer masterbatch at 3–6 wt% depending on UV exposure class and a carbon-black masterbatch at 2–4 wt% for black mulch-grade film; the tackifier addition is reduced to 1–2 wt% when compared with EVA blends because LLDPE cling is generated mainly at the cast-film surface layer. EN 13206:2017 specifies tensile and elongation requirements for thermoplastic bale-wrap films, while ISO 527-3 covers tensile testing of film specimens; migration limits under EU Regulation No 10/2011 are not applicable to silage wrap unless the film is subsequently used for wrapped feed bales that may transfer substances. Production is conducted on cast-film equipment with a slot die temperature of 260–280 °C and a chilled roll at 20–25 °C, followed by edge trimming and core cutting into 25 µm and 35 µm rolls. Terminal product types include round bale silage wrap, square bale sleeve film, and temporary silage pit covers.

    Sealant-Web Extrusion Across Aluminum Foil and PET Laminates

    In flexible packaging laminates, a film-grade 2.0 g/10 min LLDPE provides a heat-seal initiation range of 95–110 °C at 40 psi sealing pressure and 0.5–1.0 s dwell, with hot-tack retention sufficient for vertical form-fill-seal filling of 1 kg pouches. The sealant web is coextruded as a 20–50 µm layer and dry-blended with an erucamide slip masterbatch at 1.0–1.5 wt% and a synthetic silica antiblock masterbatch at 0.8–1.2 wt%; the slip additive reduces coefficient of friction to 0.15–0.25 µ after 48 hours aging per ASTM D1894, while the antiblock prevents blocking at roll-stock tension up to 1.2 N/mm. FDA 21 CFR 177.1520(c) 3.1a covers olefin polymers in food-contact film, and EU Regulation No 10/2011 requires overall migration below 10 mg/dm²; lamination adhesives must be selected from the appropriate FDA or EU positive lists because direct resin compliance does not extend to the finished laminate. Downstream conversion uses a two-component solventless adhesive lamination line running at 180–220 m/min, followed by curing for 48–72 hours at 35–40 °C before slitting. Terminal product types include stand-up pouches, three-side-seal sachets, stick packs, and lidding film for dairy cups.

    On vertical form-fill-seal lines packaging IQF vegetables at cold-storage temperatures of -30 °C, the 2.0 g/10 min LLDPE is coextruded into 60–80 µm blown film with a 2.5:1 blow-up ratio and frost-line height of 500–700 mm. The resin is blended with 10–20 wt% metallocene-catalyzed LLDPE to raise low-temperature dart impact and with an erucamide slip masterbatch at 500–1,000 ppm to control film-to-metal friction on filling tubes. Compliance for frozen-food contact includes FDA 21 CFR 177.1520(c) 3.2a and EU Regulation No 10/2011; extraction testing per 21 CFR 177.1520(d) may be required for fatty foods at room temperature, whereas frozen-food packaging typically falls under lower migration conditions. Downstream equipment includes three-layer blown-film dies, internal bubble cooling with chilled air at 8–12 °C, and gravity-fed form-fill-seal machines with sealing jaw temperatures of 140–160 °C. Terminal product types include pillow bags for green peas and corn kernels, bakery freezer bags, seafood pouches, and bag-in-box liners for ice slurry distribution.

    When Low Gel Counts Dictate Air Pillow Film Yield

    Air cushion film for void-fill and light-blocking protective packaging operates with a tight processing window at seal temperatures of 150–165 °C and dwell times of 0.3–0.6 s; gels above 200 µm may cause instant seal failure across the longitudinal seal bar. A 2.0 g/10 min virgin LLDPE is extruded on a cast-film line with a 0.5–0.7 mm slot gap and a chill roll at 18–24 °C, then slit into rolls of 20–40 µm thickness. Formulation addition includes a silica antiblock masterbatch at 0.1–0.3 wt% and an erucamide slip masterbatch at 0.1–0.3 wt%; higher slip loadings above 0.5 wt% are avoided because they lower seal strength when residual additive migrates to the seal interface. Compliance for general cushioning is governed by REACH and RoHS; where cushioning is used as a direct food-contact insert for shipped produce, FDA 21 CFR 177.1520(c) 3.1a applies, but converters must verify that finished pillow machines maintain seal-bar temperature tolerances within ±2 °C to avoid localized seal thinning. Downstream conversion is performed on air-pillow machines with heated roller sealing and inflation pressures between 0.4 bar and 0.8 bar. Terminal product types include air pillows, void-fill cushions, and interleaving films for bag-in-box wine shippers.

    Free Quote

    Competitive Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Birch Plastics LLDPE Virgin LLDPE, 2 Melt Index, Film is a film-grade linear low-density polyethylene resin supplied as virgin pellets. The identifier places the material in the ethylene α-olefin copolymer class rather than specifying a proprietary grade code; the term “virgin” indicates the absence of post-consumer or post-industrial reclaim in the base feedstock. Melt flow rate is reported as 2.0 g/10 min under 190°C and 2.16 kg load using ASTM D1238-20 or ISO 1133-1:2022. Published density values for commercial LLDPE film resins in this melt-index class typically fall between 0.918 g/cm³ and 0.922 g/cm³; because density shifts with comonomer length and comonomer content, the product-specific density must be read from the certificate of analysis. The resin can be based on 1-butene, 1-hexene, or 1-octene comonomer chemistry, and the distinction is not always disclosed in generic product descriptions. It should therefore be verified before specifying downstream conversion parameters. As a linear low-density polyethylene, the polymer contains short-chain branches along a predominantly linear backbone, producing a balance of tensile strength, dart impact resistance, and tear resistance that differs from high-pressure low-density polyethylene and from high-density polyethylene.

    How Does a 2 Melt Index LLDPE Film Grade Differ from Fractional-Melt LLDPE and High-Pressure LDPE?

    Compared with high-pressure LDPE, the molecular architecture of the 2.0 melt index LLDPE film grade is the defining difference. High-pressure LDPE is produced by free-radical polymerization and contains long-chain branching, which generates high melt elasticity and shear thinning but generally lower dart impact and tear propagation resistance. LLDPE contains short-chain branches and fewer long-chain branches; at equivalent film thickness, LLDPE grades typically exhibit higher tensile strength values measured under ISO 527-3 or ASTM D882-18 and higher dart drop impact values under ASTM D1709A. However, LLDPE is more sensitive to die-gap and shear-stress conditions and may exhibit higher extruder motor load when processed on lines optimized for LDPE.

    Against fractional-melt LLDPE grades with melt flow rates near 0.5 g/10 min, the 2.0 g/10 min product flows more readily and generally develops lower melt pressure in a given extrusion run. This is useful in cast film and in coextrusion where the LLDPE layer is not the sole structural layer. The tradeoff is reduced melt strength relative to a 0.5 g/10 min fractional-melt resin, which can narrow the stable bubble window in blown film. Against higher-flow LLDPE grades near 3.5 g/10 min, the 2.0 g/10 min resin retains greater oriented mechanical properties and better bubble stability but can limit maximum throughput on torque-limited extruders. Compared with metallocene-catalyzed LLDPE, a conventional Ziegler-Natta 2-MI film grade typically has a broader molecular weight distribution, lower melt pressure under screw shear, and more forgiving extrusion behavior, while metallocene grades often provide superior clarity, dart impact, and tear strength at equivalent density.

    Extruder Configuration and Film Fabrication Boundaries

    Processing literature for general-purpose LLDPE film grades recommends a single-screw extruder with a barrier screw, a Maddock or dispersive mixing section, and an L/D ratio of 24:1 to 30:1. Compression ratio should typically be in the range of 2.5:1 to 3.5:1, and a grooved feed section may be used to stabilize solids conveying with hard-surfaced screw root temperatures high enough to prevent melt bridging. For blown film, die gaps between 1.5 mm and 2.5 mm are normally preferred because LLDPE generates higher shear stress through narrow die gaps than LDPE at the same throughput. Melt temperature ranges for blown film processing are typically 190°C to 220°C, while cast film lines may operate from 210°C to 260°C depending on line speed and quench roll configuration. These ranges are equipment-dependent; no published data for this specific Birch Plastics configuration is available, so initial trials should begin at the lower end and adjust on the basis of melt pressure and film appearance.

    Sharkskin melt fracture can occur when the resin is forced through a die gap that produces excessive wall shear stress. If surface roughness appears on a die with gap below 1.0 mm, a polymer processing aid is usually introduced at 400 ppm to 800 ppm by weight to coat the die land and reduce melt fracture. Bubble stability in blown film is generally improved by internal bubble cooling and a lower frost-line position, but the appropriate stalk height depends on the comonomer type and molecular weight distribution. Moisture exposure above 60% relative humidity can generate surface hydrolysis effects and should be managed by sealed storage or pre-drying in a desiccant dryer at 60°C to 80°C for 1 hour to 2 hours before extrusion.

    Representative Reported Ranges for Commercial 2-MI LLDPE Film Grades
    PropertyTest MethodReported RangeProduct Verification
    Melt flow rateASTM D1238-20, ISO 1133-1:20222.0 g/10 minCertificate of analysis required
    DensityASTM D1505, ISO 1183-10.918 g/cm³ to 0.922 g/cm³Lot-specific value required
    Melting peakISO 11357-3122°C to 126°CDependent on comonomer
    Vicat softening pointISO 30698°C to 112°CDependent on density
    Dart drop impact, 25 µm blown filmASTM D1709A150 g to 300 gStrong comonomer dependence
    Tensile yield stressISO 527-311 MPa to 13 MPaConfirm on actual film
    Tensile elongation at breakISO 527-3700% to 900%Confirm on actual film

    In blown film operations, the 2.0 g/10 min flow permits extrusion of thin-gauge structures in heavy-duty sacks, agricultural films, can liners, surface-protection film, and coextruded sealable webs. The resin is often used as a core layer or as a toughness layer in multi-layer films because its puncture resistance and tear propagation resistance are measurable under ASTM D5748 and ASTM D1922, respectively. Dart impact strength is evaluated under ASTM D1709A; however, the result is strongly influenced by comonomer type, film thickness, frost-line height, and blow-up ratio. For food-contact applications, the grade must demonstrate compliance with FDA 21 CFR 177.1520 for olefin polymers and, where applicable, European Commission Regulation EU No 10/2011. Specific migration limits are not inferred from resin class alone and require product-specific documentation. For non-food industrial films, the resin is commonly specified where a balance between ease of extrusion and film toughness is required, but it is not selected for shrink-film applications that require high orientation and gloss unless it is blended or coextruded.

    If LLDPE Replaces LDPE in a Mixed Blown Film Line

    When a 2-MI LLDPE film grade is substituted for LDPE on a line previously configured for high-pressure LDPE, several processing differences should be addressed. The LLDPE will generally generate higher melt pressure and higher motor load through the same die, especially if the die gap is below 1.0 mm. A die gap increase to 1.5 mm to 2.5 mm is the first corrective action. Barrel temperature profiles may need to be raised by 10°C to 20°C relative to LDPE settings to reduce melt viscosity, though actual adjustment depends on screw design, throughput rate, and melt-temperature measurement. Bubble cooling may require modification because LLDPE does not strain-harden in the same manner as LDPE; the bubble may be less stable at high blow-up ratios unless internal bubble cooling or a higher stalk is used. Published blow-up ratio data for LLDPE film operations typically fall between 2.0:1 and 3.0:1, but product-specific data for this configuration is limited. When partial replacement is desired, LLDPE is frequently blended with LDPE at ratios such as 70/30 or 80/20 to improve modulus and dart impact while retaining LDPE processability. Full LLDPE operation can be economical but requires die-gap and bubble-management changes.

    Regulatory and Compliance Verification Matrix
    Compliance AreaStandard or RegulationVerification RequirementProduct-Specific Status
    Olefin polymer food-contact applicabiltyFDA 21 CFR 177.1520Condition of use A-H must be assigned by supplierConfirm from technical datasheet
    EU plastic food-contact materialsEU No 10/2011Overall migration and specific migration must be testedConfirm for final packaging
    REACH SVHC reportingEC 1907/2006, Article 33SVHC content below 0.1% w/w per supplier statementSupplier statement required
    Heavy metal restrictionsRoHS Directive 2011/65/EU, Annex IIVerify by IEC 62321-5:2013 or XRF screeningTypical for virgin polyolefin, verify lot
    Density classificationASTM D1505, ISO 1183-1Lot-specific density on certificate of analysisConfirm before simulation

    Operational boundaries for this 2.0 g/10 min film resin must be stated because thermal degradation and contamination produce visible film defects. Melt temperature should remain below 250°C; extended residence time above this threshold accelerates oxidative chain scission and gel formation. The resin should not be mixed with polypropylene, polystyrene, polyvinyl chloride, or high-melting engineering polymers in regrind streams, because incompatible contamination creates unmelted particles, gel-like defects, and film holes. The material is not inherently printable or bondable; corona or flame treatment is required for lamination and printing, and the treated surface should be verified to at least 38 dyn/cm using ASTM D2578. In coextrusion, tie-layer selection should be based on the specific LLDPE comonomer and the adjacent polyolefin structure; published data for this specific configuration is limited, and line trials are normally required. Storage in sealed containers below 40°C and away from direct sunlight reduces lot-to-lot variability. Lot-to-lot variation in comonomer type and additive package can shift melt pressure, dart impact, and haze, so process windows should be revalidated when the certificate of analysis changes.

    Top