Birch Plastics Lldpe Virgin L Ldpe 20 Melt Index Injection Molding

Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding

    • Product Name: Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 511424
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Melt Index 20 g/10 min
    Density 0.918 g/cm³
    Specific Gravity 0.918
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 12.4 MPa
    Tensile Elongation At Break 800%
    Flexural Modulus 0.234 GPa
    Hardness Shore D 50
    Vicat Softening Point 95 °C
    Heat Deflection Temperature At 0 46 Mpa 45 °C
    Melting Point 125 °C
    Mold Shrinkage Flow 0.025 cm/cm
    Water Absorption 0.010%
    Ul94 Flame Rating HB
    Processing Temperature 180-230 °C
    Mold Temperature 20-40 °C

    As an accredited Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding: 25 kg moisture-resistant bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL containing Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding grade, in 25 kg bags, palletized.
    Shipping Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding is shipped as non-hazardous plastic resin pellets in 25 kg bags or bulk octabins, on pallets, wrapped and labeled. Not DOT/IMDG/IATA regulated; store dry, away from heat and direct sunlight. Handle as non-regulated cargo; keep sealed to prevent moisture contamination.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep material in original, sealed, labeled containers or bags, palletized and off the floor. Protect from moisture, dust, oils, and other contaminants. Avoid prolonged UV exposure and excessive stacking. Maintain good housekeeping to prevent slipping on spilled pellets. Follow manufacturer’s SDS and local regulations.
    Shelf Life Shelf life: indefinite if stored in original, unopened packaging under cool, dry conditions, away from direct sunlight.
    Application of Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding

    Thin-Wall Food Storage Containers: Processing Window Conflicts and Regulatory Thresholds

    Under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 Annex I, unfilled virgin LLDPE with a density of 0.920–0.925 g/cm³ and melt index of 20 g/10 min at 190°C/2.16 kg (ASTM D1238-20, ISO 1133-1:2022) is permitted for direct food contact when overall migration does not exceed 10 mg/dm² under the intended food simulant. In thin-wall food storage containers with wall sections from 0.8 mm to 2.0 mm, the polymer is processed either neat at 100 wt% or as an 80–95 wt% LLDPE blend with 5–20 wt% low-density polyethylene or metallocene LLDPE to raise dart impact retention at −20°C; slip masterbatch based on erucamide is added at 500–1,500 ppm and synthetic silica antiblock at 1,000–3,000 ppm. Color concentrates, when required, are added at 1–2 wt% and must be selected from FDA-compliant carriers; post-consumer recyclate is excluded from direct food contact unless a valid FDA letter of no objection or EU 10/2011 compliance dossier exists.

    Production-scale injection molding of 470 ml rectangular bases is typically run on 2,800–3,800 kN hydraulic or hybrid two-platen machines with 24-cavity hot-runner valve-gate tooling. Observed short-shot frequency increases when the flow length/wall thickness ratio exceeds 180:1 for 0.9 mm nominal wall stock at a melt temperature below 205°C; the 20 MI LLDPE requires melt temperatures of 205–230°C, mold temperatures of 15–35°C, and injection velocities of 80–130 mm/s to maintain cavity filling before gate freeze. Holding pressure is set between 400 bar and 750 bar for 0.5–1.0 s per mm of wall thickness to compensate for semicrystalline volumetric shrinkage of approximately 2.5–3.5%. Gate freeze time for 0.8–1.2 mm walls at 20 MI is approximately 2.0–3.5 s; premature gate freeze in valve-gate systems produces part weight variation exceeding 0.8%, which appears as sink marks opposite gate bosses. Coolant temperature spread across 24 cavities must be controlled within ±2°C because differential crystallization in LLDPE alters post-demold shrinkage by 0.4–0.7 percentage points and causes warpage that prevents lid–base interlock. Terminal produced articles include 0.8–1.5 mm wall household food storage containers, freezer bases, microwave reheat bases with continuous-use temperature limits below 70°C due to the low Vicat softening point of 85–95°C, snap-on lids, and segmented portion-control trays. Thermal stacking tests per ASTM D648-18 at 0.455 MPa are commonly used to verify dimensional stability in dishwasher top-rack exposure; notched Izod impact per ASTM D256-10e1 remains no-break at 23°C for unfilled LLDPE, but low-temperature drop tests on filled containers should be conducted at −20°C with a defined drop height and impact surface. Pre-drying is not required for the resin itself because moisture absorption is below 0.01%; however, surface condensation on pellets stored below 10°C and introduced into a 200°C barrel can produce splay and surface voids, so controlled silo transition to ambient temperature is necessary when relative humidity exceeds 60%.

    Injection-molded flexible overcaps for 38 mm and 53 mm dispensing closures are produced using 20 MI LLDPE at 85–95 wt% with 5–15 wt% low-density polyethylene to set reseal force and reduce stress-whitening at the hinge; erucamide slip is maintained at 800–2,000 ppm to lower coefficient of friction during automatic capping without exceeding EU No 10/2011 overall migration limits for food-adjacent applications. For overcaps that must resist side-load deformation, 10–20 wt% high-density polyethylene is blended into the LLDPE at the cost of reduced low-temperature hinge fracture resistance. Compliance for food-adjacent closures is evaluated under FDA 21 CFR 177.1520(c) and Regulation (EC) No 1935/2004, while personal care closures are assessed under REACH Article 33 and California Proposition 65 for phthalate and PAH screening. Tooling for 16–64 cavity overcaps runs on 1,500–3,000 kN toggle machines with cold-runner or valve-gate hot-runner systems. Melt temperatures are held at 200–230°C and mold temperatures at 10–30°C; injection pressure of 600–900 bar is required to fill 0.6–1.2 mm wall sections. In 64-cavity production, gate-to-gate melt filling imbalance above 3% of shot volume is a common bottleneck; this is corrected by artificially balancing runner lengths or by adjusting valve stem timing per cavity group. Cap inner diameter is typically held to ±0.10 mm to maintain removal torque; post-mold shrinkage of 1.4–2.0% occurs within 24 h and must be accounted for in tool dimensioning. Terminal articles include snap-on overcaps, dispensing plug caps, flexible dust covers for aerosol valves, and tamper-evident snap-over lids for household chemical closures.

    What Limits Dimensional Stability in Toy Hinge Components at 20 Melt Index?

    Toy hinge components manufactured from 20 MI LLDPE are typically produced neat at 100 wt% or as a 90–95 wt% LLDPE/5–10 wt% ethylene-vinyl acetate blend to lower flexural modulus and reduce hinge stress whitening; color masterbatch at 1–3 wt% is selected against EN 71-3:2019/A1:2021 specific element migration limits and ASTM F963-23 heavy metal limits. Phthalate plasticizers are excluded because REACH Annex XVII entries 51 and 52 restrict DEHP, DBP, BBP, and DIBP, while entry 50 restricts PAH content in toys; compound suppliers must provide batch-level conformity certificates covering all colors. For outdoor toys, hindered amine light stabilizer at 0.2–0.5 wt% with 0.1 wt% phenolic antioxidant is added to control UV embrittlement. In processing on 800–2,500 kN machines, melt temperatures between 190°C and 220°C, mold temperatures of 15–30°C, and injection pressures of 350–550 bar are used for 1.0–2.5 mm wall sections. The 20 MI grade permits flow length/wall thickness ratios up to approximately 220:1 before short shots occur, but living hinge regions require gate placement offset from the hinge by at least 1.5 times the wall thickness to avoid embrittlement from shear heating. Mold vent depth should not exceed 0.02–0.03 mm for LLDPE to prevent flash while allowing air evacuation; insufficient venting causes burn marks at the end of fill. Packing pressure is reduced to the lower end of the range to avoid flash on living hinges; cycle times are typically 12–25 s. Terminal parts include squeeze toys, bath toys, soft building blocks, animal figures with living hinge limbs, and flexible ball halves joined by ultrasonic welding.

    SectorMelt temperature (°C)Mold temperature (°C)Injection pressure (bar)Wall thickness (mm)Clamp force (kN)
    Thin-wall food storage containers205–23015–35500–8000.8–2.02,000–4,500
    Flexible overcaps and dispensing closures200–23010–30600–9000.6–1.21,500–3,000
    Toy hinge components190–22015–30350–5501.0–2.5800–2,500
    Horticultural trays and irrigation emitters195–22510–35550–8500.6–1.21,500–3,500
    Industrial bins and material handling containers200–23010–30500–8001.5–4.04,000–12,000
    Thin-wall cosmetic packaging200–22510–30600–8500.7–1.51,500–3,500

    For horticultural propagation trays with 128 and 288 cell configurations, 20 MI LLDPE is processed at 90–100 wt% with carbon black masterbatch at 2–3 wt% to meet ultraviolet resistance requirements under repeated outdoor cycles; antioxidant masterbatch at 0.1–0.5 wt% and process aid at 0.1–0.3 wt% are incorporated to reduce melt fracture in thin-wall sections. Low-pressure irrigation emitters produced from the same resin use 95–100 wt% LLDPE with tight lot-to-lot viscosity control because labyrinth channel dimensional tolerance affects discharge rate. Compliance references for irrigation components include ISO 9261:2004 for emitter uniformity; for general chemical safety, REACH Regulation (EC) No 1907/2006 Annex XVII applies to cadmium and lead in color concentrates. Multi-cavity tools for seedling trays are run on 1,500–3,500 kN injection molding machines with melt temperatures of 195–225°C, mold temperatures of 10–35°C, and injection pressures of 550–850 bar. Wall sections of 0.6–1.2 mm demand high injection velocity and vacuum venting to avoid trapped air at cell bottoms; core pin deflection must be held below 0.05 mm to maintain uniform root cell volume. For emitters, cavity-to-cavity flow path variation is controlled within ±0.02 mm using tight tool tolerances and packing pressure of 350–500 bar; post-mold shrinkage of 1.5–2.0% is compensated in tool design. Terminal articles include 128/288-cell plug trays, nursery pots, saucers, dripper bodies, micro-sprinkler bases, and low-pressure irrigation fittings.

    When Industrial Material Handling Bins Require Downgauged Sidewalls

    Downgauged industrial bins in 1.5–4.0 mm wall stock are produced neat at 100 wt% or with 5–15 wt% clean post-industrial LLDPE regrind when end-use requirements permit; outside storage compounds add 0.3–0.8 wt% hindered amine light stabilizer, 0.1–0.2 wt% antioxidant, and 1–2 wt% color masterbatch. Compliance is limited to REACH Regulation (EC) No 1907/2006 Annex XVII for restricted substances and, where the bin is used to transport hazardous material, to 49 CFR Part 178 Subpart L for non-bulk plastic packagings. Food contact is not a design target; FDA 21 CFR 177.1520(c) is not automatically satisfied if recycled fraction is introduced. Large-format parts are molded on 4,000–12,000 kN machines with accumulator-assisted injection, melt temperatures of 200–230°C, and mold temperatures of 10–30°C. Injection pressure of 500–800 bar and moderate screw speed of 50–100 mm/s are used to avoid excessive shear heating; residence time should be kept below 8 min at 230°C to suppress gel formation and localized degradation. Differential cooling between sidewall and base creates post-mold warpage of 0.5–1.2% in linear dimensions; this is corrected with targeted mold temperature zoning and post-mold fixtures. Terminal products include open-top storage bins, nestable totes, agricultural bins, shipping containers, and non-food pails. Published data for this exact 20 MI grade in thick-section industrial bins is limited; the above ranges follow standard LLDPE injection molding guidance and should be validated with pilot tool trials.

    High-speed molding of 50 ml to 300 ml thin-wall cosmetic jars in multi-cavity tools uses 20 MI LLDPE at 95–100 wt% with 1–2 wt% color masterbatch and optionally 0.5–1.0 wt% pearlescent or diffusion additive; slip/anti-scratch additive is set at 800–1,500 ppm to reduce visible surface scratching in automated filling lines. Compliance is assessed under EU Regulation (EC) No 1223/2009 Article 17 safety assessment for packaging interactions, REACH Article 33 for SVHC communication, and California Proposition 65 for listed substances; direct food contact compliance under FDA 21 CFR 177.1520(c) or EU No 10/2011 is not implied unless the specific formulation and migration testing are completed. Specified processing on 1,500–3,500 kN machines uses melt temperatures of 200–225°C, mold temperatures of 10–30°C, and injection pressures of 600–850 bar for wall thicknesses of 0.7–1.5 mm. In 16–64 cavity hot-runner tools, valve gate timing must be balanced within 0.1 s across cavities to prevent overpacking of short-flow cavities and visual gate blush. Surface texture fidelity on jar exteriors requires mold surface roughness not exceeding Ra 0.4 µm and adequate venting at 0.02 mm; packing pressure of 400–600 bar is applied to control sink marks on cosmetic shoulder sections. Terminal articles include cosmetic jars, cream tubs, compact powder inserts, spatulas, and secondary packaging trays. Dimensional acceptance is frequently verified by ISO 20457:2018 for molded part tolerances and by ASTM D648-18 for heat resistance under hot-fill labeling.

    Free Quote

    Competitive Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Birch Plastics LLDPE Virgin L LDPE, 20 Melt Index, Injection Molding is a virgin linear low density polyethylene supplied as injection-molding-grade pellets. The product designation encodes the polymer family as LLDPE, the feedstock condition as virgin rather than post-consumer or post-industrial recycled material, and the melt mass-flow rate as 20 g/10 min under ASTM D1238 or ISO 1133-1 at 190 °C with a 2.16 kg load. Resins in this melt-index class are commonly produced with a density of 0.920–0.930 g/cm³ when measured according to ASTM D1505 or ISO 1183-1; the exact lot value should be taken from the certificate of analysis. The grade is intended for reciprocating-screw injection molding rather than blown film, sheet extrusion, blow molding, or rotational molding. Its 20 g/10 min flow rate supports shorter fill times in thin-walled closures, caps, overcaps, tote lids, thin-wall containers, and housewares compared with LLDPE grades in the 0.5–2.0 g/10 min film range. The linear copolymer architecture differs from LDPE in branching character; published polyolefin data indicate that at equivalent melt flow rate, LLDPE typically provides higher tensile yield and higher environmental stress-crack resistance.

    At the feed throat, the granules do not require routine desiccant drying if they remain sealed and are processed within 24 h of opening. If storage humidity exceeds 60% RH or if regrind is introduced, surface moisture can generate splay. A conservative pre-dry is 2 h at 60–70 °C in a desiccant dryer with a dew point below −20 °C. Barrel settings for a general-purpose screw with an 18:1–22:1 L/D ratio and compression ratio of 2.5:1–3.0:1 are typically profiled from 160–180 °C near the feed throat to 190–220 °C at the nozzle. Actual melt temperature should be confirmed by an immersion probe, not inferred from barrel set points, because the low viscosity of a 20 MI resin generates less shear heating than a 5 MI grade. Screw recovery speed is set to maintain a shot volume that is 25–75% of barrel capacity; excessive residence time above 5 min at melt temperatures above 220 °C can shift viscosity through oxidative chain scission. Back pressure in the range 0.5–1.5 MPa (5–15 bar) is adequate to maintain shot-size consistency, but a worn check ring will produce shot weight drift exceeding 0.5% on a 0.01 g resolution balance.

    During filling, the velocity-controlled phase should deliver 90–95% of cavity volume before transfer to pressure-controlled packing. If fill time falls below 0.3 s in thin-wall sections, gas entrapment and burn marks are common on production-scale machines. Peak injection pressure depends on gate geometry and wall thickness; for high-flow LLDPE in thin-wall packaging, cavity pressure at transfer is often 20–40 MPa. Clamp force is projected area multiplied by cavity pressure. A projected area of 100 cm² at 35 MPa imposes 350 kN; applying a safety factor of 1.15 yields 400 kN. Packing pressure is typically 50–80% of peak injection pressure for 3–8 s, followed by a hold time sufficient for gate freeze, commonly 6–12 s for a 1.5 mm wall. Mold coolant temperature is maintained at 10–40 °C; lower mold temperatures shorten cycles but may increase frozen-layer skin thickness and reduce gloss in textured areas. Published data for this specific configuration is limited; final processing windows should be established with in-mold pressure transducers and short-shot studies.

    How Does a 20 Melt Index LLDPE Injection Grade Compare with LDPE and HDPE at the Same Flow Rate?

    The architectural difference is decisive. LLDPE is a linear polyethylene backbone carrying short-chain branches introduced by an alpha-olefin comonomer. LDPE carries long-chain branches, which reduce tensile yield and stiffness but increase melt strength. In injection molding, high melt strength is less critical than in blown film; high-flow LDPE often exhibits lower yield strength and lower environmental stress-crack resistance than LLDPE at equivalent density. HDPE at lower melt index provides higher density, flexural modulus, and heat deflection but generally lower ESCR and less flexible snap-fit recovery. Those differences affect gate size, packing time, ejection force, and part weight because shrinkage and modulus alter part release behavior.

    Resin class Melt flow rate at 190 °C/2.16 kg Density Branching architecture Tensile yield range Flexural modulus range Typical injection molding role
    LLDPE 20 MI 18–22 g/10 min 0.920–0.930 g/cm³ Linear backbone with short-chain branches 11–16 MPa 300–450 MPa Thin-walled closures, containers, housewares
    LDPE 20 MI 18–22 g/10 min 0.915–0.925 g/cm³ Long-chain branched 8–12 MPa 150–300 MPa Flexible lids, snap-fit parts, soft-touch overmolding
    HDPE 8 MI 7–10 g/10 min 0.955–0.965 g/cm³ Linear with minimal branching 22–30 MPa 900–1400 MPa Rigid crates, pails, industrial caps

    The 20 MI LLDPE grade is not interchangeable with a 1 MI film grade. Film-grade LLDPE does not fill thin sections without excessive injection pressure and shear heating, while a 20 MI grade lacks the melt strength required for bubble stability in blown film. In injection molding, the 20 MI LLDPE is selected where thin walls, short cycles, snap-fit recovery, and high ESCR are required. It is not selected where the part demands the stiffness and load-bearing capacity of an HDPE pail or crate, because the LLDPE flexural modulus is lower by roughly 50–70% against an 8 MI HDPE.

    Gate Freeze, Packing, and Post-Mold Shrinkage in Thin-Walled Polyolefin Molding

    Because the supplier has not published a full lot-specific multi-point rheology curve for this grade, mold-filling simulation should not rely on a single melt-index point alone. Capillary rheometry or injection molding machine in-line viscosity data is required for accurate gate pressure prediction. In thin-wall tools, gate freeze time is controlled by the temperature difference between the melt at 190–240 °C and the tool at 10–40 °C. A small gate that freezes before packing can cause sink marks, underpacked regions, and excessive post-mold shrinkage. Short-shot studies should be used to confirm that the gate remains open through the packing phase; the pressure drop recorded by an in-mold transducer after fill is a direct indicator of gate freeze.

    Property Test method Published typical range for 20 MI LLDPE injection molding grades
    Melt mass-flow rate ASTM D1238 / ISO 1133-1 18–22 g/10 min
    Density ASTM D1505 / ISO 1183-1 0.920–0.930 g/cm³
    Tensile yield strength ASTM D638 / ISO 527-2 11–16 MPa
    Elongation at break ASTM D638 / ISO 527-2 Greater than 800%
    Flexural modulus ASTM D790 / ISO 178 300–450 MPa
    Notched Izod impact at 23 °C ASTM D256 / ISO 180/A No break or greater than 50 kJ/m²
    Environmental stress-crack resistance ASTM D1693 Condition B, 10% Igepal Greater than 1000 h
    Mold shrinkage ASTM D955 1.5–2.5%

    Dimensional inspection should follow ASTM D618 conditioning for 40 h at 23 °C and 50% RH because LLDPE continues to crystallize after ejection. Shrinkage is anisotropic; flow-parallel and flow-perpendicular values differ due to molecular orientation. For living hinge applications, flexural fatigue should be assessed through repeated bending trials, because no universal ASTM method covers all hinge geometries. Post-mold distortion in thin-walled parts is frequently caused by nonuniform mold cooling rather than resin variability; cavity-temperature uniformity should be mapped with surface thermocouples before the material is assigned blame for warpage.

    When a 20 MI Virgin LLDPE Is Introduced into an Existing Hot-Runner Tool

    Hot-runner systems balanced for a 5 MI LLDPE or an LDPE grade will generally operate with lower pressure drop on a 20 MI resin, but the viscosity change can shift manifold balance. Valve-gated or thermally gated drops with 2.5–4.0 mm orifices are typical for high-flow polyethylene; needle-valve actuation timing should be retimed to the new fill speed. Internally heated nozzles should be inspected for dead spots because LLDPE can degrade to gel-like particles when held above 240 °C for prolonged periods. The lower melt strength of a 20 MI LLDPE relative to LDPE can reduce drool but does not eliminate it if the hot sprue bushing is unheated. Relative cooling time against an HDPE tool is not assumed; cavity temperature sensors are required to confirm solidification time because published data for this specific configuration is limited.

    Clean regrind can be added in controlled ratios after verification by melt index and density, but each regrind addition may shift flow and color. The processor should not combine this grade with amine-based antistatic concentrates or certain phenolic stabilizer packages without supplier guidance; incompatibility can reduce long-term thermal stability as measured by ASTM D3895 oxidation induction time. For food-contact applications, the resin falls within the class of olefin polymers commonly referenced under FDA 21 CFR 177.1520, but compliance depends on the specific comonomer, catalyst residues, and additive package. The processor must request a food-contact statement from Birch Plastics. For electrical and electronic equipment, the polymer matrix is generally outside the scope of RoHS Directive 2011/65/EU restrictions, but pigments and processing aids must be reviewed. The barrel should be purged with a low-flow HDPE or a commercial purging compound before shutdown to limit carbonyl formation.

    Top