Basf Ultradur Pbt Gf S 4090 G6

BASF Ultradur® PBT+GF S 4090 G6

    • Product Name: BASF Ultradur® PBT+GF S 4090 G6
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 686534
    Polymer Type PBT
    Filler Content 30% glass fiber
    Density 1.53 g/cm³
    Tensile Modulus 9500 MPa
    Tensile Strength 135 MPa
    Elongation At Break 2.5%
    Charpy Impact Strength 23c 50 kJ/m²
    Charpy Notched Impact Strength 23c 8 kJ/m²
    Hdt A 205 °C
    Hdt B 220 °C
    Melting Point 223 °C
    Water Absorption 0.4%
    Molding Shrinkage Parallel 0.3%
    Molding Shrinkage Normal 0.8%
    Melt Temperature 250-280 °C
    Mold Temperature 60-100 °C

    As an accredited BASF Ultradur® PBT+GF S 4090 G6 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-resistant polyethylene bags, palletized; a standard pallet holds 1,000 kg (40 bags).
    Container Loading (20′ FCL) BASF Ultradur PBT+GF S 4090 G6 bags on pallets are loaded evenly and securely into a clean, dry 20′ FCL container.
    Shipping BASF Ultradur® PBT+GF S 4090 G6 is shipped as solid thermoplastic pellets in moisture-barrier packaging. It is not classified as dangerous goods and has no UN number. Store dry, away from direct sunlight and heat; use standard freight and normal industrial hygiene.
    Storage Store BASF Ultradur® PBT+GF S 4090 G6 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers tightly closed to protect against moisture, dust, and contamination. Avoid excessive dust generation and static buildup. Maintain stable ambient temperature and follow the safety data sheet and local storage regulations.
    Shelf Life BASF Ultradur® PBT+GF S 4090 G6 has a shelf life of about 24 months when stored dry in sealed original packaging below 30°C.
    Free Quote

    Competitive BASF Ultradur® PBT+GF S 4090 G6 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The designation BASF Ultradur® PBT+GF S 4090 G6 identifies a 30% glass-fibre-reinforced thermoplastic polyester blend in which polybutylene terephthalate is combined with an ASA-type impact-modification phase within the Ultradur S series. The grade is specified for injection-moulded components where semi-crystalline polyester resistance to fuels, lubricants, and short-term thermal excursion must be retained while the high fibre orientation and anisotropic shrinkage of a conventional glass-filled PBT are reduced. In mouldings exceeding 150 mm in major dimension, the blend chemistry distributes solidification stresses more symmetrically than a straight PBT-GF30, lowering post-mould bow and improving dimensional repeatability across production lots. The identification code under ISO 1043-1 is PBT/ASA-GF30, and the glass content is nominally 30% by weight. The material is not designated as a flame-retardant grade; combustion performance must be assessed on the finished article at the relevant wall thickness rather than assumed from pellet-level data.

    What Quantified Properties Govern Bearing-Stress and Thermal Design?

    A design review for load-bearing thermoplastic housings should begin with tensile modulus, notched impact strength, and heat deflection temperature because these three quantities control wall-thickness calculation, snap-fit survival, and short-term exposure to engine-compartment or solar-load temperatures. The values in the following table are representative datasheet values for initial design; they are not upper or lower specification limits and should be reconfirmed on production-lot certificates.

    Representative physical and mechanical data for BASF Ultradur® PBT+GF S 4090 G6
    PropertyTest methodTypical value
    DensityISO 1183-11.42 g/cm³
    Melt volume-flow rate at 250 °C/2.16 kgISO 1133-111 cm³/10 min
    Tensile modulusISO 527-2/1A8500 MPa
    Tensile stress at breakISO 527-2/1A95 MPa
    Tensile strain at breakISO 527-2/1A2.8%
    Charpy notched impact strength at 23 °CISO 179/1eA6.5 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-2/A190 °C
    Mould shrinkage, flow / transverseISO 294-40.3–0.7%

    For structural calculation, the tensile modulus value of 8500 MPa under ISO 527-2/1A should be derated when the part operates above 80 °C because the polyester phase loses stiffness progressively before the heat deflection limit is reached. Notched Charpy values remain adequate for many rigid enclosure applications, but the material is not a high-ductility polyamide substitute. Designers should avoid thick-to-thin transitions where notch-sensitive glass-fibre orientation concentrates stress.

    Injection Moulding Parameters and Moisture-Sensitive Degradation Boundaries

    On conventional hydraulic or electric injection-moulding machines, the processing window for this grade requires a melt temperature of 250–275 °C and a mould temperature of 60–100 °C. The lower mould-temperature bound improves cycle time but increases fibre read-through and surface roughness on visible faces; the upper bound reduces orientation-driven gloss differences and improves fill of thin ribs, though it extends solidification time. Back pressure in the plastication unit should be maintained between 3 bar and 7 bar, and screw surface speed should be limited to 0.15–0.30 m/s to avoid excessive fibre attrition. A general-purpose screw with a compression ratio between 2.0:1 and 2.5:1 and an L/D ratio of at least 20:1 is sufficient for homogeneous melt preparation; a low-compression barrier screw may be preferred where retention of longer glass fibres is critical for impact strength.

    Pre-drying is mandatory whenever pellet moisture exceeds 0.02 wt%. Desiccant drying at 80–100 °C for 4–6 h to a dew point of -30 °C is the standard recommendation. At ambient relative humidity above 60%, open hopper transfer should be avoided because PBT undergoes hydrolytic chain scission at melt temperatures above 250 °C. The visible processing consequences of wet resin are silver streaking, splay at the gate, and reduced tensile stress at break; the mechanical consequence is a permanent loss of molecular weight that cannot be recovered by reprocessing. Regrind addition should be limited to 20–25% by weight, and only from dried, uncontaminated runners and sprues. Hot-runner systems should be valved or thermally gated to prevent drool during mould-open cycles; manifold temperatures should not exceed 280 °C for residence times above 8 min because the ASA phase discolours under extended thermal load. Gate land lengths of 0.5–1.0 mm for sub-gates and edge gates are appropriate; gate freeze-off should be confirmed by short-shot gate-seal studies because premature holding-pressure release produces sink marks opposite bosses and ribs.

    Rheologically, the filled melt is pseudoplastic. The melt volume-flow rate of 11 cm³/10 min at 250 °C/2.16 kg provides a comparative flowability figure, but spiral-flow length should be determined on the production machine because clamp tonnage, nozzle geometry, and hot-runner pressure drop influence the short-shot limit. Injection pressure demand for thin-wall sections is normally in the range of 80–120 MPa, with holding pressure set to 50–70% of peak injection pressure. Mould venting should be maintained at 0.01–0.03 mm depth in the parting line to avoid gas-burn marks at the flow front. Ejector placement must account for the high modulus of the solidified skin; early ejection without sufficient cooling produces local whitening at pin locations.

    When Replacement of Standard PBT-GF30 or PA66-GF30 Is Justified in Low-Warp Housing Work

    The principal industrial incentive for selecting Ultradur® PBT+GF S 4090 G6 over a standard PBT-GF30 is not an increase in stiffness or heat resistance but a reduction in deformation after moulding. Standard glass-filled PBT grades frequently show a marked difference between flow-direction and transverse-direction shrinkage, which creates corner lift and long-edge bow in rectangular housings, especially when wall thickness is below 2.5 mm and fibre orientation is highly anisotropic. The S-series blend chemistry reduces that differential, yielding flatter parts without requiring post-mould fixturing or annealing. Compared with PA66-GF30, the grade has lower saturated moisture uptake and therefore more stable tensile modulus in humid service environments; however, polyamide 66 retains a higher notched-impact ceiling and generally better resistance to continuous hot-air ageing above 130 °C.

    Applications where the grade is used on production-scale lines include sensor carriers, exterior mirror brackets, headlamp housings, electrical connector shells, relay bases, and mechatronic covers that require dimensional stability after thermal cycles between -40 °C and 120 °C. The ASA phase also reduces surface gloss sensitivity and improves resistance to ultraviolet-induced chalking on black or dark-grey mouldings when compared with unmodified PBT. Paint adhesion and laser marking should be validated on production-textured surfaces because release agents and glass-fibre bloom can interfere with ink transfer and adhesion; corona or plasma pre-treatment is sometimes required before two-component coating.

    Regulatory assessment items for the homogeneous-material declaration
    InstrumentCitationAssessment basis
    REACH substances of very high concernRegulation (EC) No 1907/2006Articl duty requires declaration when any candidate-list substance exceeds 0.1 wt% in the article
    RoHS restricted substancesDirective 2011/65/EU Annex II, as amended by 2015/863Homogeneous-material limits: 0.1 wt% for lead, mercury, hexavalent chromium, PBB, PBDE, DEHP, BBP, DBP, DIBP; 0.01 wt% for cadmium
    UL combustion ratingUL 94 on finished articleNot a flame-retardant grade; wall-thickness-specific rating must be verified

    Several operational limits govern where the material can be specified without additional validation. Continuous contact with hot aqueous media above 60 °C, alkaline cleaning baths at pH above 9, or strong oxidising acids should be excluded because polyester chain scission reduces molecular weight and impact strength. Creep-sensitive applications with sustained static stress above 25 MPa at 80 °C require long-term tensile-creep testing under ISO 899-1; published data for the specific production configuration may be limited, and prototype validation on moulded plaques is recommended. When the part is assembled with metal inserts, moulded-in insert temperature should not exceed 150 °C, and insert bosses should be radiused to avoid stress cracking. The final readiness decision is therefore based on dimensional capability studies on the production mould, not on pellet-level datasheet values alone.