| HS Code | 344728 |
| Grade Designation | PBT-GF20 |
| Glass Fiber Content | 20 % |
| Density | 1.45 g/cm3 |
| Tensile Modulus | 6500 MPa |
| Tensile Strength | 110 MPa |
| Elongation At Break | 2.5 % |
| Charpy Impact Strength Unnotched 23c | 45 kJ/m2 |
| Charpy Notched Impact Strength 23c | 5 kJ/m2 |
| Heat Deflection Temperature A 1 80mpa | 205 C |
| Melting Temperature | 223 C |
| Vicat Softening Temperature B | 210 C |
| Water Absorption 23c 50rh | 0.4 % |
| Molding Shrinkage Parallel | 0.4 % |
| Molding Shrinkage Normal | 0.7 % |
| Processing Melt Temperature | 250-270 C |
| Mold Temperature | 60-100 C |
As an accredited BASF Ultradur® PBT+GF B4520 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | BASF Ultradur® PBT+GF B4520 is supplied in 25 kg moisture-proof paper sacks, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL loading: BASF Ultradur® PBT+GF B4520 in 25 kg bags, palletized, stretch-wrapped, evenly distributed and secured for ocean shipment. |
| Shipping | BASF Ultradur® PBT+GF B4520 is shipped as glass-fiber-reinforced PBT pellets in moisture-barrier bags or octabins. It is a non-hazardous polymer, not regulated for transport, with no UN number required. Keep dry, avoid humidity and high temperatures, and handle with normal industrial precautions. |
| Storage | Store BASF Ultradur® PBT+GF B4520 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep material in its original, sealed packaging to prevent moisture absorption and contamination. Avoid prolonged exposure to humid conditions. Maintain stable ambient temperature, observe shelf-life recommendations, and use oldest stock first. Handle carefully to avoid dust generation. |
| Shelf Life | BASF Ultradur® PBT+GF B4520 has a shelf life of two years when stored dry at room temperature in its unopened original packaging. |
Competitive BASF Ultradur® PBT+GF B4520 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Ultradur® B4520 is a polybutylene terephthalate injection molding grade reinforced with nominally 20% by weight glass fiber. Under ISO 1043 the material is designated PBT-GF20. Published typical values from the producer’s technical data sheet include a density of 1.45 g/cm³ per ISO 1183-1, tensile modulus of 7,000 MPa and tensile stress at break of 115 MPa per ISO 527-2/1A, nominal strain at break of 3.2%, Charpy notched impact strength of 5.5 kJ/m² at 23 °C per ISO 179-1/1eA, and heat deflection temperature under 1.8 MPa of 205 °C per ISO 75-2/A. The melting temperature is typically 223 °C per ISO 11357-3, and the material is rated UL 94 HB at 1.6 mm. The glass fiber raises stiffness and heat resistance while reducing mold shrinkage relative to unfilled PBT; the low nominal strain at break reflects a more brittle failure mode than unreinforced PBT.
The grade is applied in injection-molded parts where dimensional stability, low water uptake, and creep resistance under ambient thermal load are required. Because the polymer is semi-crystalline, the final degree of crystallinity, and therefore the part’s dimensional stability and mechanical properties, is controlled primarily by mold surface temperature and cooling rate rather than by drying history alone. The glass fiber content additionally makes flow-direction and transverse-direction shrinkage unequal, which must be accounted for in tool design.
The transition from unfilled PBT to B4520 is not a simple modulus shift. The 20 wt% glass fiber content creates anisotropic mechanical properties, lower mold shrinkage in the flow direction, and higher notched Charpy impact at 23 °C than many unfilled PBT formulations because fibers bridge the crack path. At -30 °C, notched Charpy impact is approximately 4.5 kJ/m² per ISO 179-1/1eA, illustrating the matrix’s sensitivity to sub-ambient test conditions. A 30 wt% glass-fiber PBT typically reaches 9,500 MPa tensile modulus and can exhibit higher flexural strength than B4520, but it also produces higher melt pressure, increased screw wear, and greater anisotropy in molded parts. Unfilled PBT, with a density near 1.30 g/cm³, has lower stiffness but much lower abrasive wear on barrels and screws.
| Property | Unfilled PBT | Ultradur® B4520 GF20 | 30% GF PBT | Test method |
|---|---|---|---|---|
| Density | 1.30 g/cm³ | 1.45 g/cm³ | 1.52 g/cm³ | ISO 1183-1 |
| Tensile modulus | 2,600 MPa | 7,000 MPa | 9,500 MPa | ISO 527-2/1A |
| Flexural modulus | 2,400 MPa | 6,500 MPa | 8,500 MPa | ISO 178 |
| Notched Charpy impact at 23 °C | 3.5 kJ/m² | 5.5 kJ/m² | 7.0 kJ/m² | ISO 179-1/1eA |
| Heat deflection temperature at 1.8 MPa | 60 °C | 205 °C | 210 °C | ISO 75-2/A |
| Mold shrinkage, flow direction | 1.8–2.5% | 0.3–0.6% | 0.2–0.5% | ISO 294-4 |
The mold shrinkage values in the table are flow-direction ranges and depend on gate location, wall thickness, mold temperature, and packing pressure. Transverse shrinkage is generally higher for glass-filled PBT because fiber orientation restricts shrinkage along the fiber axis but not perpendicular to it. Unfilled PBT exhibits more isotropic shrinkage but greater overall shrinkage. The comparison values are representative of producer data for general-purpose PBT grades; lot-specific certificates of analysis should be used for tooling calculations.
Processability also differs. The higher fiber content of 30% glass-fiber grades can increase nozzle pressure and abrasive wear on screw and barrel. B4520 at 20 wt% glass fiber generally produces lower melt viscosity and less screw wear than 30% GF PBT, but still requires hardened screws and bimetallic barrels compared with unfilled PBT. Published data for exact screw wear rates is limited, but molders running glass-filled PBT often specify bimetallic barrels and hardened screw flights to control maintenance intervals.
Hydrolysis is the primary processing risk for B4520. If moisture exceeds 0.04 wt% at the feed throat, splay marks, viscosity loss, and weld-line embrittlement can occur. Pre-drying in a desiccant dryer with air inlet dew point no higher than -30 °C is required after exposure to ambient relative humidity above 60%. A typical drying condition is 80 °C for 4 h; if higher temperature drying is used, 120 °C should not be exceeded for more than 2 h to limit yellowing. Moisture content can be verified by ISO 15512 or an equivalent Karl Fischer procedure. Hot air ovens are insufficient when the material has been exposed to humid storage because drying air dew point, not only temperature, determines final moisture removal.
Melt temperature at the nozzle should be held between 250 °C and 270 °C. For thin-wall parts, the upper portion of the range reduces viscosity and improves filling, but residence time above 270 °C should be limited to 8 min to avoid hydrolytic chain scission and tetrahydrofuran evolution. Barrel profiles from feed zone to nozzle may be set at 230 °C, 245 °C, 255 °C, and 260 °C; the exact profile should be adjusted to maintain consistent shot mass and avoid unmelted glass-fiber bundles at the gate. Injection speed should be moderate to high, with screw surface speed constrained to 0.1–0.3 m/s. Back pressure is typically held in the 0.3–0.7 MPa hydraulic range to homogenize fiber dispersion without excessive shear heating. A shut-off nozzle is used for low-viscosity PBT melts to prevent drool and stringing during mold separation.
Mold surface temperature is the dominant control for crystallization and dimensional stability. The recommended range is 60–100 °C. Below 60 °C, incomplete crystallization produces post-mold shrinkage and dimensional movement during service; above 100 °C, cooling time increases and the part may stick to the core. For thin-wall connector bodies, mold temperatures between 80 °C and 100 °C improve filling and weld-line strength. Venting depths of 0.02–0.04 mm are used on production tools to evacuate volatiles from moisture or additive degradation; insufficient venting produces gas burns at the end of fill and brittle weld lines.
Clamp force requirements are typically estimated at 3–5 kN/cm² of projected area, with higher values for thin-wall parts due to injection pressure. Screw L/D ratios of 18:1–24:1 with compression ratios of 2:1–3:1 are common for glass-reinforced PBT. Fiber orientation is strongly shear-dependent. Molten material freezes faster at the mold wall, creating a skin layer with high fiber alignment in the flow direction and a core layer with more random orientation. This skin-core morphology causes differential shrinkage through the wall. When injection speed is too low, the skin layer thickens and warpage can increase; when speed is too high, shear heating can cause matrix degradation. The processing window for glass-filled PBT is therefore not solely a melt temperature issue but a shear and thermal history issue.
On production-scale tools with hot runner manifolds, runner sizing should account for glass-fiber length retention. Gate diameters below 1.0 mm produce high shear and can reduce effective fiber length, lowering notched impact at the gate region. Molders often specify minimum gate diameters of 1.0–1.5 mm for glass-filled PBT when weld-line strength is critical, and use open or tab gates to avoid excessive shear heating. Wall thickness transitions should be gradual, with radii of at least 0.5 mm to avoid stress concentrations.
B4520 is employed in electrical connector housings, automotive sensor bodies, relay bases, and power-tool enclosures where the part must retain latching dimensions after moisture exposure and moderate thermal cycling. The combination of 205 °C HDT/A per ISO 75-2/A and UL 94 HB at 1.6 mm supports short-term thermal excursions in soldering operations and engine-compartment test profiles, but continuous service under mechanical load is typically validated below 120 °C unless the specific load case is characterized. The material is not inherently a high-flow PBT; very long flow paths and wall sections below 0.8 mm may require the upper melt temperature range, higher mold temperature, and additional gates.
Thin-wall sections can be filled at nominal wall thicknesses down to 1.0 mm when high-speed injection and sufficient mold temperature are available. Sections below 0.8 mm may require melt temperature near 270 °C and mold temperature near 100 °C; fiber orientation-induced warpage becomes more sensitive to gate location. The lower glass-fiber content of B4520 compared with 30% GF PBT gives better flow in thin walls and less abrasive pressure loss than 30% GF grades, but the trade-off is lower flexural modulus.
For electrical properties, the comparative tracking index and surface resistivity of glass-filled PBT depend on color package, moisture content, and additives; published data for this exact grade and color combination is limited. Therefore, end-use electrical testing should be performed according to the relevant IEC standard for the component, not inferred from neat resin data alone. The low water uptake of PBT, typically below 0.5% at saturation per ISO 62, helps limit dimensional change in humid environments.
Chemical exposure should be evaluated under service-specific temperatures. The PBT matrix in B4520 is resistant to many aliphatic hydrocarbons, glycols, and dilute acids at ambient temperature, but hot concentrated alkalis, steam autoclaving above 100 °C, and strongly acidic environments above 50 °C cause hydrolytic degradation. The natural formulation is halogen-free and flame-retardant-free, but regulatory compliance such as EU RoHS Directive 2011/65/EU Annex II, REACH Regulation EC 1907/2006, and any food-contact clearance must be confirmed for the specific lot and color from the supplier’s certificate of analysis or safety data sheet.
Incompatible processing conditions include prolonged contact with melt temperatures above 280 °C, which accelerates ester bond cleavage and generates tetrahydrofuran and carbon dioxide. Drying of regrind should be conducted in closed desiccant hoppers; crystallized dust and glass fibers separated in dryers can block filters and create hot spots if not removed. Published data for specific regrind ratios is limited, but molders generally restrict regrind to 20–30% for critical dimensional parts.