Basf Ultradur Pbt Gf B4500 Nat

BASF Ultradur® PBT+GF B4500 NAT

    • Product Name: BASF Ultradur® PBT+GF B4500 NAT
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 922006
    Density G Cm3 1.53
    Glass Fiber Content Weight Percent 30
    Tensile Modulus Mpa 9500-10000
    Tensile Strength Mpa 135-140
    Elongation At Break Percent 2.5
    Charpy Impact Strength 23c Kj M2 60
    Charpy Notched Impact Strength 23c Kj M2 9
    Hdt A C 205
    Hdt B C 220
    Melting Temperature C 223
    Water Absorption Saturation Percent 0.4
    Water Absorption Equilibrium 50rh Percent 0.2
    Mold Shrinkage Parallel Percent 0.3-0.4
    Mold Shrinkage Normal Percent 1.0-1.1
    Melt Temperature C 260-280
    Mold Temperature C 60-100

    As an accredited BASF Ultradur® PBT+GF B4500 NAT factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant polyethylene bags, palletized, for BASF Ultradur PBT+GF B4500 NAT industrial resin handling.
    Container Loading (20′ FCL) BASF Ultradur® PBT+GF B4500 NAT loaded in 20′ FCL: palletized, shrink-wrapped bags, dry conditions, evenly distributed, secured against movement.
    Shipping BASF Ultradur® PBT+GF B4500 NAT is shipped as non-hazardous polymer pellets and is not regulated for transport. It is typically supplied in moisture-proof bags or octabins on pallets. Keep dry, avoid moisture and high temperatures, and follow the supplier’s SDS and packaging instructions.
    Storage Store BASF Ultradur® PBT+GF B4500 NAT in original, sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible chemicals. Keep bags closed to prevent moisture absorption and contamination. Avoid dust, physical damage, and prolonged elevated temperatures. Use first-in, first-out stock rotation. Follow the SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months when stored dry, below 30°C, in sealed original packaging protected from moisture.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4500 NAT prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® PBT+GF B4500 NAT is a natural-colour glass-fibre-reinforced polybutylene terephthalate injection-moulding compound. The NAT designation identifies the unpigmented natural base tone; it does not denote a self-coloured or painted article. The B4500 matrix is a medium-viscosity polyester that, when reinforced with glass fibre, is directed at dimensionally demanding components such as electrical connectors, relay bases, sensor housings, and underhood automotive parts. The compound is supplied in cylindrical pellets and processed by injection moulding. Regrind levels above 30 wt% should only be introduced after validation of melt-flow retention and Charpy impact stability.

    The polyester backbone is produced by esterification or transesterification of terephthalic acid or dimethyl terephthalate with 1,4-butanediol. In the glass-filled product, E-glass fibres are dispersed in the semicrystalline matrix; the fibre sizing is selected for polyester adhesion. Unfilled PBT exhibits a melting temperature near 223 °C under ISO 11357-3 and a glass transition in the region of 45–60 °C. Glass-fibre reinforcement does not materially shift the melting temperature but raises the practical temperature limit under load.

    For 20–30 wt% glass-fibre-reinforced PBT grades comparable to B4500 NAT GF, tensile modulus under ISO 527-2 lies between 6,000 MPa and 10,000 MPa, tensile stress at break between 100 MPa and 140 MPa, flexural modulus under ISO 178 between 5,500 MPa and 9,500 MPa, and Charpy notched impact under ISO 179-1/1eA between 5 kJ/m² and 10 kJ/m². Density ranges from 1.45 g/cm³ to 1.55 g/cm³ under ISO 1183-1. Mould shrinkage is anisotropic: typical flow-direction values are 0.2–0.5%, while transverse values reach 0.6–1.0%. Published data for the exact B4500 NAT glass-fibre-filled configuration is limited; lot-specific datasheets should govern final tooling and acceptance criteria.

    Electrical performance for reinforced PBT grades is characterised by high surface and volume resistivity. Volume resistivity under IEC 62631-3-1 is commonly above 1014 Ω·m, but glass-fibre surfaces can reduce comparative tracking index relative to unfilled PBT. Dielectric strength at 1.0 mm is reported in the range 20–30 kV/mm under IEC 60243-1. The exact CTI and dielectric values for B4500 NAT glass-fibre compound should be obtained from the supplier certificate, because natural pigments and glass sizing vary between production campaigns.

    The following comparison of unfilled B4500 NAT and reinforced PBT grades is based on publicly available typical values for comparable Ultradur materials and should not be used as a release specification.

    Property Test method Unfilled B4500 NAT PBT+GF 20 wt% PBT+GF 30 wt%
    Density ISO 1183-1 1.30–1.31 g/cm³ 1.44–1.46 g/cm³ 1.52–1.55 g/cm³
    Tensile modulus ISO 527-2 2,500–2,600 MPa 7,000–8,000 MPa 9,500–10,500 MPa
    Tensile stress at break ISO 527-2 55–60 MPa 110–125 MPa 130–145 MPa
    Flexural modulus ISO 178 2,300–2,500 MPa 6,000–7,000 MPa 8,500–9,500 MPa
    Charpy notched impact ISO 179-1/1eA 4–5 kJ/m² 5–7 kJ/m² 7–9 kJ/m²
    HDT at 1.8 MPa ISO 75-2 60–65 °C 195–205 °C 200–210 °C
    Melting temperature ISO 11357-3 223 °C 223 °C 223 °C

    Drying Kinetics and the Hydrolysis Threshold for Melt Processing

    Pre-drying is mandatory for PBT+GF B4500 NAT because residual moisture hydrolyses ester linkages at melt temperature and lowers molecular weight. The standard drying recommendation for reinforced PBT is 120 °C for 4 h in a dehumidifying desiccant dryer with dew point below −30 °C, targeting residual moisture below 0.04% as determined by ISO 15512. In production-scale dryers, the hopper inlet temperature should be confirmed with a surface probe, because temperatures above 120 °C can cause pellet deformation and bridging in the feed zone. At ambient relative humidity above 60% RH, the dry-to-dry time is extended and the regeneration cycle of the desiccant bed should be verified.

    When a previous batch has remained in the machine hopper for more than 8 h, re-drying is required even if the hopper is covered, because moisture uptake in natural glass-filled PBT can exceed 0.08% in humid plants. A failed desiccant wheel with outlet dew point above −20 °C produces the same defect pattern: lower melt viscosity, splay at the gate, reduced Charpy impact by 10–20% relative to dry pellets, and volatile condensation on cold tool surfaces. Mould deposits in long production runs are frequently misdiagnosed as gas burns when the actual root cause is hydrolysis-induced oligomer formation.

    What Melt-Temperature and Residence-Time Limits Prevent Thermal Decomposition?

    The melt-temperature window for glass-reinforced PBT is normally 250–270 °C measured at the nozzle with an immersion thermocouple. Barrel setpoints are usually arranged as a flat or reverse profile: rear zone 240–250 °C, centre zone 250–260 °C, front zone 260–270 °C, nozzle 250–265 °C. Extended operation above 280 °C accelerates thermal oxidation and should be avoided because the stabilizer package is not designed for prolonged exposure at that temperature. Melt temperature should be recorded after screw recovery is completed and before injection, not during rapid decompression.

    Residence time at melt temperature should be kept below 10 min in the barrel; hot-runner manifold residence should be evaluated separately. For hot-runner systems, the manifold temperature is normally set 10–20 °C below nozzle melt temperature to avoid local degradation. A general-purpose screw with an L/D ratio of 20:1–22:1 and compression ratio below 2.5:1 is typical. High-compression screws above 3.0:1 cause excessive fibre attrition, reducing mean fibre length from 200–300 µm to below 150 µm; the resulting loss of tensile modulus and notched impact is often wrongly attributed to insufficient glass content.

    The following processing reference window is based on general BASF Ultradur glass-fibre-reinforced PBT injection-moulding guidance and should be confirmed against the current product datasheet.

    Processing parameter Reference window Instrument/check
    Drying temperature 120 °C Desiccant dryer inlet
    Drying time 4 h Continuous dry-air dryer
    Residual moisture below 0.04% ISO 15512
    Melt temperature 250–270 °C Nozzle thermocouple
    Mould temperature 80–100 °C Tool surface probe
    Back pressure 0.3–0.7 MPa Machine hydraulic pressure
    Injection speed 80–150 mm/s Screw velocity
    Holding pressure time 3–5 s Timer
    Regrind limit 30 wt% Feed system

    When Multi-Cavity Tools Require Reduced Differential Shrinkage

    For connectors, relay bases, and sensor housings, differential shrinkage between flow and transverse directions controls flatness and weld-line strength. Glass-reinforced B4500 NAT exhibits anisotropic shrinkage; flow-direction shrinkage may be 0.2–0.5% while transverse shrinkage reaches 0.6–1.0%. Tooling trials usually require holding pressure at 60–80% of peak injection pressure for 3–5 s, injection speed between 80 mm/s and 150 mm/s, and mould temperature at 80–100 °C. The higher mould temperature promotes crystallinity and reduces post-mould dimensional change but increases cycle time by 10–20% compared with a 50 °C tool.

    Weld-line strength in glass-reinforced PBT is typically 30–50% lower than the bulk tensile strength, depending on gate position, melt temperature, and filler orientation. Multi-cavity layouts should avoid direct flow impingement after long flow lengths because fibre alignment at the weld plane creates a plane of weakness. Sequential valve-gate control can shift the weld line to non-critical areas but requires documented melt-pressure validation; published data for this specific product in sequential valve-gate tools is limited.

    Observed production-scale failure modes with reinforced PBT include feed-throat bridging, nozzle freeze-off due to low front-zone setpoints below 250 °C, and gate blush from excessive injection velocity above 200 mm/s. Mould deposits in multi-cavity tools often trace to use of regrind above 30 wt% or moisture above 0.06%, not to glass-fibre content. When a tool exhibits intermittent short shots, the first verification is screw recovery time relative to cooling time; recovery should be 60–80% of cooling time to avoid an unstable melt cushion.

    Compared with unfilled B4500 NAT, the glass-fibre-reinforced version increases density by 0.15–0.25 g/cm³ and raises tensile modulus by a factor of 2.5–4.0. The trade-off is mould-filling flow length: melt volume-flow rate at 250 °C and 2.16 kg load is lower in the glass-filled grade than in the unfilled base resin, and the exact value depends on glass content and lot-average fibre length. Glass reinforcement also raises heat distortion temperature under 1.8 MPa from approximately 60–65 °C to above 195 °C, which is the primary reason for selecting the reinforced product in underhood and high-ambient electrical applications.

    Against PBT+ASA blends, the glass-filled B4500 NAT offers higher modulus and better resistance to creep at elevated temperature, but lower impact at −30 °C and reduced weather resistance. PBT+ASA is selected when low-temperature impact and ultraviolet exposure dominate; the glass-filled PBT is selected when dimensional stability under load is the leading requirement. Published quantitative impact difference for the exact B4500 NAT glass-filled product is limited; comparative evaluation under ISO 179-1/1eA is required.

    Relative to polyamide 66 GF, PBT+GF B4500 NAT absorbs much less water. Polyamide 66 GF conditioned to equilibrium at 50% RH can lose 30–40% of dry-as-moulded tensile modulus, whereas reinforced PBT retains more than 95% of its dry modulus under the same conditioning. The polyester grade is therefore preferred for precision electrical connectors where moisture-induced dimensional change must remain below 0.1%. However, polyamide 66 GF typically has higher notched impact and better resistance to continuous hot-oil exposure; PBT+GF is not recommended for sustained contact with hot water above 80 °C, strong acids below pH 2, or strong bases above pH 10.

    Compared with PBT+PET glass-fibre blends, the straight PBT grade offers faster crystallisation and generally better chemical resistance to automotive fuels and oils, but higher post-mould shrinkage and lower surface gloss. PBT+PET is sometimes selected for lower shrinkage and better surface appearance in large housings; the B4500 NAT product is selected where the injection moulding cycle must be short and hot-runner stability is paramount. Quantitative comparison requires tooling trials because mould temperature and wall thickness control crystallinity.

    Regulatory documentation for the compound is supplied through the BASF material safety data sheet and product stewardship declarations. The material is not a candidate for continuous hot-water potable applications because hydrolysis at temperatures above 80 °C reduces service life. RoHS and REACH statements must be confirmed against the current product code, since glass-fibre sizing and heat-stabilizer packages are revised over time. No statement is made here that the material is suitable for medical devices or food contact; those uses require separate grade-specific confirmation under FDA 21 CFR and EU 10/2011.

    Representative application categories include automotive underhood connectors, ignition coil bobbins, power window motor housings, relay bases, industrial control switch bodies, and similar parts requiring a balance of flow, stiffness, and creep resistance. The natural colour is suitable for laser marking if the marking additive package is qualified for the required tracking index and melt-flow stability. Parts exposed to hot air above 130 °C for extended periods require stabilizer-consumption validation, because published continuous-use temperature data for the exact B4500 NAT glass-filled configuration is limited. End-use validation under the relevant OEM performance standard remains necessary.

    Top