Basf Ultradur Pbt Gf B4406g6 Q113

BASF Ultradur® PBT+GF B4406G6 Q113

    • Product Name: BASF Ultradur® PBT+GF B4406G6 Q113
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 244842
    Product Name BASF Ultradur® PBT+GF B4406G6 Q113
    Material Type Polybutylene terephthalate (PBT), 30% glass-fiber reinforced, flame-retardant
    Glass Fiber Content 30%
    Density approx. 1.63 g/cm³
    Tensile Modulus approx. 10,000 MPa
    Tensile Stress At Break approx. 120 MPa
    Tensile Strain At Break approx. 2.5%
    Charpy Notched Impact Strength 23c approx. 7 kJ/m²
    Heat Deflection Temperature A approx. 205 °C
    Heat Deflection Temperature B approx. 215 °C
    Vicat Softening Temperature B approx. 210 °C
    Melting Temperature approx. 220-225 °C
    Molding Shrinkage approx. 0.3-0.6%
    Ul94 Flame Rating V-0 (at 0.75 mm)
    Water Absorption Saturation 23c approx. 0.4%
    Processing Method Injection molding

    As an accredited BASF Ultradur® PBT+GF B4406G6 Q113 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-proof paper bags stacked on pallets, with protective liners, for BASF Ultradur PBT+GF B4406G6 Q113.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of BASF Ultradur® PBT+GF B4406G6 Q113, palletized, shrink-wrapped, and secured for export.
    Shipping BASF Ultradur® PBT+GF B4406G6 Q113 is supplied as solid thermoplastic pellets, usually in moisture-proof bags or octabins. It is non-hazardous and not regulated for transport. Ship in clean, dry containers at ambient temperature, protect from moisture and heat, and keep packages sealed until use.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed in original packaging to prevent moisture uptake and contamination. Avoid prolonged humid storage; dry material before processing per supplier recommendations. Follow the SDS and local regulations.
    Shelf Life Shelf life is approximately 24 months when stored dry in closed containers at temperatures not exceeding 30°C.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4406G6 Q113 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® B4406G6 Q113 is a polybutylene terephthalate injection-molding compound reinforced with glass fiber at a nominal level of 30% by mass. The designation places the material within the Ultradur short-glass-fiber portfolio, with the fiber component surface-treated and dispersed in the semicrystalline polyester matrix to increase modulus, creep resistance, and heat-deflection behavior above the baseline available from unfilled PBT. The Q113 suffix identifies a producer-assigned color or delivery configuration; it does not alter the base resin composition, and mechanical data for Q113 lots are normally referenced to the B4406G6 data set. Published density is 1.53 g/cm³ under ISO 1183-1, and the melt volume rate is typically 11 cm³/10 min at 250 °C with a 2.16 kg load under ISO 1133-1.

    The glass-fiber content introduces pronounced anisotropy in molded parts. Because fiber orientation follows the melt-flow path, modulus and shrinkage parallel to flow differ from those perpendicular to flow. In a gated tensile specimen, the elastic response is dominated by the fiber phase, while the PBT matrix controls creep and chemical resistance. The compound is therefore specified where dimensional stability under heat and mechanical load is a primary requirement, rather than where high elongation or unfilled ductility is needed.

    How Does the Short-Glass Fiber Architecture Shift the Mechanical and Thermal Baseline?

    Under ISO 527-2 tensile loading, the material exhibits a tensile modulus near 10,000 MPa. This is roughly four times the tensile modulus of a typical unfilled PBT grade, which commonly remains between 2,500 MPa and 2,800 MPa. Tensile stress at break is approximately 140 MPa, while tensile strain at break is bounded around 2.5%. The low strain at break means snap-fit designs cannot rely on large post-yield deflection; the material should be designed as a stiff, load-bearing resin rather than as a ductile replacement for polyamide or polypropylene.

    Flexural modulus under ISO 178 is approximately 9,000 MPa. Charpy notched impact strength under ISO 179-1/1eA is about 9 kJ/m², while unnotched Charpy impact strength under ISO 179-1/1eU is near 50 kJ/m². The notched value indicates moderate damage tolerance; weld lines, flow-front hesitation, and heavily shear-thinned regions can reduce the notched result in production parts. The following table consolidates representative property values used for preliminary design work.

    PropertyTest StandardUnitRepresentative Value
    DensityISO 1183-1g/cm³1.53
    Tensile modulusISO 527-2MPa10,000
    Tensile stress at breakISO 527-2MPa140
    Tensile strain at breakISO 527-2%2.5
    Flexural modulusISO 178MPa9,000
    Charpy notched impact strengthISO 179-1/1eAkJ/m²9
    Charpy unnotched impact strengthISO 179-1/1eUkJ/m²50
    Heat deflection temperature, HDT-AISO 75-2°C200
    Melting temperatureISO 3146°C223
    Melt volume rateISO 1133-1cm³/10 min11
    Water absorption, equilibriumISO 62%0.45

    These values are representative, not lot-specific. Shrinkage, impact, and heat-deflection results can shift with gate position, wall thickness, mold temperature, and fiber-length retention. Published data for this specific Q113 configuration are limited; for critical dimensions, batch-specific certificates and prototype-tool measurements should be used.

    Flow-induced fiber orientation also controls shrinkage anisotropy. In a plaque gated at one end, longitudinal shrinkage may be near 0.3%, while transverse shrinkage can approach 0.9–1.1%. In rectangular housings, differential shrinkage between the gate region and the far edge generates warpage. Mold designers compensate with variable wall stock, gate relocation, sequenced cooling, and, where required, post-molding fixture anneals. Shrinkage should be measured on prototype cavities under ISO 294-4 because laboratory plaques do not reproduce the stress state of a complex connector housing.

    Pre-drying in a desiccant dryer is required when resin has been exposed to ambient humidity above 40% RH. The recommended drying envelope is 80–110 °C for 2–4 h, with residual moisture measured below 0.04% by weight using ISO 15512. At melt temperatures above 260 °C, moisture-driven hydrolysis attacks the ester linkages in the PBT backbone, reducing intrinsic viscosity and creating weld-line weakening. On production-scale injection molding machines with general-purpose screws of 20:1–25:1 L/D ratio, the melt temperature should be held between 250 °C and 270 °C. Mold wall temperature should be selected in the range 60–100 °C. At the lower end of that range, rapid solidification suppresses crystallinity and can increase post-molding dimensional movement; at the upper end, cycle time increases but the part gains additional heat-deflection margin and better resistance to annealing-induced shrinkage.

    Thin-wall sections below 1.2 mm normally require profile-controlled injection velocity. On screw diameters between 35 mm and 45 mm, injection speeds are commonly profiled from 100 mm/s near the gate to 250 mm/s during cavity filling, but the exact profile depends on flow length, gate diameter, and cavity balance. Runner diameters below 3 mm in cold-runner tools can restrict the high-filled melt; for parts with wall thickness under 1.5 mm, full-round runners of 4–6 mm are generally required to avoid pressure-limited filling. Residence time at melt temperature should not exceed 5 min. Longer hold-up times accelerate thermal degradation, producing black specks and lowering mechanical property retention. If an interruption exceeds 15 min, purging with a compatible PBT purging compound is required before restarting production.

    Weld lines in this material are mechanically weak because the reinforcing fibers do not cross the weld-line plane. In multi-gated parts, tensile strength at a weld line can fall to 40–60% of the bulk value, depending on melt-front temperature and fiber orientation. Gate placement should therefore move weld lines away from snap arms, latch bosses, and contact-retention features. If weld-line location cannot be changed, higher mold temperature and faster injection speed are the primary process levers for preserving melt-front temperature.

    When Selection Pressure Moves from Unfilled PBT and PA66 GF30

    Comparative selection between B4406G6 Q113 and unfilled PBT is governed primarily by modulus and heat deformation. An unfilled PBT can offer tensile modulus near 2,600 MPa and HDT-A under 1.8 MPa in the range of 55–65 °C. Replacing unfilled PBT with B4406G6 Q113 raises the HDT-A to approximately 200 °C under ISO 75-2. This change is critical in underhood connectors and terminal carriers where spring force must be maintained after exposure to under-hood soak temperatures. The trade-off is lower tensile elongation and a more brittle failure mode.

    Compared with a 30% glass-fiber polyamide 66, PBT GF30 offers lower saturated moisture uptake. Saturated moisture content for PA66 can exceed 7% by mass under ISO 62, whereas PBT GF30 typically absorbs 0.4–0.5%. In humid environments, the lower moisture uptake reduces dimensional growth and the depression of mechanical properties associated with plasticization. However PA66 GF30 generally offers higher notched impact and better resistance to heat aging at temperatures above 180 °C in air. B4406G6 Q113 should not be selected where continuous exposure to hot oil at 150 °C or higher is combined with high dynamic load, unless comparative data from ISO 527-2 and ISO 179-1/1eA on aged specimens confirm adequate performance.

    Within the Ultradur PBT GF30 range, B4406G6 Q113 is positioned as a low-viscosity injection-molding grade. Medium-viscosity PBT GF30 alternatives have lower melt volume rate at the same 250 °C/2.16 kg condition, which can increase injection pressure in thin-wall multi-cavity tools. The higher melt volume rate of B4406G6 Q113 improves flow-length capability, but the fiber length retained after high-shear compounding may be slightly shorter, and notched Charpy values can therefore be marginally lower. Designers should not transfer impact data from a medium-viscosity PBT GF30 grade without verifying ISO 179-1/1eA results on production moldings.

    Power-electronics housings, terminal strips, and underhood connector bodies impose simultaneous requirements for dimensional stability, contact retention, and heat resistance. The material is applied where flame-retardance requirements are limited; it is not inherently formulated for V-0 performance. Flame-retardance claims for a specific color and thickness must be checked against the UL Yellow Card for the actual production configuration. Standard PBT grades resist automotive fuels, oils, and many solvents at room temperature, but prolonged exposure to alkaline aqueous solutions, hot water, and concentrated acids degrades the polyester matrix. Hydrolysis-resistant variants are preferred for coolant-contacted parts.

    Unmodified PBT GF30 is not recommended for outdoor load-bearing use without UV stabilization if surface appearance retention is specified. In continuous service near the HDT-A limit, creep under ISO 899-1 should be evaluated because clamp load and terminal normal force can decay over time. The grade is therefore best applied in geometrically stable, stiff, short-fiber-reinforced components where low moisture uptake and high flow must be balanced against limited ductility and weld-line sensitivity.

    Top