Basf Ultradur Pbt Gf B4330g6hr Bk15045

BASF Ultradur® PBT+GF B4330G6HR BK15045

    • Product Name: BASF Ultradur® PBT+GF B4330G6HR BK15045
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 752918
    Grade Ultradur B4330G6 HR BK15045
    Polymerbase Polybutylene terephthalate (PBT)
    Glassfibercontent 30% by weight
    Color Black
    Hydrolysisresistance Improved
    Density 1.53 g/cm³
    Tensilemodulus 10000 MPa
    Tensilestrength 140 MPa
    Elongationatbreak 2.5%
    Charpynotchedimpactstrength23c 8 kJ/m²
    Charpyunnotchedimpactstrength23c 55 kJ/m²
    Hdt A 1 8mpa 205 °C
    Hdt B 0 45mpa 220 °C
    Meltingtemperature 223 °C
    Moldingshrinkageparallel 0.3%
    Moldingshrinkagetransverse 0.9%
    Processingmelttemperature 250-270 °C
    Moldtemperature 80-100 °C
    Waterabsorptionsaturation 0.4%

    As an accredited BASF Ultradur® PBT+GF B4330G6HR BK15045 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing BASF Ultradur® PBT+GF B4330G6HR BK15045 is supplied in 25 kg polyethylene-lined paper bags, palletized for industrial storage and handling.
    Container Loading (20′ FCL) BASF Ultradur® PBT+GF B4330G6HR BK15045 loaded in 20′ FCL using standard export packaging, palletized, dry, ambient, moisture-protected, and evenly distributed.
    Shipping BASF Ultradur® PBT+GF B4330G6HR BK15045 is shipped as black, 30% glass-fiber reinforced PBT pellets in moisture-proof 25 kg bags or octabins on pallets. Packages are labeled with product name, batch, and safety information. It is non-hazardous for transport; keep dry and avoid heat, moisture, and UV exposure.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizers. Keep original bags/containers tightly closed to prevent moisture pickup and contamination. Rotate stock and avoid prolonged humid exposure; if moisture uptake is suspected, dry according to BASF processing guidelines before molding.
    Shelf Life When stored dry, sealed in original packaging, and protected from moisture at moderate temperatures, typical shelf life is 12 months.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4330G6HR BK15045 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® PBT+GF B4330G6HR BK15045 is a 30% glass-fiber-reinforced polybutylene terephthalate/acrylonitrile-styrene-acrylate blend intended for injection molding. The model designation encodes the polymer system: B4330 identifies the PBT/ASA base, G6 signifies the glass-fiber loading, HR indicates hydrolysis-resistant stabilization, and BK15045 is the black color designation. The grade is supplied as pellets and is specified where components must retain tensile strength, dimensional stability, and surface integrity after exposure to moisture, ethylene glycol, thermal cycling, or road salt. Equilibrium water absorption at 23°C and 50% relative humidity is approximately 0.2% according to ISO 62. That value is lower than the conditioned moisture content of many glass-reinforced polyamides used in similar housings, making the grade suitable for humid automotive exterior applications where dimensional change arising from moisture ingress is a design constraint. The material remains a polyester compound, however, and requires the same controlled drying discipline as standard PBT grades before melt processing.

    Why Does the ASA Fraction Reduce Moisture Uptake and Post-Mold Shrinkage?

    Chain scission in PBT proceeds by hydrolysis of ester linkages, and the reaction is accelerated by carboxyl end groups generated during degradation. In standard PBT GF30, prolonged exposure to 80°C water or 121°C steam reduces molecular weight and produces a measurable fall in tensile stress at break. The HR stabilization package in B4330G6HR is designed to retard carboxyl end group autocatalysis, while the ASA phase contributes an amorphous, lower-polarity domain that reduces equilibrium moisture ingress and alters shrinkage anisotropy after molding. Density is approximately 1.41 g/cm³ when tested to ISO 1183-1. The lower density is not an indicator of reduced glass content; ash content remains 30% according to ISO 3451-1. Rather, the ASA-rich matrix lowers matrix density and changes fiber wetting relative to a neat PBT matrix. Tensile modulus is approximately 9,000 MPa when measured according to ISO 527-1/-2, which is below the 10,000–11,000 MPa range that is typical for high-stiffness PBT GF30. The trade-off is deliberately centered on humidity-aged property retention rather than dry maximum stiffness.

    The representative dry-as-molded values for the BK15045 black formulation are summarized in the following table. Values vary with part geometry, gate location, fiber orientation, melt temperature, and mold temperature.

    PropertyTest standardRepresentative value
    Glass fiber contentISO 3451-130%
    DensityISO 1183-11.41 g/cm³
    Melt volume-flow rateISO 1133-1:2022, 275°C/5 kg12 cm³/10 min
    Tensile modulusISO 527-1/-29,000 MPa
    Tensile stress at breakISO 527-1/-2110 MPa
    Nominal strain at breakISO 527-1/-22.5%
    Flexural modulusISO 1788,200 MPa
    Charpy notched impact strength, 23°CISO 179-1/1eA6.0 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-2/A180°C
    Linear mold shrinkageISO 294-40.2–0.4% parallel / 0.7–1.0% transverse

    The shrinkage anisotropy shown in the table is significant because glass fibers orient preferentially in the flow direction. Parts designed with a single gate and a long flow path will exhibit greater differential shrinkage between the parallel and transverse directions. If the gate is located at the center of a large housing, the resulting radial fiber orientation can produce predictable but non-uniform post-mold distortion. Tool design should therefore include gate location studies using mold-filling simulation, and post-mold dimensional inspection should follow ISO 294-4 specimen conditioning.

    Drying, Melt Temperature, and Hot Runner Boundaries

    Pre-drying is required before injection molding. The pellets should be dried in a desiccant dryer at 120°C for 4 h, with a dew point below −30°C and airflow above 0.03 m³/min per kg/h of throughput. Residual moisture at hopper discharge should remain below 0.04%. If ambient relative humidity exceeds 60%, hopper loading should be closed-conveyor, and open hopper residence time should be limited to 30 min to prevent surface moisture regain. Insufficient drying produces splay, silver streaks, loss of surface gloss, and reduced tensile stress at break due to hydrolysis during plastication.

    Melt temperature at the nozzle is typically maintained at 250–270°C. Mold temperature is set at 40–80°C, with the higher range used for thin-wall housings, better flow-length capability, and improved weld-line strength. The lower range is used for cycle-time reduction and dimensionally tolerant parts. Injection velocity is usually set between 100 mm/s and 200 mm/s screw forward velocity. Packing pressure is commonly 50–80 MPa, and hold time should be based on gate freeze time measured by part-mass stabilization rather than a fixed value. Back pressure is normally kept low to moderate, around 3–7 MPa, because excessive shear heating can degrade the polyester phase.

    Residence time at full melt temperature should remain below 5 min. If machine interruption exceeds 10 min, the barrel should be purged with a glass-filled PBT or a low-viscosity polypropylene. Hot runner systems should use manifold temperatures of 250–270°C and tip temperatures of 260–280°C. Dead zones, sharp bends, and intentional melt-restriction points should be avoided because stagnating melt in glass-filled polyester degrades into low-molecular-weight fragments, producing black specks, odor, and surface defects. At hot runner tip temperatures above 300°C, the probability of thermal decomposition increases sharply.

    Mold design must also account for fiber abrasion. Gate inserts, valve pins, and sprue bushings should be fabricated from hardened tool steel, and wear surfaces in high-fiber-flow regions should be inspected for abrasive erosion at intervals defined by shot count. The use of hydraulically actuated valve gates is acceptable, but pin seating should be designed to prevent glass fibers from wedging in the pin bore.

    Technical literature for B4330G6HR BK15045 identifies automotive mirror housings, exterior door handles, wiper arm covers, headlamp frames, sensor brackets, and electrical connectors as application areas where cyclic moisture, road splash, and thermal exposure occur together. The black color code provides carbon black pigmentation, which contributes to ultraviolet weathering resistance, but black pigmentation can also reduce weld-line strength when two flow fronts meet after an extended glass-fiber orientation path. In a gated tensile specimen, weld-line tensile strength for a 30% glass-reinforced polyester is commonly reduced by 20–30% compared with the non-weld value. Mold-filling simulation should be used to position weld lines in low-stress regions, or the part should be gated so that the weld line is formed in a locally thickened zone.

    When Dimensional Stability in Wet Conditions Outweighs Dry Heat Deflection

    The product differs from a standard PBT GF30 in density, dry stiffness, and humidity-aged property retention. A typical PBT GF30 grade exhibits density near 1.52–1.53 g/cm³ and dry tensile modulus near 10,000–11,000 MPa. B4330G6HR has lower density and lower dry modulus, but the hydrolysis-resistant formulation is intended to retain a larger fraction of its initial tensile stress at break after exposure to hot water, coolant, or saturated humidity. The heat deflection temperature at 1.8 MPa is approximately 180°C for this grade, whereas standard PBT GF30 grades frequently appear in the range of 200–205°C under ISO 75-2/A. These values are not intrinsic continuous-use limits under load; creep modulus, stress level, and service temperature must be examined separately.

    Compared with a glass-reinforced PA66, the PBT/ASA grade absorbs less moisture and therefore shows less modulus shift after humid conditioning. A glass-reinforced PA66 at 50% relative humidity typically absorbs approximately 1.5–2.0% water, which reduces glass transition temperature and stiffness. B4330G6HR absorbs about 0.2% under the same conditions, so the dry-to-conditioned modulus shift is smaller. The trade-off is lower dry strength, lower notched impact at low temperature, and lower heat resistance than a high-molecular-weight PA66 GF30. The PBT/ASA grade is selected where humidity-driven dimensional change, warpage, or hydrolysis is the dominant failure mode, not where maximum dry heat resistance is required.

    Chemical exposure limits for this polyester-based product include continuous contact with strong alkalis, concentrated nitric acid, or saturated steam above 121°C. These conditions can attack the ester linkage and reduce molecular weight even in hydrolysis-stabilized grades. Ethylene glycol-water mixtures, automotive coolant, and alcohol-based cleaners are generally less aggressive, but published data for extended coolant exposure of this exact black formulation is limited. End-application validation under OEM-specific coolant, salt spray, and thermal cycling conditions is therefore required before use in under-hood coolant-contact positions.

    Supplier documentation identifies conformity with RoHS 2011/65/EU Annex II and REACH SVHC candidate list requirements. The flame rating is UL 94 HB at 1.5 mm. These are supplier declarations for the molded compound and do not automatically certify the final assembled article, because coatings, adhesives, gaskets, and secondary operations can alter the regulatory profile of the finished component.