Basf Ultradur Pbt Gf B4300g6 Nc010

BASF Ultradur® PBT+GF B4300G6 NC010

    • Product Name: BASF Ultradur® PBT+GF B4300G6 NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 880666
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Melt Volume Flow Rate 12 cm³/10 min (250 °C/2.16 kg)
    Water Absorption At Saturation 0.4%
    Equilibrium Moisture Absorption 0.2%
    Tensile Modulus 10000 MPa
    Tensile Stress At Break 140 MPa
    Elongation At Break 2.5%
    Charpy Notched Impact Strength At 23 C 8 kJ/m²
    Hdt A 205 °C
    Hdt B 220 °C
    Vicat Softening Temperature B 210 °C
    Melting Temperature 220-225 °C
    Melt Processing Temperature 260-280 °C
    Mold Temperature 80-100 °C
    Molding Shrinkage In Flow Direction 0.3%
    Molding Shrinkage Transverse To Flow 0.8%
    Flammability Ul 94 HB

    As an accredited BASF Ultradur® PBT+GF B4300G6 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-barrier bags on pallets, protecting BASF Ultradur® PBT+GF B4300G6 NC010 pellets from moisture and contamination.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of BASF Ultradur® PBT+GF B4300G6 NC010, shrink-wrapped and secured for transport.
    Shipping BASF Ultradur® PBT+GF B4300G6 NC010 is supplied as 30% glass-fiber reinforced PBT pellets in moisture-barrier packaging. Ship in clean, dry, ventilated containers at ambient temperature, protected from moisture, sunlight, and contamination. Classified as non-hazardous for transport.
    Storage Store BASF Ultradur® PBT+GF B4300G6 NC010 in original, sealed, moisture-proof packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, and oxidizing materials. Protect from humidity and water; reseal opened bags promptly. Recommended ambient storage is approximately 15–25 °C. Avoid prolonged exposure to high temperatures or UV light to maintain material properties.
    Shelf Life The shelf life is typically 12 months when stored in original sealed packaging, dry, cool, and protected from moisture and heat.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4300G6 NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® PBT+GF B4300G6 NC010 is a glass-fiber-reinforced polybutylene terephthalate injection-molding compound. Under ISO 1043-1, the material is designated PBT-GF30 because the nominal glass-fiber content is 30% by mass. The B4300G6 designation places the grade in the medium-viscosity Ultradur B injection-molding series; the NC010 suffix identifies the standard natural-color pellet form. The material is processed on conventional reciprocating-screw injection-molding machines and is normally selected where higher stiffness, lower moisture regain, and faster crystallization than unfilled PBT are required.

    Published typical property data at 23°C are obtained from BASF product literature and ISO test standards. Density under ISO 1183-1 is approximately 1.53 g/cm³. Tensile modulus under ISO 527-1/-2 is approximately 10,000 MPa, flexural modulus under ISO 178 is approximately 9,800 MPa, and tensile stress at break is approximately 130 MPa. Notched Charpy impact strength under ISO 179/1eA is approximately 10 kJ/m². Heat deflection temperature HDT/A at 1.80 MPa is commonly reported near 190°C under ISO 75-1/-2. Tensile strain at break is typically below 3%, placing the grade in the rigid, low-elongation category. These values are not guaranteed specification limits; current lot-specific datasheets should be consulted before final part approval.

    Fiber orientation in injection-molded PBT-GF30 is anisotropic. Tensile bars cut transverse to the main flow direction may exhibit modulus values 20–30% lower than flow-direction specimens. This anisotropy affects snap-arm design, weld-line placement, and ultrasonic welding behavior. Edge-gated dog-bone specimen data can overpredict load-bearing capacity in complex parts where the principal stress is transverse to flow.

    What changes when the glass level moves from 20% to 30%?

    Replacing a 20% glass-fiber PBT with B4300G6 typically raises the tensile modulus by approximately 3,000 MPa and increases density by approximately 0.07 g/cm³. Compared with unfilled PBT, the 30% glass-fiber reinforcement reduces total mold shrinkage in the flow direction but increases the difference between parallel and transverse shrinkage. The material also becomes more sensitive to gate location because the filled melt freezes earlier at the outer layers. The gate should be placed in the thickest section, and abrupt flow-front velocity changes should be avoided with generous radii.

    Representative glass-fiber level comparison for selected Ultradur grades
    GradeNominal glass fiberDensity (ISO 1183-1)Tensile modulus (ISO 527-1/-2)Notched Charpy (ISO 179/1eA)
    Ultradur B4300G420%1.46 g/cm³7,000 MPa8 kJ/m²
    Ultradur B4300G630%1.53 g/cm³10,000 MPa10 kJ/m²
    Ultradur B4300G1050%1.70 g/cm³16,000 MPa11 kJ/m²

    The matrix values are representative datasheet summaries, not normalized for moisture content or test speed. The trend is non-linear: moving from 20% to 30% glass content improves modulus by roughly 43%, while the additional 20% glass from G6 to G10 improves modulus by about 60% but increases melt pressure and tool wear disproportionately. B4300G6 is therefore frequently chosen as the practical balance for parts that do not require the maximum stiffness of a 50% glass-filled grade.

    Unfilled PBT may exhibit tensile strain at break above 20%; B4300G6 reduces that value to approximately 2.5–3.0%. Snap-fit and press-fit features require lower assembly strain, larger lead-in angles, and controlled deflection. The grade is not suitable for flexible latching features that depend on high elongation. It is better suited to rigid connectors, housings, brackets, and structural components where creep resistance under spring contact load is required over time.

    Pre-drying parameters and moisture thresholds for hydrolytically sensitive PBT

    PBT is hydrolytically degraded by moisture at melt temperature. Residual moisture above 0.04% by mass before plastication can cause random chain scission of ester groups, reducing number-average molecular weight. The observable result may be a drop in tensile stress at break and notched Charpy impact without an obvious visual defect in the molded part. The recommended pre-drying procedure for B4300G6 NC010 is a desiccant dryer at 80–100°C with a dew point below -30°C for 2–4 h. Material exposed to ambient air above 60% relative humidity for more than 1 h should be re-dried before use.

    Processing window for B4300G6 NC010
    ParameterRecommended rangeMeasurement/equipment basis
    Residual moisture limit0.04% maxISO 15512 or calibrated halogen moisture analyzer
    Pre-drying temperature80–100°CDesiccant dryer, dew point -30°C
    Pre-drying time2–4 hDry-air hopper residence
    Melt temperature250–270°CNozzle/barrel thermocouple
    Mold temperature60–80°CPressurized water thermolator

    Barrel temperatures from feed to front zone are typically profiled from 240°C to 260°C, with the nozzle held near 250°C. Residence time above 270°C should be restricted; continuous residence beyond 5 min can cause surface streaking and loss of impact strength. Screw backpressure should be kept below 0.5 MPa during screw recovery to minimize glass-fiber length reduction. High backpressure increases fiber breakage and raises melt temperature, which is not beneficial for this grade.

    Mold temperature also controls the degree of crystallinity and subsequent post-mold dimensional shift. At mold temperatures below 40°C, the skin freezes before crystallization is complete, and post-molding shrinkage can continue for 24–48 h. Molding at 60–80°C produces a more uniform crystalline structure and reduces warpage in flat connector decks, but cycle time increases. For parts with length exceeding 100 mm, dimensional audits should be delayed until 48 h after ejection because shrinkage anisotropy continues after initial cooling.

    If a hot-runner tool is used, what modifications to hold pressure are advised?

    Hot-runner systems for B4300G6 require more attention to valve-pin and manifold wear than unfilled PBT. The 30% glass-fiber content is abrasive; valve pins and gate inserts made from hardened H13 or D2 tool steel are preferred over untreated low-alloy steels such as AISI 4130. Hold pressure should not be transferred directly from unfilled PBT. A 10–15% higher hold pressure than a 20% glass-filled PBT is commonly required because the filled melt solidifies faster and the packing window shortens. Part-weight stability is the correct process metric; if weight continues to increase after 3 s of additional hold time, the gate or runner is too large, and cooling is controlling the cycle.

    The melt exhibits pseudoplastic shear-thinning; apparent viscosity at injection shear rates of 100–1,000 s⁻¹ is lower than at low-shear capillary measurements. Pressure-drop predictions based on low-shear melt-flow data alone will therefore overestimate filling pressure. Injection speed is best established through short-shot sequence studies. Flow should remain continuous across the part without jetting. Excessive injection speed can shear heat the material near the gate above 280°C, causing local molecular-weight loss and gate-area brittleness. A gate land of 0.5–1.0 mm and a gate diameter of 0.8–1.2 mm are practical starting points for small connector parts, but gate dimensions require mold-specific pressure-drop verification.

    Cold-runner systems should maintain runner diameters above 3 mm for most small-to-medium parts; smaller runners freeze prematurely because glass-filled PBT develops a thick solidified layer early in filling. A cold slug well of at least 1.5 times the runner diameter is standard. Cavity-to-cavity weight imbalance above 5% in multicavity tools will typically translate into visible dimensional variation because the filled material has lower melt compressibility and less time to redistribute during packing.

    Electrical connector housings, relay bases, switch components, and power-distribution modules are common application fields for B4300G6 NC010. The grade is specified where dimensional stability, low creep under contact spring load, and resistance to common automotive and appliance chemicals are required. Electrical properties such as comparative tracking index and dielectric strength are not fixed in the same way as mechanical properties; they vary with wall thickness, color, and filler orientation. Values should be measured under IEC 60112 and IEC 60243-1 on final molded plaques or parts rather than assumed from general PBT literature. The standard grade is not inherently flame-retardant; applications requiring UL 94 V-0 thin-wall performance require a flame-retarded PBT variant.

    For automotive underhood applications, the low moisture regain of PBT compared with glass-reinforced polyamide 66 is often decisive. Water absorption after 24 h under ISO 62 is typically below 0.2%, while a comparable PA66 GF30 can absorb several percent by weight. This stabilizes dimensions and electrical behavior under humidity cycling. However, continuous exposure to hot ethylene glycol/water coolant under pressure can attack PBT. Published data for this specific grade in long-term coolant immersion is limited; component qualification must include actual fluid exposure at maximum service temperature and pressure. Prolonged steam above 120°C and strongly alkaline media are also outside the intended operating envelope unless validated separately.

    For load-bearing housings that carry spring contact forces at elevated temperature, creep modulus under ISO 899-1 is more relevant than instantaneous tensile modulus. At 80°C, creep modulus is generally higher for the G6 grade than for unfilled PBT, but published data for this specific configuration is limited and should be obtained for the actual mold orientation. If the service load exceeds 30% of the short-term tensile stress at break after temperature derating, finite-element analysis using tensile creep data at the defined temperature and humidity is required.

    Compliance verification depends on current declarations and application-specific testing

    Regulatory status for Ultradur® PBT+GF B4300G6 NC010 is not a static property. RoHS compliance is assessed against Directive 2011/65/EU and its amendments; REACH SVHC status depends on the candidate list at the time of shipment. A molder adding color concentrate, flame-retardant masterbatch, or processing aid must separately verify that those additives do not change the regulatory position of the finished component. The natural-color grade is not automatically food-contact approved; separate positive-list evaluation under the applicable regional regulation is required for each final article and application.

    When wall thickness falls below 0.8 mm, mold temperature should be increased toward 80°C and injection speed moderated to avoid jetting. Cycle time may extend by 5–8 s compared with a 60°C mold, but the improvement in flow-front uniformity and dimensional repeatability is usually acceptable for precision electrical parts. Post-molding dimensional audits should be performed at 24 h and 48 h after ejection, because cold-crystallization and moisture uptake can produce measurable shifts beyond the immediate shrinkage recorded at the press. Tool-specific shrinkage calibration under ISO 294-4 is required; published nominal shrinkage values cannot account for gate location, fiber orientation, or variation in hold pressure.