Basf Ultradur Pbt Gf B4300g6

BASF Ultradur® PBT+GF B4300G6

    • Product Name: BASF Ultradur® PBT+GF B4300G6
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 468304
    Polymer Type PBT
    Reinforcement 30% glass fiber
    Ul94 Flame Rating HB
    Volume Resistivity Ohm Cm >1E15

    As an accredited BASF Ultradur® PBT+GF B4300G6 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags, typically 40 bags per 1,000 kg pallet, suitable for industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL loading of BASF Ultradur® PBT+GF B4300G6 in moisture-proof bags, palletized and secured for safe ocean transport.
    Shipping BASF Ultradur® PBT+GF B4300G6 is shipped as dry polymer pellets in sealed, moisture-barrier bags or octabins. It is generally non-hazardous for transport and requires no special dangerous-goods classification. Store in a cool, dry place, protected from moisture, heat, and direct sunlight.
    Storage Store in a dry, cool, well-ventilated warehouse, away from direct sunlight, heat sources, and moisture. Keep in original sealed packaging or tightly closed containers to prevent humidity uptake. Avoid prolonged high-temperature exposure and open flames. Maintain good housekeeping and keep away from oxidizing agents. Follow first-in/first-out stock rotation and all local regulations and the safety data sheet.
    Shelf Life Store dry in original sealed, moisture-proof packaging at 5–30°C; typical shelf life is 24 months from production date.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4300G6 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® B4300G6 is a 30% glass-fibre reinforced polybutylene terephthalate injection-moulding compound designated according to ISO 1043 as PBT-GF30. It is supplied as pellets in natural and pigmented forms. Published typical values from the BASF datasheet include a density of 1.53 g/cm³ under ISO 1183-1 and a melt volume-flow rate of 12 cm³/10 min under ISO 1133-1 at 250°C and 2.16 kg. Dry-as-moulded tensile testing under ISO 527-2 gives a tensile modulus of approximately 10,000 MPa, tensile stress at break of approximately 135 MPa, and nominal tensile strain at break of 2.5%. Heat deflection temperature under ISO 75-2/A is approximately 205°C; Vicat softening temperature under ISO 306/B50 is approximately 215°C. The material is therefore a rigid, low-elongation PBT grade whose short-term tensile failure is fibre-dominated and brittle in comparison with unfilled PBT. The 30% glass content also raises notch sensitivity and weld-line sensitivity, so impact performance depends on part radius, gate position, fibre orientation, and moulded-in stress.

    Before melt processing, the pellet charge is dried in a dehumidifying air dryer. The recommended drying condition is 80°C for 4 h once the original moisture-proof packaging has been opened. Residual moisture should be held below 0.04% by weight; long flow-path or thin-wall tools benefit from a lower residual moisture target near 0.02%. Pneumatic conveying air should be dried to a low dew point because the PBT backbone is hydrolytically sensitive. At ambient relative humidity above 60%, a hot-air oven is not a substitute for a dehumidifying dryer because surface moisture is not the controlling variable; the polymer must be dried from the pellet core.

    The principal datasheet values are summarised below. They are typical values for natural, dry-as-moulded specimens and are not specification minima.

    PropertyTest methodTypical value
    Glass-fibre contentISO 3451-130%
    DensityISO 1183-11.53 g/cm³
    Melt volume-flow rateISO 1133-112 cm³/10 min at 250°C/2.16 kg
    Tensile modulusISO 527-210,000 MPa
    Tensile stress at breakISO 527-2135 MPa
    Tensile strain at breakISO 527-22.5%
    Charpy notched impact strength, 23°CISO 179-1/1eA9 kJ/m²
    Charpy unnotched impact strength, 23°CISO 179-1/1eU55 kJ/m²
    Heat deflection temperature, HDT/AISO 75-2205°C
    Vicat softening temperature, VST/B50ISO 306215°C
    Flammability classificationUL 94HB at 1.6 mm

    What Melt and Mould Temperature Limits Control Moulded-In Stress and Warpage?

    A practical injection-moulding window for B4300G6 is a melt temperature of 250°C to 270°C and a mould surface temperature of 60°C to 100°C. At the lower mould-temperature boundary, the PBT matrix crystallises rapidly, but the glass fibres freeze in a highly oriented state before relaxation. The consequence is differential shrinkage: flow-direction shrinkage is constrained by oriented fibres while transverse shrinkage is higher. This mismatch is the main source of out-of-plane bow in flat, multi-gated parts. At the upper mould-temperature boundary, crystallisation is more complete and moulded-in stress falls, but cycle time rises and surface appearance can shift when the tool is not insulated uniformly. For hot-runner moulds, thermal uniformity across the manifold should be held within ±5°C to prevent flow-front imbalance and variable glass-fibre distribution.

    Processing equipment should use a conventional three-zone screw with an L/D ratio of at least 20:1 and a non-return valve. A compression ratio between 2.0:1 and 2.5:1 is adequate for glass-reinforced polyester. High screw speed or excessive back pressure generates shear heating; this is particularly relevant at the upper melt-temperature limit because the PBT backbone undergoes moisture-assisted chain scission. Holding the melt residence time below 10 min at 260°C is a common production control for this chemistry. Shot size should be between 30% and 70% of barrel capacity to avoid excessive hold-up or poor plastication. If the machine nozzle is equipped with a shut-off valve, the valve design must allow free passage of long glass fibres; needle shut-off systems can increase fibre breakage and reduce weld-line strength.

    Shrinkage data for this grade follow ISO 294-4 and are anisotropic. Typical parallel shrinkage is 0.2–0.5%; transverse shrinkage can be 0.7–1.0% depending on wall thickness, hold pressure, gate diameter, and mould temperature. The gate location should therefore be selected to place the dominant flow direction along the longest functional dimension of the part. A centre gate or sequential valve-gate programme is preferable to multiple edge gates for flat rectangular housings because it reduces the number of weld lines and aligns fibre orientation with the primary dimensional tolerance. Weld-line strength in B4300G6 is lower than for unfilled PBT and decreases further at low melt temperature and high injection speed. For applications requiring tensile load across a weld line, mould-flow simulation and destructive testing under the actual injection-speed profile are required; generic published values do not capture tool-specific fibre attrition.

    Gate and runner sizing must account for the brittle reinforcement. A gate thickness of 50–70% of the part wall thickness is frequently used for glass-filled PBT; tunnel gates or pinpoint gates can break fibres and are generally reserved for small parts where weld-line appearance is not critical. Full-round or trapezoidal cold runners with generous radii reduce pressure drop and fibre attrition. For hot-runner systems, externally heated manifolds with free-flow channels are preferred over internally heated torpedo systems because they expose the melt to lower local wall temperatures and allow more uniform fibre distribution. Pressure sensors at the runner drop can detect asymmetry before it becomes dimensional scrap.

    Injection speed should be selected for not only filling time but also orientation. Slow filling at low mould temperature produces a highly oriented skin and increases shrinkage anisotropy; fast filling can create jetting and weld-line weakening. A common process-development approach is to fill the cavity in a time between 0.8 s and 2.0 s for wall thicknesses of 2 mm to 3 mm, but this must be confirmed by short-shot studies and cavity pressure measurement. The actual values depend on gate area, part volume, and fibre length distribution after plastication. Published data for this specific configuration is limited.

    In multi-cavity production, part-to-part variation is governed less by pellet-to-pellet melt flow than by cavity-to-cavity thermal balance. For B4300G6, a temperature difference of 3°C across the mould face can change the crystallisation rate enough to alter post-mould shrinkage by several tenths of a percentage point. Conformal cooling or baffle-type water circuits are preferable to straight-line cooling channels in tools with deep cores. If tooling is not balanced, the resulting flow-front velocity differences may produce inconsistent fibre orientation and variable surface gloss. Cavity pressure transducers are recommended for high-volume parts where post-mould dimensional stability is critical; switch-over based on hydraulic pressure alone is often insufficient because glass-filled melts exhibit shear-thinning and yield-stress behaviour that differs from unfilled PBT.

    Post-mould moisture conditioning changes dimensions. As with other PBT compounds, B4300G6 absorbs moisture slowly; water uptake under ISO 62 at 23°C is low, but absorbed moisture acts as a plasticiser. Dimensional measurements should therefore be made after a defined conditioning period, not immediately after demoulding. If post-mould annealing is used to stabilise crystallinity, the part should be fixtured because annealing above the glass transition can relieve oriented-fibre stress and cause further anisotropic shrinkage. Annealing is typically performed below the HDT/A value, for example at 150°C to 180°C, but this is tool- and part-specific.

    Thermal Ageing, Hydrolysis, and Chemical Exposure Boundaries

    For B4300G6 specifically, published long-term ageing curves are limited; the following statements are class-level observations for PBT-GF30 polyesters unless a BASF test report is available. Under dry thermal ageing at 120°C, this class typically retains useful tensile strength for several thousand hours. The ester linkage, however, is susceptible to hydrolysis in hot aqueous media. Continuous hot-water or coolant immersion above 60°C is not recommended without fluid-specific testing. Alkaline solutions, strong acids, and oxidising cleaning agents attack the polyester matrix at elevated temperature. Methanol, ethanol, and ketone-based solvents may reduce service life or induce environmental stress crazing in moulded-in stress zones. Resistance to mineral oil and light splash contact is generally acceptable; aggressive biodiesel blends and aromatic solvents require validated immersion testing because dimensional change and surface degradation may occur.

    Chemical resistance screening is conducted by immersion or contact under ISO 175 or an OEM equivalent. A change in tensile strength of more than 25% after exposure is often used internally as an exclusion criterion, but pass-fail limits are application-specific. B4300G6 should not be exposed to boiling water or steam sterilisation because hydrolysis attack accelerates; this is a chemical limitation, not a thermal one. For repeated steam sterilisation, higher-hydrolysis-resistant materials such as PBT/ASA blends or polyphenylene sulphide are more appropriate.

    The 30% glass-fibre phase increases surface hardness and reduces wear against unfilled PBT but makes the compound abrasive. In moving-part applications, mating surfaces should be hardened or lubricated; the abrasiveness also shortens tool life, especially at gate lands and mould parting lines when unfilled or low-glass PBT would be marginal. Tool steel selection for high-volume B4300G6 production typically favours hardened or coated mould surfaces in high-shear areas. This effect is well established in production-scale injection moulding of glass-filled polyesters; specific mass-loss rates depend on gate pressure, fibre length distribution after plastication, and filler-to-wall contact frequency.

    The product’s position within the Ultradur portfolio is defined by glass-fibre loading. B4300G4 contains 20% glass fibre and typically exhibits a tensile modulus near 7,000 MPa; B4300G10 contains 50% glass fibre and typically exhibits a tensile modulus near 16,000 MPa. B4300G6 occupies the intermediate 30% loading, with its 10,000 MPa tensile modulus. Flowability moves inversely with fibre content: the 30% grade fills longer flow paths than B4300G10 but not as readily as B4300G4. Shrinkage magnitude decreases as glass content rises, but shrinkage anisotropy increases. In flat parts, the absolute shrinkage is not the only problem; the differential between flow and transverse directions is the primary warp driver. B4300G10 therefore may require more sequential valve-gating and more frequent tool maintenance than B4300G6, while B4300G4 may be preferred when thin walls or complex multi-level flow paths require lower viscosity and when stiffness demands are moderate.

    For unfilled Ultradur PBT grades, heat deflection temperature and tensile modulus are substantially lower. The glass reinforcement in B4300G6 raises the continuous load-bearing temperature and improves dimensional stability under screw torque and clamp load. This makes the grade relevant for electrical connectors, sensor housings, actuator frames, cooling-fan impellers, structural brackets, and pump components that require a balance of rigidity, heat resistance, and processability. In connector applications, the material provides creep resistance under spring contact pressure; the specific contact-pressure retention should be verified according to ISO 899-2 or the OEM test specification. In fan impeller applications, the high glass content increases tool abrasion and can shift mass balance; published data for this specific configuration is limited.

    In electrical applications, B4300G6 has volume resistivity and dielectric strength typical of glass-reinforced PBT. Comparative tracking index and arc tracking index values can be used for low-voltage connector spacing; however, the exact value depends on colorant and filler surface treatment. Design for insulator spacing should be based on the printed datasheet or BASF certificate, not on generic PBT-GF30 values. The grade is not recommended for direct exposure to high-voltage arc environments unless the specific arc tracking index is confirmed.

    B4300G6 is not a flame-retarded grade. Its flammability classification under UL 94 is HB at 1.6 mm thickness. For enclosures requiring V-2, V-1, or V-0 ratings, flame-retarded Ultradur grades or other polymer families must be selected instead. The base resin is customarily supplied against the REACH Regulation EC 1907/2006 and the RoHS Directive 2011/65/EU for general industrial articles; however, the exact colorant and additive package can affect food-contact, medical, or automotive compliance, and no universal declaration should be assumed. The ISO 1043 designation PBT-GF30 should appear on design drawings and material databases to prevent substitution with unfilled or flame-retarded PBT.

    Top